Aobo Steel · Tool Steel Supplier · Huangshi, China
1.2080 Tool Steel Round Bar & Plate
DIN 1.2080 / X210Cr12 / AISI D3 / JIS SKD1 · Wholesale round bar and plate
Round bar and plate in stock, cut to your lengths. Wholesale supply for shear blades, cutting tools and blanking dies, from one bar to a full container.
Grade1.2080 · X210Cr12 · AISI D3 · SKD1 · Cr12
In stockRound bar Ø70–600 mm · plate 20–400 mm thick, width to 810 mm
Cut to sizeAny length or plate size cut from stock, send your cut list
Forged to orderOther diameters and thicknesses to your spec
SurfaceBlack · turned bright · milled plate
DocumentsMTC EN 10204 3.1 per heat · UT on request to SEP 1921-82
Also supplied as D3 tool steel and Cr12, same steel and same mill certificate. Part of the cold work tool steels family. Hardening and tempering steps are in the D3 heat treatment guide