AISI 1025 Carbon Steel Properties and Applications
AISI 1025 carbon steel is a frequently specified plain carbon steel utilized across various industrial sectors. It is classified as low-carbon steel, though depending on the specific context, it is sometimes referenced within medium-carbon listings. Its characteristics make it a versatile material for numerous applications.

1. 1025 Carbon Steel Chemical Composition (ASTM Standards)
The chemical makeup of 1025 steel is governed by established industry standards, ensuring consistency. Key specifications include:
- Szabványok:ASTM A29/A29M, ASTM A108, ASTM A576-90b (2000)
- Szén (C): 0.22% – 0.28%
- Mangán (Mn): 0.30% – 0.60%
- Foszfor (P): 0,040% maximum
- Kén (S): 0,050% maximum
- UNS Designation: G10250
These composition ranges define the grade’s fundamental properties.
2. 1025 Szén Steel Mechanical Properties
The mechanical properties of 1025 steel, such as tensile strength and yield strength, are influenced by its condition (e.g., hot-rolled, cold-finished) and any subsequent heat treatment.
- Melegen hengerelt: Typical values for hot-rolled bars (e.g., 16mm diameter) show moderate strength levels suitable for many general-purpose applications. Specific strength figures can vary. [Original document source 11 provides figures like 125-175 ksi TS / 80 ksi YS, while other sources suggest lower values typical for low-carbon steel. It’s best to consult specific mill certifications for guaranteed minimums].
- General Characteristics: Compared to higher carbon or alloy steels, 1025 offers lower tensile strength but generally good ductility and toughness.
1025 steel possesses good machinability, a key advantage, particularly when supplied in a cold-finished (CF) condition. Its lower carbon content contributes to easier machining compared to harder steels.
3. 1025 Szén Steel Applications
- Shafting: Good machinability makes it a popular choice for industrial shafting.
- Structural Components: These are used in structural applications and are often supplied as hot-rolled products conforming to standards like EN 10025 or as sheet/strip under ASTM A1011/A1011M, where formability can be important.
4. Heat Treatment Guide for 1025 Steel
1025 steel is a versatile low-carbon steel. Its mechanical properties can be significantly altered through various heat treatment processes. Understanding these treatments is key to optimizing 1025 steel for specific industrial applications. This guide outlines the common heat treatments applicable to 1025 steel and their effects.
4.1 Lágyítás
Cél: Annealing is primarily used to soften 1025 steel, making it more ductile and easier to form. It also relieves internal stresses and refines the grain structure.
Folyamat:
- Heat the steel uniformly to a temperature within the annealing range, typically 880-930°C for low-carbon grades like 1025.
- Hold at this temperature long enough for complete austenitization (transforming the steel’s structure to austenite).
- Cool the steel slowly, usually within the furnace.
Eredmény: Slow cooling promotes the formation of a soft microstructure, mainly consisting of ferrite and pearlite. This enhances ductility and formability, preparing the steel for subsequent manufacturing steps.
4.2 Normalizálás
Cél: Normalizing refines the grain size and improves microstructural uniformity. It results in slightly higher strength and hardness than annealed 1025 steel while maintaining good ductility.
Folyamat:
- Heat the steel to the austenitizing temperature range (similar to annealing, around 880-930°C).
- Hold at temperature for uniform heating.
- Cool the steel in still air outside the furnace.
Eredmény: The faster cooling rate (compared to annealing) produces a finer, more uniform grain structure. Normalizing is often applied to as-rolled or forged steel to prepare it for machining or further heat treatment.
4.3 Edzés (kioltás)
Cél: To increase the hardness and strength of the steel. Note that due to its low carbon content, 1025 steel has limited hardenability compared to medium or high-carbon steels.
Folyamat:
- Heat the steel to its specific austenitizing temperature (around 770-800°C for low-carbon steel).
- Rapidly cool (quench) the steel in a suitable medium, such as water, brine, or oil.
Eredmény: Rapid cooling transforms the austenite phase into martensite, a hard microstructure. However, the martensite formed in 1025 steel is relatively low in hardness. Quenching introduces significant internal stresses and carries a risk of distortion. Achieving a fully martensitic structure can be challenging due to low hardenability; other microstructures like ferrite or pearlite might form even with aggressive quenching.
4.4 Edzés
Cél: Tempering is performed után hardening (quenching) to reduce the brittleness inherent in martensite and increase toughness.
Folyamat:
- Reheat the previously quenched steel to a specific temperature below the lower critical point (Ac1, approximately 727°C).
- Hold at the tempering temperature for a predetermined time.
- Cool the steel, typically in air.
Eredmény: Tempering modifies the martensitic structure, achieving a desired balance between hardness, strength, and toughness. The final properties depend directly on the chosen tempering temperature and duration – higher temperatures generally yield lower hardness and higher toughness.
4.5 Karburálás
Cél: Carburizing is a surface-hardening treatment. It creates a hard, wear-resistant outer layer (case) on the steel while maintaining a softer, tougher interior (core).
