M2 Tool Steel Heat Treatment Guide
The heat treatment of M2 steel plays a significant role in its excellent performance as a cutting tool. The heat treatment of M2 involves transforming the fully annealed microstructure (primarily composed of ferrite and alloy carbides) into a quenched and tempered martensitic microstructure containing carbides, thereby achieving the desired cutting tool properties. This process typically […]