{"id":9395,"date":"2025-08-03T00:45:36","date_gmt":"2025-08-02T16:45:36","guid":{"rendered":"https:\/\/aobosteel.com\/?page_id=9395"},"modified":"2026-11-01T22:37:30","modified_gmt":"2026-11-01T14:37:30","slug":"h11-tool-steel","status":"publish","type":"page","link":"https:\/\/aobosteel.com\/pt\/h11-tool-steel\/","title":{"rendered":"Fornecedor de a\u00e7o ferramenta H11 | Fabricante de a\u00e7o para trabalho a quente 1.2343 \/ SKD6 | Aobo Steel"},"content":{"rendered":"<style id=\"aobo-steel-rebuild\" data-noptimize=\"1\">\n\/* Rebuilt tool-steel page: banner is full-bleed, the body keeps the site's normal\n   content width. All layout rules live in this page, so a missing external\n   stylesheet can no longer collapse the page. *\/\n.ads2 *, .ads2 *::before, .ads2 *::after { box-sizing: border-box; }\n.ads2 { font-size: 16px; line-height: 1.75; color: #2b2b2b; }\n.ads2-hero { position: relative; width: 100vw !important; max-width: 100vw !important;\n  margin-left: calc(50% - 50vw) !important; margin-right: 0 !important;\n  min-height: 430px; display: flex; align-items: center; overflow: hidden; background: #1d1d1d; }\n.ads2-hero-img { position: absolute; inset: 0; width: 100%; height: 100%; object-fit: cover; }\n.ads2-hero-ov { position: absolute; inset: 0; background: #4e4b40; opacity: .5; }\n.ads2-hero-scrim { position: absolute; inset: 0;\n  background: linear-gradient(90deg, rgba(0,0,0,.42) 0%, rgba(0,0,0,.32) 45%, rgba(0,0,0,.16) 78%, rgba(0,0,0,.04) 100%); }\n.ads2-hero-in { position: relative; width: 100%; max-width: 1200px; margin: 0 auto; padding: 56px 24px; color: #fff; }\n.ads2-crumb, .ads2-crumb a, .ads2-crumb h6, .ads2-crumb mark { color: #dfe6ef !important; font-size: 13px;\n  text-decoration: none; letter-spacing: .2px; }\n.ads2-crumb h6 { display: inline; font-weight: 400; margin: 0; }\n.ads2-crumb a:hover { color: #fff !important; text-decoration: underline; }\n.ads2-tag { margin: 10px 0 6px; color: #eef1f5 !important; font-size: 14px; text-shadow: 0 1px 6px rgba(0,0,0,.8); }\n.ads2-h1 { margin: 0 0 12px; font-size: 40px; line-height: 1.2; font-weight: 800; color: #fff !important;\n  letter-spacing: -.2px; max-width: 900px; text-shadow: 0 2px 14px rgba(0,0,0,.85), 0 0 4px rgba(0,0,0,.55); }\n.ads2-sub { margin: 0 0 20px; font-size: 17px; color: #fff !important; text-shadow: 0 1px 8px rgba(0,0,0,.9), 0 0 3px rgba(0,0,0,.6); }\n.ads2-checks { list-style: none; margin: 0 0 26px; padding: 0; display: flex; flex-wrap: wrap; gap: 8px 22px; }\n.ads2-checks li { position: relative; margin: 0; padding-left: 20px; font-size: 15px; color: #fff !important;\n  text-shadow: 0 1px 6px rgba(0,0,0,.85); }\n.ads2-checks li::before { content: \"\\2713\"; position: absolute; left: 0; top: 0; color: #4ade80; font-weight: 700; }\n.ads2-cta { margin: 24px 0 6px; text-align: center; }\n.ads2-hero .ads2-cta { text-align: left; margin-top: 26px; }\n.ads2-btn { display: inline-block; background: #074fd0; color: #fff !important; font-weight: 400;\n  font-size: 16px; line-height: 16px; padding: 14px 30px; border-radius: 100px;\n  text-decoration: none !important; cursor: pointer; }\n.ads2-btn:hover { background: #063c9e; color: #fff !important; }\n.ads2-body { max-width: 1200px; margin: 0 auto; padding: 48px 24px 64px; }\n.ads2-sec { margin: 0 0 54px; }\n.ads2-sec:last-child { margin-bottom: 0; }\n.ads2 h2 { font-size: 27px; line-height: 1.3; color: #062a5a; font-weight: 700; margin: 0 0 20px;\n  padding-bottom: 12px; border-bottom: 1px solid #e6eaef; }\n.ads2 h3 { font-size: 21px; color: #062a5a; margin: 28px 0 12px; }\n.ads2 h4 { font-size: 18px; color: #062a5a; margin: 22px 0 10px; }\n.ads2 p { margin: 0 0 16px; }\n.ads2 a { color: #005fcf; text-decoration: none; }\n.ads2 a:hover { text-decoration: underline; }\n.ads2 ul, .ads2 ol { margin: 0 0 18px; padding-left: 22px; }\n.ads2 li { margin: 0 0 8px; }\n.ads2-cols2 { display: grid; grid-template-columns: 1fr 1fr; gap: 8px 40px; }\n.ads2-cols2 ul { margin-bottom: 0; }\n.ads2-row { display: grid; grid-template-columns: 1.05fr .95fr; gap: 36px; align-items: center; }\n.ads2-row-flip .ads2-col-i { order: -1; }\n.ads2-row .ads2-col-t > *:last-child { margin-bottom: 0; }\n.ads2-row .ads2-cta { margin-top: 16px; }\n.ads2-fig { margin: 0 0 22px; }\n.ads2-fig img { width: 100%; height: auto; display: block; }\n.ads2-gal { display: grid; grid-template-columns: repeat(3, 1fr); gap: 16px; margin: 0 0 22px; }\n.ads2-gal .ads2-fig { margin: 0; }\n.ads2-row .ads2-fig { margin: 0; }\n.ads2-tw { margin: 0 0 22px; overflow-x: auto; }\n.ads2-t { width: 100%; border-collapse: collapse; font-size: 15px; }\n.ads2-t td, .ads2-t th { border: 1px solid #e3e7ec; padding: 11px 14px; vertical-align: top; text-align: left; }\n.ads2-t.kv td:first-child { background: #f6f8fa; font-weight: 600; color: #062a5a; width: 34%; }\n.ads2-t.data { font-size: 14.5px; }\n.ads2-t.data td, .ads2-t.data th { padding: 9px 11px; }\n.ads2-t.data thead th, .ads2-t.data tr:first-child td { background: #eef3f9; font-weight: 700; color: #062a5a; }\n.ads2-t.data tbody tr:nth-child(odd) td { background: #fbfcfd; }\n@media (max-width: 1000px) {\n  .ads2-row { grid-template-columns: 1fr; gap: 22px; }\n  .ads2-row-flip .ads2-col-i { order: 0; }\n  .ads2-cols2 { grid-template-columns: 1fr; }\n  .ads2-h1 { font-size: 30px; }\n  .ads2-hero { min-height: 340px; }\n}\n@media (max-width: 700px) {\n  .ads2-gal { grid-template-columns: 1fr; }\n  .ads2-body { padding: 32px 18px 44px; }\n  .ads2-t { font-size: 14px; }\n  .ads2-t td, .ads2-t th { padding: 9px 10px; }\n  .ads2-t.kv td:first-child { width: 42%; }\n  .ads2-tw { -webkit-overflow-scrolling: touch; }\n}\n@media (max-width: 640px) {\n  .ads2-hero-in { padding: 34px 18px 38px; }\n  .ads2-h1 { font-size: 25px; }\n  .ads2 h2 { font-size: 22px; }\n  .ads2-tag { font-size: 13px; }\n  .ads2-sub { font-size: 15px; }\n  .ads2-checks { gap: 6px 16px; }\n  .ads2-checks li { font-size: 14px; }\n  .ads2-btn { padding: 12px 24px; font-size: 15px; }\n  .ads2-sec { margin-bottom: 40px; }\n}\n<\/style>\n<div class=\"ads2\">\n<section class=\"ads2-hero\">\n  <img class=\"ads2-hero-img\" src=\"https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/05\/banner3.webp\" sizes=\"100vw\" alt=\"Bulk tool steel bar stock in the Aobo Steel warehouse\" loading=\"eager\" decoding=\"async\">\n  <div class=\"ads2-hero-ov\"><\/div>\n  <div class=\"ads2-hero-scrim\"><\/div>\n  <div class=\"ads2-hero-in\">\n    <nav class=\"ads2-crumb\"><a href=\"https:\/\/aobosteel.com\/pt\/\">In\u00edcio <\/a>&gt; <a href=\"https:\/\/aobosteel.com\/pt\/tool-steels\/\">cat\u00e1logo de a\u00e7os para ferramentas <\/a>A\u00e7o ferramenta H11<\/nav>\n    <p class=\"ads2-tag\"><em>Aobo Steel | Fornecedor global de a\u00e7o para ferramentas na China<\/em><\/p>\n    <h1 class=\"ads2-h1\">A\u00e7o ferramenta AISI H11 | 1.2343 | A\u00e7o para trabalho a quente com cromo SKD6<\/h1>\n    <ul class=\"ads2-checks\">\n      <li>Garantia de qualidade com 100% de ensaio UT<\/li>\n      <li>SEP 1921-82 Classe D\/d Garantido<\/li>\n      <li>Entrega no Estado Recozido<\/li>\n      <li>Superf\u00edcie: Casca Preta, Torneada, Laminada a Quente ou Polida<\/li>\n    <\/ul>\n    <div class=\"ads2-cta popmake-16052\"><a class=\"ads2-btn\" href=\"#\">Consulta r\u00e1pida sobre o material H11<\/a><\/div>\n  <\/div>\n<\/section>\n<div class=\"ads2-body\">\n<section class=\"ads2-sec\">\n<p>H11 tool steel is an air-hardening hot work steel known for its excellent toughness, thermal strength, and resistance to thermal fatigue. It offers good wear resistance at medium temperatures, low heat-treatment distortion, and strong resistance to corrosion by molten aluminum. H11 is widely used in die casting, forging, extrusion, and plastic mold applications. It is designated as H11 (ASTM A681), with equivalent grades including <a href=\"https:\/\/aobosteel.com\/pt\/1-2343-tool-steel\/\">1.2343 (DIN)<\/a> and SKD6 (JIS).<\/p>\n<\/section>\n<section class=\"ads2-sec\">\n<h2>Vis\u00e3o geral do fornecimento de a\u00e7o ferramenta H11<\/h2>\n<div class=\"ads2-tw\"><table class=\"ads2-t kv\"><tbody><tr><td>Grau<\/td><td>AISI H11\/DIN 1.2343\/JIS SKD6<\/td><\/tr><tr><td>Condi\u00e7\u00f5es de entrega<\/td><td>Totalmente recozido (condi\u00e7\u00e3o macia para usinagem)<\/td><\/tr><tr><td>Formul\u00e1rios dispon\u00edveis<\/td><td>Barra redonda \/ Barra plana \/ Chapa \/ Bloco forjado<\/td><\/tr><tr><td>Capacidade de produ\u00e7\u00e3o mensal<\/td><td>Aprox. 1.200 toneladas m\u00e9tricas<\/td><\/tr><tr><td>Quantidade recomendada para exporta\u00e7\u00e3o<\/td><td>Cont\u00eainer 20GP completo (aproximadamente 26 toneladas)<\/td><\/tr><tr><td>MOQ<\/td><td>5 toneladas<\/td><\/tr><tr><td>Prazo de entrega (com estoque de lingotes)<\/td><td>Aproximadamente 20 dias<\/td><\/tr><tr><td>Prazo de entrega (derretido)<\/td><td>30 a 45 dias<\/td><\/tr><tr><td>Prazo de entrega (n\u00edvel ESR)<\/td><td>Aproximadamente 60 dias<\/td><\/tr><tr><td>Inspe\u00e7\u00e3o<\/td><td>Equipe interna de ultrassom + Inspe\u00e7\u00e3o por terceiros dispon\u00edvel<\/td><\/tr><tr><td>Documenta\u00e7\u00e3o<\/td><td>MTC (EN 10204 3.1) + Relat\u00f3rio UT<\/td><\/tr><\/tbody><\/table><\/div>\n<\/section>\n<section class=\"ads2-sec\">\n<h2>Por que os distribuidores globais adquirem o a\u00e7o H11 da Aobo Steel?<\/h2>\n<div class=\"ads2-cols2\"><div><ul>\n<li>Fornecimento mensal cont\u00ednuo de cerca de 1.200 toneladas<\/li>\n\n\n\n<li>Quantidade m\u00ednima de encomenda a partir de 5 toneladas para pedidos por atacado.<\/li>\n\n\n\n<li>Comprimentos de barras e pratos otimizados para cont\u00eaineres<\/li>\n\n\n\n<li>S\u00e3o permitidos carregamentos de tamanhos mistos para exporta\u00e7\u00e3o.<\/li>\n\n\n\n<li>Entrega de material recozido para usinagem subsequente.<\/li>\n\n\n\n<li>Fornecimento est\u00e1vel por meio de parceiros integrados na cadeia de suprimentos.<\/li>\n<\/ul><\/div><div><ul>\n<li>Inspe\u00e7\u00e3o UT dispon\u00edvel para SEP 1921-82 D\/d ou E\/e<\/li>\n\n\n\n<li>Rastreabilidade MTC e de lote para cada remessa.<\/li>\n\n\n\n<li>Rastreamento do n\u00famero de lote para controle de pedidos<\/li>\n\n\n\n<li>Op\u00e7\u00f5es de superf\u00edcie preta, torneada e polida<\/li>\n\n\n\n<li>Embalagem a granel para exporta\u00e7\u00e3o mar\u00edtima.<\/li>\n\n\n\n<li>Caminho de convers\u00e3o claro para a p\u00e1gina dedicada ao fornecimento em massa.<\/li>\n<\/ul><\/div><\/div>\n<div class=\"ads2-row\">\n  <div class=\"ads2-col-t\"><h2>Produ\u00e7\u00e3o est\u00e1vel para fornecimento em larga escala a longo prazo<\/h2>\n<ul>\n<li>Produ\u00e7\u00e3o mensal cont\u00ednua de cerca de 1.200 toneladas<\/li>\n\n\n\n<li>Ciclos de produ\u00e7\u00e3o cont\u00ednuos para reposi\u00e7\u00e3o de estoque<\/li>\n\n\n\n<li>A tecnologia ESR (Refus\u00e3o por Eletroesc\u00f3ria) est\u00e1 dispon\u00edvel mediante solicita\u00e7\u00e3o.<\/li>\n\n\n\n<li>Fornecimento est\u00e1vel de ligas met\u00e1licas para reduzir o risco de interrup\u00e7\u00e3o no fornecimento<\/li>\n\n\n\n<li>Rastreabilidade completa do lote, vinculada ao n\u00famero de lote original.<\/li>\n<\/ul>\n<div class=\"ads2-cta popmake-16052\"><a class=\"ads2-btn\" href=\"#\">Solicite um or\u00e7amento para grandes volumes.<\/a><\/div><\/div>\n  <div class=\"ads2-col-i\"><figure class=\"ads2-fig\"><img decoding=\"async\" src=\"https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/02\/IMG_20171115_153016-1024x576.avif\" alt=\"\"><\/figure><\/div>\n<\/div>\n<\/section>\n<section class=\"ads2-sec\">\n<h2>Formas dispon\u00edveis em a\u00e7o ferramenta H11<\/h2>\n<figure class=\"ads2-fig\"><img decoding=\"async\" src=\"https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/03\/dd399cbb-cb1f-40f8-8398-03acefc1a0cd-1024x206.avif\" alt=\"\"><\/figure>\n<div class=\"ads2-row ads2-row-flip\">\n  <div class=\"ads2-col-t\"><h2>Controle de Qualidade para Encomendas em Grande Quantidade<\/h2>\n<p>Cada lote de a\u00e7o ferramenta fornecido pela Aobo Steel \u00e9 verificado antes do envio para garantir a precis\u00e3o da classifica\u00e7\u00e3o, a integridade interna e a rastreabilidade de pedidos em grande quantidade.