Folyamat:
- Heat the 1025 steel component in a carbon-rich atmosphere (gas, liquid, or solid pack) at temperatures typically between 880-930°C. Carbon diffuses into the steel’s surface.
- Control the process time and temperature to achieve the desired case depth and carbon concentration.
- Follow carburizing with quenching to harden the high-carbon case.
- Temper the component to refine the properties of the case and the core.
Eredmény: Ideal for components requiring high surface wear resistance combined with core ductility and toughness.
4.6 Carbonitriding
Cél: Like carburizing, carbonitriding is a surface-hardening process that introduces carbon and nitrogen into the steel’s surface layer.
Folyamat:
- Heat the steel in an atmosphere containing carbon and nitrogen sources, typically at slightly lower temperatures than carburizing (around 900°C).
- Both elements diffuse into the surface. The addition of nitrogen increases the hardenability of the case.
- Quench the component. Thanks to the increased hardenability, a less severe quench (e.g., oil) can often be used compared to carburizing.
- Temper as required.
Eredmény: Produces a hard, wear-resistant case. The enhanced hardenability allows for effective hardening with potentially less distortion, making it suitable for components requiring good dimensional control.
4.7 Stresszoldás
Cél: To reduce internal stresses locked into the steel from prior manufacturing processes like heavy machining, cold forming, or welding.
Folyamat:
- Heat the steel component uniformly to a temperature below the lower critical point (Ac1), typically around 600°C.
- Hold at temperature for a sufficient duration (e.g., 1 hour per inch of thickness, minimum).
- Cool slowly to minimize the reintroduction of thermal stresses.
Eredmény: Improves dimensional stability during subsequent machining or use, and reduces the risk of distortion or cracking caused by residual stress.
4.8 Selecting the Appropriate Treatment
The optimal heat treatment for 1025 steel depends entirely on the final requirements of the component:
- For maximum formability and softness: Válasszon Lágyítás.
- For a refined structure with balanced strength and ductility: Consider Normalizálás.
- For increased hardness (within limits) followed by improved toughness: Use Edzés és megeresztés.
- For high surface hardness and wear resistance with a tough core: Employ Karburálás vagy Carbonitriding.
- To minimize internal stresses from fabrication: Apply Stresszoldás.
Choosing the correct process ensures that the 1025 steel performs reliably in its intended application. If you require further assistance in selecting the best heat treatment for your specific needs, please consult with our technical team.
GYIK
1. What is the difference between 4130 and 1025 steel?
The fundamental difference lies in the alloying elements. 4130 acél is a chromium-molybdenum alloy steel with higher hardenability and the ability to achieve significantly greater strength and toughness through heat treatment compared to 1025 steel, which is a plain carbon steel with lower strength and hardenability, typically used in less demanding applications.
2. Does 1025 carbon steel rust?
Yes, 1025 carbon steel is susceptible to rusting when exposed to various environments. Rust, a form of corrosion specific to iron and its alloys like carbon steel, is an electrochemical process in which iron reacts with oxygen and water (or moisture in the air) to form hydrated iron oxide, commonly known as rust.
3. What is the difference between A36 and 1025 steel?
While A36 and 1025 are carbon steels, A36 is specifically engineered and certified for structural load-bearing applications with a guaranteed minimum yield strength. 1025 steel is a more general-purpose carbon steel with a slightly higher carbon content range and typically lower manganese content, leading to a different set of mechanical properties that may be suitable for a broader range of manufacturing processes and applications beyond primary structural support. The selection between these two grades in your factory should be guided by the specific engineering requirements of your components, including the stresses they will endure and the forming or fabrication processes involved.
Fedezze fel további termékeinket
D2/1.2379/SKD11
D3/1.2080/SKD1
D6/1.2436/SKD2
A2/1.23663/SKD12
O1/1.2510/SKS3
O2/1,2842
S1/1.2550
S7/1.2355
DC53
H13/1.2344/SKD61
H11/1.2343/SKD6
H21/1.2581/SKD7
L6/1.2714/SKT4
M2/1.3343/SKH51
M35/1.3243/SKH55
M42/1.3247/SKH59
P20/1.2311
P20+Ni/1,2738
420/1.2083/2Cr13
422 rozsdamentes acél
52100 csapágyacél
440C rozsdamentes acél
4140/42CrMo4/SCM440
4340/34CrNiMo6/1.6582
4130
5140/42Cr4/SCR440
SCM415
Ingyenes árajánlat és szakértői anyagtanácsadás kérése – 1025-ös szénacél
Megbízható 1025-ös szénacél beszállítót keres?
At Aobo acél, kínálunk:
✅ Versenyképes gyári árak
✅ Minden megrendeléshez gyári teszt tanúsítvány (MTC) jár
✅ Gyors szállítás – Globális szállítás elérhető
✅ Ingyenes technikai támogatás – Szerezze be a megfelelő acélt a projektjéhez