SKD1 tool steel is a high-carbon, high-chromium alloy widely used in manufacturing tools, dies, and molds. Known for its exceptional wear resistance, hardness, and toughness, SKD1 is a popular choice in industries that require materials capable of withstanding heavy loads and abrasive conditions. It belongs to the D3 steel family and is widely used in cold-working applications, making it suitable for tools that encounter intense friction and wear.

Most cost-effective, high-quality supplier of D2 steel

We offer both D2 electric furnace steel and D2 ESR steel. Considering our customers’ purchasing costs, we produce D2 round bars with diameters under 200mm using the electric furnace method, which can meet Ultrasonic testing (UT) Sep 1921-84 D/d flaw detection. Customers can purchase high-standard D2 round bars at a lower cost. We adopt the ESR process for diameters above 200mm to ensure that the internal structure can meet Ultrasonic testing (UT) Sep 1921-84 E/e flaw detection.

Excellent D2 Forged Steel Supplier

Aobo Steel has over 20 years of experience in forging D2 steel, giving us a deep practical understanding of quality control in this field. Our D2 forged steel products mainly come in round bar, plate, and block shapes. We have over 40 suppliers providing the best processing services, enabling us to offer advantages such as short lead times, stable quality, and competitive prices.

我们如何保证质量

这是测试文本,单击 “编辑” 按钮更改此文本。

Suply Range

The shapes of steel that Aobo Steel produces include A2 tool round bars and A2 plates. 

ShapeSizeLengthSurface finishtolerance
round bardiameter 20mm-400mmlength 2500mm-5800mmblack0/+5mm
peeled0/+5mm
turned(machined)0/+2mm
platewidth*thickness 100mm-800mm*10mm-400mmlength 2500mm-5800mmblack0/+5mm
peeled0/+5mm
turned(machined)0/+2mm

SKD1 steel Chemical Composition

ElementComposition (%)
Carbon (C)1.40 – 1.60
Chromium (Cr)11.00 – 13.00
Manganese (Mn)0.20 – 0.40
Silicon (Si)0.10 – 0.40
Vanadium (V)0.15 max
Phosphorus (P)≤ 0.030
Sulfur (S)≤ 0.030

Equivalent Grades

StandardEquivalent Grade
AISI (USA)D3
DIN (Germany)1.2080
GB (China)Cr12

Physical Properties

PropertyValue
Density7.75 g/cm³
Thermal Conductivity20.0 W/m·K
Hardness (After Heat Treatment)58 – 64 HRC
Tensile Strength950 – 1200 MPa
Modulus of Elasticity210 GPa

SKD1 heat treatment

ProcessTemperature RangePurposeCooling Method
Annealing800°C – 850°C (1472°F – 1562°F)Relieves internal stresses and improves machinabilitySlow cooling in the furnace
Hardening950°C – 1000°C (1742°F – 1832°F)Increases hardness and wear resistanceOil or air quenching
Tempering150°C – 250°C (302°F – 482°F)Reduces brittleness and improves toughnessAir cooling

1.2080 Applications

1. Cold-Working Dies:
SKD1 is widely used for cold-working tools such as stamping dies, shear blades, and punches that require wear resistance.

2. Molds and Dies:
The tool steel’s high hardness and wear resistance make it an excellent material for injection molds and die-casting tools.

3. Shear Blades:
SKD1’s wear resistance ensures a long service life for shear blades used to cut metal sheets and other hard materials.

4. Cold-Working Tools:
SKD1 is suitable for use in cold-pressing and forming tools, where high impact resistance and hardness are required.

Why should you choose Aobo Steel as your tool steel supplier?

At Aobo Steel, we pride ourselves on our exceptional supply capacity and dedication to meeting customer demands. Our monthly shipments exceed 1,500 tons in the Chinese market, reflecting our robust production and delivery capabilities. With a strong network of over 40 trusted suppliers, we ensure a steady supply of high-quality tool steels to meet various industry needs.

To provide even greater flexibility, we maintain stock for select products, allowing us to fulfill urgent orders quickly. Additionally, we specialize in fully customizable solutions, tailoring our products to your exact specifications for optimal application performance.

Our strategic location near the Yangtze River gives us a significant advantage in export logistics, enabling fast and cost-effective shipping to customers worldwide. Whether you need standard products or custom orders, Aobo Steel is committed to delivering reliability, quality, and service excellence.

At Aobo Steel, quality control is at the heart of our operations. Our dedicated testing team with over 20 years of experience ensures every product meets the highest standards before leaving our facility. Our comprehensive quality assurance process includes chemical composition analysis, metallographic examination, hardness testing, physical performance evaluation, and ultrasonic testing (UT) to detect internal defects.

To guarantee reliability, we perform 100% quality inspection on all products before shipment, ensuring they meet the required specifications and industry standards. Additionally, we support third-party inspections upon request to provide our customers with extra confidence in the quality of our materials. With this rigorous approach, Aobo Steel consistently delivers tool steels that offer superior performance and dependability in various applications.

At Aobo Steel, our service capacity is designed to meet diverse customer needs efficiently and precisely. We provide fully customizable products, offering surface treatments, descaling, and custom-length cutting options to suit specific requirements. Our experienced foreign trade team is well-versed in handling international orders, ensuring smooth communication and seamless transactions.

To provide the best service, we guarantee a 24-hour rapid response to all inquiries, allowing us to address your needs promptly and effectively. At Aobo Steel, we are committed to delivering high-quality tool steels and exceptional customer service to support your success.

FAQs

en_USEnglish