{"id":20327,"date":"2026-09-30T07:08:32","date_gmt":"2026-09-29T23:08:32","guid":{"rendered":"https:\/\/aobosteel.com\/?page_id=20327"},"modified":"2026-10-19T22:56:45","modified_gmt":"2026-10-19T14:56:45","slug":"astm-grain-size-chart-tool-steel","status":"publish","type":"page","link":"https:\/\/aobosteel.com\/pt\/astm-grain-size-chart-tool-steel\/","title":{"rendered":"Tabela de Tamanho de Gr\u00e3o ASTM para A\u00e7o Ferramenta"},"content":{"rendered":"<h1 class=\"wp-block-heading has-text-align-center\" id=\"h-astm-grain-size-chart-for-tool-steel\">Tabela de Tamanho de Gr\u00e3o ASTM para A\u00e7o Ferramenta<\/h1>\n\n\n\n<p class=\"wp-block-paragraph\">N\u00famero de tamanho de gr\u00e3o ASTM versus di\u00e2metro m\u00e9dio do gr\u00e3o em microns, as faixas em que a escala \u00e9 agrupada, e como o n\u00famero \u00e9 definido durante a austenitiza\u00e7\u00e3o. Um resumo de refer\u00eancia da pr\u00e1tica publicada e n\u00e3o uma especifica\u00e7\u00e3o da Aobo Steel.<\/p>\n\n\n\n<h2 id=\"h-what-the-astm-grain-size-number-measures\" class=\"wp-block-heading\">O que o n\u00famero de tamanho de gr\u00e3o ASTM mede<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">O n\u00famero de tamanho de gr\u00e3o ASTM \u00e9 uma contagem, n\u00e3o uma medi\u00e7\u00e3o. Uma micrografia \u00e9 obtida com amplia\u00e7\u00e3o de 100x; os gr\u00e3os que caem dentro de uma polegada quadrada s\u00e3o contados, e a contagem \u00e9 convertida em um n\u00famero de tamanho de gr\u00e3o. Uma contagem de n gr\u00e3os por polegada quadrada a 100x fornece um n\u00famero G atrav\u00e9s de n igual a dois elevado \u00e0 pot\u00eancia G menos um, o que se rearranja para G igual a um mais o logaritmo de n dividido pelo logaritmo de dois. Dobrar a contagem de gr\u00e3os eleva o n\u00famero em exatamente um passo, de modo que cada passo na escala reduz pela metade o n\u00famero de gr\u00e3os naquela polegada quadrada. Percorrendo a tabela no sentido inverso, um passo reduz o di\u00e2metro m\u00e9dio do gr\u00e3o em cerca de 1,41, a raiz quadrada de dois que a duplica\u00e7\u00e3o da contagem fixa.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">Os contornos entre os gr\u00e3os s\u00f3 aparecem depois que a amostra \u00e9 polida e atacada, raz\u00e3o pela qual uma leitura de tamanho de gr\u00e3o \u00e9 citada ao lado do ataque e da amplia\u00e7\u00e3o com que foi obtida. A contagem n\u00e3o \u00e9 afetada pela liga, de modo que a mesma escala \u00e9 usada para uma barra de a\u00e7o carbono comum, uma tira inoxid\u00e1vel e um bloco de a\u00e7o ferramenta.<\/p>\n\n\n\n<h2 id=\"h-grain-size-number-and-average-grain-diameter\" class=\"wp-block-heading\">N\u00famero de tamanho de gr\u00e3o e di\u00e2metro m\u00e9dio de gr\u00e3o<\/h2>\n\n\n\n<h3 id=\"h-astm-number-against-average-diameter-and-band\" class=\"wp-block-heading\">N\u00famero ASTM em rela\u00e7\u00e3o ao di\u00e2metro m\u00e9dio e faixa<\/h3>\n\n\n\n<figure class=\"wp-block-table is-style-stripes\"><table class=\"has-fixed-layout\"><thead><tr><th class=\"has-text-align-left\" data-align=\"left\">N\u00ba ASTM<\/th><th class=\"has-text-align-left\" data-align=\"left\">Di\u00e2metro m\u00e9dio (m\u00edcrons)<\/th><th class=\"has-text-align-left\" data-align=\"left\">Tamanho relativo<\/th><\/tr><\/thead><tbody><tr><td class=\"has-text-align-left\" data-align=\"left\">-1<\/td><td class=\"has-text-align-left\" data-align=\"left\">510<\/td><td class=\"has-text-align-left\" data-align=\"left\">Muito grosso<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">0<\/td><td class=\"has-text-align-left\" data-align=\"left\">360<\/td><td class=\"has-text-align-left\" data-align=\"left\">Muito grosso<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">1<\/td><td class=\"has-text-align-left\" data-align=\"left\">250<\/td><td class=\"has-text-align-left\" data-align=\"left\">Grosso<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">2<\/td><td class=\"has-text-align-left\" data-align=\"left\">180<\/td><td