O1 tool steel is a low-alloy cold-worked tool steel. It has a certain degree of hardenability and wear resistance, with minimal quenching deformation. The carbide distribution is uniform, and the particles are fine. Manufacturers typically use tool steel O1 for manufacturing cold punching dies with small cross-sections, complex shapes, and various gauges and measuring tools. The equivalent grades of O1 are DIN 1.2510 (Germany), JIS SKS3 (Japan), and GB 9CrWMn (China).
1. Applications
- Dies & Punches: Blanking dies, Coining dies, Drawing dies, Forming dies, General Stamping (punches & dies for short/moderate runs), Thread-rolling dies, Cold-trimming dies
 - Cutting & Machining Tools: General shop tool bits (economical choice), Shear blades (especially smaller ones), Taps, Reamers, Hobs, Slitting saws, Circular cutters, Drills
 - Molds & Precision Parts: Plastic mold components (inserted cavities, master hubs), Gauges, Master tools
 - General Tooling & Wear Parts: Cams, Bushings, Guides, Plain sliding bearings, Cam followers, Burnishing tools, Knurling tools, Feed rolls, Roll forming tooling (moderate runs)
 
2. O1 Steel Composition1
| C | Mn | Si | Cr | W | V | Ni | Mo | P | S | 
| 0.85 – 1.00% | 1.00 – 1.40% | Max 0.50% | 0.40 – 0.60% | 0.40 – 0.60% | Max 0.30% | Max 0.30% | Max 0.30% | Max 0.03% | Max 0.03% | 
The O1 tool steel equivalent grades’ composition
| Grade | Standard | C (%) | Si (%) | Mn (%) | Cr (%) | W (%) | V (%) | 
| 1.2510 | DIN | 0.90-1.05 | 0.15-0.35 | 1.00-1.20 | 0.50-0.70 | 0.50-0.70 | 0.05-0.15 | 
| SKS3 | JIS | 0.90-1.00 | ≤0.35 | 0.90-1.20 | 0.50-1.00 | 0.50-1.00 | – | 
| 9CrWMn | GB | 0.85-0.95 | ≤0.40 | 0.90-1.20 | 0.50-0.80 | 0.50-0.80 | – | 
3. Properties
- Hardness: O1 steel hardness is 57-64 Rockwell C (HRC) through oil quenching. As the tempering temperature increases, the hardness decreases. For example, after tempering at 900°F (482°C), the hardness can be reduced to 47 HRC.
 - Strength (Tensile and Yield): Tool steel O1 exhibits a tensile strength of 846 MPa and a 0.2% Offset Yield Strength of 829 MPa, with a general yield strength of 758 MPa. For a specific O1 composition, tensile strength can be as high as 1725 MPa (250 ksi) when tempered at 800°F (425°C), decreasing with higher tempering temperatures.
 - Ductility and Toughness: O1 steel exhibits noticeable necking before fracture, with a substantial area reduction at fracture of nearly 20%. Its fracture surface typically displays a cup–cone mode. While generally having medium toughness, it shows superior impact strength compared to other O-type steels within the common working hardness range of 57 to 64 HRC. The ductility usually improves with increasing tempering temperature.
 - Modulus of Elasticity: 211 GPa.
 - Dimensional Stability: Good dimensional stability during heat treatment. When oil is quenched from the correct hardening temperature, it typically expands by about 0.0015 inches per inch (0.0015 mm/mm). However, factors like part geometry and distortion (bending, bowing, or twisting) can influence the final dimensional changes.
 - Machinability: Very good machinability. If the machinability of steel with 1% carbon content is set at 100, the machinability of O1 steel is 90.
 
4. O1 Heat treatment
The heat treating of O1 steel generally involves four primary steps: preheating, austenitizing (hardening), quenching, and tempering.
4.1 Preheating
Preheating is an essential step for virtually all tool steels, including O1. Metallurgically, it doesn’t directly contribute to the hardening reaction but serves several crucial functions:
- Reduces Thermal Shock: Placing a cold tool into a hot furnace can cause thermal shock, leading to excessive distortion or cracking. Preheating minimizes this risk.
