Cr12MoV vs D2 Tool Steel: Equivalent & Selection Guide
Cr12MoV vs D2 Tool Steel: Are They Equivalent? Cr12MoV is not equivalent to AISI D2 tool steel. Both are high-carbon, high-chromium cold-work tool steels, but they differ in alloy content, heat treatment response, wear resistance, and international grade equivalency. The main difference is between molybdenum and vanadium. D2 contains higher Mo and V than Cr12MoV,