Premium SKD6 Tool Steel Supplier for Unmatched Durability
SKD6 tool steel is a high-quality alloy used primarily to manufacture molds and dies. Known for its superior toughness, wear resistance, and ability to withstand high-temperature environments, SKD6 is widely used in industries such as automotive, aerospace, and heavy machinery. This steel grade’s performance in demanding applications has made it a popular choice for tools that require durability and precision.
![](https://aobosteel.com/wp-content/uploads/2025/01/D2.png)
Most cost-effective, high-quality supplier of D2 steel
We offer both D2 electric furnace steel and D2 ESR steel. Considering our customers’ purchasing costs, we produce D2 round bars with diameters under 200mm using the electric furnace method, which can meet Ultrasonic testing (UT) Sep 1921-84 D/d flaw detection. Customers can purchase high-standard D2 round bars at a lower cost. We adopt the ESR process for diameters above 200mm to ensure that the internal structure can meet Ultrasonic testing (UT) Sep 1921-84 E/e flaw detection.
Excellent D2 Forged Steel Supplier
Aobo Steel has over 20 years of experience in forging D2 steel, giving us a deep practical understanding of quality control in this field. Our D2 forged steel products mainly come in round bar, plate, and block shapes. We have over 40 suppliers providing the best processing services, enabling us to offer advantages such as short lead times, stable quality, and competitive prices.
![](https://aobosteel.com/wp-content/uploads/2025/01/D2.png)
![](https://aobosteel.com/wp-content/uploads/2025/01/D2-768x768.png)
Suply Range
The shapes of steel that Aobo Steel produces include A2 tool round bars and A2 plates.
Shape | Size | Length | Surface finish | tolerance |
round bar | diameter 20mm-400mm | length 2500mm-5800mm | black | 0/+5mm |
peeled | 0/+5mm | |||
turned(machined) | 0/+2mm | |||
plate | width*thickness 100mm-800mm*10mm-400mm | length 2500mm-5800mm | black | 0/+5mm |
peeled | 0/+5mm | |||
turned(machined) | 0/+2mm |
SKD6 steel Chemical Composition
Element | Composition (%) |
---|---|
Carbon (C) | 0.50 – 0.60 |
Manganese (Mn) | 0.20 – 0.80 |
Chromium (Cr) | 5.00 – 5.50 |
Vanadium (V) | 0.30 – 0.60 |
Silicon (Si) | 0.10 – 0.40 |
Phosphorus (P) | ≤ 0.030 |
Sulfur (S) | ≤ 0.030 |
Equivalent Grades
Standard | Equivalent Grade |
---|---|
AISI (USA) | H11 |
DIN (Germany) | 1.2343 |
GB (China) | 4Cr5MoSiV1 |
Physical Properties
Property | Value |
---|---|
Density | 7.80 g/cm³ |
Thermal Conductivity | 24.0 W/m·K |
Hardness (After Heat Treatment) | 58 – 62 HRC |
Elastic Modulus | 200 GPa |
Tensile Strength | 900 – 1100 MPa |
Melting Point | 1420°C (2588°F) |
SKD6 heat treatment
Process | Temperature Range | Purpose | Cooling Method |
---|---|---|---|
Annealing | 850°C – 880°C (1562°F – 1616°F) | Softens the steel for improved machinability | Slow cooling in furnace |
Hardening | 1000°C – 1050°C (1832°F – 1922°F) | Increases hardness and wear resistance | Oil or air quenching |
Tempering | 500°C – 600°C (932°F – 1112°F) | Reduces brittleness and improves toughness | Air cooling |
SKD6 Applications
1. Molds and Dies:
SKD6 is commonly used in hot-working and extrusion dies, where high wear resistance and toughness are critical.
2. Forging Tools:
The tool steel is frequently employed in forging operations, where it can withstand high pressures and temperatures.
3. Industrial Blades:
SKD6 is often used to produce industrial blades and knives, which require high hardness and durability.
4. Press Tools:
The steel’s resistance to wear and thermal stability make it suitable for press tools in heavy machinery applications.
Why should you choose Aobo Steel as your tool steel supplier?
At Aobo Steel, we pride ourselves on our exceptional supply capacity and dedication to meeting customer demands. Our monthly shipments exceed 1,500 tons in the Chinese market, reflecting our robust production and delivery capabilities. With a strong network of over 40 trusted suppliers, we ensure a steady supply of high-quality tool steels to meet various industry needs.
To provide even greater flexibility, we maintain stock for select products, allowing us to fulfill urgent orders quickly. Additionally, we specialize in fully customizable solutions, tailoring our products to your exact specifications for optimal application performance.
Our strategic location near the Yangtze River gives us a significant advantage in export logistics, enabling fast and cost-effective shipping to customers worldwide. Whether you need standard products or custom orders, Aobo Steel is committed to delivering reliability, quality, and service excellence.
![](https://aobosteel.com/wp-content/uploads/2025/01/IMG_20170828_111642-1024x768.jpg)
![](https://aobosteel.com/wp-content/uploads/2025/01/IMG_20221028_111745.jpg)
At Aobo Steel, quality control is at the heart of our operations. Our dedicated testing team with over 20 years of experience ensures every product meets the highest standards before leaving our facility. Our comprehensive quality assurance process includes chemical composition analysis, metallographic examination, hardness testing, physical performance evaluation, and ultrasonic testing (UT) to detect internal defects.
To guarantee reliability, we perform 100% quality inspection on all products before shipment, ensuring they meet the required specifications and industry standards. Additionally, we support third-party inspections upon request to provide our customers with extra confidence in the quality of our materials. With this rigorous approach, Aobo Steel consistently delivers tool steels that offer superior performance and dependability in various applications.
At Aobo Steel, our service capacity is designed to meet diverse customer needs efficiently and precisely. We provide fully customizable products, offering surface treatments, descaling, and custom-length cutting options to suit specific requirements. Our experienced foreign trade team is well-versed in handling international orders, ensuring smooth communication and seamless transactions.
To provide the best service, we guarantee a 24-hour rapid response to all inquiries, allowing us to address your needs promptly and effectively. At Aobo Steel, we are committed to delivering high-quality tool steels and exceptional customer service to support your success.
![](https://aobosteel.com/wp-content/uploads/2025/01/IMG_20171127_153124.jpg)