H11 vs H13 steel: everythig you should know

H11 vs H13 steel: H11 tool steel and H13 tool steel are both hot-work tool steels. They belong to the H series of the American Society for Testing and Materials (ASTM) system.

H11 and H13 are representative of hot work tool steels. They offer a good balance of cost and performance, making them a reference point for various applications in hot-forming molds. These materials were initially developed for die casting and exhibit high hardenability, minimal deformation during heat treatment, minimal oxidation tendency, good tempering performance, resistance to liquid aluminum corrosion, and high resistance to thermal fatigue. Their heat treatment is as follows: please reference H11 steel heat treatment and H13 steel heat treatment.

The primary difference between H11 and H13 steel is that H13 contains approximately 0.5% more vanadium. This additional vanadium content further increases hot hardness and resistance to tempering, but it may also slightly reduce toughness, especially during quenching and tempering.

H13 is slightly more resistant to softening after heat treatment, but its toughness is slightly lower. Compared to H11, H13 may tend to have an uneven distribution of vanadium carbides. This is especially important under homogenization manufacturing conditions to maximize toughness.

This article compares H11 and H13 based on specific data. Some of the data is sourced from literature and has been cited accordingly.


Chemical composition of H11 and H13

AISI TypeUNS No.C (%)Mn (%)Si (%)Cr (%)Ni (%)Mo (%)V (%)
H11T208110.33-0.430.20-0.500.80-1.204.75-5.500.30 max1.10-1.600.30-0.60
H13 steel compositionT208130.32-0.450.20-0.500.80-1.204.75-5.500.30 max1.10-1.750.80-1.20

Major Factors comparison of H11 and H13 tool steel

comparison of H11 AND H13 TOOL STEEL
  • Wear Resistance: H11 and H13 have the same value of 3.
  • Toughness: Both have a value of 9, suggesting high toughness for both types.
  • Hot Hardness: Both have the same value of 6, indicating similar hot hardness properties.

Based on this table, H11 and H13 appear to have very similar properties in wear resistance, toughness, and hot hardness.


Comparison of manufacturing factors for H11 and H13 tool steels

comparison of manufacturing factors for H11 AND H13 TOOL STEEL
  • Availability: Both H11 and H13 tool steel have an availability rating of 4, suggesting they are equally available.
  • Cost: Both types of steel have a cost rating of 1, indicating they are similarly priced.
  • Machinability: Both H11 and H13 have a machinability rating of 8, suggesting they are both relatively easy to machine.

The table shows that H11 and H13 tool steel are similar regarding these three manufacturing factors.


Comparison of other parameters

FactorH11 tool steelsH13 tool steels
Usual Working Hardness, HRC38-5540-53(H13 steel hardness)
Depth of HardeningDD
Finest Grain Size at Full Hardness, Shepherd Standard88
Surface Hardness as-Quenched, HRC53-5551-54
Core Hardness (25 mm, or 1 in., diam round), HRC53-5551-54
Quenching MediumAA
Hardening Temperature, °C (°F)995-1025 (1825-1875)995-1040 (1825-1900)
Dimensional Change on HardeningLL
Safety on HardeningHH
Susceptibility to DecarburizationHH
Approximate Hardness as-Rolled or Forged, HB500500
Annealed Hardness, HB192-229192-229
Annealing Temperature, °C (°F)845-900 (1550-1650)845-900 (1550-1650)
Tempering Range, °C (°F)540-650 (1000-1200)540-650 (1000-1200)
Forging Temperature, °C (°F)1065-1150 (1950-2100)1065-1150 (1950-2100)

H11 and H13 tool steels share many similarities regarding their mechanical properties, heat treatment characteristics, and forging capabilities. The primary difference lies in their hardness range, with H13 offering slightly higher hardness for more demanding applications1. The choice between these two steels depends on the specific requirements of the intended application, such as the level of wear resistance, toughness, and dimensional stability needed.


Tensile Properties of H11 and H13 Tool Steels at Elevated Temperatures

Steel TypeTesting Temperature (°C)Testing Temperature (°F)Tensile Strength (MPa)Tensile Strength (ksi)Yield Strength (0.2% offset) (MPa)Yield Strength (0.2% offset) (ksi)Elongation (50 mm) (%)Reduction of Area (%)Room-Temperature Hardness (HRC) Before
testing 
Room-Temperature Hardness (HRC) After
testing 
H11RoomRoom180626214822151035.85050
1503001689245135819710.136.15050
260500160023213451959.834.55050
345650157922913171911035.25050
4258001510219128918711.438.75050
4809001427207114516612.238.95050
540100012411809651401135.45050
595110097914272410512.846.25047
6501200586854346318.966.65041
H132480900153122293752
54010001413205114352
59511001193173154952
6501200814118225952

Note:

  • The “-” in the Yield Strength columns for H13 steel indicates that the data was unavailable.
  • The Room-Temperature Hardness (HRC) column shows values before and after testing, separated by a comma.
  • Data from Teledyne VASCO. Allegheny Ludlum Industries, and Universal-Cyclops Steel Corp. 

CVN impact toughness of H11 and H13 tool steels as a function of testing temperature.

the relationship between testing temperature in Fahrenheit and Celsius, and impact strength in both Joules (J) and foot-pounds force (ft lbf) for two materials, H11 and H13

This graph suggests that H11 and H13 become more resistant to impact at higher temperatures. However, H13 is more sensitive to temperature changes, showing a more significant increase in impact strength with rising temperatures. 

  1. H13 tool steel applications. ↩︎
  2. H13 acél tulajdonságai. ↩︎

Get a Competitive Quote for H11 and H13 Tool Steel

With over 20 years of forging expertise, Aobo Steel is your trusted partner for high-performance H11 and H13 tool steel. We provide not just materials, but solutions. Leverage our deep industry knowledge and reliable supply chain for your project’s success.

✉ Contact us by filling out the form below.