7CrSiMnMoV tool steel, often referred to as CH-1 steel, is a standout low-alloy cold work die steel that’s earned its reputation in the industry for its exceptional qualities. What makes it special? It’s particularly well-suited for flame hardening, offering excellent hardenability, a broad quenching temperature range, and a low tendency to overheat. This means it remains stable during heat treatment with minimal deformation—a significant advantage for manufacturers seeking reliability and precision.
1. 7CrSiMnMoV tool steel Chemical Composition
- Carbon (C): 0.65 – 0.75%
- Silicon (Si): 0.85 – 1.15%
- Manganese (Mn): 0.65 – 1.05%
- Phosphorus (P): ≤ 0,030%
- Sulfur (S): ≤ 0,030%
- Chromium (Cr): 0.90 – 1.20%
- Molybdenum (Mo): 0.20 – 0.50%
- Vanadium (V): 0.15 – 0.30%
This mix is what gives the steel its strength, toughness, and wear resistance, making it perfect for heavy-duty applications.
2. 7CrSiMnMoV tool steel Applications
This steel is a real workhorse, finding its way into a wide range of tools and dies. Here’s where it shines:
- Large insert dies and blanking dies
- Punches and forming dies
- Deep drawing dies and cold stamping dies
- Specialized molds like bakelite and clay molds
- Cutting tools such as shear blades and paper cutting knives
- Industrial components, including rollers and machine tool guide strips
It’s also a go-to for large dies, like those used for automotive outer panels and cold-bending dies. In fact, it outperforms other steels, such as GCr15 and Cr12MoV, in terms of tool lifespan for piercing and blanking tasks. Plus, it’s handy as inserts in big stamping dies, where localized hardening simplifies production.
3. 7CrSiMnMoV tool steel Heat Treatment Processes
To achieve the best results with 7CrSiMnMoV steel, heat treatment is crucial. Here’s how it’s done:
3.1 Forging
Start by heating the steel billets to 1100-1200°C, then finish at 800-850°C, and let them cool slowly. A preheat to 800-900°C ensures everything heats evenly, setting the stage for a solid result.
3.2 Pre-heat Treatment
- Normalizing: Heat it to 840-860°C to refine the grain structure, clear out network carbides, and make it easier to machine.
- Isothermal Annealing: Heat to 820-840°C, hold for several hours, then cool slowly to approximately 680-700°C before finishing with air cooling. Both methods hit a hardness of 217-241 HBW.
3.3 Quenching
This is where the steel gets tough. Heat it to 860-920°C and cool it fast—oil or air works. Oil quenching at 860°C can achieve a hardness of 62 HRC, while air cooling reaches 59 HRC. Even in an 80mm sample, you’ll still achieve 60 HRC at 30mm depth, showcasing its impressive hardenability.
3.4 Tempering
After quenching, temper at 160-200°C to fine-tune the balance between hardness and toughness, achieving a hardness of 58-62 HRC. For smaller parts, self-tempering may be the solution.
3.5 Surface Hardening Treatments
Flame hardening is a game-changer here—preheat the mold to 180-200°C, then heat it to 900-1000°C and air cool. It’s perfect for boosting die lifespan, especially in automotive uses. Another option? Vanadium diffusion treatment in a borax bath, creating a 10-15 μm layer with a hardness of 2820-3010 HV for top-notch wear resistance.
4. Physical Properties
Here’s a quick look at what makes this steel tick:
- Critical Temperatures: Ac1: ~776°C, Ac3: ~834°C, Ar1: ~694°C, Ar3: ~732°C, Ms: ~211°C
- Linear Expansion Coefficient: Ranges from 12.7 × 10^ (- 6)/°C (11-100°C) to 14.3 × 10^ (- 6)/°C (11-500°C), varying with temperature.
These stats help predict how it’ll handle heat and stress on the job.
5. Conclusion
When it comes to cold work dies and tools, 7CrSiMnMoV steel is a standout choice. Its blend of high hardness, great wear resistance, and solid toughness—plus that flame-hardening edge—makes it a favorite for everything from automotive dies to precision cutting tools. With the right heat treatment, this steel delivers performance and durability that manufacturers can count on.
Explore Our Other Products
D2/1.2379/SKD11
D3/1.2080/SKD1
D6/1.2436/SKD2
A2/1.23663/SKD12
O1/1.2510/SKS3
O2/1.2842
S1/1.2550
S7/1.2355
DC53
H13/1.2344/SKD61
H11/1.2343/SKD6
H21/1.2581/SKD7
L6/1.2714/SKT4
M2/1.3343/SKH51
M35/1.3243/SKH55
M42/1.3247/SKH59
P20/1.2311
P20+Ni/1.2738
420/1.2083/2Cr13
422 stainless steel
52100 bearing steel
440C stainless steel
4140/42CrMo4/SCM440
4340/34CrNiMo6/1.6582
4130
5140/42Cr4/SCR440
SCM415
🔥 Special Offer for 7CrSiMnMoV Tool Steel Inquiries
Looking for a reliable supplier of 7CrSiMnMoV tool steel?
Aobo Steel is here to support your production with premium-quality steel and professional service.
✅ Free Technical Consultation – Not sure if 7CrSiMnMoV fits your application? Our experts will help you choose the right grade.
✅ Fast Quote Within 12 Hours – Time is money. Send your inquiry now and receive a complete quote with price, lead time, and mill test certificate – fast.
✅ Mill-Direct Pricing – Save your cost by buying directly from a trusted manufacturer with 20+ years of forging experience.
✅ MOQ as Low as 1 Piece – Testing? Small batch production? No problem.
✅ Available Stock & Fast Delivery – Common sizes are ready to ship.