 - Relieves Stress: It helps relieve some stress developed during machining or forming processes.
 - Increases Equipment Productivity: By bringing the tool to a uniform temperature before the high-heat furnace, it decreases the time required in the austenitizing furnace.
 - Reduces Surface Degradation: If the high-heat furnace isn’t neutral, preheating reduces carburization and decarburization.
 
The preheat temperature is 1200°F (650°C). The steel should be held at this temperature for 10 to 15 minutes, or until it is uniformly heated throughout its cross-section. Please DO NOT soak the tool steel for too long at this temperature, as it can upset the molecular structure. Based on our experience, if placing the part in a preheated furnace (up to 1200°F/650°C), first place it at the top of the furnace to remove any chill, which helps reduce thermal shock and lower the risk of cracking.
4.2 Austenitizing (Hardening)
After preheating, set the furnace temperature to the austenitizing temperature of 1500°F (815°C). We must heat the material until it fully reaches this temperature, which can be confirmed by observing its color matching the furnace. Once the temperature is consistent, begin calculating the soaking time. Soaking for an additional 5 minutes per inch of the smallest cross-section. While O1 steel may be damaged by over-soaking, its tolerance is generally higher compared to high-alloy steels.
4.3 Quenching2
O1 steel is classified as an O-type steel because it is steel that uses oil as a quenching medium. Oil as a quenching medium is slower than water but safer, reducing internal stress and the tendency for cracking and deformation. After quenching, it should be cooled to 125 to 150°F (52 to 65°C). Once this temperature range is reached, tempering should be performed immediately.
4.4 Tempering
After quenching, the steel is in a highly stressed state and susceptible to cracking. Tempering serves to:
- Relieve Internal Stresses: It reduces the internal stresses set up during hardening, which can cause brittleness.
 - Increase Toughness: Tempering significantly increases the steel’s toughness.
 - Transform Retained Austenite: It transforms retained austenite from the quenching step into fresh martensite.
 
This steel typically requires only one tempering process, but in some cases, two tempering processes may be necessary. Two tempering processes can refine the grain structure to enhance toughness, making it suitable for parts with complex details or those requiring high strength.
The single tempering temperature is 350°F (175°C), with a soaking time of 2 hours per inch (25mm) of cross-section.
If a second tempering is performed, the temperature should be slightly lower, typically 325°F (160°C), and the part should be allowed to cool to room temperature between the two tempering processes.
O1 Tool Steel Tempering Temperatures and Resulting Hardness
| TEMPERING TEMPERATURE | Rockwell C | 
| As quenched | 66 | 
| 300°F/150°C | 63 | 
| 400°F/205°C | 60 | 
| 500°F/260°C | 57 | 
| 600°F/315°C | 54 | 
O1 Tempering Size Change Chart
These changes are approximate values based on good heat treating practice.

If you would like to discuss O1 tool steel with us, please complete the form below to contact us.
