Aobo Steel 1.2436 Tool Steel for Sale

Aobo Steel supply 1.2436 tool steel for your project

For businesses seeking a dependable 1.2436 tool steel supplier, Aobo Steel offers a comprehensive range of solutions. If you are looking for high wear resistance in tool steel, then 1.2436 steel is an excellent choice. Specifically, 1.2436 steel is a chromium-rich, cold-work tool steel engineered for extreme durability. In fact, this high-carbon steel provides 3-4 times the wear resistance of typical low-alloy steel. Furthermore, it offers excellent hardness, toughness, and dimensional stability, making it ideal for demanding tooling applications.

1.2436 tool steel
1.2436 steel

Applications

Extrusion Dies
gripper dies
stamping dies

1.2436 tool steel is widely used, especially to make cold work molds with large cross-sections and complex shapes. These molds are often subjected to significant impact forces and require high wear resistance. Applications include silicon steel punching dies, thread rolling dies, and drawing dies.

  •  1.2436 is primarily suitable for medium-load stamping dies. It excels at punching stainless steel, copper, silicon, and aluminum.  
  •  1.2436 is commonly used for stainless steel and silicon steel sheet stamping dies under medium load. It is also effective for deep cup part stamping dies.

Cold Forming Tools: Aobo Steel – 1.2436 Steel Supplier

For robust cold-forming tools, rely on Aobo Steel, your 1.2436 steel supplier. 1.2436 steel provides high compressive strength for demanding forming operations. Select Aobo Steel, the 1.2436 tool steel supplier, for reliable forming tools.

1.2436 steel overview

Chemical composition

C (Carbon)Si (Silicon)Mn (Manganese)P (Phosphorus)S (Sulfur)Cr (Chromium)W (Tungsten)
2.00% – 2.25%0.10% – 0.40%0.15% – 0.45%≤0.030%≤0.030%11.0% – 12.0%0.60% – 0.80%

 

Heat treatment

1. Soft Annealing

Purpose: Reduce hardness and improve machinability.

  • Heating temperature: 780-820°C

  • Holding time: 2-4 hours (depending on workpiece size)

  • Cooling method: Furnace cool to 500°C, then air cool

  • Hardness after annealing: ≤ 229 HB

2. Quenching

Purpose: Achieve high hardness and wear resistance.

  • Preheating temperature: 600-650°C (to reduce thermal stress)

  • Austenitizing temperature: 950-980°C

  • Holding time: 30 minutes per 25mm (workpiece thickness)

  • Cooling medium: Oil or air

  • Hardness after quenching: 62-64 HRC

3. Tempering

Purpose: Relieve quenching stress and improve toughness.

  • Tempering temperature: Selected based on target hardness (see table below)

  • Holding time: 2 hours per 25mm (workpiece thickness)

  • Cooling method: Air cooling

Tempering Temperature (°C)Hardness (HRC)Application
150-20060-62High wear resistance
200-30058-60Balanced wear resistance and toughness
300-40055-58High toughness

Deep Drawing Tools: Aobo Steel – 1.2436 Supplier

Consider Aobo Steel, a dependable supplier of 1.2436 steel for demanding deep drawing tools. This steel is tough and wear-resistant for deep drawing applications—partner with Aobo Steel for durable tooling.