<\/p>\n<ul>\n<li>Composi\u00e7\u00e3o qu\u00edmica verificada por espectr\u00f4metro<\/li>\n\n\n\n<li>Teste ultrass\u00f4nico dispon\u00edvel (SET 1921-82)<\/li>\n\n\n\n<li>Entregue em condi\u00e7\u00e3o esferoidizada e recozida<\/li>\n\n\n\n<li>Certificado de Ensaio de F\u00e1brica (EN 10204 3.1) com n\u00famero de lote<\/li>\n\n\n\n<li>Inspe\u00e7\u00e3o dimensional e de superf\u00edcie antes do envio.<\/li>\n<\/ul>\n<div class=\"ads2-cta popmake-16052\"><a class=\"ads2-btn\" href=\"#\">Solicite um or\u00e7amento para fornecimento em grande quantidade de H11<\/a><\/div><\/div>\n  <div class=\"ads2-col-i\"><figure class=\"ads2-fig\"><img decoding=\"async\" src=\"https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/02\/IMG_20221028_111745.avif\" alt=\"\"><\/figure><\/div>\n<\/div>\n<div class=\"ads2-row\">\n  <div class=\"ads2-col-t\"><h2>Embalagem para exporta\u00e7\u00e3o e carregamento de cont\u00eaineres<\/h2>\n<ul>\n<li>Embalagem profissional para exporta\u00e7\u00e3o mar\u00edtima<\/li>\n\n\n\n<li>Carregamento otimizado para cont\u00eaineres de 20 p\u00e9s (20GP) at\u00e9 aproximadamente 26 toneladas.<\/li>\n\n\n\n<li>Suporte para diferentes graus e tamanhos<\/li>\n\n\n\n<li>Prote\u00e7\u00e3o anticorrosiva para longos transportes mar\u00edtimos.<\/li>\n<\/ul>\n<p>Para remessas internacionais, recomenda-se fortemente o carregamento de cont\u00eaineres completos para garantir a efici\u00eancia de custos e um processamento alfandeg\u00e1rio mais \u00e1gil.<\/p>\n<div class=\"ads2-cta popmake-16052\"><a class=\"ads2-btn\" href=\"#\">Solicite um or\u00e7amento para carga completa de cont\u00eainer (FCL).<\/a><\/div><\/div>\n  <div class=\"ads2-col-i\"><figure class=\"ads2-fig\"><img decoding=\"async\" src=\"https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/02\/photobank-2.avif\" alt=\"\"><\/figure><\/div>\n<\/div>\n<\/section>\n<section class=\"ads2-sec\">\n<h2>Composi\u00e7\u00e3o qu\u00edmica<\/h2>\n<div class=\"ads2-tw\"><table class=\"ads2-t data\"><thead><tr><td>C<\/td><td>Mn<\/td><td>Si<\/td><td>Cr<\/td><td>Mo<\/td><td>V<\/td><\/tr><\/thead><tbody><tr><td>0,33 \u2013 0,43%<\/td><td>0,20 \u2013 0,60%<\/td><td>0,80 \u2013 1,25%<\/td><td>4,75 \u2013 5,50%<\/td><td>1.10 \u2013 1.60%<\/td><td>0,30 \u2013 0,60%<\/td><\/tr><\/tbody><\/table><\/div>\n<p>Graus equivalentes de a\u00e7o para ferramentas H11 e suas composi\u00e7\u00f5es<\/p>\n<div class=\"ads2-tw\"><table class=\"ads2-t data\"><thead><tr><td>Graus<\/td><td>C<\/td><td>Si<\/td><td>Mn<\/td><td>P<\/td><td>S<\/td><td>Cr<\/td><td>Mo<\/td><td>V<\/td><\/tr><\/thead><tbody><tr><td>DIN 1.2343<\/td><td>0,33 \u2013 0,43%<\/td><td>0,80 \u2013 1,25%<\/td><td>0,20 \u2013 0,60%<\/td><td>\u2264 0,030%<\/td><td>\u2264 0,030%<\/td><td>4,75 \u2013 5,50%<\/td><td>1.10 \u2013 1.60%<\/td><td>0,30 \u2013 0,60%<\/td><\/tr><tr><td>JIS SKD6<\/td><td>0,32 \u2013 0,42%<\/td><td>0,80 \u2013 1,20%<\/td><td>0,20 \u2013 0,50%<\/td><td>\u2264 0,030%<\/td><td>\u2264 0,030%<\/td><td>4,50 \u2013 5,50%<\/td><td>1,00 \u2013 1,50%<\/td><td>0,30 \u2013 0,60%<\/td><\/tr><tr><td>GB 4Cr5MoSiV <\/td><td>0,33 \u2013 0,43%<\/td><td>0,80 \u2013 1,20%<\/td><td>0,20 \u2013 0,50%<\/td><td>\u2264 0,030%<\/td><td>\u2264 0,030%<\/td><td>4,75 \u2013 5,50%<\/td><td>1.10 \u2013 1.60%<\/td><td>0,30 \u2013 0,60%<\/td><\/tr><\/tbody><\/table><\/div>\n<\/section>\n<section class=\"ads2-sec\">\n<h2>Propriedades<\/h2>\n<p>O a\u00e7o para ferramentas H11 possui uma combina\u00e7\u00e3o excepcional de dureza alcan\u00e7\u00e1vel, dureza a quente (dureza ao rubro), tenacidade e resist\u00eancia ao desgaste. Cada propriedade, e o modo de falha que ela controla, \u00e9 examinado no <a href=\"https:\/\/aobosteel.com\/pt\/h11-tool-steel-properties\/\">Guia de propriedades e desempenho do H11<\/a>.<\/p>\n<ul>\n<li>Resist\u00eancia: Pode ser tratado termicamente para atingir limites de escoamento de 0,2% bem acima de 1380 MPa (200 ksi) e resist\u00eancias \u00e0 tra\u00e7\u00e3o superiores a 2070 MPa (300 ksi).\u00a0<\/li>\n\n\n\n<li>Dureza: As durezas de trabalho normais variam tipicamente de 40 a 55 HRC. Para aplica\u00e7\u00f5es como fundi\u00e7\u00e3o sob press\u00e3o de alum\u00ednio, uma dureza preferida de 47 HRC \u00e9 indicada. Na fundi\u00e7\u00e3o sob press\u00e3o, matrizes de H11 podem ser temperadas a 42\u201352 HRC; insertos e machos a 46\u201352 HRC; \u00eambolos a 46\u201350 HRC; slides a 46\u201352 HRC; <a href=\"https:\/\/aobosteel.com\/pt\/shot-sleeve-and-plunger-tip-materials\/\">camisas de inje\u00e7\u00e3o<\/a> a 44\u201348 HRC; e bicos a 32\u201342 HRC. Para pun\u00e7\u00f5es e matrizes de forjamento a quente, a dureza varia tipicamente de 44\u201348 HRC. Cilindros de lamina\u00e7\u00e3o a quente (para corridas curtas e baixas temperaturas) s\u00e3o feitos de H11 a 40\u201348 HRC. Matrizes de estampagem a quente s\u00e3o tipicamente 48\u201352 HRC.<\/li>\n\n\n\n<li>Dureza a Quente\/Dureza ao Rubro: Boa resist\u00eancia ao revenimento, mantendo alta dureza e resist\u00eancia em temperaturas elevadas. Resiste ao amolecimento durante exposi\u00e7\u00e3o cont\u00ednua a temperaturas de at\u00e9 540 \u00b0C (1000 \u00b0F). Embora sua dureza a quente seja inferior \u00e0 de alguns outros a\u00e7os para trabalho a quente, como H19 ou H21, ainda ret\u00e9m dureza melhor do que outros a\u00e7os de m\u00e9dia liga em temperaturas mais altas. A Dureza a Quente\/Dureza ao Rubro \u00e9 uma propriedade muito importante para a\u00e7os para ferramentas de trabalho a quente.