Customise Consent Preferences

We use cookies to help you navigate efficiently and perform certain functions. You will find detailed information about all cookies under each consent category below.

The cookies that are categorised as "Necessary" are stored on your browser as they are essential for enabling the basic functionalities of the site. ... 

Always Active

Necessary cookies are required to enable the basic features of this site, such as providing secure log-in or adjusting your consent preferences. These cookies do not store any personally identifiable data.

No cookies to display.

Functional cookies help perform certain functionalities like sharing the content of the website on social media platforms, collecting feedback, and other third-party features.

No cookies to display.

Analytical cookies are used to understand how visitors interact with the website. These cookies help provide information on metrics such as the number of visitors, bounce rate, traffic source, etc.

No cookies to display.

Performance cookies are used to understand and analyse the key performance indexes of the website which helps in delivering a better user experience for the visitors.

No cookies to display.

Advertisement cookies are used to provide visitors with customised advertisements based on the pages you visited previously and to analyse the effectiveness of the ad campaigns.

No cookies to display.

D2 tool steel FAQ

Here are the most frequently asked questions about D2 steel by our customers. We’ve gathered and organized them for your convenience. To learn more or to purchase D2 tool steel, please click here

D2 tool steel flat bar

1.Is D2 tool steel good for blades?

Yes, D2 tool steel can be a very good choice for certain types of blades. Let’s break down why.

D2 is a high-carbon, high-chromium tool steel known for its air-hardening properties. This means it hardens simply by cooling in air after heat treatment, which helps minimize distortion compared to steels needing oil or water quenching.

Key Strengths:

  • Excellent Wear Resistance: This is D2’s primary advantage. Thanks to its high carbon and chromium content, it forms hard carbides, making it highly resistant to abrasion and wear. If you need a blade that retains its edge for an extended period under abrasive conditions, D2 is a strong contender.

Considerations:

  • Moderate Toughness: While D2 excels in wear resistance, its toughness is moderate. It’s generally less demanding than other tool steels, such as those in the A-series or S-series. This means it might not be the best fit for blades that experience heavy impacts or shocks.

Common Blade Applications:

D2 is frequently used for:

  • Shear Blades: Especially for cutting thin to medium-thickness materials in high-volume production, where their wear resistance ensures long tool life.
  • Trimming Blades/Dies: Used in forging operations, often chosen over other grades like A2 for better longevity due to superior wear resistance.
  • Cropping Blades: A suitable application as well.

In simple terms, D2 is ideal for blades that require high wear resistance for extended production runs, such as shearing and trimming. However, if your blade needs to withstand significant impact, a tougher steel might be a better option.

Yes, D2 tool steel is considered difficult to sharpen compared to many other steels.

This characteristic is directly linked to one of D2’s main advantages: its excellent wear resistance. Here’s why:

  • Composition: D2 is a high-carbon (approx. 1.55%) and high-chromium (approx. 11.50%) air-hardening tool steel.
  • Microstructure: This specific composition results in a high volume of hard alloy carbides forming within the steel’s microstructure.
  • Wear Resistance: These hard carbides are precisely what give D2 its high resistance to abrasive wear, making tools last longer in demanding applications.
  • Sharpening Difficulty: Sharpening is fundamentally an abrasive process, removing material to form an edge. Since D2 strongly resists abrasion due to its hard carbides, grinding or sharpening it requires more effort and the proper techniques compared to steels with lower wear resistance.

In short, the same properties that make D2 highly durable and wear-resistant also make it more challenging to sharpen.

D2 steel provides excellent edge retention, as it remains sharp for an extended period due to its high wear resistance.

However, it’s a trade-off:

  • Toughness: It’s not as tough as some other tool steels. For heavy bushcraft tasks like chopping or prying, there’s a higher risk of chipping the blade compared to tougher steels.
  • Corrosion Resistance: It resists rust better than simple carbon steels, but it’s not stainless steel. It needs care to prevent rusting, especially in wet conditions.
  • Sharpening: It can be more challenging to sharpen than simpler steels.

Bottom Line: D2 is excellent if your primary concern is maintaining a very sharp edge for an extended period. However, be aware that it’s less durable and requires more care against rust than true stainless options. Choose based on what’s most important for your specific bushcraft needs.

No, D2 steel resists rust better than many other tool steels because it contains a high amount of chromium (11.5-12%). This chromium helps protect the surface.

However, D2 is designed for high wear resistance, not to be fully rust-proof like stainless steel. So, while it has good rust resistance for a tool steel, it can still rust if exposed to harsh conditions or if the surface is damaged. It’s more rust-resistant than low-chromium steels, but less resistant than true stainless steels.

Neither D2 nor D3 is simply “better.” The best choice depends on your specific needs. Both are high-carbon, high-chromium tool steels, but they balance properties differently.

Here’s the main difference in simple terms:

  • D3: Offers higher wear resistance but has lower toughness and is harder to heat treat without distortion (usually oil-hardened).
  • D2:Provides a great balance of very good wear resistance and better toughness. It’s also easier to heat treat with less distortion (air-hardening) and is more commonly available.

Choose D3 if: Your absolute top priority is maximum wear resistance, and you can accept lower toughness and manage the heat treatment risks.

Choose D2 if: You need a strong all-around performer with excellent wear resistance, good toughness, and more stable heat treatment.

Yes, D2 is considered a high-quality, high-performance tool steel. It’s a standard in the industry for many cold work applications.

