AISI 1075 Carbon Steel Technical Overview
AISI 1075 carbon steel is a high-carbon steel grade valued for its specific properties, which can be achieved through heat treatment. Understanding its composition and characteristics is key to leveraging its application capabilities.

1. Chemical Composition
1075 steel falls squarely into the high-carbon steel category, which typically encompasses steels with carbon content ranging from 0.60% to 2.40%.
The standard chemical composition for 1075 grade steel, identified by UNS Number G10750 and specified under SAE J403, is as follows:
- Carbon (C): 0.70% – 0.80%
- Manganese (Mn): 0.50% – 0.80%
- Phosphorus (P): 0.040% maximum
- Sulfur (S): 0.050% maximum
Note: Related carbon tool steel specifications may list tighter maximum limits for Phosphorus and Sulfur (e.g., 0.03%).
2. Hardness
The significant carbon content allows 1075 steel to achieve substantial hardness levels when properly hardened. Steels with carbon levels around this range (approx. 0.83%) can reach hardness values up to Rockwell C 67 (RC 67). This high hardness potential makes 1075 suitable for applications demanding excellent wear resistance.
3. Heat Treatment
Its composition makes 1075 sensitive to thermal processing. It is a candidate for various hardening techniques, including induction hardening, particularly for applications requiring localized hardness on the steel surface. Careful control during heat treatment is necessary to achieve the desired properties.
4. Machinability and Applications
The high hardness achievable with 1075 steel makes it a common choice for tooling and components requiring durability.
Regarding machining, reference data suggests specific parameters for operations like turning with high-speed steel (HSS) tools. For AISI 1075, a suggested speed is 30 surface feet per minute (SFM), with a feed rate of 0.0115 inches per revolution (ipr) and a depth of cut of 0.075 inches for medium operations.
5. Equivalent Steel Grade
For international comparison, a closely corresponding European standard is available:
- EN Standard: EN 10132-4:2000
- Grade: C75S
- Steel Number: 1.1248
FAQs
1. Is 1075 a good knife steel?
1075 steel can indeed be a good knife steel, particularly where high edge retention is a primary concern and the application does not subject the blade to extreme wear or highly corrosive environments.
2. Is 1075 better than 1095?
If maximum hardness and wear resistance are paramount and brittleness is acceptable, 1095 might be preferred. If a better combination of hardness and toughness is needed, 1075 could be a more appropriate selection.
3. Can you quench 1075 in water?
From a metallurgical standpoint, 1075 steel can be quenched in water. As a high-carbon steel, with a nominal carbon content in the range of 0.70-0.80%, it possesses the requisite carbon percentage to undergo martensitic transformation when subjected to rapid cooling from its austenitizing temperature. This transformation is the fundamental mechanism by which we achieve the desired hardness in such steel grades.
Explore Our Other Products
D2/1.2379/SKD11
D3/1.2080/SKD1
D6/1.2436/SKD2
A2/1.23663/SKD12
O1/1.2510/SKS3
O2/1.2842
S1/1.2550
S7/1.2355
DC53
H13/1.2344/SKD61
H11/1.2343/SKD6
H21/1.2581/SKD7
L6/1.2714/SKT4
M2/1.3343/SKH51
M35/1.3243/SKH55
M42/1.3247/SKH59
P20/1.2311
P20+Ni/1.2738
420/1.2083/2Cr13
422 stainless steel
52100 bearing steel
440C stainless steel
4140/42CrMo4/SCM440
4340/34CrNiMo6/1.6582
4130
5140/42Cr4/SCR440
SCM415
🔥 Need 1075 Carbon Steel Fast? Let Aobo Steel Handle It
Get a free quote within 12 hours — plus expert guidance on grades, sizes, and heat treatment options.
✅ Precision-cut to your required dimensions
✅ Competitive prices direct from the manufacturer
✅ Worldwide shipping available