D2 steel

AISI D2 / DIN 1.2379 / JIS SKD11

Highly wear-resistant cold work tool steel for stamping and shearing dies.

D3 tool steel

AISI D3 / DIN 1.2080 / JIS SKD1

Excellent wear resistance cold work tool steel for high hardness stamping and cutting tools.

A2 TOOL STEEL

AISI A2 / DIN 1.2363 / JIS SKD12

Good toughness and wear resistance cold work tool steel, suitable for medium speed stamping and forming dies.

o1 steel

AISI O1 / DIN 1.2510 / JIS SKS3

Oil-hardened cold work tool steel for tools, punches and shear edges

O2 tool steel

AISI O2 / DIN 1.2842 

High manganese oil hardened steel with good toughness for cold work molds and cutting tools.

H11 tool steel

AISI H11 / DIN 1.2343 / SKD6

Hot work tool steel, good heat fatigue resistance, suitable for forging and die casting molds.

h13 TOOL STEEL

AISI H13 / DIN 1.2344 / SKD61

High quality hot work tool steel, high temperature resistant, suitable for die casting molds.

S7 tool steel

S7 / DIN 1.2355

High impact toughness die steel for hot and cold work dies and heavy duty stamping tools.

1.2436 steel

DIN 1.2436

Highly wear-resistant cold work die steel for high precision stamping and shearing dies.

1.2714 steel

DIN 1.2714

Hot work die steel with high thermal shock resistance, suitable for forging and extrusion dies.

DC53 STEEL

DC53

High toughness cold work steel, widely used in precision stamping dies.

What is tool steel

Tool steels have good strength, toughness, hardness, wear resistance, and tempering stability. According to their different uses, tool steel can be divided into cutting edge, mold, and gauge steel. Depending on its chemical composition, tool steel can be divided into carbon, alloy, and high-speed steel.
High hardness and wear resistance are among the most important properties of tool steel. High wear resistance ensures and improves the tool life under the necessary conditions. In addition, different uses of tool steel have their own special performance requirements; for example, cutting edge steel also requires red hardness and a certain degree of strength and toughness, and gauge steel also requires high dimensional stability. High hardness, high wear resistance is one of the most important tool steel performance. High wear resistance ensures and improves the tool life under the necessary conditions. In addition, different uses of tool steel have their own special performance requirements; for example, cutting edge steel also requires red hardness and a certain degree of strength and toughness, and gauge steel also requires high dimensional stability.
Tool steel can be mainly used to manufacture various cutting, molding, and measuring tools.
The main properties of tool steel include hardness, wear resistance, strength, toughness, machinability, quenching temperature range, hardenability, decarburization sensitivity, heat treatment deformation, grinding, etc..

We have a more detailed article explaining tool steel. If you want more information, please click “What is tool steel?

 

Basic information of various tool steels offered by Aobo Steel

AISI D2 / DIN 1.2379 / JIS SKD11

Chemical composition

ElementCarbon (C)Chromium (Cr)Molybdenum (Mo)Vanadium (V)Silicon (Si)Manganese (Mn)Phosphorus (P)Sulfur (S)
D21.40 – 1.6011.00 – 13.000.70 – 1.200.50 – 1.100.10 – 0.600.10 – 0.600.030 max0.030 max
1.23791.40 – 1.6011.00 – 13.000.70 – 1.200.50 – 1.100.10 – 0.600.10 – 0.600.030 max0.030 max
SKD11 1.40 – 1.6011.00 – 13.000.80 – 1.200.2 – 0.5≤0.4≤0.6≤0.03≤0.03

Characteristics

Exceptional wear resistance and edge retention, ideal for cutting tools and dies requiring long-lasting sharpness.

Applications

Blanking and Forming Dies/Drawing Dies/Extrusion Dies/Roll Forming Rolls/Thread Rolling Dies/Long-Run Tooling/Gauges/Liners/ Wear Plates/Machine Parts/Shear Blades/Slitters/Knives


AISI D3 / DIN 1.2080 / JIS SKD1

Chemical composition

ElementCarbon (C)Chromium (Cr)Manganese (Mn)Silicon (Si)Phosphorus (P)Sulfur (S)
AISI D3 (%)1.50 – 2.3511.0 – 13.50.10 – 0.600.10 – 0.60Max 0.030Max 0.030
DIN 1.2080 (%)1.90 – 2.3511.0 – 13.50.15 – 0.600.10 – 0.60Max 0.030Max 0.030
JIS SKD1 (%)1.90 – 2.2011.0 – 13.00.20 – 0.600.10 – 0.60Max 0.030Max 0.030

Characteristics

D3 Offers extreme hardness and wear resistance, suited for applications demanding maximum abrasion resistance despite reduced toughness.