class=\"has-text-align-left\" data-align=\"left\">Grosso<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">3<\/td><td class=\"has-text-align-left\" data-align=\"left\">125<\/td><td class=\"has-text-align-left\" data-align=\"left\">Grosso<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">4<\/td><td class=\"has-text-align-left\" data-align=\"left\">90<\/td><td class=\"has-text-align-left\" data-align=\"left\">M\u00e9dio<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">5<\/td><td class=\"has-text-align-left\" data-align=\"left\">65<\/td><td class=\"has-text-align-left\" data-align=\"left\">M\u00e9dio<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">6<\/td><td class=\"has-text-align-left\" data-align=\"left\">45<\/td><td class=\"has-text-align-left\" data-align=\"left\">M\u00e9dio<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">7<\/td><td class=\"has-text-align-left\" data-align=\"left\">32<\/td><td class=\"has-text-align-left\" data-align=\"left\">Fino<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">8<\/td><td class=\"has-text-align-left\" data-align=\"left\">22<\/td><td class=\"has-text-align-left\" data-align=\"left\">Fino<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">9<\/td><td class=\"has-text-align-left\" data-align=\"left\">16<\/td><td class=\"has-text-align-left\" data-align=\"left\">Fino<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">10<\/td><td class=\"has-text-align-left\" data-align=\"left\">11<\/td><td class=\"has-text-align-left\" data-align=\"left\">Muito fino<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">11<\/td><td class=\"has-text-align-left\" data-align=\"left\">8.0<\/td><td class=\"has-text-align-left\" data-align=\"left\">Muito fino<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">12<\/td><td class=\"has-text-align-left\" data-align=\"left\">5.6<\/td><td class=\"has-text-align-left\" data-align=\"left\">Muito fino<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">13<\/td><td class=\"has-text-align-left\" data-align=\"left\">4.0<\/td><td class=\"has-text-align-left\" data-align=\"left\">Ultrafino<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">14<\/td><td class=\"has-text-align-left\" data-align=\"left\">2.8<\/td><td class=\"has-text-align-left\" data-align=\"left\">Ultrafino<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">15<\/td><td class=\"has-text-align-left\" data-align=\"left\">2.0<\/td><td class=\"has-text-align-left\" data-align=\"left\">Ultrafino<\/td><\/tr><\/tbody><\/table><\/figure>\n\n\n\n<p class=\"wp-block-paragraph\"><em>Fonte, n\u00fameros de tamanho de gr\u00e3o ASTM, Tabela 8.1 na fonte.<\/em><\/p>\n\n\n\n<p class=\"wp-block-paragraph\"><em>O di\u00e2metro m\u00e9dio \u00e9 dado em m\u00edcrons, onde um m\u00edcron \u00e9 0,001 mm. A coluna de tamanho relativo \u00e9 o pr\u00f3prio agrupamento da escala em faixas feito pela fonte, cada faixa com tr\u00eas n\u00fameros de largura, exceto a primeira, que cobre menos um e zero.<\/em><\/p>\n\n\n\n<h2 id=\"h-which-band-a-size-falls-in\" class=\"wp-block-heading\">Em qual faixa um tamanho se enquadra<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">A coluna da direita da tabela \u00e9 o agrupamento da pr\u00f3pria fonte para a escala, n\u00e3o uma medi\u00e7\u00e3o separada. Muito grosso cobre menos um e zero e aparece apenas em lingotes grandes ou em a\u00e7o mantido pr\u00f3ximo do ponto de fus\u00e3o por muito tempo. Grosso cobre um a tr\u00eas, m\u00e9dio cobre quatro a seis, e fino cobre sete a nove; essas s\u00e3o as faixas em que um austenitizar-e-temperar normal se enquadra. Muito fino cobre 10 a 12, e ultrafino cobre 13 a 15, e ambos precisam de algo para conter os gr\u00e3os. Uma leitura de oito em um certificado de usina e uma leitura de oito em um bloco de matriz s\u00e3o o mesmo oito.