Cos'è l'acciaio per utensili

Che cos'è l'acciaio per utensili?

Definition of tool steel In terms of use, tool steel is the steel used to make various tools such as cutting tools, molds, and gauges. Among the various types of steel materials, tool steel was the first to be developed and utilized. In the early 1900s, most of the major tool steels were produced. Production-wise, compared […]

Che cos'è l'acciaio per utensili? Read More »

Negozi dei clienti

THE FOLLOWING STORIES OF OUR CLIENTS ARE ALL REAL. TO PROTECT THE PRIVACY OF OUR CLIENTS, WE HAVE REFRAINED FROM MENTIONING THEIR NAMES. Stories from an Indian client In 2017, we had the privilege of forming a partnership with one of India’s largest importers of tool steel, thanks to an introduction from one of our

Negozi dei clienti Read More »

D2 vs D3 tool steel

When choosing the right tool steel for your project, you may come across D2 and D3 tool steels. Both tool steels are high-carbon, high-chromium tool steels that are widely used in the tool and die industry for cold work tools such as cutting tools, dies and punches. They are classified as D series in the

D2 vs D3 tool steel Read More »

Apparecchiature ESR

cos'è la VES

In the tool steel industry, ESR means Electroslag Remelting. To improve quality, some steel grades undergo remelting processes, such as vacuum arc remelting (VAR) and electro-slag remelting (ESR). As molds become bigger and require more specialized features, the use of remelted steel has been growing. Compared to VAR, ESR offers several advantages. It is cheaper because it doesn’t

cos'è la VES Read More »

confronto tra l'acciaio per utensili h11 e h13

Acciaio per utensili H11 e H13

H11 tool steel and H13 tool steel are both hot work tool steels. They belong to the H series of the American Society for Testing and Materials (ASTM) system. H11 and H13 are representative of hot work tool steels. They offer a good balance of cost and performance, making them a reference point for various applications in hot-forming

Acciaio per utensili H11 e H13 Read More »

ACCIAIO UTENSILE D2

Acciaio per utensili D2 vs. A2

D2 tool steel and A2 tool steel are often used in industrial production. This article compares the data of the two steels so that the user can choose in practice. So, let’s look at the following article about D2 vs. A2 tool steel! D2 and A2 tool steel equivalent grades USA/ASTM USA/UNS Germany/DIN Germany/W-Nr. Japan/JIS ISO China/GB D2

Acciaio per utensili D2 vs. A2 Read More »

deep drawing die

Selection of drawing die steel

Drawing dies stretch and deform metal sheets between a punch and a die to produce a cup-shaped workpiece. Their effectiveness depends on excellent wear resistance and anti-seizure properties. In many applications, choosing the right tool steel is critical. For example, steels like D2, D3, H13, H11, 1.2379, 1.2080, 1.2343, or 1.2344 can achieve optimal performance.

Selection of drawing die steel Read More »