5. Compare O1 steel with other steels
5.1 A2 Vs. O1 Tool Steel
We provide a direct comparison of the key properties and characteristics of O1 and A2 cold-work tool steels. For more information about this topic, please refer to A2 Vs. O1 tool steel
| Feature | O1 Tool Steel | A2 Tool Steel | 
| Classification | Oil-hardening, manganese type. | Air-hardening, medium-alloy type. | 
| General Characteristics | Good edge-holding, high hardness, widely available, inexpensive. | Excellent dimensional stability (low distortion), high abrasion resistance. | 
| Primary Advantage | Good all-around performance and ease of heat treat for a lower cost. | Superior dimensional stability during heat treatment and better wear resistance. | 
| Hardness (Typical) | 57–62 HRC | 57–62 HRC | 
| Wear Resistance | Good | Very Good to Excellent; a standard for abrasion resistance. Better than O1. | 
| Toughness | High; Modulus of Toughness is 68 MPa. | Higher than O1; provides better toughness. Modulus of Toughness is 81 MPa. | 
| Dimensional Stability | Very low distortion, but less stable than A2. Expands ~0.0015 in./in. | Minimum movement during hardening; considered a standard for stability. | 
| Machinability | Excellent (rated 90 vs. 1% carbon steel at 100). | High. | 
| Austenitizing Temp. | Lower: 802–816 °C (1475–1500 °F) | Higher: 925–980 °C (1700–1800 °F) | 
| Quenching Medium | Oil | Air | 
| Tempering | Single temper is often sufficient. | Double tempering is recommended. Higher resistance to softening. | 
| Typical Applications | Short-run blanking/forming dies, punches, woodworking knives, master hubs. | Long-run blanking/forming dies, punches, mold inserts, thread-rolling dies. | 
5.2 O1 Vs. O2 steel
For detailed information about this topic, please refer to O1 Vs. O2 steel
| Feature | O1 Tool Steel | O2 Tool Steel | 
| Hardness (Typical) | 57-62 HRC | 57-62 HRC | 
| Wear Resistance | Good | High | 
| Toughness | Good; slightly higher than other oil-hardening steels. | Medium | 
| Dimensional Stability | Very Low Distortion | Very Low Distortion | 
| Machinability | Excellent | Good | 
| Hardenability | Medium | Medium | 
| Hardening Temperature | 802–816°C (1475–1500°F) | 760–790°C (1400–1450°F) | 
| Heat Treat Concerns | Prone to decarburization and thermal shock cracking. | Not specified as a primary concern. | 
5.3 O1 tool steel Vs. D2
For detailed information about this topic, please refer to O1 tool steel Vs. D2
| Feature | O1 Tool Steel | D2 Tool Steel | 
| AISI Group | Oil-hardening cold-work tool steel | High-carbon, high-chromium cold-work die steel | 
| Quenching Medium | Oil-quenching | Air-hardening | 
| Hardness (typical) | 57-62 HRC (can be 62-63 HRC) | 54-61 HRC (can be 60-62 HRC) | 
| Wear Resistance | Good, relies on hardened martensite | Very high, superior to O1, due to high Cr-carbides | 
| Toughness | Sufficient/Good, generally better than D2 | Moderate/Fair, generally lower than O1 | 
| Dimensional Stability | Small changes, good | Minimum movement/distortion, good | 
| Machinability | Excellent (Rating 90/100) | Poor/Difficult (Rating 45/100) | 
| Hardenability | Medium | Deep | 
| Necking (Tensile) | Clear necking (19.7% area reduction) | Almost no necking (1.3% area reduction) | 
| Fracture Mode | Cup-cone | Flat surface | 
| Yield Strength (0.2%) | 829 MPa | 411 MPa | 
| Ultimate Tensile Strength (UTS) | 846 MPa | 758 MPa | 
| Cost | Low | Good balance of properties vs. cost | 
| Typical Applications | General-purpose, small tools, punches, and woodworking knives | Long-run dies, blanking, forming, piercing, forging, trimming | 
O1 is a more machinable and tougher steel with generally higher tensile properties; however, D2 offers significantly better wear resistance and dimensional stability after heat treatment due to its air-hardening nature and higher alloy content, particularly chromium carbides.
5.4 O1 tool steel Vs. 1095
| Feature | O1 Tool Steel | 1095 Steel (as W1 Tool Steel) | 
| Classification | Oil-hardening, cold-work tool steel (AISI O-series) | Water-hardening, plain high-carbon steel | 
| Primary Use | Versatile cold-work tooling | General-purpose cutting tools and parts | 
| Hardenability | High, deep hardening. Can through-harden in sections up to 2.5 inches (63.5 mm). | Low, shallow hardening. Hardens only to about 1/16 inch deep. | 
| Quenching Medium | Oil. Offers better stability and lower risk of distortion. | Water or Brine. Severe quench leads to high risk of cracking and warping. | 
| Dimensional Stability | Good. Exhibits minimal size changes after quenching. | Poor. Highly prone to distortion and cracking during heat treatment. | 
| Hardness (Typical) | 57-64 HRC. | Can achieve 62 HRC or higher, but only at the surface. | 
| Wear Resistance | Medium. Better than simple carbon steels due to alloying elements. | Lower. Develops a keen edge but has poor hot hardness. | 
| Toughness | Medium. Slightly higher toughness than other oil-hardening steels. | Good. The unhardened, ductile core provides good toughness. | 
| Machinability | Excellent. Rated at 90 (compared to W1 at 100). | Excellent. Rated at 100, serving as a baseline. | 
| Typical Applications | Blanking/forming dies, gauges, shear blades, machine ways, plastic molds. | Small dies, vise jaws, centering pins, and tools where a sharp edge is needed but high wear resistance is not critical. | 
While both O1 tool steel and 1095 steel are high-carbon steels capable of achieving high hardness, O1 is a more alloyed tool steel designed for oil quenching, offering deeper hardening, better dimensional stability, and slightly better wear resistance. 1095, being a plain carbon steel, relies on water quenching for maximum hardness, which leads to shallow hardening and a higher risk of distortion and cracking; however, it offers excellent machinability.