<\/p>\n\n\n\n<h2 id=\"h-how-austenitizing-sets-the-grain-size\" class=\"wp-block-heading\">Como a austenitiza\u00e7\u00e3o define o tamanho de gr\u00e3o<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">O tamanho de gr\u00e3o \u00e9 definido enquanto o a\u00e7o est\u00e1 austen\u00edtico, portanto a etapa de austenitiza\u00e7\u00e3o o decide. Quando o a\u00e7o \u00e9 aquecido para a faixa austen\u00edtica, os novos gr\u00e3os de austenita est\u00e3o no seu menor tamanho imediatamente ap\u00f3s a perlita ter sido consumida e antes que o crescimento de gr\u00e3o tenha tido tempo de ocorrer. O crescimento de gr\u00e3o \u00e9 impulsionado pela tens\u00e3o superficial nos contornos de gr\u00e3o; gr\u00e3os pequenos encolhem enquanto os maiores tomam seu lugar, de modo que o tamanho m\u00e9dio se move em uma dire\u00e7\u00e3o uma vez que o a\u00e7o est\u00e1 quente. H\u00e1 duas maneiras de chegar ao menor tamanho inicial. Uma taxa de aquecimento mais r\u00e1pida nucleia austenita em mais lugares, e uma estrutura inicial mais fina produz austenita mais fina porque novos gr\u00e3os nucleiam nos contornos antigos. Uma temperatura de austenitiza\u00e7\u00e3o mais baixa dentro da faixa e um patamar mais curto reduzem tanto o tempo quanto a for\u00e7a motriz para o crescimento.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">Ciclar o a\u00e7o atrav\u00e9s da transforma\u00e7\u00e3o \u00e9 a outra alavanca. Cada passe aquece para a faixa austen\u00edtica, mant\u00e9m brevemente e tempera; cada passe parte de uma estrutura mais fina que o anterior, de modo que o n\u00famero de tamanho de gr\u00e3o sobe a cada ciclo. Repetir o ciclo v\u00e1rias vezes \u00e9 a forma padr\u00e3o de atingir n\u00fameros muito finos e ultrafinos sem alterar o grau.<\/p>\n\n\n\n<h2 id=\"h-why-the-number-matters-in-tool-steel-work\" class=\"wp-block-heading\">Por que o n\u00famero importa no trabalho com a\u00e7o ferramenta<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">Um gr\u00e3o de austenita mais fino torna a martensita mais fina tamb\u00e9m, porque o tamanho da ripa e da placa na martensita segue a austenita pr\u00e9via. A tenacidade acompanha isso, raz\u00e3o pela qual uma leitura de tamanho de gr\u00e3o importa para um a\u00e7o ferramenta usado em aplica\u00e7\u00e3o de choque. Dois lotes do mesmo grau, temperados para a mesma dureza, podem ficar dois ou tr\u00eas n\u00fameros distantes nesta escala e se comportar de forma diferente em servi\u00e7o. O n\u00famero \u00e9 tamb\u00e9m a coisa mais f\u00e1cil de verificar em rela\u00e7\u00e3o ao que foi encomendado, portanto pertence \u00e0 ordem de compra ao lado da dureza e da condi\u00e7\u00e3o de entrega, e pertence ao certificado que acompanha o a\u00e7o. Uma leitura obtida em um pequeno corpo de prova aplica-se apenas a esse corpo de prova, e o tratamento t\u00e9rmico do corpo de prova deve corresponder ao da pe\u00e7a antes que voc\u00ea possa compar\u00e1-los.<\/p>\n\n\n\n<div class=\"wp-block-group has-background is-layout-constrained wp-container-core-group-is-layout-3e4fb3d2 wp-block-group-is-layout-constrained\" style=\"border-radius:8px;background-color:#f4f8ff;margin-bottom:24px;padding-top:20px;padding-right:24px;padding-bottom:20px;padding-left:24px\">\n<p class=\"wp-block-paragraph\"><strong>Tabela de tamanho de gr\u00e3o, PDF para impress\u00e3o<\/strong><\/p>\n\n\n\n<p class=\"wp-block-paragraph\">A escala completa de menos um a quinze com o di\u00e2metro m\u00e9dio para cada n\u00famero, em um PDF com nossos dados de contato.<\/p>\n\n\n\n<div class=\"wp-block-buttons is-layout-flex wp-block-buttons-is-layout-flex\">\n<div class=\"wp-block-button\"><a class=\"wp-block-button__link wp-element-button\" href=\"https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/09\/Aobo-Steel-ASTM-Grain-Size-Chart-for-Tool-Steel.pdf\">Baixar PDF, 371 KB<\/a><\/div>\n<\/div>\n<\/div>\n\n\n\n<h2 id=\"h-related-reference-data\" class=\"wp-block-heading\">Dados de refer\u00eancia relacionados<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">As temperaturas que definem o n\u00famero est\u00e3o em <a href=\"https:\/\/aobosteel.com\/pt\/tool-steel-annealing-normalizing-temperature-chart\/\">gr\u00e1fico de temperaturas de recozimento e normaliza\u00e7\u00e3o de a\u00e7o ferramenta<\/a> e