Fatores que afetam a dureza do aço para ferramentas D2
D2 tool steel is a high-carbon, high-chromium, air-hardening steel. Its hardness is affected by chemical composition, heat treatment parameters, and microstructural interactions. Here are the detailed factors affecting D2 tool steel hardness. The Critical Role of Chemical Composition The composition of D2 steel is1 Carbon (C) Chromium (Cr) Molybdenum (Mo) Vanadium (V) Manganese (Mn) Silicon […]
Fatores que afetam a dureza do aço para ferramentas D2 Ler mais »