6. Limitation of O1 tool steel
- Low Resistance to Softening at Elevated Temperatures. O1 tool steel is categorized as a cold-work steel, meaning its applications are limited to low temperatures, typically room temperature. It possesses a low resistance to softening when exposed to elevated temperatures. If used in hot-work applications, it is prone to annealing or cracking due to thermal shock loading.
 - Limited Carbide Content for Wear Resistance. O1 is a low-alloy tool steel with a low alloy content and almost no carbides in its microstructure. Unlike high-carbon, high-chromium steels (D-grades) that rely on coarse carbides for superior wear resistance, O1’s wear resistance primarily depends on its hardness, which is derived from its high-carbon martensitic matrix. This makes it less suitable for applications requiring extremely high abrasive wear resistance compared to steels like D2 or D3.
 - Susceptibility to Cracking During Quenching. O1 is susceptible to cracking from thermal shock during oil quenching, especially in parts with sharp corners or intricate designs, such as those with holes close to the edge. While oil quenching is considered safer and results in less distortion than water quenching, rapid heating to forging temperatures also makes O1 steels somewhat sensitive to cracking.
 - Decarburization. O1 tool steel is prone to decarburization during heat treatment. To prevent this, it should be annealed and/or hardened in a controlled neutral atmosphere, vacuum, or neutral-salt furnace. While it is generally considered highly resistant to decarburization compared to some other steel types, precautions are still necessary.
 - Hardenability and Section Size Limitations. While O1 has sufficient hardenability for small to moderate sections to achieve full hardness when oil quenched, its hardenability may not be enough for very large tools and dies.
 - Dimensional Changes During Heat Treatment. When O1 steel is oil quenched at the correct quenching temperature, its dimensions may expand by approximately 0.0015 inches/inch (0.0015 mm/mm).
 - Retained Austenite Issues. Overheating during austenitizing can lead to an increased amount of retained austenite in quenched O1 parts, which can compromise dimensional stability and contribute to cracking.
 
7. Surface Treatment
- Boriding (Boronizing). After quenching, O1 steel undergoes boronizing treatment at a temperature of 850-950°C. This process forms an extremely hard, wear-resistant layer of iron borides (FeB and Fe2B) with a hardness value between 1450 and 5000 HV. Boronized O1 steel has three times the wear resistance of untreated steel.
 - Physical Vapor Deposition (PVD) Coatings. The PVD process for O1 steel is carried out at relatively low temperatures (200–500°C) to minimize tempering effects on the core. Thin films of hard materials such as titanium nitride (TiN) or titanium carbide (TiC) are deposited onto the surface of O1 tool steel. PVD coatings exhibit extremely high hardness (2000 HV for TiN and 3500 HV for TiC) and chemical inertness, reducing pitting wear and preventing chip adhesion to the tool.
 - Hard Chromium Plating. This is a commonly used electroplating process for tool steel. O1 steel can be electroplated with a chromium layer up to 25 µm thick.
 - Nitriding. A thermochemical diffusion process that introduces nitrogen into the tool surface, creating a hard layer (0.013 to 0.05 mm thick). It’s typically applied after finishing grinding at temperatures between 400°C and 550°C.
