2025. május 12.

o1 szerszámacél

O1 Tool Steel: Understanding Its Rockwell Hardness for Your Applications

Understanding O1 tool steel‘s hardness is critical for performance and tool life in factory applications. At Aobo Steel, this is a common question we address. To be direct, properly heat-treated O1 tool steel typically shows a Rockwell C hardness (HRC) from the low 50s to the mid-60s. In its as-quenched state—immediately after hardening and before

O1 Tool Steel: Understanding Its Rockwell Hardness for Your Applications Read More »