440C Stainless Steel Properties
440C is a high-carbon, high-chromium martensitic stainless steel built for maximum hardness and wear resistance among corrosion-resistant steels. After proper heat treatment, it can reach up to 60 HRC and is typically used at 57 to 60 HRC, providing strong resistance to abrasion, edge wear, and surface deformation under contact loading.
Its high carbon content also means low ductility and limited impact toughness. This makes 440C a material for wear-dominated parts under stable loading, not for shock-loaded or structural service. Everything on this page follows from that single trade-off, so it helps to read the properties as a balance rather than as a list of strengths.
440C Stainless Steel Chemical Composition
The composition of 440C (UNS S44004) balances hardenability, carbide formation, and usable corrosion resistance.
Typical composition (wt%):
| Element | Content (%) |
|---|---|
| Carbon (C) | 0.95 to 1.20 |
| Chromium (Cr) | 16.00 to 18.00 |
| Molybdenum (Mo) | 0.75 max |
| Manganese (Mn) | 1.00 max |
| Silicon (Si) | 1.00 max |
| Phosphorus (P) | 0.040 max |
| Sulfur (S) | 0.030 max |
High carbon and chromium levels produce a martensitic matrix with a large volume of chromium-rich carbides. That structure drives hardness, wear resistance, and compressive strength, and it also reduces toughness. Reading the rest of these properties through the carbide structure is the fastest way to understand 440C.
440A vs 440B vs 440C: How Carbon Changes the Grade
The 440 family shares a chromium base and is separated mainly by carbon content. Carbon controls how hard the grade can become and how much toughness it sacrifices.
| Grade | Carbon (%) | Max Hardness | Wear Resistance | Relative Toughness |
|---|---|---|---|---|
| 440A | 0.60 to 0.75 | 56 HRC | Medium | Higher |
| 440B | 0.75 to 0.95 | 58 HRC | Medium to high | Medium |
| 440C | 0.95 to 1.20 | 60 HRC | High | Lower |
More carbon forms chromium-rich carbides, which raise hardness and wear resistance but reduce ductility and impact strength. Choose 440A when corrosion resistance and toughness matter more than edge life. Choose 440C when hardness and wear resistance are the priority and the part can be designed around limited toughness. 440B sits between the two.
440C Stainless Steel Equivalent Grades
| Standard System | Designation |
|---|---|
| AISI / SAE | 440C / 51440C |
| UNS | S44004 |
| EN / DIN | 1.4125 |
| EN Name | X105CrMo17 |
| ASTM | A276 (Bars and Shapes) |
| Powder Metallurgy | MIM 440C |
EN grade 1.4125 (X105CrMo17) is the closest European equivalent to AISI 440C, with a carbon range of roughly 0.95 to 1.20% and a chromium range of 16 to 18%.
440C Stainless Steel Mechanical Properties
The mechanical behavior of 440C changes sharply between the annealed and hardened conditions. In practice, it is supplied annealed for machining, then heat-treated to reach its final performance. Physical property data across the stainless grades is collected in the stainless steel physical properties chart.
| Property | Annealed Condition | Hardened and Tempered Condition |
|---|---|---|
| Hardness | About 230 HB (270 HB max) | 57 to 60 HRC |
| Tensile Strength | About 758 MPa | About 1970 MPa |
| Yield Strength | About 430 to 450 MPa | About 1896 to 1900 MPa |
| Elongation | 13 to 14% | About 2% |
| Reduction of Area | About 25% | About 10% |
| Toughness (Charpy V-notch) | Not typically reported | 3 to 5 ft·lbf |
| Machinability | About 40% (vs AISI 1212) | Very poor |
The modulus of elasticity is about 200 GPa, similar to most steels, so it isn’t a selection factor. After heat treatment, the steel gains very high strength and hardness, while ductility and impact resistance fall away. The 2% elongation and low Charpy values are the numbers to keep in mind: 440C carries load well but does not redistribute it, so failure under overload or impact is sudden rather than gradual.
440C Stainless Steel Heat Treatment Overview
440C performance depends heavily on heat treatment. Controlled hardening and tempering achieve its hardness, wear resistance, and dimensional stability.
| Process | Temperature Range | Key Purpose |
|---|---|---|
| Annealing | 845 to 900°C | Soften structure for machining |
| Preheating | About 790°C (multi-step for large parts) | Reduce thermal stress and distortion |
| Austenitizing | 1010 to 1065°C (up to 1095°C) | Dissolve carbides and enable hardening |
| Quenching | Air or oil | Form martensite and reach hardness |
| Subzero Treatment | About -75°C or lower | Reduce retained austenite |
| Tempering | About 150 to 370°C (typical 315°C) | Adjust hardness and relieve stress |
Tempering temperature is the main control variable for the final result. For a full breakdown of as-quenched versus tempered values and why reported numbers vary, see the 440C hardened hardness page.
How 440C Properties Translate to Performance
The headline properties only matter in context. In real service, 440C behavior depends on the trade-off among hardness, wear resistance, corrosion resistance, and toughness. You can’t read any of these in isolation, because the same carbide structure that raises one usually lowers another.
