Aobo Steel supplies high-quality M35 steel for demanding tool and die manufacturers. As a high-speed tool steel, M35 offers excellent wear resistance, a balanced combination of toughness and hardness, and good machinability. Additionally, its cobalt content ensures outstanding hardness at high temperatures.

M35 high speed steel

 Applications

m35 steel cold forging dies

M35 steel can be used to manufacture various high-hardness and ultra-high-hardness saw blades, drills, taps, broaches, hobs, and various milling cutters.

ultra-high-hardness saw blades m35 steel

M35 is used for cold forging dies, deep drawing dies, cutting tools, etc.

drills-M35 STEEL

Recommended for use in cold stamping product industries such as watch case factories and screw factories.

Why Choose M35 Tool Steel?

Ideal for High-Speed Cutting:

Its red hardness ensures knives stay sharp during fast, demanding operations, minimizing downtime.

Ideal for Heavy-Duty Use:

High wear resistance and toughness make it perfect for drills, milling cutters, and rugged knives.

M35 steel overview

M35 steel composition

The M35 steel we provide fully meets the standard requirements. Due to its cobalt content, M35 steel has some special properties compared to other ordinary tool steels. Its composition table is as follows:

ElementCarbonChromiumMolybdenumTungstenVanadiumCobaltManganeseSilicon
Composition (%)0.80–0.903.75–4.504.50–5.505.50–6.751.75–2.204.50–5.500.20–0.450.20–0.45

Physical Properties

Density: Approximately 8.3-8.5 g/cm³

Melting Point: Approximately 1420-1450°C

Thermal Conductivity: Approximately 20-25 W/(m·K)

Thermal Expansion Coefficient: Approximately 11-13×10⁻⁶/°C

Elastic Modulus: Approximately 210-220 GPa

Mechanical Properties

m35 material hardness after heat treatment: HRC 65-67 (quenching + multiple tempering).

High-Temperature Hardness: At 600°C: Still maintains HRC 54-58 (cobalt improves red hardness).

Tensile Strength: Approximately 2000-2500 MPa

Toughness: Impact toughness is low (approximately 4-8 J/cm²),

Wear Resistance: Excellent, especially for high-speed cutting and processing of high-hardness materials (such as stainless steel and titanium alloys).

Compressive Strength: Approximately 3000-3500 MPa

Take the Next Step Today

Seamless performance, unmatched durability, and industry-leading results—M35 steel is your trusted partner in tooling excellence.

M35 steel equivalents DIN 1.3243 and JIS SKH55

M35 steel equivalent DIN 1.3243 and JIS SKH55 have similar compositions and properties in the German and Japanese steel systems.

Introduction to DIN 1.3243

1.3243 Chemical composition

Carbon (C)Silicon (Si)Manganese (Mn)Phosphorus (P)Sulfur (S)Chromium (Cr)Molybdenum (Mo)Tungsten (W)Vanadium (V)Cobalt (Co)
0.87 – 0.95≤ 0.45≤ 0.40≤ 0.03≤ 0.033.8 – 4.54.7 – 5.25.9 – 6.71.7 – 2.14.5 – 5.0

1.3243 steel Properties

PropertyValue
Density8.12 g/cm³
Hardness (HRC)60 – 64
Modulus of Elasticity210 GPa
Thermal Conductivity20.0 W/m·K
Specific Heat Capacity420 J/kg·K
Coefficient of Thermal Expansion11.0 × 10⁻⁶ /K (20 – 100°C)

Introduction to DIN 1.3243

SKH55 Chemical composition

CSiMnCrMoWVCo
0.85 ~ 0.95≤ 0.40≤ 0.403.8 ~ 4.54.6 ~ 5.55.7 ~ 6.71.7 ~ 2.24.5 ~ 5.5

SKH55 steel Properties

PropertyValue
Density8.12 g/cm³
Hardness (HRC)60 – 66
Modulus of Elasticity210 GPa
Thermal Conductivity20.0 W/m·K
Specific Heat Capacity420 J/kg·K
Coefficient of Thermal Expansion10.5 × 10⁻⁶ /K (20 – 100°C)

 