AISI D2 Tool Steel (1.2379 / SKD11) Supplier in China

Bulk Supply for Global Distributors | 1,200 Tons Monthly Capacity | 20GP Container Optimized

  • 100% UT Tested (SEP 1921-82 D/d)
  • Annealed Delivery · Black / Turned / Polished
  • MTC (EN 10204 3.1) with Heat Number
  • Round bar and flat bar in stock in selected sizes

Check stock & price

Send the sizes, quantity and destination port and we confirm stock and price within one working day.

    Or contact us directly

    Scan to chat

    D2 tool steel (DIN 1.2379 / JIS SKD11) is one of the most widely used cold-work tool steels for wear-resistant tooling. How the grade differs from its Japanese equivalent in composition, working hardness and service behaviour is set out in the D2 vs SKD11 comparison. D2 round bar and flat bar are held in stock in Huangshi in selected sizes, drawn from our 1,000 t tool steel stock, and every size that is not on the stock list is rolled or forged to order.

    D2 Tool Steel Supply Overview

    GradeAISI D2 / DIN 1.2379 / JIS SKD11
    SteelmakingEAF + LF + VD, ESR on request (about 60 days)
    Delivery ConditionFully Annealed (Soft Condition for Machining)
    Available FormsRound Bar / Flat Bar / Plate / Forged Block
    Plate also milled square or ground flat to finished size as precision ground tool steel plate
    StockRound bar, flat bar and plate in stock in Huangshi, drawn from the 1,000 t of tool steel we hold; sizes outside the stock list are produced to order
    Size RangeFlat bar 6–400 mm thick, up to 810 mm wide · Round bar Φ12–Φ600 mm · full size table
    Monthly Production CapacityApprox. 1,200 metric tons
    Recommended Export QuantityFull 20GP container (~26 tons)
    MOQNo minimum for stock items
    Lead TimeIn stock, ships immediately. Sizes not in stock are produced to order in 30 days.
    InspectionIn-house UT team + Third-party inspection available
    DocumentationMTC (EN 10204 3.1) + UT Report
    Blue-painted D2 tool steel plates stacked in stock at Aobo Steel, Huangshi

    Get the current stock list

    Tell us the sizes and quantity you are after.

      Or contact us directly

      Scan to chat

      D2 Round Bar and Plate in Stock1.2379 / SKD11

      Send the sizes you need and we send back the current stock list, with the heat numbers and the price, within one working day. There is no minimum order and stock items ship immediately. Sizes we do not hold are produced to order in 30 days.

      Why Global Distributors Source D2 from Aobo Steel

      • Continuous monthly supply of around 1,200 tons
      • No minimum order for stock items and any tonnage can ship
      • Container-optimized bar and plate lengths
      • Mixed sizes are supported for export loading
      • Annealed delivery for downstream machining
      • Stable sourcing through integrated supply chain partners
      • UT inspection available to SEP 1921-82 D/d or E/e
      • MTC and batch traceability with each shipment
      • Heat number tracking for order control
      • Black, turned, and polished surface options
      • Bulk export packing for sea shipment
      • Clear conversion path to the dedicated bulk supply page

      Stable Production for Long-Term Bulk Supply

      • Continuous monthly output of around 1,200 tons
      • Continuous production cycles for inventory replenishment
      • ESR (Electro-Slag Remelting) is available upon request
      • Stable alloy sourcing to reduce supply interruption risk
      • Full batch traceability linked to the original heat number

      Available D2 Tool Steel Forms and Size Range

      ShapeThickness / Diameter (mm)Width (mm)Length
      Flats (forged, black surface)35–400200–8102–5 m
      Flats (forged, machined surface)30–400200–8102–5 m
      Flats (hot rolled, black surface)6–60210–6103–5 m
      Rounds (forged, black and turned)Φ60–Φ600—2–5 m
      Rounds (rolled, black and turned)Φ12–Φ60—3–5.8 m

      Flat bar 6–400 mm thick and up to 810 mm wide, round bar Φ12–Φ600 mm. Sizes that are not on the stock list are produced to order in 30 days.

      Quality Control for Bulk Orders

      Every batch of tool steel supplied by Aobo Steel is verified before shipment to ensure grade accuracy, internal soundness, and traceability for bulk orders. How buyers specify D2 before ordering is set out step by step in the D2 selection and bulk supply guide.

      • Chemical composition verified by a spectrometer
      • Ultrasonic testing available (SEP 1921-82)
      • Delivered in spheroidized annealed condition
      • Mill Test Certificate (EN 10204 3.1) with heat number
      • Dimensional and surface inspection before shipment
      Metallographic inspection of tool steel during quality control before bulk shipment

      Export Packaging and Container Loading

      • Professional seaworthy export packing
      • 20GP loading optimized up to ~26 tons
      • Mixed grades and mixed sizes supported
      • Anti-rust protection for long sea transit

      For international shipments, full-container loading is strongly recommended to ensure cost efficiency and smoother customs processing.

      AISI D2 / DIN 1.2379 / JIS SKD11 Gallery

      1.2379
      SKD11

      Typical Industrial Applications of D2 Tool Steel

      D2 Tool Steel and the Equivalent Grades’ Composition

      CCrMoVMnSiPS
      1.40 – 1.60%11.00 – 13.00%0.70 – 1.20%0.50 – 1.10%0.10 – 0.60%0.10 – 0.60%≤ 0.030%≤ 0.030%

      The equivalent grades’ composition

       CSiMn CrMo VPS
      Germany/W-Nr. 1.23791.45 – 1.60%0.10 – 0.60%0.20 – 0.60%11.00 – 13.00%0.70 – 1.00%0.70 – 1.00%≤0.030%≤0.030%
      Japan/JIS SKD111.40 – 1.60%≤0.40%≤0.60%11.00 – 13.00%0.80 – 1.20%0.20 – 0.50%≤0.030%≤0.030%
      China/GB Cr12Mo1V11.40 – 1.60%≤0.60%≤0.60%11.00 – 13.00%0.70 – 1.20%0.50 – 1.10%≤0.030%≤0.030%

      We guarantee that all materials are manufactured in strict compliance with the specified chemical compositions for D2, 1.2379, and SKD11. The EN number has its own material page, with the ISO 4957 and ASTM A681 rows for 1.2379 tool steel set side by side. Buyers working to the Japanese designation can order from the SKD11 tool steel page, which lists forms, annealed delivery and certificates.

      D2 Steel Heat Treatment Overview

      D2 is an air-hardening tool steel. Controlled heat treatment is critical to achieve optimal wear resistance and dimensional stability.

      • Preheat: 650°C
      • Austenitizing: 1010–1024°C
      • Quenching: Air quench
      • Recommended Tempering: Double temper

      D2 Steel Properties

      Modulus of Elasticity0.2% Offset Yield StrengthYield StrengthUTS(Tensile Strength)
      203 GPa411 MPa350 MPa758 MPa
      Modulus of ToughnessFracture StrengthElongation at BreakGauge LengthFracture StrainArea Reduction
      81 MPa723 MPa0.61 mm30 mm1.97%1.30%