Wear Resistance
440C delivers high wear resistance through a hard martensitic matrix combined with a high volume of chromium-rich carbides. At 57-60 HRC, it withstands both adhesive and abrasive wear. The hard matrix limits surface deformation, adhesion, scuffing, and galling, while the carbides resist cutting and plowing during sliding or rolling contact. This is why 440C keeps a stable surface and edge longer than most stainless steels.
The same carbides set the limit. When they are coarse or unevenly distributed, they create local stress points that can start microcracks under cyclic or rolling contact. In that situation, the failure mode shifts from steady wear to surface fatigue. Sub-zero treatment improves dimensional stability by reducing retained austenite, but it does not change this mechanism. 440C is reliable under stable loading but becomes less predictable when contact fatigue drives failure.
Corrosion Resistance
440C offers moderate corrosion resistance and suits mild service, such as atmospheric exposure, lubricated systems, and light industrial conditions. The limit again comes from the carbides. Part of the chromium is locked into carbides and cannot support the passive oxide layer, so the protective film is weaker than in austenitic grades.
Heat treatment shifts this further. High austenitizing temperatures dissolve more alloy and improve corrosion resistance, while tempering can reduce it by altering local composition. Tuning for mechanical performance can therefore come at the expense of corrosion stability. Do not use 440C in chloride-rich environments, aggressive chemical media, or high-temperature corrosion.
Toughness and Mechanical Behavior
In the hardened condition, 440C is strong but very low in ductility, with an elongation of about 2%. Under load, it cannot redistribute stress, so once a local point exceeds its limit, the part fails with little warning. Typical failure modes include edge chipping, crack initiation at stress concentrators, and sudden brittle fracture under impact or bending. Low ductility and carbides acting as crack starters drive these failures.
The practical conclusion is consistent across all three properties. 440C performs well under stable, well-distributed loading, but becomes unreliable when impact, shock, or stress concentration governs the outcome.
440C vs Other Stainless and Tool Steels
Choosing 440C is easier when you see how it balances hardness, wear resistance, corrosion resistance, and toughness against the steels it usually competes with.
| Property | 440C | 420 | 440A / 440B | D2 | 316 |
|---|---|---|---|---|---|
| Steel Type | Martensitic Stainless | Martensitic Stainless | Martensitic Stainless | Tool Steel | Austenitic Stainless |
| Max Hardness | About 60 HRC | 46 to 54 HRC | 56 to 58 HRC | 60 to 62 HRC | Not hardenable |
| Wear Resistance | High | Medium | Medium | Very High | Low |
| Corrosion Resistance | Medium | Medium | Medium to high | Low | Excellent |
| Toughness | Low | Medium | Medium | Very Low | High |
| Machinability | Poor | Moderate | Moderate | Poor | Good |
440C balances wear resistance against corrosion resistance. Against 420 or 440A, it offers higher hardness and longer wear life. Compared with D2, it trades some wear resistance for better corrosion resistance. Compared with 316, it offers much higher strength and hardness but much lower corrosion resistance.
When to Use 440C Stainless Steel
440C suits applications that require high hardness and wear resistance, moderate corrosion resistance, and stable loading.
It is common in precision cutting tools such as knives, surgical instruments, and fine blades, where edge retention is critical. It performs well in rolling-contact parts such as bearing balls and races, especially where corrosion resistance exceeds that of standard bearing steels. In fluid systems, it is used for valve seats, needle valves, and pump parts running in fresh water or mild industrial media. It also serves as a plastic mold insert for abrasive or mildly corrosive polymers, where surface hardness and dimensional stability matter. For a full breakdown by component type, see the 440C applications page.
When NOT to Use 440C Stainless Steel
Choose 440C only when toughness, strong corrosion resistance, or easy manufacturing are the main requirements.
Its low toughness makes it perform poorly under impact or bending, making it unsuitable for structural or dynamically loaded parts. Its corrosion resistance is limited in chloride-rich or marine environments, where austenitic grades such as 316 are more reliable. The high carbon content and air-hardening behavior make welding unreliable. It loses hardness at elevated temperatures and is not suited to high-temperature service. Machining is difficult even when annealed, and tool wear is high, so free-machining grades are often more practical for complex or high-volume parts.
440C Applications Based on Properties
The application range follows directly from the mix of high hardness, wear resistance, and moderate corrosion resistance. 440C is mainly used in parts subject to friction, rolling contact, or repeated surface loading, including corrosion-resistant bearings, valve components, precision instruments, cutting tools, and industrial blades. Where both wear resistance and basic corrosion protection are needed, it appears in medical instruments, food-processing equipment, and selected aerospace or petroleum components. Powder metallurgy routes, such as metal injection molding, are used to produce small, complex parts where machining is inefficient, including precision automotive components, locking mechanisms, and miniature wear-resistant assemblies.
Because of its low toughness and limited thermal stability, 440C is generally avoided in impact-loaded, structural, and high-temperature applications.
Related Pages
440C Applications Common uses for 440C stainless steel based on hardness, wear resistance, corrosion resistance, and toughness limits. 440C Heat Treatment Guide Annealing, hardening, quenching, subzero treatment, and tempering guidance for 440C stainless steel.
Need 440C Stainless Steel for Wear-Resistant Parts?
Send your grade, size, quantity, surface condition, and application. Aobo Steel can support annealed 440C stainless steel bar and plate supply for machining, heat treatment, bearings, valves, cutting tools, and precision wear parts.