Bulk tool steel bar stock in the Aobo Steel warehouse

Aobo Steel | Global Tool Steel Supplier in China

H13 Tool Steel Supplier | 1.2344 | SKD61 | Annealed Bulk Supply

Annealed Condition | Stable 20GP Container Supply | For Global Distributors

  • 100% UT Tested – SEP 1921-82 Class D/d or E/e
  • Full Batch Traceability with MTC
  • ESR Grade Available Upon Request
  • Surface: Black / Turned / Polished

H13 tool steel (1.2344 / SKD61) is the industry benchmark hot-work tool steel, widely used for aluminum die casting, hot forging, and extrusion tooling. For press-hardening (hot stamping) dies, the grade selection is set out in the hot stamping die steel selection page.

H13 Tool Steel Supply Overview

GradeAISI H13 / DIN 1.2344 / JIS SKD61
Delivery ConditionFully Annealed (Soft Condition for Machining)
Available FormsRound Bar / Flat Bar / Plate / Forged Block
Monthly Production CapacityStable hot work steel scheduling
Recommended Export QuantityFull 20GP container (~26 tons)
MOQ5 tons
Lead Time (With Ingot Stock)Approx. 25 days
Lead Time (Fresh Melt)35–50 days
Lead Time (ESR Grade)Approx. 60 days
InspectionIn-house UT team + Third-party inspection available
DocumentationMTC (EN 10204 3.1) + UT Report

Why Global Distributors Source H13 from Aobo Steel

  • Continuous monthly supply of around 1000 tons
  • MOQ from 5 tons for wholesale orders
  • Container-optimized bar and plate lengths
  • Mixed sizes are supported for export loading
  • Annealed delivery for downstream machining
  • Stable sourcing through integrated supply chain partners
  • UT inspection available to SEP 1921-82 D/d or E/e
  • MTC and batch traceability with each shipment
  • Heat number tracking for order control
  • Black, turned, and polished surface options
  • Bulk export packing for sea shipment
  • Clear conversion path to the dedicated bulk supply page

Production Stability

  • Dedicated production planning for hot work tool steel
  • Strict segregation control for large cross-section sizes
  • Optional ESR (Electro-Slag Remelting) for higher cleanliness
  • Controlled alloy sourcing to ensure stable thermal fatigue performance
  • Full batch traceability linked to the original heat number

Available H13 Tool Steel Forms

Quality Control for Bulk Orders

Every batch of tool steel supplied by Aobo Steel is verified before shipment to ensure grade accuracy, internal soundness, and traceability for bulk orders.

  • Chemical composition verified by a spectrometer
  • Ultrasonic testing available (SEP 1921-82)
  • Delivered in spheroidized annealed condition
  • Mill Test Certificate (EN 10204 3.1) with heat number
  • Dimensional and surface inspection before shipment
Metallographic inspection of tool steel during quality control before bulk shipment

Export Packaging and Container Loading

  • Professional seaworthy export packing
  • 20GP loading optimized up to ~26 tons
  • Mixed grades and mixed sizes supported
  • Anti-rust protection for long sea transit

For international shipments, full-container loading is strongly recommended to ensure cost efficiency and smoother customs processing.

AISI H13 Tool Steel | 1.2344 | SKD61 Gallery

H13 STEEL
H13 steel
1.2344 tool steel

Applications of H13 Tool Steel

Hardness and grade selection for each of these applications is covered in the H13 properties and applications reference.

 H13 Steel and Its Equivalent Grades’ Composition

CCrMoVSiMnPS
0.32 – 0.45%4.75 – 5.50%1.10 – 1.75%0.80 – 1.20%0.80 – 1.25%0.20 – 0.60%≤ 0.030%≤ 0.030%

H13 tool steel equivalent grades’ composition. The limits for the base AISI grade, element by element, are listed on the H13 chemical composition page.

GradeStandardC (%)Si (%)Mn (%)P (%)S (%)Cr (%)Mo (%)V (%)
1.2344DIN0.37-0.420.90-1.200.30-0.50≤0.030≤0.0304.80-5.501.20-1.500.90-1.10
SKD61JIS0.35-0.420.80-1.200.25-0.50≤0.030≤0.0304.80-5.501.00-1.500.80-1.15
4Cr5MoSiV1GB0.32-0.420.80-1.200.20-0.50≤0.030≤0.0304.75-5.501.10-1.750.80-1.20

We guarantee that all materials are manufactured in strict compliance with the specified chemical compositions for H13, 1.2344, and SKD61.

The full list of designations this grade family carries across standards, and how closely each one matches, is in the H13 equivalent grades reference.

H13 tool steel properties

Property tables for this grade — mechanical, high-temperature, wear and physical — are in the H13 steel properties reference. Hardness ranges by application are on the H13 hardness chart, and machinability and grinding behaviour on the H13 machinability page.

The specific properties depend heavily on the tempering temperature. Here are typical longitudinal mechanical properties when air-cooled from 1025 °C (1875 °F) and tempered:

Mechanical Properties (Typical Values at Room Temperature, Double Tempered 2h + 2h)

Property527 °C (980 °F) Temper555 °C (1030 °F) Temper575 °C (1065 °F) Temper
Hardness52 HRC50 HRC48 HRC
Tensile Strength (Rm)1960 MPa (284 ksi)1835 MPa (266 ksi)1730 MPa (251 ksi)
Yield Strength (Rp0.2)1570 MPa (228 ksi)1530 MPa (222 ksi)1470 MPa (213 ksi)
Elongation (in 4D)13.0%13.1%13.5%
Reduction in Area46.2%50.1%52.4%
Charpy V-notch Impact16 J (12 ft·lbf)24 J (18 ft·lbf)27 J (20 ft·lbf)

Physical properties

PropertyValue
Density7.75 – 7.80 g/cm3
Tensile Strength, Ultimate1200 – 2050 MPa (174000 – 231000 psi)
Tensile Strength, Yield1000 – 1380 MPa (145000 – 200000 psi)
Hardness45-52 HRC (Rockwell C Hardness)
Impact Toughness20-40 J/cm2
Compressive Strength2550 MPa

H13 Tool Steel Guides

Reference pages for this grade, and how it compares with the other hot-work and cold-work grades:

H13 Tool Steel Heat Treatment Overview

The full schedules — austenitizing, soak times, cooling and tempering curves — are in the H13 heat treatment guide.

Hardening

Preheating to around 815°C (1500°F) is recommended before hardening.

Austenitizing temperature: 1010–1040°C (1850–1900°F).

H13 is typically air quenched to minimize distortion and residual stress. Hardness after quenching: 52–54 HRC.

Tempering

Tempering should be performed immediately after quenching.

Typical tempering range: 540–620°C (1000–1150°F). Double tempering is commonly recommended for hot work tooling.

Typical hardness after tempering:

  • 540°C: ~47–48 HRC
  • 620°C: ~36–38 HRC

Tempering around 500°C (930°F) should generally be avoided due to reduced toughness.