Tool Steel Selection for Gages & Precision Tools

Select tool steel by dimensional stability, abrasive wear resistance, polishing ability, galling risk, and long-term size control. For plug gages, ring gages, thread gages, snap gages, templates, measuring blocks, and micrometer anvils, the main choice is usually between stability, wear resistance, and precision surface finish.

Quick Selection Guide by Tool Steel Grade

Choose the grade according to whether the tool is used for fixed gages, thread gages, templates, measuring tools, long-run plug or ring gages, or precision knife-edge parts.

Precision Gages

Acero para herramientas O2 1.2842

Recommended for gages, squares, straight edges, templates, and micrometer anvils.

Reason: O2 can be hardened from relatively low temperatures, helping reduce thermal shock and improve dimensional stability.
Thread Gages

Acero para herramientas O1 1.2510 / SKS3

Recommended for thread gages, stamps, and general precision tools requiring good abrasion resistance.

Reason: O1 is a general-purpose oil-hardening steel with good dimensional accuracy and useful wear resistance for precision tooling.
Long-Run Plug Gages

Acero para herramientas D2 1.2379 / SKD11 / Cr12Mo1V1

Recommended for plug and ring gages used in high-volume or long-run production.

Reason: D2 contains hard chromium carbides, giving strong wear resistance and good non-deforming characteristics during heat treatment.
High Wear Gages

Acero para herramientas D3 1.2080 / SKD1 / Cr12

Recommended for plug and ring gages where high abrasive wear resistance is required.

Reason: D3 provides high carbide volume and strong resistance to abrasive wear for gaging surfaces exposed to repeated sliding contact.
Knife Edges & Arbors

Acero para herramientas L6 1.2714 / SKT4

Recommended for precision gages, knife edges, arbors, and tools requiring a balance of toughness and wear resistance.

Reason: L6 is selected where moderate hardenability, toughness, and wear resistance are needed in precision tool components.

Selection Summary

This table gives a faster comparison when the buyer already knows the precision tool type and main performance requirement.

Precision Tool ApplicationRequisito principalAobo Steel Grades
Gages, squares, straight edges, templates, and micrometer anvilsExtreme dimensional stability and low heat-treatment movementO2
Thread gages, stamps, and general precision toolsGood dimensional accuracy and abrasion resistanceO1
High-volume plug and ring gagesHigh wear resistance and non-deforming heat-treatment behaviorD2, D3
Precision gages, knife edges, and arborsBalance of toughness and wear resistanceL6
Sliding gaging surfacesWear resistance, polished finish, and galling controlO1, O2, D2, D3