<\/li>\n\n\n\n<li>Tenacidade e Ductilidade: Boa ductilidade e resist\u00eancia ao impacto. Tem melhor resist\u00eancia \u00e0 fratura fr\u00e1gil do que a\u00e7os com maior teor de liga, como H14, H19 e H21. Os processos de refus\u00e3o por eletroesc\u00f3ria (ESR) ou refus\u00e3o a arco a v\u00e1cuo (VAR) podem melhorar significativamente a ductilidade e a tenacidade.<\/li>\n\n\n\n<li>Resist\u00eancia \u00e0 fadiga: Este material oferece alta resist\u00eancia \u00e0 fadiga e estabilidade t\u00e9rmica em uma faixa de temperatura de 75 a 540 \u00b0C (167 a 1000 \u00b0F). Comparado ao a\u00e7o 4340 submetido ao mesmo tratamento t\u00e9rmico de alta intensidade, o H11 apresenta melhor resist\u00eancia \u00e0 fadiga.<\/li>\n\n\n\n<li>Resist\u00eancia ao desgaste: Sua resist\u00eancia ao desgaste \u00e9 menor que a do H13.<\/li>\n\n\n\n<li>Soldabilidade: \u00c9 facilmente sold\u00e1vel, mesmo em se\u00e7\u00f5es pesadas.\u00a0<\/li>\n\n\n\n<li>Usinabilidade: Boa usinabilidade, avaliada em cerca de 70% de um a\u00e7o carbono padr\u00e3o de 1%.<\/li>\n\n\n\n<li>Propriedades t\u00e9rmicas: Possui um coeficiente de expans\u00e3o t\u00e9rmica relativamente baixo e uma condutividade t\u00e9rmica de 26 W\/m\u00b7K.<\/li>\n\n\n\n<li>Resist\u00eancia \u00e0 corros\u00e3o: Resist\u00eancia \u00e0 oxida\u00e7\u00e3o e \u00e0 corros\u00e3o acima da m\u00e9dia.<\/li>\n\n\n\n<li>Resist\u00eancia ao trincamento t\u00e9rmico: Boa resist\u00eancia \u00e0 fadiga t\u00e9rmica (trincamento t\u00e9rmico).<\/li>\n<\/ul>\n<\/section>\n<section class=\"ads2-sec\">\n<h2>Tratamento t\u00e9rmico do a\u00e7o ferramenta H11<\/h2>\n<p>Preciso\u00a0<em>o tratamento t\u00e9rmico<\/em>\u00a0do a\u00e7o para ferramentas H11 \u00e9 crucial para alcan\u00e7ar o desempenho ideal como a\u00e7o para matrizes de trabalho a quente com 5% de cromo e a\u00e7o de ultra-alta resist\u00eancia, semelhante ao H11 Modified e H13. Esse processo ajusta a microestrutura para ferramentas de f\u00e1brica exigentes.\u00a0<\/p>\n<h3>Forjamento<\/h3>\n<p>Este a\u00e7o \u00e9 facilmente forjado, com faixa de temperatura de forjamento adequada de 1120 a 1150\u00b0C (2050 a 2100\u00b0F). Recomendamos pr\u00e9-aquecer o tarugo a 790-815\u00b0C (1450-1500\u00b0F), depois aquec\u00ea-lo uniformemente at\u00e9 a temperatura de forjamento. A temperatura de forjamento N\u00c3O deve ser inferior a 925\u00b0C (1700\u00b0F). Se a temperatura cair pr\u00f3xima a esse n\u00edvel, deve ser reaquecida antes de continuar o processo de forjamento.<\/p>\n<h3>Austenitiza\u00e7\u00e3o<\/h3>\n<p>A austenitiza\u00e7\u00e3o, etapa prim\u00e1ria de endurecimento, envolve o aquecimento para transformar sua estrutura em austenita. Isso permite a convers\u00e3o e dissolu\u00e7\u00e3o uniformes dos elementos de liga e dos carbonetos.<\/p>\n<ul>\n<li>Pr\u00e9-aquecimento: Pr\u00e9-aque\u00e7a o H11 a 760-815 \u00b0C (1400-1500 \u00b0F) antes da austenitiza\u00e7\u00e3o para minimizar choque t\u00e9rmico e trincamento, especialmente para este material de alta liga.<\/li>\n\n\n\n<li>Temperaturas de Austenitiza\u00e7\u00e3o e Tempos de Imers\u00e3o: A Temperatura de Austenitiza\u00e7\u00e3o \u00e9 995-1025 \u00b0C (1825-1875 \u00b0F). O tempo de imers\u00e3o \u00e9 de 20 minutos + 5 minutos por 25 mm (1 polegada) de espessura.<\/li>\n<\/ul>\n<p>Manter a temperatura de austenitiza\u00e7\u00e3o garante transforma\u00e7\u00e3o e dissolu\u00e7\u00e3o uniformes.<\/p>\n<h3>T\u00eampera<\/h3>\n<p>Ap\u00f3s a austenitiza\u00e7\u00e3o, o a\u00e7o H11 \u00e9 temperado rapidamente para formar martensita dura. O H11 \u00e9 um a\u00e7o de endurecimento ao ar que proporciona endurecimento uniforme em grandes se\u00e7\u00f5es com tens\u00f5es residuais e varia\u00e7\u00f5es dimensionais m\u00ednimas. O resfriamento ao ar \u00e9 o m\u00e9todo padr\u00e3o e preferido para o a\u00e7o para ferramentas H11. Embora o resfriamento ao ar seja padr\u00e3o, a t\u00eampera em \u00f3leo a partir de 995 \u00b0C (1825 \u00b0F) \u00e9 uma alternativa poss\u00edvel. O H11 e outros a\u00e7os para ferramentas de trabalho a quente nunca devem ser temperados em \u00e1gua, pois isso pode levar ao trincamento.<\/p>\n<h3>Revenimento<\/h3>\n<p>Ap\u00f3s o endurecimento, o revenimento do a\u00e7o para ferramentas H11 por reaquecimento a uma temperatura mais baixa \u00e9 crucial para melhorar a tenacidade, aliviar tens\u00f5es e estabilizar propriedades. O a\u00e7o H11 \u00e9 um a\u00e7o de endurecimento secund\u00e1rio. Ele alcan\u00e7a seu melhor desempenho quando revenido em temperaturas acima de 510\u00b0C (950\u00b0F). Recomendamos realizar m\u00faltiplos tratamentos de revenimento para alcan\u00e7ar tenacidade ideal e prolongar a vida \u00fatil da ferramenta. Deixe as pe\u00e7as esfriarem \u00e0 temperatura ambiente entre os ciclos de revenimento para minimizar a austenita retida.\u00a0<\/p>\n<p><strong>Tabela de Dureza e Temperatura de Revenimento para A\u00e7o H11<\/strong><\/p>\n<div class=\"ads2-tw\"><table class=\"ads2-t kv\"><tbody><tr><td><strong>Temperatura de revenimento<\/strong><\/td><td><strong>Rockwell C<\/strong><\/td><\/tr><tr><td>Ap\u00f3s a t\u00eampera<\/td><td>56<\/td><\/tr><tr><td>700\u00b0F\/370\u00b0C<\/td><td>54<\/td><\/tr><tr><td>800\u00b0F\/425\u00b0C<\/td><td>55<\/td><\/tr><tr><td>900\u00b0F\/480\u00b0C<\/td><td>57<\/td><\/tr><tr><td>1000\u00b0F\/540\u00b0C<\/td><td>56<\/td><\/tr><tr><td>1100\u00b0F\/595\u00b0C<\/td><td>46<\/td><\/tr><tr><td>1200\u00b0F\/650\u00b0C<\/td><td>36<\/td><\/tr><\/tbody><\/table><\/div><figcaption>Condi\u00e7\u00f5es experimentais: 1. TEMPERATURA DE PR\u00c9-AQUECIMENTO 1200\u00b0F\/650\u00b0C 2. TEMPERATURA DE ENDURECIMENTO 1850\u00b0F\/1010\u00b0C 3. T\u00c9RMINA\u00c7\u00c3O AO AR 4. QU\u00cdMICA Carbono 0,40% Mangan\u00eas 0,30% Sil\u00edcio 1,00% Cromo 5,00% Molibd\u00eanio 1,30% Van\u00e1dio 0,50%<\/figcaption>\n<h3>Recozimento\u00a0<\/h3>\n<p>A temperatura de recozimento varia de 845 a 900\u00b0C (1550-1650\u00b0F). A taxa de resfriamento \u00e9 de 22-40\u00b0C\/h (40-75\u00b0F\/h). A dureza ap\u00f3s o recozimento \u00e9 de 192-229 HB.