Tool Steel Equivalent Grade Finder
Cross-reference of tool steel grades across the main national standards — US AISI/ASTM, German DIN and Werkstoff numbers, Japanese JIS, Chinese GB, British BS and French AFNOR — plus trade names and standard specifications for each grade. A dash means no equivalent is listed in the current reference data.
Tool Steel Equivalent Grade Comparison Chart
| Grade (AISI / ASTM) | UNS | Germany (DIN / W.-Nr.) | Japan (JIS) | China (GB) | UK (BS) | France (AFNOR) |
|---|---|---|---|---|---|---|
| Cold Work Tool Steels | ||||||
| D2 | T30402 | 1.2379; X155CrMoV12-1 | SKD11 | Cr12Mo1V1 | BD2 | X160CrMoV12 |
| D3 | T30403 | 1.2080; X210Cr12 | SKD1 | Cr12 | BD3 | Z200C12 |
| D6 | T30406 | 1.2436; X210CrW12 | SKD2 | Cr12W | – | – |
| A2 | T30102 | 1.2363 | SKD12 | – | BA2 | Z100CDV5 |
| O1 | T31501 | 1.2510 | SKS3 | 9CrWMn | BO1 | 90MWCV5 |
| O2 | T31502 | 1.2842; 90MnCrV8 | – | – | BO2 | 90MV8 |
| S1 | T41901 | 1.2550; 45WCrV7 | SKS41; SKS4 | 5CrW2Si | BS1 | 55WC20 |
| S7 | T41907 | – | – | – | – | – |
| 52100 | G52986 | 1.3505; 100Cr6 | SUJ2 | GCr15 | En31; 534A99; 535A99 | 100C6 |
| Hot Work Tool Steels | ||||||
| H10 | T20810 | 1.2365; X32CrMoV3-3; 32CrMoV12-28 | – | 4Cr3Mo3SiV; 4Cr3Mo-3SiV | BH10 | 32CrMoV12-28 |
| H11 | T20811 | 1.2343; X38CrMoV5-1 | SKD6 | 4Cr5MoSiV | BH11 | Z38CDV5; X38CrMoV5 |
| H13 | T20813 | 1.2344; X40CrMoV5-1 | SKD61 | 4Cr5MoSiV1 | BH13 | Z40CDV5 |
| H21 | T20821 | 1.2581 | SKD5 | 3Cr2W8V | BH21 | Z30WCV9 |
| L6 | T61206 | 1.2714 | SKT4; SKS51 | – | – | 55NCDV7 |
| High Speed Steels | ||||||
| M2 | T11302 | 1.3343 | SKH51; SKH9 | W6Mo5Cr4V2 | BM2 | Z85WDCV06-05-04-02 |
| M35 | T11335 | 1.3243 | SKH55 | W6Mo5Cr4V2Co5 | BM35 | Z85WDKCV06-05-05-04-02; Z90WDKC06-05-05-04 |
| M42 | T11342 | 1.3247 | SKH59 | W2Mo9Cr4VCo8; T72948 | BM42 | Z110DKCWV09-08-04-02-01 |
| Plastic Mold Steels | ||||||
| P20 | T51620 | 1.2311; 40CrMnMo7 | – | 3Cr2Mo; SM3Cr2Mo | BP20 | 40CMD8 |
| P20+Ni | – | 1.2738 | – | 3Cr2NiMo; SM3CrNiMo | – | – |
| P20+S | – | 1.2312 | – | – | – | – |
Substitution reminder
Equivalent grade names are reference information. For real orders, confirm chemical composition, delivery condition, inspection standard, size, surface condition, and application before substitution. Where two equivalent names still behave differently in service, the difference is covered in the grade comparison pages, for example D2 vs SKD11.
From equivalent grade to delivered steel
Send the grade (AISI, DIN, JIS or GB), size and quantity — we reply with the mill grade and condition we supply, price, certificate and lead time within one working day.
Prefer email? [email protected] · WhatsApp +86 180 6294 5370