 
8. Supply forms and dimensions
The O1 tool steel we supply is available in various forms, including round bars, sheet plates, slabs, flat bars, square bars, and blocks. The dimensions of the flat bar range from: width 20–600 mm × thickness 20–400 mm × length 1,000–5,500 mm. The dimensions of the round bar range from a diameter of 20–400 mm × a length of 1,000–5,500 mm. The block dimensions are obtained by cutting the flat bar.
For smaller sizes, such as round bars with a diameter less than 70 mm, we use the hot-rolled process. For sizes greater than 70 mm, we offer forged products.
UT testing: Sep 1921-84 D/d, E/e.
Surface Treatment: original black, peeled, machined/turned, polished, grounded, or milled surface finishes.
Inventory Status: We do not maintain a stock of O1 tool steel. We arrange production based on customer orders.
Delivery time: Electric Arc Furnace (EAF) materials are 30-45 days. ESR materials are approximately 60 days.



- Davis, J. R. (Ed.). (1998). Metals handbook desk edition (2nd ed., p. 815). ASM International. ↩︎
 - Bryson, W. E. (2007). Heat Treatment, Selection, and Application of Tool Steels (p. 91). Hanser Publications. ↩︎
 
FAQs
O1 tool steel is an oil-hardening, “non-shrinking” cold-work tool steel known for its high hardenability and dimensional stability during heat treatment. It is a general-purpose steel suitable for applications where alloy steels may not provide sufficient hardness, strength, and wear resistance.
German DIN grade: 1.2510
Japan JIS standard grade: SKS3 or SKS31
China GB standard grade: 9CrWMn
British BS standard grade: BO1
France NF standard grade: 90MnWCrV5
International Organization for Standardization (ISO) standard grade: 95MnWCr1
Sweden SS standard grade: 2140
Japan Daido (DAIDO) standard grade GOA
Korea KS standard grade STS3
Russian ГОСТ standard: 9ХВГ
O1 steel is an oil-hardened tool steel with low heat treatment distortion and is suitable for precision tools; A2 steel is an air-cooled tool steel with higher wear resistance and good toughness.
If you are looking for the ultimate in hardness and wear resistance and can accept the risk of distortion, choose 1095 steel; if the balance of hardness and toughness is more important and the risk of distortion is lower, O1 steel is usually a better choice.
O1 steel is quenched by quenching in oil.
O1 steel is easy to machine in the annealed condition.
O1 steel is a versatile and economical choice for cold-work applications requiring high hardness, good wear resistance, and reliable heat treatment with minimal distortion. However, its performance is limited at higher temperatures, and it requires careful atmospheric control during heat treatment to prevent decarburization.
Yes, O1 tool steel is a great material for knives. It is very easy to work with, reliable to heat-treat, and can be hardened to a Rockwell C 65 range. It holds a very fine edge for a long time, is easy to sharpen, and forms very fine carbides. While not “stainless” or “semi-stainless,” it has a decent amount of chromium, making it more corrosion resistant than plain carbon steels like 1095 or 52100. It will likely develop a patina, but with care, it won’t rust severely.
O1 tool steel has excellent machinability, rated at 85-90% compared to a 1% carbon steel. When drilling, it’s crucial to use a drill press, industrial-grade bits (like tungsten carbide drill bits for hardened O1), and adequate pressure to prevent work hardening. If the steel has accidentally air-hardened or work-hardened due to improper heating (e.g., heating raw stock to soften it) or light pressure during drilling, it will need to be re-annealed to become machinable again.
O1 tool steel can achieve a high hardness range of 58-65 HRC (Rockwell Hardness) after heat treatment. It offers good wear resistance due to its tungsten and higher chromium content, excellent machinability (85-90% of a 1% carbon steel), and good cutting edge retention. It is also considered “non-shrinking” due to its dimensional stability during heat treatment.
O1 tool steel is commonly used for blanking and stamping dies (for cutting sheets up to 6mm thickness), threading tools, drills, broaches, gauges, measuring tools, plastic moulds, shear blades, and guide rails. It is also used for medium-run dies, intricate press tools, drawing punches, bushings, lathe centers, chuck jaws, master cavity sinking hobs, paper cutting machine knives, and various types of cutters and machine parts.