<\/p>\n<h3>Outras considera\u00e7\u00f5es importantes sobre o tratamento t\u00e9rmico H11<\/h3>\n<ul>\n<li>Normaliza\u00e7\u00e3o: Este processo geralmente n\u00e3o \u00e9 recomendado para a\u00e7os para ferramentas H11 ou H13 devido ao alto risco de trincamento, particularmente quando ocorre descarboneta\u00e7\u00e3o superficial.<\/li>\n\n\n\n<li>Al\u00edvio de Tens\u00f5es: Ap\u00f3s o H11 ter sido processado, como retifica\u00e7\u00e3o, soldagem ou EDM (usinagem por descarga el\u00e9trica), recomendamos fortemente o tratamento de al\u00edvio de tens\u00f5es a 650\u00b0C. Este tratamento deve ser realizado a uma temperatura 14\u201328\u00b0C (25\u201350\u00b0F) inferior \u00e0 temperatura de revenimento anterior. Ap\u00f3s o al\u00edvio de tens\u00f5es, resfrie lentamente a uma taxa m\u00e1xima de 300\u00b0C\/h para evitar a forma\u00e7\u00e3o de novas tens\u00f5es.<\/li>\n\n\n\n<li>Tratamento Criog\u00eanico: O tratamento sub-zero (por exemplo, -73\u00b0C \/ -100\u00b0F) pode reduzir a austenita retida; no entanto, as altas temperaturas de revenimento do H11 geralmente o tornam desnecess\u00e1rio para alcan\u00e7ar o endurecimento secund\u00e1rio m\u00e1ximo.<\/li>\n\n\n\n<li>Prote\u00e7\u00e3o Superficial: Proteger suas superf\u00edcies contra oxida\u00e7\u00e3o e descarboneta\u00e7\u00e3o durante tratamentos em alta temperatura, como austenitiza\u00e7\u00e3o e recozimento, \u00e9 vital. Isso \u00e9 frequentemente alcan\u00e7ado usando atmosferas controladas, fornos a v\u00e1cuo ou banhos de sal.<\/li>\n<\/ul>\n<\/section>\n<section class=\"ads2-sec\">\n<h2>Aplica\u00e7\u00f5es<\/h2>\n<ul>\n<li>Matrizes de fundi\u00e7\u00e3o sob press\u00e3o<\/li>\n\n\n\n<li>Matrizes de forjamento<\/li>\n\n\n\n<li>Ferramentas de extrus\u00e3o<\/li>\n\n\n\n<li>L\u00e2minas de corte a quente:<\/li>\n\n\n\n<li>Componentes aeroespaciais<\/li>\n<\/ul>\n<div class=\"ads2-gal\"><figure class=\"ads2-fig\"><img decoding=\"async\" src=\"https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/04\/H11-TOOL-STEEL-FLAT.avif\" alt=\"A\u00e7o para ferramentas H11\"><figcaption>A\u00e7o ferramenta H11<\/figcaption><\/figure><figure class=\"ads2-fig\"><img decoding=\"async\" src=\"https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/08\/1.2343-steel.avif\" alt=\"A\u00e7o 1.2343\"><figcaption>A\u00e7o Ferramenta 1.2343<\/figcaption><\/figure><figure class=\"ads2-fig\"><img decoding=\"async\" src=\"https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/06\/1.2343.webp\" alt=\"A\u00e7o Ferramenta 1.2343\"><figcaption>A\u00e7o Ferramenta 1.2343<\/figcaption><\/figure><\/div>\n<div class=\"ads2-cta popmake-16052\"><a class=\"ads2-btn\" href=\"#\">Abrir formul\u00e1rio de solicita\u00e7\u00e3o de cota\u00e7\u00e3o<\/a><\/div>\n<\/section>\n\n\n<script type=\"application\/ld+json\">{\n    \"@context\": \"https:\\\/\\\/schema.org\\\/\",\n    \"@type\": \"Product\",\n    \"name\": \"Forged H11 \\\/ 1.2343 \\\/ SKD6 Hot Work Tool Steel Round Bar\",\n    \"image\": \"https:\\\/\\\/aobosteel.com\\\/wp-content\\\/uploads\\\/2025\\\/04\\\/H11-TOOL-STEEL-FLAT.avif\",\n    \"description\": \"High-quality Forged H11 (1.2343 \\\/ SKD6) Hot Work Tool Steel directly from Aobo Steel factory. Exceptional toughness and resistance to thermal cracking. Suitable for heavy hammer forging dies. Manufacturer price.\",\n    \"brand\": {\n        \"@type\": \"Brand\",\n        \"name\": \"Aobo Steel\"\n    },\n    \"manufacturer\": {\n        \"@type\": \"Organization\",\n        \"name\": \"Aobo Steel\"\n    },\n    \"sku\": \"AOBO-H11-Round\",\n    \"mpn\": \"AOBO-H11-MFG\",\n    \"offers\": {\n        \"@type\": \"AggregateOffer\",\n        \"url\": \"https:\\\/\\\/aobosteel.com\\\/h11-tool-steel\\\/\",\n        \"priceCurrency\": \"USD\",\n        \"lowPrice\": \"1100\",\n        \"highPrice\": \"1400\",\n        \"offerCount\": \"5\",\n        \"availability\": \"https:\\\/\\\/schema.org\\\/InStock\",\n        \"itemCondition\": \"https:\\\/\\\/schema.org\\\/NewCondition\",\n        \"seller\": {\n            \"@type\": \"Organization\",\n            \"name\": \"Aobo Steel\",\n            \"telephone\": \"+86 180 6294 5370\",\n            \"address\": {\n                \"@type\": \"PostalAddress\",\n                \"streetAddress\": \"No. 141 Huangjiawan, Shileishan Village, Xisai District\",\n                \"addressLocality\": \"Huangshi City\",\n                \"addressRegion\": \"Hubei Province\",\n                \"postalCode\": \"435000\",\n                \"addressCountry\": \"CN\"\n            }\n        }\n    }\n}<\/script>\n\n\n\n<\/div>\n<\/div>","protected":false},"excerpt":{"rendered":"<p>Home &gt; Tool Steel Catalog &gt; H11 Tool Steel Aobo Steel | Global Tool Steel Supplier in China AISI H11 Tool Steel | 1.2343 | SKD6 Chromium Hot Work Steel 100% UT Tested Quality Assurance SEP 1921-82 Class D\/d Guaranteed Annealed State Delivery Surface: Black Scale, Turned, Mill Finish, or Polished Quick Inquiry For H11 [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":14815,"parent":0,"menu_order":0,"comment_status":"closed","ping_status":"closed","template":"","meta":{"_uag_custom_page_level_css":"","site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"default","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"disabled","ast-breadcrumbs-content":"","ast-featured-img":"disabled","footer-sml-layout":"","ast-disable-related-posts":"","theme-transparent-header-meta":"","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"default","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"footnotes":"[]"},"class_list":["post-9395","page","type-page","status-publish","has-post-thumbnail","hentry"],"yoast_head":"<!