Tool Steel Hardness Conversion Calculator | HRC HRB HV HBW HBS
Aobo Steel Technical Tool

Tool Steel Hardness Conversion Calculator

Enter any hardness value and the calculator returns the nearest equivalents across the Rockwell C, Rockwell B, Vickers, and Brinell scales. It is built for the readings that do not have a ready answer, such as turning a single Vickers number from a test report into HRC, or checking a Brinell supply limit against a drawing called out in Rockwell. The conversion data follow ASTM E140 for non-austenitic steels. As a quick reference point, 60 HRC is close to 697 HV and about 654 HBW.

Hardened Tool Steel / HRC Range

Use this range for hardened and tempered tool steels, including D2, A2, O1, S7, H11, H13, M2, M35, and M42. Valid input ranges: HRC 20-68, HV 238-940, HBW 226-739, HBS 226-500.

Enter one value above. The calculator uses the last edited field as the input source.

Annealed or Soft Steel / HRB Range

Use this range for annealed, normalized, or softer steel where HRC is not suitable. This range is useful when reviewing MTC hardness values or soft supply hardness. Valid input ranges: HRB 55-100, HV 100-240, HBS 100-240.

Enter one value above. The calculator uses the last edited field as the input source.
The values are approximate equivalents, not exact conversions. Use them for comparison and communication. For inspection, acceptance, or MTC confirmation, test hardness by the method specified in the order or standard.

HRC Hardness Conversion Table — Hardened Tool Steel

Full conversion chart for Rockwell C (HRC) to Vickers (HV), Brinell steel ball (HBS), and Brinell tungsten carbide ball (HBW) for hardened and tempered tool steel. Data based on ASTM E140 for non-austenitic steels.

HRCHVHBSHBW
68940——
67900——
66865——
65832—739
64800—722
63772—705
62746—688
61720—670
60697—654
59674—634
58653—615
57633—595
56613—577
55595—560
54577—543
53560—525
52544500512
51528487496
50513475481
49498464469
48484451455
47471442443
46458432432
45446421421
44434409409
43423400400
42412390390
41402381381
40392371371
39382362362
38372353353
37363344344
36354336336
35345327327
34336319319
33327311311
32318301301
31310294294
30302286286
29294279279
28286271271
27279264264
26272258258
25266253253
24260247247
23254243243
22248237237
21243231231
20238226226

HRB Hardness Conversion Table — Annealed or Soft Steel

Full conversion chart for Rockwell B (HRB) to Vickers (HV) and Brinell (HBS) for annealed, normalized, or soft steel. Data based on ASTM E140 for non-austenitic steels.

HRBHVHBS
100240240
99234234
98228228
97222222
96216216
95210210
94205205
93200200
92195195
91190190
90185185
89180180
88176176
87172172
86169169
85165165
84162162
83159159
82156156
81153153
80150150
79147147
78144144
77141141
76139139
75137137
74135135
73132132
72130130
71127127
70125125
69123123
68121121
67119119
66117117
65116116
64114114
63112112
62110110
61108108
60107107
59106106
58104104
57103103
56101101
55100100

Hardness Conversions This Calculator Covers

The calculator works in both directions across five scales: Rockwell C (HRC), Rockwell B (HRB), Vickers (HV), and Brinell measured with either a tungsten carbide ball (HBW) or a steel ball (HBS). You enter the value you already have, and it returns the nearest listed equivalent on each of the other scales, so you do not need to read across a printed chart by eye.

The conversions people run here most often are the ones a single chart row cannot answer on its own. Converting Brinell to Rockwell C matters when an annealed supply limit is given in HBW but the drawing specifies HRC. Converting Vickers to Rockwell C is common when a surface or microhardness reading is reported in HV and you need the equivalent working HRC. HBW to HRC and HRB to HRC come up when a mill certificate lists one scale while your own specification uses another. Each of these is a single entry in the calculator above rather than a manual lookup.

Because soft and hardened steel are measured by different methods, the tool keeps two separate ranges. The HRC range covers hardened and tempered tool steel, and the HRB range covers annealed or normalized steel. This split prevents a low soft reading from being matched into the hardened range by mistake. As a worked example in the soft range, 95 HRB is close to 210 HV.

Which Range Should You Use?

Use the HRC range when the steel has been hardened and tempered. Use the HRB range when the steel is still soft, annealed, or normalized. This separation prevents low HB or HV values from being incorrectly matched to a hardened steel range.

HRC for hardened tool steel HRC is the common working hardness scale for hardened tool steel, such as D2 at 58-60 HRC, H13 at 44-52 HRC, or high-speed steel above 60 HRC.
HB and HRB for soft supply Annealed tool steel is usually checked by Brinell hardness. Many supply specifications and MTCs use values such as maximum 229 HB or maximum 255 HB.
HV for technical comparison HV is common in technical references, inspection reports, surface hardness checks, and heat-treatment data. It is useful for comparison, but it does not replace the required test method.

Data Source and Use Limit

The calculation data are simplified from ASTM E140 hardness conversion tables for non-austenitic steels. The HRC range is based on the Rockwell C hardness range table, and the HRB range is based on the Rockwell B hardness range table. For this tool steel calculator, only the practical front-end scales are retained: HRC, HRB, HV, HBS, and HBW.

Why the values are approximate

Rockwell, Brinell, and Vickers tests use different indenters, loads, indentation shapes, and measurement principles. A value such as 60 HRC can be compared with about 697 HV, but it is not a mathematical unit conversion like millimeters to inches.

Tool steel grade, carbide distribution, heat treatment condition, surface preparation, sample thickness, and testing equipment can all affect the reading. Use the converted value for quick comparison, not for final acceptance.

Need Tool Steel Supplied in Annealed Condition?

Aobo Steel supports bulk orders of tool steel round bar and plate, with MTC per order and practical grade selection support for distributors, stockists, and industrial buyers. Size range, tolerances, minimum order and lead times are set out on our tool steel supply capability page.

Data source: ASTM E140 hardness conversion tables for non-austenitic steels. Data compiled from public references and industry standards.