Applications

Cold work dies/Blanking and forming dies/Punches/Shear blades/Trimming dies/Gauges/Wear plates


AISI A2 / DIN 1.2363 / JIS SKD12

Chemical composition

ElementCarbon (C)Chromium (Cr)Molybdenum (Mo)Vanadium (V)Silicon (Si)Manganese (Mn)Phosphorus (P)Sulfur (S)
AISI A2 Steel 0.95 – 1.054.75 – 5.500.90 – 1.400.15 – 0.500.10 – 0.500.40 – 1.00≤0.03≤0.03
DIN 1.2363 Steel0.95 – 1.055.00 – 5.201.10 – 1.200.20.30.5N/AN/A
JIS SKD12 Steel 0.95 – 1.054.80 – 5.500.90 – 1.200.15 – 0.350.10 – 0.400.40 – 0.80≤0.030≤0.030

Characteristics

Combines good toughness with moderate wear resistance and minimal distortion during heat treatment, making it versatile for various tooling applications.

Applications

Cutting tools/Dies and molds/Knives and blades/Industrial shear blades/Gauges and precision instruments/Thread rolling dies/Stamping tools


AISI O1 / DIN 1.2510 / JIS SKS3

Chemical composition

ElementCarbon (C)Manganese (Mn)Silicon (Si)Chromium (Cr)Tungsten (W)Vanadium (V)Phosphorus (P)Sulfur (S)
AISI O1 (%)0.85 – 1.001.00 – 1.400.10 – 0.500.40 – 0.700.40 – 0.60Max 0.30Max 0.030Max 0.030
DIN 1.2510 (%)0.90 – 1.051.00 – 1.200.15 – 0.350.50 – 0.700.50 – 0.700.05 – 0.15Max 0.030Max 0.030
JIS SKS3 (%)0.90 – 1.000.90 – 1.20Max 0.350.50 – 1.000.50 – 1.00Max 0.030Max 0.030

Characteristics

Valued for its ease of machining and heat treatment, providing a balanced performance for general-purpose tools.

Applications

Cutting tools/Blanking dies/Forming dies/Gauges/Knives and blades/Punches/Jigs and fixtures


AISI O2 / DIN 1.2842 

Chemical composition

ElementCarbon (C)Manganese (Mn)Silicon (Si)Chromium (Cr)Vanadium (V)Phosphorus (P)Sulfur (S)
AISI O2 (%)0.85 – 0.951.40 – 1.80Max 0.50Max 0.35Max 0.30Max 0.030Max 0.030
DIN 1.2842 (%)0.85 – 0.951.80 – 2.200.10 – 0.400.20 – 0.500.05 – 0.20Max 0.030Max 0.030

Characteristics

Similar to O1 but with slightly enhanced wear resistance while maintaining good machinability and toughness.

Applications

Blanking dies/Forming dies/Punches/Trimming dies/Gauges/Shear blades/Precision tools


AISI H11 / DIN 1.2343 / JIS SKD6

Chemical composition

ElementCarbon (C)Chromium (Cr)Molybdenum (Mo)Vanadium (V)Silicon (Si)Manganese (Mn)Phosphorus (P)Sulfur (S)
AISI H11 (%)0.32 – 0.424.75 – 5.501.25 – 1.750.30 – 0.500.80 – 1.200.20 – 0.50Max 0.030Max 0.030
DIN 1.2343 (%)0.35 – 0.424.80 – 5.301.10 – 1.400.30 – 0.500.90 – 1.200.25 – 0.50Max 0.030Max 0.030
JIS SKD6 (%)0.30 – 0.404.50 – 5.501.00 – 1.500.20 – 0.500.25 – 1.000.20 – 0.50Max 0.030Max 0.030

Characteristics

Excels in hot-work applications due to its high toughness and resistance to thermal fatigue, ideal for forging and extrusion tools.

