What does HSS stand for?

HSS primarily stands for High-Speed Steel or High-Speed Tool Steel. It is a crucial category of alloy steels predominantly used for creating engineering cutting tools.

M2 TOOL STEEL

Definition and Primary Function

High-Speed Steels (HSS) are a class of alloy steels specifically designed for applications requiring materials that can maintain their hardness and cutting edge even at elevated temperatures generated during high-speed machining operations. They are extensively utilized to manufacture various engineering cutting tools.

Chemical Composition

The following table shows the composition of the high-speed steel we produce.

Steel TypeCSiMnKrV.WMoCo
M20.78-1.05%0.20-0.45%0.15-0.40%3.75-4.50%1.60-2.20%5.50-6.75%4.50-5.50%
M350.80–0.90%0.20–0.45%0.20–0.45%3.75–4.50%1.75–2.20%5.50–6.75%4.50–5.50%4.50–5.50%
M421.05 – 1.1%0.15 – 0.65%0.15 – 0.40%3.5 – 4.25%0.95 – 1.35%1.15 – 1.85%9.0 – 10.0%7.75 – 8.75%

Key Characteristics and Properties

  • High Hardness: HSS exhibits high hardness, which is important for resisting penetration and deformation during cutting.
  • Red Hardness (Heat Resistance): Refers to its ability to resist softening or annealing at temperatures of 400°F (205°C) and above. However, these abilities decline rapidly at temperatures above 540°C to 600°C.
  • Wear Resistance: HSS has good resistance to abrasive wear.
  • Toughness and Shock Resistance: HSS demonstrates excellent fracture toughness and resistance to shock loading, allowing tools to withstand impact forces without brittle fracture.
  • Machinability: HSS can be hot-rolled and forged into rough shapes, then machined before heat treatment and finish grinding. 
  • Cost-Effectiveness: HSS tools are relatively inexpensive compared to other tool materials, making them a common choice, especially for monolithic tools.

Classification and Grades

  • T-type Steels: These grades primarily use tungsten as the major alloying element. They tend to be less tough than M-types but are easier to heat-treat.
  • M-type Steels: These grades primarily use molybdenum. They are more commonly used for rotary tools, such as drills, end mills, and taps. M2 is a commonly used grade for drills and taps, while M42 exhibits the greatest hot strength.
  • International and National Standards: HSS grades are specified in various standards, such as BS 4659:1989 in the UK, which includes details on hot-work, cold-work, and plastic molding tool steels. The ISO Standard 4957 and the German system (prefix ‘S’ for Schnellstahl) also classify HSS by chemical composition and application. ISO designations, like HS2-9-1-8, denote the percentages of tungsten, molybdenum, vanadium, and cobalt.

Applications

HSS is a versatile material used in a wide array of tools:

  • Cutting Tools: Common applications include drills, reamers, taps, milling cutters, broaches, and gear hobs. It is also used for turning operations, especially in multi-spindle machines.
  • Specialized Machining: HSS tools are employed for machining challenging materials like titanium and aluminum alloys.
  • Industrial Tools: This includes saw blades (especially bi-metal steel strips for band saws), precision punching tools, and various punches and dies.
  • Dies: Used for presses and hammers, hot trimming, hot swaging, and hot extrusion tools and mandrels.
M2/M35/M42 Tool Steel Offer – Aobo Steel

Source High-Performance M2, M35 & M42 Steel With Confidence

Choosing the correct high-speed tool steel is critical for performance and cost-effectiveness. Don’t leave it to chance. Partner with an expert to get the exact material grade and quality your project demands.

Expert Material Consultation

Leverage my 15+ years of experience to select the optimal steel for your application, saving you time and preventing costly errors.

Guaranteed Quality & Certification

All materials are 100% UT tested and sourced from our network of 40+ trusted suppliers, backed by Aobo Steel’s 20 years in forging.

Evan, Tool Steel Specialist

Evan, your Tool Steel Specialist

“My goal is your success. Let’s find the perfect steel together.”

Aobo Steel | www.aobosteel.com