Steel Bar Weight Table
Theoretical weight of steel bars (kg/m) based on specific gravity 7.85 g/cm³. Read the unit weight for each size from the tables below, then multiply it by the length you need.
Round bar and square bar weight
Unit weight for round bar and square bar from 5 to 300 mm, calculated from nominal size at a density of 7.85 g/cm³. Density varies a little by grade, and the measured values are in the tool steel density and thermal expansion chart.
| Size (mm) | Round bar (kg/m) | Square bar (kg/m) |
|---|---|---|
| 5 | 0.15 | 0.20 |
| 6 | 0.22 | 0.28 |
| 7 | 0.30 | 0.38 |
| 8 | 0.39 | 0.50 |
| 9 | 0.50 | 0.64 |
| 10 | 0.62 | 0.79 |
| 11 | 0.75 | 0.95 |
| 12 | 0.89 | 1.13 |
| 13 | 1.04 | 1.33 |
| 14 | 1.21 | 1.54 |
| 15 | 1.39 | 1.77 |
| 16 | 1.58 | 2.01 |
| 17 | 1.78 | 2.27 |
| 18 | 2.00 | 2.54 |
| 19 | 2.23 | 2.83 |
| 20 | 2.47 | 3.14 |
| 21 | 2.72 | 3.46 |
| 22 | 2.98 | 3.80 |
| 23 | 3.26 | 4.15 |
| 24 | 3.55 | 4.52 |
| 25 | 3.85 | 4.91 |
| 26 | 4.17 | 5.31 |
| 27 | 4.49 | 5.72 |
| 28 | 4.83 | 6.15 |
| 29 | 5.19 | 6.60 |
| 30 | 5.55 | 7.07 |
| 31 | 5.92 | 7.54 |
| 32 | 6.31 | 8.04 |
| 33 | 6.71 | 8.55 |
| 34 | 7.13 | 9.07 |
| 35 | 7.55 | 9.62 |
| 36 | 7.99 | 10.2 |
| 37 | 8.44 | 10.8 |
| 38 | 8.90 | 11.3 |
| 39 | 9.38 | 11.9 |
| 40 | 9.86 | 12.6 |
| 41 | 10.4 | 13.2 |
| 42 | 10.9 | 13.9 |
| 43 | 11.4 | 14.5 |
| 44 | 11.9 | 15.2 |
| 45 | 12.5 | 15.9 |
| 46 | 13.1 | 16.6 |
| 47 | 13.6 | 17.3 |
| 48 | 14.2 | 18.1 |
| 49 | 14.8 | 18.9 |
| 50 | 15.4 | 19.6 |
| 51 | 16.0 | 20.4 |
| 52 | 16.7 | 21.2 |
| 53 | 17.3 | 22.1 |
| 54 | 18.0 | 22.9 |
| 55 | 18.7 | 23.8 |
| 56 | 19.3 | 24.6 |
| 57 | 20.0 | 25.5 |
| 58 | 20.7 | 26.4 |
| 59 | 21.5 | 27.3 |
| 60 | 22.2 | 28.3 |
| 61 | 22.9 | 29.2 |
| 62 | 23.7 | 30.2 |
| 63 | 24.5 | 31.2 |
| 64 | 25.3 | 32.2 |
| 65 | 26.1 | 33.2 |
| 66 | 26.9 | 34.2 |
| 67 | 27.7 | 35.2 |
| 68 | 28.5 | 36.3 |
| 69 | 29.4 | 37.4 |
| 70 | 30.2 | 38.5 |
| 71 | 31.1 | 39.6 |
| 72 | 32.0 | 40.7 |
| 73 | 32.8 | 41.8 |
| 74 | 33.8 | 43.0 |
| 75 | 34.7 | 44.2 |
| 76 | 35.6 | 45.3 |
| 77 | 36.6 | 46.5 |
| 78 | 37.5 | 47.8 |
| 79 | 38.5 | 49.0 |
| 80 | 39.5 | 50.2 |
| 81 | 40.5 | 51.5 |
| 82 | 41.5 | 52.8 |
| 83 | 42.5 | 54.1 |
| 84 | 43.5 | 55.4 |
| 85 | 44.5 | 56.7 |
| 86 | 45.6 | 58.1 |
| 87 | 46.7 | 59.4 |
| 88 | 47.7 | 60.8 |
| 89 | 48.8 | 62.2 |
| 90 | 49.9 | 63.6 |
| 91 | 51.1 | 65.0 |
| 92 | 52.2 | 66.4 |
| 93 | 53.3 | 67.9 |
| 94 | 54.5 | 69.4 |
| 95 | 55.6 | 70.9 |
| 96 | 56.8 | 72.4 |
| 97 | 58.0 | 73.9 |
| 98 | 59.2 | 75.4 |
| 99 | 60.4 | 76.9 |
| 100 | 61.7 | 78.5 |
| 105 | 68.9 | 86.6 |