-- This site is optimized with the Yoast SEO Premium plugin v28.9 (Yoast SEO v28.9) - https:\/\/yoast.com\/product\/yoast-seo-premium-wordpress\/ -->\n<title>H11 Tool Steel Supplier | 1.2343 | SKD6 Hot Work Steel | Aobo Steel<\/title>\n<meta name=\"description\" content=\"H11 tool steel (1.2343 \/ SKD6) supplier for bulk orders. High toughness hot work steel for die casting, forging, and extrusion. MOQ 5 tons, stable supply, MTC available.\" \/>\n<meta name=\"robots\" content=\"index, follow, max-snippet:-1, max-image-preview:large, max-video-preview:-1\" \/>\n<link rel=\"canonical\" href=\"https:\/\/aobosteel.com\/pt\/h11-tool-steel\/\" \/>\n<meta property=\"og:locale\" content=\"pt_BR\" \/>\n<meta property=\"og:type\" content=\"article\" \/>\n<meta property=\"og:title\" content=\"H11 Tool Steel Supplier | 1.2343 \/ SKD6 Hot Work Steel Manufacturer | Aobo Steel\" \/>\n<meta property=\"og:description\" content=\"H11 tool steel (1.2343 \/ SKD6) supplier for bulk orders. High toughness hot work steel for die casting, forging, and extrusion. MOQ 5 tons, stable supply, MTC available.\" \/>\n<meta property=\"og:url\" content=\"https:\/\/aobosteel.com\/pt\/h11-tool-steel\/\" \/>\n<meta property=\"og:site_name\" content=\"AoboSteel\" \/>\n<meta property=\"article:publisher\" content=\"https:\/\/www.facebook.com\/profile.php?id=61565368220197\" \/>\n<meta property=\"article:modified_time\" content=\"2026-11-01T14:37:30+00:00\" \/>\n<meta property=\"og:image\" content=\"https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/04\/H11-TOOL-STEEL-AD.avif\" \/>\n\t<meta property=\"og:image:width\" content=\"1254\" \/>\n\t<meta property=\"og:image:height\" content=\"1254\" \/>\n\t<meta property=\"og:image:type\" content=\"image\/png\" \/>\n<meta name=\"twitter:card\" content=\"summary_large_image\" \/>\n<meta name=\"twitter:label1\" content=\"Est. tempo de leitura\" \/>\n\t<meta name=\"twitter:data1\" content=\"9 minutos\" \/>\n<script type=\"application\/ld+json\" class=\"yoast-schema-graph\">{\"@context\":\"https:\\\/\\\/schema.org\",\"@graph\":[{\"@type\":\"TechArticle\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/h11-tool-steel\\\/#article\",\"isPartOf\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/h11-tool-steel\\\/\"},\"author\":{\"name\":\"Evan\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#\\\/schema\\\/person\\\/96118415c30ca6bb52eaf1127b052ef7\"},\"headline\":\"H11 Tool Steel Supplier | 1.2343 \\\/ SKD6 Hot Work Steel Manufacturer | Aobo Steel\",\"datePublished\":\"2025-08-02T16:45:36+00:00\",\"dateModified\":\"2026-11-01T14:37:30+00:00\",\"mainEntityOfPage\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/h11-tool-steel\\\/\"},\"wordCount\":1430,\"publisher\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#organization\"},\"image\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/h11-tool-steel\\\/#primaryimage\"},\"thumbnailUrl\":\"https:\\\/\\\/aobosteel.com\\\/wp-content\\\/uploads\\\/2026\\\/04\\\/H11-TOOL-STEEL-AD.avif\",\"inLanguage\":\"pt-BR\"},{\"@type\":\"WebPage\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/h11-tool-steel\\\/\",\"url\":\"https:\\\/\\\/aobosteel.com\\\/h11-tool-steel\\\/\",\"name\":\"H11 Tool Steel Supplier | 1.2343 | SKD6 Hot Work Steel | Aobo Steel\",\"isPartOf\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#website\"},\"primaryImageOfPage\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/h11-tool-steel\\\/#primaryimage\"},\"image\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/h11-tool-steel\\\/#primaryimage\"},\"thumbnailUrl\":\"https:\\\/\\\/aobosteel.com\\\/wp-content\\\/uploads\\\/2026\\\/04\\\/H11-TOOL-STEEL-AD.avif\",\"datePublished\":\"2025-08-02T16:45:36+00:00\",\"dateModified\":\"2026-11-01T14:37:30+00:00\",\"description\":\"H11 tool steel (1.2343 \\\/ SKD6) supplier for bulk orders. High toughness hot work steel for die casting, forging, and extrusion. MOQ 5 tons, stable supply, MTC available.\",\"breadcrumb\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/h11-tool-steel\\\/#breadcrumb\"},\"inLanguage\":\"pt-BR\",\"potentialAction\":[{\"@type\":\"ReadAction\",\"target\":[\"https:\\\/\\\/aobosteel.com\\\/h11-tool-steel\\\/\"]}]},{\"@type\":\"ImageObject\",\"inLanguage\":\"pt-BR\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/h11-tool-steel\\\/#primaryimage\",\"url\":\"https:\\\/\\\/aobosteel.com\\\/wp-content\\\/uploads\\\/2026\\\/04\\\/H11-TOOL-STEEL-AD.avif\",\"contentUrl\":\"https:\\\/\\\/aobosteel.com\\\/wp-content\\\/uploads\\\/2026\\\/04\\\/H11-TOOL-STEEL-AD.avif\",\"width\":1254,\"height\":1254},{\"@type\":\"BreadcrumbList\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/h11-tool-steel\\\/#breadcrumb\",\"itemListElement\":[{\"@type\":\"ListItem\",\"position\":1,\"name\":\"\u9996\u9875\",\"item\":\"https:\\\/\\\/aobosteel.com\\\/\"},{\"@type\":\"ListItem\",\"position\":2,\"name\":\"H11 Tool Steel Supplier | 1.2343 \\\/ SKD6 Hot Work Steel Manufacturer | Aobo