H13 vs. H11 vs. H21: Choosing the Right Hot Work Tool Steel

Key Takeaways

  • H13, H11, and H21 steel are top choices for hot-working applications due to their unique properties and performance under extreme conditions.
  • H13 offers excellent wear resistance and is ideal for high-stress environments like die-casting molds and hot forging dies.
  • H11 is known for its toughness, ductility, and high strength, making it suitable for aerospace components and high-speed forging dies.
  • H21 excels in high temperatures, providing exceptional red hardness and softening resistance for hot extrusion and forging applications.
  • Choosing among H13, H11, and H21 steel depends on specific needs like wear resistance, toughness, and thermal hardness.

Estimated reading time: 9 minutes

Extreme temperatures and pressures encountered in hot-working applications, such as forging, die casting, and extrusion, pose significant challenges to tool steels, often leading to failure due to wear, plastic deformation, and thermal fatigue. Selecting tool steel that maintains performance under severe conditions and prevents premature failure is crucial for achieving efficient and cost-effective production. Within the AISI H-series hot-work tool steels, H11, H13, and H21 are popular choices for high-temperature applications. Though belonging to the hot-work steels, each exhibits distinct characteristics suited to different scenarios. This article aims to provide a clear and professional comparison of H11, H13, and H21, guiding readers in selecting the most cost-effective and high-performance material for their specific projects. It focuses on elucidating the critical balance between toughness, heat resistance (heat hardness), and cost.

What Are Hot Work Tool Steels

Hot-work tool steel is a material used for metal forming operations under high temperatures and pressures, such as forging, die casting, and extrusion. Its primary characteristics include exceptional thermal hardness (also known as red hardness or temper resistance), which is the ability to maintain high hardness and strength under high-temperature working conditions (typically ranging from 200°C to 600°C or higher, equivalent to 390°F to 1100°F). Furthermore, they must exhibit excellent toughness to resist mechanical and thermal shock, as well as high resistance to thermal fatigue, which manifests as heat checking (fine surface cracks) caused by repeated heating and cooling cycles.

The American Iron and Steel Institute (AISI) classifies tool steels into multiple categories, with the “H series” specifically referring to hot-work tool steels. AISI H11 and H13 are chromium-based hot work tool steels, offering balanced properties and broad applicability; whereas AISI H21 is a tungsten-based hot work tool steel. Compared to H11 and H13, H21 contains tungsten. These differences in chemical composition directly translate into variations in performance characteristics such as heat resistance and thermal shock resistance.

At a Glance: H13 vs. H11 vs. H21 Comparison Table

To facilitate a quick understanding of the distinct performance profiles, the table below provides a head-to-head technical comparison of AISI H13, H11, and H21 hot work tool steels, highlighting their primary characteristics, hot hardness, toughness, wear resistance, and typical applications.

FeatureH13 (Chromium-based)H11 (Chromium-based)H21 (Tungsten-based)
Primary AlloysCr, Mo, VCr, Mo, VW, Cr, V
Key CharacteristicsSecondary hardening; deep air-hardenable (low distortion); excellent resistance to heat, wear, and thermal fatigue; higher V contentSecondary hardening; deep air-hardenable (minimal stress/dimensional change); good ductility, fatigue, and thermal stability up to 540°C (1000°F); good weldabilityMaximum hot strength and resistance to softening; lower toughness; more prone to brittleness; requires higher hardening temperatures; susceptible to quench embrittlement
Hot Hardness / Temper ResistanceHigh; performs well up to 700°C (1300°F); superior to H11 at high temperatures/long exposureGood; resists softening up to 540°C (1000°F); less resistant than H21 at higher temperaturesVery High; superior resistance to high-temperature softening and erosion due to substantial W content
ToughnessGood overall; excellent impact strength; slightly lower fracture toughness than H11High; higher fracture toughness than H13; better resistance to brittle fracture than H19, H21Low to Medium; less ductile than H11; generally more brittle
Wear ResistanceVery Good/Excellent; higher than H11 due to V contentMediumMaximum hot strength and resistance to softening; lower toughness; more prone to brittleness; requires higher hardening temperatures; susceptible to quench embrittlement.
Typical ApplicationsDie casting (Al, Zn, Mg), hot forging/extrusion, plastic molds, hot shear blades, aerospace partsExtrusion dies (brass, bronze, steel, high-temp alloys), hot blanking/press dies, heavy-duty hot shear blades, and high thermal stress parts.Medium to High; suitable for high-temperature applications
Tool Steel Comparison Charts

Shock Resistance Comparison Chart

Based on “V” Notch Charpy Test Results

0 Ft. lbs. 0 Joules
25 Ft. lbs. 34 Joules
50 Ft. lbs. 68 Joules
75 Ft. lbs. 102 Joules
100 Ft. lbs. 135 Joules
H21
H13
H11

*Values are estimated based on typical ranges for visualization purposes.

Machinability Rating

Based on machinability rated against W1 at 100.

0
20
40
60
80
100
120
H21
H13
H11

*Values are estimated based on the provided chart for visualization purposes.

