Selection of Steels for Cold Extrusion

Aobo steel for Cold Extrusion

Among our products, the following are suitable for cold extrusion

h11 tool steel

AISI H11 / DIN 1.2344 / JIS SKD6

A2 TOOL STEEL

AISI O1 / DIN 1.2510 / JIS SKS3

M2 HIGH SPEED STEEL

AISI A2 / DIN 1.2363 / JIS SKD12

D2 steel

AISI D2 / DIN 1.2379 / JIS SKD11

1.2714 steel

AISI L6 / DIN 1.2714 / JIS SKT4

Cold extrusion process and steel selection

Cold extrusion is a process that deforms metal flow by stabilizing pressure. It is divided into forward and backward extrusion, of which cold impact extrusion is a special form. It requires a high steel compressive strength (hardness), often at the expense of toughness. Commonly used steels such as A2, D2, and M2 have low toughness (ratings 1-5), and the dies need to be prestressed and fitted with shrink rings made from H11 steel to increase durability. M2 steel provides longer mold life, while the more ductile H11 steel (ratings 6-9) is recommended for best results in difficult cases where cracking is a concern.

Cold Extrusion Tool Steel Recommendation Form

Table 1: Tool Steels for Cold Extrusion – Punches

SteelWear Resistance (Rating)Toughness (Rating)Working Hardness (HRC)
T159164-66
M49264-66
D48162-64
ดีทู8260-62

Table 2: Tool Steels for Cold Extrusion – Punch Shank or Mandrel

SteelWear Resistance (Rating)Toughness (Rating)Working Hardness (HRC)
เอ26556-58
S14356-58
S52856-58

Table 3: Tool Steels for Cold Extrusion – Die Insert

SteelWear Resistance (Rating)Toughness (Rating)Working Hardness (HRC)
T159165-67
M49264-66
D48162-64
M27364-65
ดีทู8260-62

Table 4: Tool Steels for Cold Extrusion – Die Base

SteelWear Resistance (Rating)Toughness (Rating)Working Hardness (HRC)
เอ26554-56
S14854-56
L63654-56
โอวัน4354-56

Table 5: Tool Steels for Cold Extrusion – Die Holder

SteelWear Resistance (Rating)Toughness (Rating)Working Hardness (HRC)
เอช113948-50

Table 6: Tool Steels for Cold Extrusion – Knockout Pin

SteelWear Resistance (Rating)Toughness (Rating)Working Hardness (HRC)
เอช113953-55
S52854-56
L63654-56
โอวัน4354-56
S14854-56

Table 7: Tool Steels for Cold Extrusion – Die Anvil

SteelWear Resistance (Rating)Toughness (Rating)Working Hardness (HRC)
M49260-62
ดีทู8258-60
เอ26558-60
โอวัน4358-60

Why choose us

  • With over 20 years of experience in forged tool steel production, we have a deep understanding of our products.
  • With over 40 processing suppliers surrounding us, we can deliver more than 2,000 tons of steel monthly.
  • Under the premise of ensuring quality, our prices are approximately 3% lower than the market price.
thไทย