Key Points about D2:

  • Very Wear Resistant:Its main advantage is excellent resistance to wear, making it great for long production runs.
  • Keeps its Shape:It has good dimensional stability during heat treatment.
  • Widely Used:You’ll find D2 used in many demanding cold work tools like blanking dies, forming dies, and shear blades.

While it offers a good balance of properties, its standout feature is wear resistance. It’s a reliable workhorse steel for tough jobs.

D2 steel is popular because it’s a tough, reliable choice for many tool-making needs, especially for tasks that don’t involve high heat (cold-work). Here’s why people choose it:

  • Lasts Long:It’s very resistant to wear and scraping because it has high amounts of carbon and chromium. Tools made from D2 keep their edge and shape longer.  
  • Holds Its Shape:When hardened, D2 doesn’t warp or change size much. This is important for making precise tools.  
  • Good All-Around: It works well with various tools, such as dies for cutting or shaping metal, and blades.  
  • Good Balance: It offers a good balance of wear resistance and toughness, providing resistance to chipping.  
  • Easy to Find & Fair Price: D2 is widely available and offers good value for its performance.  

Essentially, D2 offers a great combination of long life, stability, and versatility for many typical tooling applications.  

The hardness of D2 tool steel before heat treatment typically ranges from 217 to 255 HB. This is because it’s supplied in the annealed condition, making it soft enough for machining before we harden it up for its final use.

D2 steel holds a sharp edge for a very long time because it has excellent wear resistance. This is its main strength.

However, D2 is not as tough as some other steels. This means it’s more likely to chip or break if the knife hits something hard, like bone, or if it’s used for prying.

So, the answer is:

  • Yes, if your main need is a blade that stays extremely sharp for cutting.
  • Maybe not, if you need a knife that can handle impacts and rougher use without chipping.

It’s a trade-off between staying sharp (wear resistance) and resisting chips/breaks (toughness). D2 is also harder to sharpen and not stainless (though it resists rust better than basic carbon steels). You need to decide which quality is more important for your specific hunting needs.

For D2 tool steel, the generally recommended and preferred method is a high-temperature double temper, typically between 480°C and 516°C (900°F and 960°F). A common practice is using 515°C (960°F) for the first temper and 480°C (900°F) for the second.

Yes, D2 tool steel can be forged.

However, forging D2 is known to be difficult compared to simpler alloy steels. Its high chromium and high carbon content give it air-hardening properties, but also increase the risk of issues if not handled correctly during the process.

Success requires careful control, especially with temperature:

  1. Heating: Heat the D2 steel slowly and uniformly. Bringing it up to the correct forging temperature is critical. Avoid overheating. Follow the specific temperature range recommended for D2.
  2. Forging: Perform the forging within the recommended temperature range. Do not work the steel once it cools below the minimum forging temperature. D2 generally requires more force to forge than lower alloy steels.
  3. Cooling: After forging, slow cooling is essential. This minimizes internal stress and prevents cracking, which D2 is susceptible to if cooled too quickly. Furnace cooling or cooling in an insulating material is often necessary.

Incorrect heating, forging at the wrong temperature, or cooling too rapidly can lead to cracking or undesirable grain structures.

While D2 steel offers great wear resistance, it has some drawbacks:

  • Hard to Machine: Its high chromium and carbon content makes D2 difficult to machine and grind.
  • Less Tough: D2 isn’t as tough as some other tool steels (like A or S series). If toughness is key, another grade might be better.
  • Tricky Heat Treatment: D2 can be prone to cracking during quenching and may not hold dimensions perfectly over time due to its structure after heat treatment.
  • Difficult to Weld: Welding D2 is challenging due to its composition.
  • Directional Properties: D2’s strength can vary depending on the direction of the steel grain.
  • Needs Preheating: You must preheat D2 before forging or hardening to avoid cracking.

The “better” steel depends entirely on your needs. They are good for different things.

  • Choose D2 if:Your main goal is high wear resistance (it doesn’t wear down easily) for things like tools and dies. It keeps its shape well when hardened.  
  • Choose 440C if:You need corrosion resistance (it resists rust) along with good hardness. It’s a stainless steel.  

Simple Answer: D2 is tougher against wear. 440C is better against rust. Pick the one that matches the most important requirement for your specific job.

Yes, D2 steel must be hardened to function properly for its intended uses, such as making tools and dies. 

The process is straightforward:

  1. Heating:The steel is carefully heated in stages to prepare its internal structure for hardening.
  2. Air Cooling (Quenching):D2 is designed to be hardened by cooling it in the air. This process makes it hard but also brittle.
  3. Tempering:To reduce brittleness and increase toughness, the hardened steel is reheated (tempered). For D2, tempering twice (double tempering) is highly recommended for the best results.

Essentially, hardening unlocks the key properties that make D2 a reliable choice for demanding cold-work applications. Without this process, the steel won’t perform as expected.

Yes, D2 is often a good choice, especially if you want a lasting edge.

Here’s the simple breakdown:

1. Pros:

  • Holds an Edge:Its best feature is excellent wear resistance, meaning the blade stays sharp longer.
  • Hard:It gets very hard (up to ~63 HRC), which helps keep the edge sharp.

2. Cons:

  • Can Chip:It’s not the toughest steel. It might chip or break with hard impacts or bending.
  • Can Rust:It resists rust better than basic tool steels but isn’t truly stainless. You’ll need to keep it clean and dry.
  • Hard to Work With:Making things from D2 is difficult; it’s tough to machine, grind, and weld.

Bottom Line: D2 gives you great edge retention. Just be aware it’s less tough than some other steels and needs care to avoid rust. It’s a popular choice for many knives for good reason.