ASTMDINHardening Temp.As Quench (HRC)400°C (750°F)450°C (840°F)500°C (930°F)525°C (980°F)550°C (1020°F)600°C (1110°F)625°C (1160°F)
H111.23431010°C (1850°F)5553545454544641
H131.23441020°C (1870°F)5554545555534742
H211.25811100°C (2010°F)5049505152515048
Tempering diagrams for the most common hot work tool steels, showing hardness after two times tempering for 2 h. Data from brochures of traditional tool steel producers. (From Uddeholm Tooling, Technical catalogue for tool steels, Available online at: http://www.uddeholm.com/files/, Accessed December 2015; Böhler Edelstahl, Technical catalogue for tool steels, Available online at: http://www.bohler-edelstahl.com/english/1853_ENG_HTML.php, Accessed December 2015; Villares Metals, Technical catalogue for tool steels, Available online at: http://www.villaresmetals.com.br/pt/Produtos/Acos-Ferramenta,Accessed December 2015.)

How Alloying Elements Define Performance

Small differences in the chemical composition of hot work tool steels lead to significant variations in their performance characteristics, particularly concerning hot hardness, wear resistance, and toughness.

H13 (Chromium-Molybdenum-Vanadium): The All-Rounder

H13 steel typically contains about 0.38-0.45% Carbon, 4.75-5.50% Chromium, 1.10-1.75% Molybdenum, and 0.80-1.20% Vanadium. The key differentiator from H11 is its higher Vanadium content, which is usually around 1%. Vanadium promotes the formation of very hard, stable MC-type carbides, significantly increasing the steel’s wear resistance and, to a lesser extent, its hot hardness. This makes H13 well-suited for high-speed cutting, applications involving hard or scaly materials, and machining materials such as aluminum, stainless steels, and refractory metals, offering a good balance of properties for various hot-forming dies.

H11 (Chromium-Molybdenum): The Tough Specialist

H11 steel’s composition is similar to H13, typically containing 0.33-0.43% Carbon, 4.75-5.50% Chromium, 1.10-1.60% Molybdenum, but with a lower Vanadium content, usually 0.30-0.60%. This lower Vanadium content results in slightly less wear resistance compared to H13. However, H11 generally offers superior toughness and ductility. As an air-hardening steel, it exhibits minimal residual stress and dimensional changes after hardening. H11 maintains high strength and moderate toughness at elevated temperatures up to 540 °C (1000 °F) and is widely used for structural applications, particularly in aerospace technology.

H21 (Tungsten-Chromium): The High-Heat Champion

H21 steel is characterized by its high Tungsten content, typically 8.50-10.00%, along with 0.26-0.36% Carbon, 3.00-3.75% Chromium, and 0.30-0.60% Vanadium. Tungsten is the primary source of its exceptional red hardness. Tungsten forms very hard, stable carbides, making H21 highly resistant to softening at temperatures where H11 and H13 would significantly soften. This high alloy content also enhances resistance to “washing” (erosive wear). However, the high alloy content results in H21 having lower toughness than H11 and H13 steels. Therefore, H21 is suitable for applications requiring high resistance to softening at elevated temperatures but relatively lower toughness requirements.

Selection of Three Materials

When to Choose H13 Tool Steel

When to Choose H13 Tool Steel. H13 steel combines excellent red hardness, wear resistance, and superior resistance to thermal cracking, making it an ideal choice for high-stress, high-temperature environments. Primary applications include die-casting molds for aluminum, zinc, and magnesium alloys, as well as plastic injection molds (particularly suitable for high-precision parts like automotive lenses). ESR-refined H13 exhibits enhanced performance. It is also extensively used in hot forging dies, hot extrusion dies for aluminum, magnesium, and steel, hot rolling dies, hot stamping dies, fixture dies, mandrels, and hot shear blades. In aerospace and missile structures that demand ultra-high strength, it is employed for manufacturing structural components.

When to Choose H11 Tool Steel

H11 is particularly suitable for components that require high strength, ductility, toughness, fatigue resistance, and thermal stability within the temperature range of 75 to 540°C (167 to 1000°F). It is widely used in structural applications, especially in aerospace technology, including aircraft landing gear components, airframe parts, internal components of steam and gas turbines, fasteners, and springs. In mold manufacturing, H11 has proven successful for high-speed forging dies, hot extrusion dies, and die-casting molds for zinc, aluminum, and magnesium alloys, especially for long-term continuous operation. Even under sustained exposure to temperatures up to 540°C (1000°F), H11 maintains its toughness and ductility while effectively resisting softening.

When to Choose H21 Tool Steel

H21 is suitable for applications demanding exceptionally high thermal strength and resistance to softening. Typical uses include hot extrusion dies, hot press dies, dummy dies, hot forging drawing dies, hot shear blades, and hot punches for brass, bronze, and steel. This steel grade is also used in brass casting dies and mold components that are subjected to high thermal stress. H21 also finds application in forging steel and high-temperature alloys, as well as in billet shears and hot rolls for medium runs at medium temperatures.

Conclusion

When selecting among the three hot-work tool steels H13, H11, and H21, factors such as wear resistance, toughness, and thermal hardness must be considered based on specific application requirements. H13 stands as the versatile top choice, with its comprehensive properties suitable for a wide range of hot forming and plastic working tasks, including die casting molds and hot forging. H11 serves as the toughness-focused choice for high-impact applications, with its exceptional ductility proving invaluable in aerospace structural components and high-speed forging dies. When facing extreme temperature environments demanding stringent hardness retention, H21 maintains outstanding red hardness and resistance to softening at elevated temperatures.