Selection of Steels for Shears
| Applications | Steel |
| For shock conditions, hot or cold shearing; hot shearing heavy sections | S2 |
| S5 | |
| S1 | |
| For shock conditions, hot or cold shearing, hot shearing heavy sections | H11 |
| A8 | |
| Cold-work shears for high production on thin or medium-thickness stock | O1 |
| A2 | |
| D2 | |
| Long-lift cold shears for thin or medium-thickness stock; highest wear resistance | M3 |
| M4 |
Comparison of data on abrasion resistance, toughness, and hot hardness of these materials