Steel\"}]},{\"@type\":\"WebSite\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#website\",\"url\":\"https:\\\/\\\/aobosteel.com\\\/\",\"name\":\"AoboSteel\",\"description\":\"\",\"publisher\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#organization\"},\"potentialAction\":[{\"@type\":\"SearchAction\",\"target\":{\"@type\":\"EntryPoint\",\"urlTemplate\":\"https:\\\/\\\/aobosteel.com\\\/?s={search_term_string}\"},\"query-input\":{\"@type\":\"PropertyValueSpecification\",\"valueRequired\":true,\"valueName\":\"search_term_string\"}}],\"inLanguage\":\"pt-BR\"},{\"@type\":\"Organization\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#organization\",\"name\":\"AoboSteel\",\"url\":\"https:\\\/\\\/aobosteel.com\\\/\",\"logo\":{\"@type\":\"ImageObject\",\"inLanguage\":\"pt-BR\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#\\\/schema\\\/logo\\\/image\\\/\",\"url\":\"https:\\\/\\\/aobosteel.com\\\/wp-content\\\/uploads\\\/2025\\\/01\\\/cropped-aobo-steel-1.avif\",\"contentUrl\":\"https:\\\/\\\/aobosteel.com\\\/wp-content\\\/uploads\\\/2025\\\/01\\\/cropped-aobo-steel-1.avif\",\"width\":1052,\"height\":592,\"caption\":\"AoboSteel\"},\"image\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#\\\/schema\\\/logo\\\/image\\\/\"},\"sameAs\":[\"https:\\\/\\\/www.facebook.com\\\/profile.php?id=61565368220197\",\"https:\\\/\\\/www.linkedin.com\\\/in\\\/aobosteel-evan\\\/\"]},{\"@type\":\"Person\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#\\\/schema\\\/person\\\/96118415c30ca6bb52eaf1127b052ef7\",\"name\":\"Evan\",\"image\":{\"@type\":\"ImageObject\",\"inLanguage\":\"pt-BR\",\"@id\":\"https:\\\/\\\/secure.gravatar.com\\\/avatar\\\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g\",\"url\":\"https:\\\/\\\/secure.gravatar.com\\\/avatar\\\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g\",\"contentUrl\":\"https:\\\/\\\/secure.gravatar.com\\\/avatar\\\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g\",\"caption\":\"Evan\"},\"sameAs\":[\"http:\\\/\\\/www.aobosteel.com\",\"https:\\\/\\\/www.facebook.com\\\/profile.php?id=61565368220197\",\"https:\\\/\\\/www.instagram.com\\\/aobosteel\\\/\",\"https:\\\/\\\/www.linkedin.com\\\/in\\\/aobosteel-evan\\\/\",\"https:\\\/\\\/x.com\\\/AobosteelEvan\",\"https:\\\/\\\/www.youtube.com\\\/@aobosteel\"],\"url\":\"https:\\\/\\\/aobosteel.com\\\/pt\\\/blog\\\/author\\\/admin\\\/\"}]}<\/script>\n<!-- \/ Yoast SEO Premium plugin. -->","yoast_head_json":{"title":"Fornecedor de a\u00e7o ferramenta H11 | 1.2343 | A\u00e7o para trabalho a quente SKD6 | Aobo Steel","description":"Fornecedor de a\u00e7o ferramenta H11 (1.2343 \/ SKD6) para grandes encomendas. A\u00e7o de alta tenacidade para trabalho a quente, ideal para fundi\u00e7\u00e3o, forjamento e extrus\u00e3o. Pedido m\u00ednimo de 5 toneladas, fornecimento est\u00e1vel, certificado de qualidade dispon\u00edvel.","robots":{"index":"index","follow":"follow","max-snippet":"max-snippet:-1","max-image-preview":"max-image-preview:large","max-video-preview":"max-video-preview:-1"},"canonical":"https:\/\/aobosteel.com\/pt\/h11-tool-steel\/","og_locale":"pt_BR","og_type":"article","og_title":"H11 Tool Steel Supplier | 1.2343 \/ SKD6 Hot Work Steel Manufacturer | Aobo Steel","og_description":"H11 tool steel (1.2343 \/ SKD6) supplier for bulk orders. High toughness hot work steel for die casting, forging, and extrusion. MOQ 5 tons, stable supply, MTC available.","og_url":"https:\/\/aobosteel.com\/pt\/h11-tool-steel\/","og_site_name":"AoboSteel","article_publisher":"https:\/\/www.facebook.com\/profile.php?id=61565368220197","article_modified_time":"2026-11-01T14:37:30+00:00","og_image":[{"width":1254,"height":1254,"url":"https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/04\/H11-TOOL-STEEL-AD.avif","type":"image\/png"}],"twitter_card":"summary_large_image","twitter_misc":{"Est. tempo de leitura":"9 minutos"},"schema":{"@context":"https:\/\/schema.org","@graph":[{"@type":"TechArticle","@id":"https:\/\/aobosteel.com\/h11-tool-steel\/#article","isPartOf":{"@id":"https:\/\/aobosteel.com\/h11-tool-steel\/"},"author":{"name":"Evan","@id":"https:\/\/aobosteel.com\/#\/schema\/person\/96118415c30ca6bb52eaf1127b052ef7"},"headline":"H11 Tool Steel Supplier | 1.2343 \/ SKD6 Hot Work Steel Manufacturer | Aobo Steel","datePublished":"2025-08-02T16:45:36+00:00","dateModified":"2026-11-01T14:37:30+00:00","mainEntityOfPage":{"@id":"https:\/\/aobosteel.com\/h11-tool-steel\/"},"wordCount":1430,"publisher":{"@id":"https:\/\/aobosteel.com\/#organization"},"image":{"@id":"https:\/\/aobosteel.com\/h11-tool-steel\/#primaryimage"},"thumbnailUrl":"https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/04\/H11-TOOL-STEEL-AD.avif","inLanguage":"pt-BR"},{"@type":"WebPage","@id":"https:\/\/aobosteel.com\/h11-tool-steel\/","url":"https:\/\/aobosteel.com\/h11-tool-steel\/","name":"Fornecedor de a\u00e7o ferramenta H11 | 1.2343 | A\u00e7o para trabalho a quente SKD6 | Aobo Steel","isPartOf":{"@id":"https:\/\/aobosteel.com\/#website"},"primaryImageOfPage":{"@id":"https:\/\/aobosteel.com\/h11-tool-steel\/#primaryimage"},"image":{"@id":"https:\/\/aobosteel.com\/h11-tool-steel\/#primaryimage"},"thumbnailUrl":"https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/04\/H11-TOOL-STEEL-AD.avif","datePublished":"2025-08-02T16:45:36+00:00","dateModified":"2026-11-01T14:37:30+00:00","description":"Fornecedor de a\u00e7o ferramenta H11 (1.2343 \/ SKD6) para grandes encomendas. A\u00e7o de alta tenacidade para trabalho a quente, ideal para fundi\u00e7\u00e3o, forjamento e extrus\u00e3o. Pedido m\u00ednimo de 5 toneladas, fornecimento est\u00e1vel, certificado de qualidade dispon\u00edvel.","breadcrumb":{"@id":"https:\/\/aobosteel.com\/h11-tool-steel\/#breadcrumb"},"inLanguage":"pt-BR","potentialAction":[{"@type":"ReadAction","target":["https:\/\/aobosteel.com\/h11-tool-steel\/"]}]},{"@type":"ImageObject","inLanguage":"pt-BR","@id":"https:\/\/aobosteel.com\/h11-tool-steel\/#primaryimage","url":"https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/04\/H11-TOOL-STEEL-AD.avif","contentUrl":"https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/04\/H11-TOOL-STEEL-AD.avif","width":1254,"height":1254},{"@type":"BreadcrumbList","@id":"https:\/\/aobosteel.com\/h11-tool-steel\/#breadcrumb","itemListElement":[{"@type":"ListItem","position":1,"name":"\u9996\u9875","item":"https:\/\/aobosteel.com\/"},{"@type":"ListItem","position":2,"name":"H11 Tool Steel Supplier | 1.2343 \/ SKD6 Hot Work Steel Manufacturer | Aobo