Selection of Steels for Shears
Aobo steel for shears
We have the following products suitable for use in shears
Selection of Steels for Shears
Applications | Steel |
Cold shearing heavy stock; scrap shears; hot shears for moderate life | S2 |
S5 | |
S1 | |
For shock conditions; hot or cold shearing; hot shearing heavy sections | เอช11 |
A8 | |
Cold-work shears for high production on thin or medium-thickness stock | โอวัน |
เอ2 | |
ดีทู | |
Long-lift cold shears for thin or medium-thickness stock; highest wear resistance | M3 |
M4 |