Is 420 stainless steel good for knives

Yes, 420 stainless steel is widely regarded as a good material for knives and cutlery, particularly for general-purpose applications. 420 steel is a martensitic stainless steel characterized by its hardenability and magnetic properties. This steel grade typically contains 12-14% chromium and a carbon content of no less than 0.15%, though in actual production, a carbon content specification of 0.3-0.4% is commonly used. The high carbon content gives it high hardness and strength, characteristics that are ideal for knives.

In this article, we will discuss the advantages of using 420 stainless steel for knives from the perspective of its characteristics.

420 Stainless Steel Knives’ Strength

420 stainless steel can significantly improve its performance through heat treatment. After quenching, its hardness can reach 50-52 HRC, which is very high for knife applications. Its 0.2% yield strength can be as high as 200 ksi (1379 MPa), and its tensile strength can reach up to 250 ksi (1724 MPa). This high strength makes it suitable for applications requiring durable cutting edges.

420 Stainless Steel Knives’ Edge Retention and Wear Resistance

The ability of 420 stainless steel to achieve high hardness, especially with its chromium carbides, contributes to good wear resistance and the capacity to hold a sharp edge. The chromium carbides in 420 stainless steel give it excellent wear resistance and the ability to maintain a sharp edge. To improve wear resistance, steel grades with higher carbon content, more carbides, or greater hardness (such as the 440 series) can be designed, but 420 stainless steel still offers excellent performance.

Ductility and temper brittleness

After 420 stainless steel heat treatment, it exhibits significant ductility in its annealed state, and after tempering, it achieves a balance between hardness and ductility. Martensitic stainless steels, including 420 stainless steel, are susceptible to temper brittleness in the tempering temperature range of 800–1050°F (427–566°C).

Corrosion Resistance

420 stainless steel exhibits excellent corrosion resistance, particularly in the quenched state, and can withstand corrosion from water, alkaline, and mildly acidic media. If cleaned regularly, its corrosion resistance can be maintained at a high level. However, its corrosion resistance tends to decrease in the annealed state, and tempering in the 400-600°C range can lead to corrosion decay due to chromium carbide precipitation (sensitization1), which depletes chromium in the surrounding matrix. This sensitization can be “healed” by tempering above 600°C because of chromium diffusion, though this is less effective in high-carbon steels like 440 series.

Machinability

When properly annealed, 420 stainless steel has a machinability rating of 70, compared to a 1% carbon steel with a rating of 100. In comparison, stainless steels in general can be more difficult to machine than other metals due to their toughness and tendency to produce long, stringy chips. The specific structure of 420 stainless steel results in reasonably good chip breakage. This characteristic makes it easy to be machined when used as a knife.

Conclusion for Knife Use

420 stainless steel is a foundational choice for cutlery, including table knives, carving knives, pocket knives, and razors. Its ability to achieve high hardness, wear resistance, and good edge retention, combined with moderate corrosion resistance, makes it a practical and serviceable material for knife blades. Its widespread use in the cutlery industry since its discovery in 1913 by Harry Brearley further solidifies its position as a suitable material for knives. If you would like to purchase 420 steel or learn more about it, please feel free to contact us.

  1. Pramanik, A., & Basak, A. K. (Eds.). (2016). Stainless Steel: Microstructure, Mechanical Properties and Methods of Application (p. 125). Apple Academic Press.  ↩︎

Get a Competitive Quote for Premium 420 Stainless Steel

Leverage our 20+ years of forging expertise. We provide consistent, high-quality 420 stainless steel tailored to your exact specifications. Partner with an industry expert for reliable supply and service.

Ready to start? Fill out the form below to get a no-obligation quote from our specialists.