H13 Steel Heat Treatment Guide
H13 tool steel is a hot-work tool steel containing 5% chromium (Cr). Its equivalent grades are N 1.2344, X40CrMoV5-1, or JIS SKD61. It is widely used in the manufacture of die-casting molds, hot-forging dies, and hot-extrusion tools. H13 exhibits excellent red hardness, high wear resistance, and superior resistance to thermal cracking. These outstanding properties must […]