Applications

Hot forging dies/Extrusion dies/Die-casting tools/Hot shear blades/Mandrels/Punches/Aerospace components


AISI H13 / DIN 1.2344 / JIS SKD61

Chemical composition

ElementCarbon (C)Chromium (Cr)Molybdenum (Mo)Vanadium (V)Silicon (Si)Manganese (Mn)Phosphorus (P)Sulfur (S)
AISI H13 (%)0.32 – 0.454.75 – 5.501.10 – 1.750.80 – 1.200.80 – 1.200.20 – 0.50Max 0.030Max 0.030
DIN 1.2344 (%)0.37 – 0.434.80 – 5.501.10 – 1.400.85 – 1.150.90 – 1.200.25 – 0.50Max 0.030Max 0.030
JIS SKD61 (%)0.35 – 0.424.50 – 5.501.00 – 1.500.80 – 1.200.25 – 1.000.20 – 0.50Max 0.030Max 0.030

Characteristics

Preferred for high-temperature applications, offering superior heat resistance and thermal fatigue resistance for die-casting and forming tools.

Applications

Hot forging dies/Extrusion dies/Die-casting molds/Hot shear blades/Plastic injection molds/Mandrels/Aerospace structural components


S7 / DIN 1.2355

Chemical composition

ElementCarbon (C)Silicon (Si)Manganese (Mn)Chromium (Cr)Molybdenum (Mo)Vanadium (V)Phosphorus (P)Sulfur (S)
AISI S7 (%)0.45 – 0.550.20 – 0.400.20 – 0.903.00 – 3.501.30 – 1.600.20 – 0.30Max 0.030Max 0.030
DIN 1.2355 (%)0.45 – 0.550.20 – 0.400.30 – 0.503.00 – 3.501.30 – 1.600.20 – 0.30Max 0.030Max 0.030

Characteristics

Engineered for shock resistance, providing exceptional impact toughness for tools subjected to heavy loads or sudden blows.

Applications

Shock-resistant dies/Punches/Shear blades/Cold forging dies/Chisels/Pneumatic tools/Plastic molds


DIN 1.2436

Chemical composition

ElementCarbon (C)Chromium (Cr)Tungsten (W)Manganese (Mn)Silicon (Si)Phosphorus (P)Sulfur (S)
Percentage (%)2.00–2.25%11.00–12.00%0.60–0.80%0.20–0.40%0.10–0.40%≤ 0.03%≤ 0.03%

Characteristics

High hardness and wear resistance, ideal for demanding cold-work applications requiring extreme durability.

Applications

Cold work dies/Blanking dies/Punches/Trimming dies/Shear blades/Forming dies/Wear-resistant tools


DIN 1.2714

Chemical composition

ElementCarbon (C)Chromium (Cr)Molybdenum (Mo)Nickel (Ni)Silicon (Si)Manganese (Mn)Vanadium (V)Phosphorus (P)Sulfur (S)
Percentage (%)0.50 – 0.601.00 – 1.200.45 – 0.551.50 – 1.800.10 – 0.400.60 – 0.900.05 – 0.15Max 0.030Max 0.030

Characteristics

A robust hot-work steel with excellent toughness and heat resistance, suitable for forging dies and plastic molds.

Applications

Hot forging dies/Hot extrusion dies/Hammer dies/Plastic molds/Hot shear blades/Die inserts/Mandrels


DC53

Chemical composition

ElementCarbon (C)Chromium (Cr)Nickel (Ni)Molybdenum (Mo)Vanadium (V)Manganese (Mn)Silicon (Si)Phosphorus (P)Sulfur (S)
Percentage0.50–0.60%0.80–1.20%1.50–1.80%0.35–0.55%0.05–0.15%0.60–0.90%0.10–0.40%≤ 0.03%≤ 0.03%

Characteristics

Stands out for its unique blend of high toughness and wear resistance, often used as an advanced alternative to D2 in cold-work applications.

Applications

Precision stamping dies/Cold forging dies/Deep drawing dies/Thread rolling dies/Blanking dies/Punches/Shear blades

Why choose Aobo Steel as your tool steel supplier

Under the premise of ensuring quality, our prices are approximately 3% lower than the market price.

Before shipment, all goods undergo 100% strict component, UT, and hardness testing.

The goods are strictly reinforced during container loading to ensure safe sea transportation.

We are online 24 hours a day to answer any questions from customers at any time.

With over 20 years of experience in forged tool steel production, we have a deep understanding of our products.

We offer over 100 types of steel, including tool, alloy, stainless, alloy structural, and carbon steel.

We provide free cutting services.

With over 40 processing suppliers surrounding us, we can deliver more than 2,000 tons of steel monthly.

fr_FRFrançais