¿Por qué D2 es la opción estándar para los rodillos de trabajo de la laminadora en racimo Sendzimir?
Why AISI D2 Tool Steel Is the Standard Choice for Sendzimir Cluster Mill Work Rolls Cold rolling mills that use a Sendzimir configuration, commonly called 20-High or Z-Hi cluster mills, are built around one core design decision: the work rolls are made deliberately small in diameter. A smaller work roll lowers the rolling force needed