Comparación de la microestructura del acero para herramientas metalúrgico en polvo (PM) frente al acero para herramientas convencional.

Powder Metallurgy Tool Steel vs Conventionally Melted Tool Steel Two tool steel bars can carry the same grade name and still behave completely differently on the shop floor. The alloy chemistry is often close, sometimes identical, yet one bar came from a static ingot and the other came from atomized powder consolidated under pressure. That

Comparación de la microestructura del acero para herramientas metalúrgico en polvo (PM) frente al acero para herramientas convencional. Leer más "»