Cold Work Tool Steel Introduction
At present, the common cold work die steel in the world can be divided into three categories: (1) low alloy cold work die steel; (2) medium alloy cold work die steel; (3) high alloy cold work die steel. In addition, several new cold work die steels have also been developed as […]