Steel"}]},{"@type":"WebSite","@id":"https:\/\/aobosteel.com\/#website","url":"https:\/\/aobosteel.com\/","name":"AoboSteel","description":"","publisher":{"@id":"https:\/\/aobosteel.com\/#organization"},"potentialAction":[{"@type":"SearchAction","target":{"@type":"EntryPoint","urlTemplate":"https:\/\/aobosteel.com\/?s={search_term_string}"},"query-input":{"@type":"PropertyValueSpecification","valueRequired":true,"valueName":"search_term_string"}}],"inLanguage":"pt-BR"},{"@type":"Organization","@id":"https:\/\/aobosteel.com\/#organization","name":"AoboSteel","url":"https:\/\/aobosteel.com\/","logo":{"@type":"ImageObject","inLanguage":"pt-BR","@id":"https:\/\/aobosteel.com\/#\/schema\/logo\/image\/","url":"https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/01\/cropped-aobo-steel-1.avif","contentUrl":"https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/01\/cropped-aobo-steel-1.avif","width":1052,"height":592,"caption":"AoboSteel"},"image":{"@id":"https:\/\/aobosteel.com\/#\/schema\/logo\/image\/"},"sameAs":["https:\/\/www.facebook.com\/profile.php?id=61565368220197","https:\/\/www.linkedin.com\/in\/aobosteel-evan\/"]},{"@type":"Person","@id":"https:\/\/aobosteel.com\/#\/schema\/person\/96118415c30ca6bb52eaf1127b052ef7","name":"Evan","image":{"@type":"ImageObject","inLanguage":"pt-BR","@id":"https:\/\/secure.gravatar.com\/avatar\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g","url":"https:\/\/secure.gravatar.com\/avatar\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g","contentUrl":"https:\/\/secure.gravatar.com\/avatar\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g","caption":"Evan"},"sameAs":["http:\/\/www.aobosteel.com","https:\/\/www.facebook.com\/profile.php?id=61565368220197","https:\/\/www.instagram.com\/aobosteel\/","https:\/\/www.linkedin.com\/in\/aobosteel-evan\/","https:\/\/x.com\/AobosteelEvan","https:\/\/www.youtube.com\/@aobosteel"],"url":"https:\/\/aobosteel.com\/pt\/blog\/author\/admin\/"}]}},"uagb_featured_image_src":{"full":["https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/04\/H11-TOOL-STEEL-AD.avif",1254,1254,false],"thumbnail":["https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/04\/H11-TOOL-STEEL-AD-150x150.avif",150,150,true],"medium":["https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/04\/H11-TOOL-STEEL-AD-300x300.avif",300,300,true],"medium_large":["https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/04\/H11-TOOL-STEEL-AD-768x768.avif",768,768,true],"large":["https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/04\/H11-TOOL-STEEL-AD-1024x1024.avif",1024,1024,true],"1536x1536":["https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/04\/H11-TOOL-STEEL-AD.avif",1254,1254,false],"2048x2048":["https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/04\/H11-TOOL-STEEL-AD.avif",1254,1254,false],"trp-custom-language-flag":["https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/04\/H11-TOOL-STEEL-AD-12x12.avif",12,12,true]},"uagb_author_info":{"display_name":"Evan","author_link":"https:\/\/aobosteel.com\/pt\/blog\/author\/admin\/"},"uagb_comment_info":0,"uagb_excerpt":"Home &gt; Tool Steel Catalog &gt; H11 Tool Steel Aobo Steel | Global Tool Steel Supplier in China AISI H11 Tool Steel | 1.2343 | SKD6 Chromium Hot Work Steel 100% UT Tested Quality Assurance SEP 1921-82 Class D\/d Guaranteed Annealed State Delivery Surface: Black Scale, Turned, Mill Finish, or Polished Quick Inquiry For H11&hellip;","rttpg_featured_image_url":{"full":["https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/04\/H11-TOOL-STEEL-AD.avif",1254,1254,false],"landscape":["https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/04\/H11-TOOL-STEEL-AD.avif",1254,1254,false],"portraits":["https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/04\/H11-TOOL-STEEL-AD.avif",1254,1254,false],"thumbnail":["https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/04\/H11-TOOL-STEEL-AD-150x150.avif",150,150,true],"medium":["https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/04\/H11-TOOL-STEEL-AD-300x300.avif",300,300,true],"large":["https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/04\/H11-TOOL-STEEL-AD-1024x1024.avif",1024,1024,true],"1536x1536":["https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/04\/H11-TOOL-STEEL-AD.avif",1254,1254,false],"2048x2048":["https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/04\/H11-TOOL-STEEL-AD.avif",1254,1254,false],"trp-custom-language-flag":["https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/04\/H11-TOOL-STEEL-AD-12x12.avif",12,12,true]},"rttpg_author":{"display_name":"Evan","author_link":"https:\/\/aobosteel.com\/pt\/blog\/author\/admin\/"},"rttpg_comment":0,"rttpg_category":null,"rttpg_excerpt":"Home &gt; Tool Steel Catalog &gt; H11 Tool Steel Aobo Steel | Global Tool Steel Supplier in China AISI H11 Tool Steel | 1.2343 | SKD6 Chromium Hot Work Steel 100% UT Tested Quality Assurance SEP 1921-82 Class D\/d Guaranteed Annealed State Delivery Surface: Black Scale, Turned, Mill Finish, or Polished Quick Inquiry For H11&hellip;","_links":{"self":[{"href":"https:\/\/aobosteel.com\/pt\/wp-json\/wp\/v2\/pages\/9395","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/aobosteel.com\/pt\/wp-json\/wp\/v2\/pages"}],"about":[{"href":"https:\/\/aobosteel.com\/pt\/wp-json\/wp\/v2\/types\/page"}],"author":[{"embeddable":true,"href":"https:\/\/aobosteel.com\/pt\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/aobosteel.com\/pt\/wp-json\/wp\/v2\/comments?post=9395"}],"version-history":[{"count":7,"href":"https:\/\/aobosteel.com\/pt\/wp-json\/wp\/v2\/pages\/9395\/revisions"}],"predecessor-version":[{"id":24892,"href":"https:\/\/aobosteel.com\/pt\/wp-json\/wp\/v2\/pages\/9395\/revisions\/24892"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/aobosteel.com\/pt\/wp-json\/wp\/v2\/media\/14815"}],"wp:attachment":[{"href":"https:\/\/aobosteel.com\/pt\/wp-json\/wp\/v2\/media?parent=9395"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}