P20 Tool Steel in Plastic Molds and Die Casting Applications
P20 tool steel finds extensive application in mold manufacturing and die casting. This low-alloy steel is typically supplied in a pre-hardened state (hardness approximately 30-40 HRC), enabling direct machining into complex molds without additional high-temperature heat treatment, thereby minimizing deformation and dimensional changes. It offers excellent machinability, polishability, and wear resistance. Primary applications include plastic […]