Key physical properties of O1 tool steel include a density of approximately 7.83-7.85 g/cm³ (0.282-0.283 lb/in³), a melting point of around 1410-1421°C (2570-2590°F), and a Modulus of Elasticity of 210-214 GPa (31 x 10⁶ psi). Its thermal conductivity at 20°C is 33.4 W/(m*K).
The hardening process for O1 tool steel generally involves preheating slowly to 1200-1300°F (649-704°C), then raising the temperature to the austenitizing (high heat) range of 1475-1500°F (802-816°C). After soaking, it is oil-quenched to a temperature of no lower than 125-150°F (51-66°C) and then tempered immediately.
The recommended austenitizing (hardening) temperature for O1 tool steel is between 1475-1500°F (802-816°C). For light sections, oil quenching from the lower end of this range (780-820°C) is suggested.
After reaching the hardening temperature, O1 tool steel should be soaked for 30 minutes for the first inch (25.4 mm) of thickness, plus 15 minutes for each additional inch. For knives or thin blades, a soak time of 5-10 minutes (or up to 20 minutes for optimal results) is often recommended after the blades become non-magnetic.
O1 tool steel is an oil-hardening steel and should be quenched in warm oil, ideally at a temperature of 125-200°F (51-93°C), with some sources recommending 130°F or 149-204°C (300-400°F). It’s crucial to remove the part from the oil before it cools to ambient temperature.
Tempering O1 tool steel should occur immediately after quenching. The typical tempering range is 350-400°F (177-204°C), though ranges from 100°C to 450°F are mentioned depending on desired hardness. The steel should be held at a temperature for 1 hour per inch of thickness, with a minimum of 2 hours. Double tempering is sometimes preferred.
Annealing is a heat treatment process that makes the steel soft and machinable. It is necessary after hot working (such as forging) and before rehardening. New O1 tool steel stock is typically supplied in the annealed condition.
To anneal O1 tool steel, heat slowly at a rate not exceeding 400°F (222°C) per hour to 1425-1450°F (774-816°C). Hold at this temperature for 1 hour per inch of maximum thickness (minimum 2 hours). Then, cool slowly in the furnace at a rate not exceeding 50°F (28°C) per hour to 900-1000°F (482-538°C), and continue cooling to ambient temperature in the furnace or air. The resulting hardness should be a maximum of 212-229 Brinell.
Yes, O1 tool steel is somewhat prone to quench cracking, especially if there are significant changes in section thickness or sharp internal corners. Warping issues, particularly with thin blades, are also common. Overheating or heating too quickly can cause cracks and large grain size.
Yes, O1 tool steel is considered a good, versatile, and economical choice. It offers a balance of properties, including good hardness, wear resistance, and sufficient toughness for a wide range of tooling applications. It’s widely available and has excellent machinability.
O1 tool steel can be easily hardened to 62-63 Rockwell C (HRC). Its typical working hardness is around 58-60 HRC. When oil quenched from the proper hardening temperature, it can achieve 64-65 HRC as-quenched.
Yes, O1 tool steel is magnetic. As a tool steel, it is primarily an iron-based alloy with alloying elements, and typically, iron-based steels are ferromagnetic (magnetic) unless they are specifically austenitic stainless steels. O1 is not stainless steel.
Yes, O1 steel can rust. It is a tool steel, not a stainless steel, and contains relatively low chromium content (0.40–0.60%) compared to the minimum 10.5% chromium required for stainless steels. Therefore, it is susceptible to corrosion and will rust if not protected in corrosive environments.
No, O1 tool steel is an oil-hardening steel and is primarily quenched in oil. Water quenching is a more severe process, and O1 is already susceptible to cracking from thermal shock during oil quenching. Using water would significantly increase the risk of quench cracks and distortion.
Looking for Premium O1 Tool Steel?
At Aobo Steel, we leverage over 20 years of specialized forging experience to deliver top-tier O1 tool steel, precisely tailored to your application needs. Our expert team is dedicated to helping you find the optimal material solution.
Ready to enhance your project? Fill out the form below to connect with us for a personalized quote or expert consultation.