DC53 tool steel plates stacked at the mill, each plate marked DC53 LF VD at 610 mm width

Aobo Steel | Global Tool Steel Supplier in China

DC53 Tool Steel Supplier for Bulk Orders

High-Toughness Cold Work Die Steel | Annealed Delivery | For Global Distributors

  • 100% UT Tested – SEP 1921-82 Class D/d Guaranteed
  • Annealed State Delivery · MTC (EN 10204 3.1)
  • Surface: Black Scale / Turned / Mill Finish / Polished
  • Ready stock in Huangshi — 1,000 t of tool steel

Check stock & price

Send the sizes, quantity and destination port and we confirm stock and price within one working day.

    Or contact us directly

    Scan to chat

    DC53 steel is a high-chromium steel and a general-purpose high-toughness cold-work die steel. After quenching and tempering at 520-530°C, its hardness can reach 62-63 HRC, exceeding that of SKD11 steel. Although its hardness is 2-3 HRC higher, its wear resistance and impact toughness are significantly improved, making it an excellent steel grade for replacing D2. DC53 round bar and plate are held in stock in Huangshi, drawn from our 1,000 t tool steel stock; sizes outside the range below are produced to order.

    DC53 Tool Steel Supply Overview

    GradeJIS DC53
    Delivery ConditionFully Annealed (Soft Condition for Machining)
    Available FormsRound Bar / Flat Bar / Plate / Forged Block
    Plate also milled square or ground flat to finished size — precision ground tool steel plate
    Stock1,000 t of tool steel in stock in Huangshi — DC53 is supplied from it within the size range below
    Size RangeFlat bar 8–810 mm · Round bar Φ12–Φ500 mm — full size table
    Monthly Production CapacityApprox. 1,200 metric tons
    Recommended Export QuantityFull 20GP container (~26 tons)
    MOQ5 tons
    Lead Time (With Ingot Stock)Approx. 20 days
    Lead Time (Fresh Melt)30–45 days
    Lead Time (ESR Grade)Approx. 60 days
    InspectionIn-house UT team + Third-party inspection available
    DocumentationMTC (EN 10204 3.1) + UT Report

    Why Global Distributors Source DC53 from Aobo Steel

    • Continuous monthly supply of around 1,200 tons
    • MOQ from 5 tons for wholesale orders
    • Container-optimized bar and plate lengths
    • Mixed sizes are supported for export loading
    • Annealed delivery for downstream machining
    • Stable sourcing through integrated supply chain partners
    • UT inspection available to SEP 1921-82 D/d or E/e
    • MTC and batch traceability with each shipment
    • Heat number tracking for order control
    • Black, turned, and polished surface options
    • Bulk export packing for sea shipment
    • Clear conversion path to the dedicated bulk supply page

    Stable Production for Long-Term Bulk Supply

    • Continuous monthly output of around 1,200 tons
    • Continuous production cycles for inventory replenishment
    • ESR (Electro-Slag Remelting) is available upon request
    • Stable alloy sourcing to reduce supply interruption risk
    • Full batch traceability linked to the original heat number

    Available DC53 Tool Steel Forms and Size Range

    ShapeThickness / Diameter (mm)Width (mm)Length
    Flats (forged, black surface)35–400200–8102–5 m
    Flats (forged, machined surface)30–400200–8102–5 m
    Flats (hot rolled, black surface)8–60210–6103–5 m
    Rounds (forged, black and turned)Φ60–Φ500—2–5 m
    Rounds (rolled, black and turned)Φ12–Φ60—3–5.8 m

    Supply range for forged and rolled tool steel — not a stock list. Stock is held on part of this range; anything outside it is produced to order: about 25 days with ingot in stock, 30–45 days for a fresh melt, 60 days for ESR.

    Quality Control for Bulk Orders

    Every batch of tool steel supplied by Aobo Steel is verified before shipment to ensure grade accuracy, internal soundness, and traceability for bulk orders.

    • Chemical composition verified by a spectrometer
    • Ultrasonic testing available (SEP 1921-82)
    • Delivered in spheroidized annealed condition
    • Mill Test Certificate (EN 10204 3.1) with heat number
    • Dimensional and surface inspection before shipment
    Metallographic inspection of tool steel during quality control before bulk shipment

    Export Packaging and Container Loading

    • Professional seaworthy export packing
    • 20GP loading optimized up to ~26 tons
    • Mixed grades and mixed sizes supported
    • Anti-rust protection for long sea transit

    For international shipments, full-container loading is strongly recommended to ensure cost efficiency and smoother customs processing.

    Application

    Blanking dies, cold-forming dies, cold-drawing dies, forming roll punches, and cold-extrusion dies are essential for shaping and cutting materials in cold-working processes.

    Precision blanking and various types of stamping dies for wire-cutting processing are ideal for intricate, accurate cutting tasks.

    Plastic deformation dies for difficult-to-machine materials: This includes cold-forging, deep-drawing, and thread-rolling dies, as well as high-speed blanking punches and stainless-steel sheet punches, suited for challenging material processing.

    Cold-stamping dies requiring high wear resistance, hardness, and toughness are ideal for demanding stamping operations that require durability and strength.

    Dies with higher performance requirements than D2 steel and molds needing exceptional toughness: DC53 offers superior performance and excellent cost-effectiveness in these scenarios.

    Large molds and precision molds: Suitable for applications where size and precision are critical.

    Composition

    ElementCarbon (C)Silicon (Si)Manganese (Mn)Chromium (Cr)Molybdenum (Mo)Vanadium (V)
    Percentage (%)0.90 – 1.1010.4820.3

    Heat treatment

    Hardening process

    The first step is quenching. The process involves heating the material to 940-960°C, then rapidly cooling, typically with air or oil.

    Tempering

    After quenching, a tempering treatment is applied. There are two types of tempering for DC53 steel:

    • Low-temperature tempering (180-220°C): This method is suitable for molds requiring very high hardness. The hardness after tempering can reach 60-62 HRC, which is particularly wear-resistant.
    • High-temperature tempering (520-530°C): This method maintains high hardness (62-63 HRC) while increasing ductility, which is ideal for molds that need to be strong and durable.

    Heat treatment precautions

    1. It should be in a step-warming manner to avoid heating too fast and causing the material to open up.
    2. After tempering the material, the air cools to room temperature.
    3. If the material is used to make precision molds, it is recommended that it be tempered at 520-530°C for optimal results.
    >