In-depth study of D2 Steel Composition
D2 tool steel is a prominent high-carbon, high-chromium cold-work tool steel, widely recognized for its excellent wear resistance and dimensional stability. It is a standard against which other tool steels are often measured for abrasion resistance. D2 steel is primarily applied in long-run cold-work tooling such as blanking, cold forming, drawing, lamination, and thread rolling […]