| 110 | 74.6 | 95.0 |
| 115 | 81.5 | 104 |
| 120 | 88.8 | 113 |
| 125 | 96.3 | 123 |
| 130 | 104 | 133 |
| 135 | 112 | 143 |
| 140 | 121 | 154 |
| 145 | 130 | 165 |
| 150 | 139 | 177 |
| 155 | 148 | 189 |
| 160 | 158 | 201 |
| 165 | 168 | 214 |
| 170 | 178 | 227 |
| 175 | 189 | 240 |
| 180 | 200 | 254 |
| 185 | 211 | 269 |
| 190 | 223 | 283 |
| 195 | 234 | 299 |
| 200 | 247 | 314 |
| 210 | 272 | 346 |
| 220 | 298 | 380 |
| 230 | 326 | 415 |
| 240 | 355 | 452 |
| 250 | 386 | 491 |
| 260 | 417 | 531 |
| 270 | 449 | 572 |
| 280 | 483 | 615 |
| 290 | 518 | 660 |
| 300 | 555 | 707 |
Hexagonal bar and octagonal bar weight
Hexagonal and octagonal bar from 5 to 56 mm. Size is measured across the flats for both profiles.
| Size (mm) | Hexagonal bar (kg/m) | Octagonal bar (kg/m) |
|---|---|---|
| 5 | 0.17 | 0.16 |
| 6 | 0.25 | 0.23 |
| 7 | 0.33 | 0.32 |
| 8 | 0.44 | 0.42 |
| 9 | 0.55 | 0.53 |
| 10 | 0.68 | 0.65 |
| 11 | 0.82 | 0.79 |
| 12 | 0.98 | 0.94 |
| 13 | 1.15 | 1.10 |
| 14 | 1.33 | 1.27 |
| 15 | 1.53 | 1.46 |
| 16 | 1.74 | 1.66 |
| 17 | 1.97 | 1.88 |
| 18 | 2.20 | 2.11 |
| 19 | 2.45 | 2.35 |
| 20 | 2.72 | 2.60 |
| 21 | 3.00 | 2.87 |
| 22 | 3.29 | 3.15 |
| 23 | 3.60 | 3.44 |
| 24 | 3.92 | 3.74 |
| 25 | 4.25 | 4.06 |
| 26 | 4.60 | 4.40 |
| 27 | 4.96 | 4.74 |
| 28 | 5.33 | 5.09 |
| 29 | 5.72 | 5.47 |
| 30 | 6.12 | 5.85 |
| 31 | 6.53 | 6.25 |
| 32 | 6.96 | 6.66 |
| 33 | 7.41 | 7.08 |
| 34 | 7.86 | 7.52 |
| 35 | 8.33 | 7.97 |
| 37 | 9.31 | 8.90 |
| 39 | 10.3 | 9.89 |
| 41 | 11.4 | 10.9 |
| 43 | 12.6 | 12.0 |
| 45 | 13.8 | 13.2 |
| 47 | 15.0 | 14.4 |
| 50 | 17.0 | 16.3 |
| 53 | 19.1 | 18.3 |
| 56 | 21.3 | 20.4 |
Calculation basis
Specific gravity 7.85 g/cm³, standard for carbon and alloy steel. Round bar 0.00617 × d², square bar 0.00785 × d².
Size definition
Round and square bar, size is the diameter or the side length. Hexagonal and octagonal bar, size is the distance between opposite sides.
Weight adjustment by grade
Molybdenum HSS (M2, M35, M42) approx. +3%, tungsten HSS 18-4-1 type (T1) approx. +10%.
Related reference pages
Tool steel hardness conversion calculator · Tool steel properties chart · Tool steel material finder · How to select tool steels · Tool steel supply and stock sizes
Theoretical unit weights calculated from nominal dimensions at a density of 7.85 g/cm³. Actual weight varies with rolling tolerance, machining allowance and cutting loss, so use the figures for estimating and quotation.
Table values follow Appendix 7, Weight Tables for Steel Bars, in Steel Heat Treatment Handbook, 2nd edition, volume 2 (G. E. Totten, ed.).