o <a href=\"https:\/\/aobosteel.com\/pt\/tool-steel-forging-temperature-guide\/\">Guia de Temperatura de Forjamento de A\u00e7o Ferramenta<\/a>, e a sequ\u00eancia completa de t\u00eampera e revenimento por grau est\u00e1 em <a href=\"https:\/\/aobosteel.com\/pt\/tool-steel-heat-treatment-guide\/\">guia de tratamento t\u00e9rmico de a\u00e7o ferramenta<\/a>. Os graus que mantemos e enviamos incluem <a href=\"https:\/\/aobosteel.com\/pt\/d2-tool-steel\/\">a\u00e7o ferramenta D2<\/a> e <a href=\"https:\/\/aobosteel.com\/pt\/h13-tool-steel\/\">A\u00e7o ferramenta H13<\/a>, e suas etapas de tratamento t\u00e9rmico est\u00e3o descritas em <a href=\"https:\/\/aobosteel.com\/pt\/d2-tool-steel-heat-treatment-guide\/\">Guia de tratamento t\u00e9rmico D2<\/a>. Como a microestrutura que resulta desse tratamento se comporta \u00e9 abordado em <a href=\"https:\/\/aobosteel.com\/pt\/tool-steel-impact-toughness-chart\/\">Tabela de tenacidade ao impacto do a\u00e7o ferramenta<\/a>. A prepara\u00e7\u00e3o e a contagem por tr\u00e1s do n\u00famero s\u00e3o abordadas em uma p\u00e1gina separada, <a href=\"https:\/\/aobosteel.com\/pt\/steel-inclusion-and-grain-size-measurement\/\">medi\u00e7\u00e3o de inclus\u00f5es e tamanho de gr\u00e3o do a\u00e7o<\/a>.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">Fonte: Metallurgy of Steel for Bladesmiths and Others Who Heat Treat and Forge Steel (John D. Verhoeven).<\/p>","protected":false},"excerpt":{"rendered":"<p>ASTM Grain Size Chart for Tool Steel ASTM grain size number versus average grain diameter in microns, the bands the scale is grouped into, and how the number is set during austenitizing. A reference summary of published practice and not an Aobo Steel specification. What the ASTM grain size number measures The ASTM grain size [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":0,"parent":0,"menu_order":0,"comment_status":"closed","ping_status":"closed","template":"","meta":{"_uag_custom_page_level_css":"","site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"default","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"disabled","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","ast-disable-related-posts":"","theme-transparent-header-meta":"","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"set","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"footnotes":""},"class_list":["post-20327","page","type-page","status-publish","hentry"],"yoast_head":"<!-- This site is optimized with the Yoast SEO Premium plugin v28.8 (Yoast SEO v28.8) - https:\/\/yoast.com\/product\/yoast-seo-premium-wordpress\/ -->\n<title>ASTM Grain Size Chart for Tool Steel | Aobo Steel<\/title>\n<meta name=\"description\" content=\"ASTM grain size number against average grain diameter in microns, the bands from very coarse to ultrafine, and how austenitizing sets the number in tool steel.\" \/>\n<meta name=\"robots\" content=\"index, follow, max-snippet:-1, max-image-preview:large, max-video-preview:-1\" \/>\n<link rel=\"canonical\" href=\"https:\/\/aobosteel.com\/pt\/astm-grain-size-chart-tool-steel\/\" \/>\n<meta property=\"og:locale\" content=\"pt_BR\" \/>\n<meta property=\"og:type\" content=\"article\" \/>\n<meta property=\"og:title\" content=\"ASTM Grain Size Chart for Tool Steel\" \/>\n<meta property=\"og:description\" content=\"ASTM grain size number against average grain diameter in microns, the bands from very coarse to ultrafine, and how austenitizing sets the number in tool steel.\" \/>\n<meta property=\"og:url\" content=\"https:\/\/aobosteel.com\/pt\/astm-grain-size-chart-tool-steel\/\" \/>\n<meta property=\"og:site_name\" content=\"AoboSteel\" \/>\n<meta property=\"article:publisher\" content=\"https:\/\/www.facebook.com\/profile.php?id=61565368220197\" \/>\n<meta property=\"article:modified_time\" content=\"2026-10-19T14:56:45+00:00\" \/>\n<meta name=\"twitter:card\" content=\"summary_large_image\" \/>\n<meta name=\"twitter:label1\" content=\"Est. tempo de leitura\" \/>\n\t<meta name=\"twitter:data1\" content=\"5 minutos\" \/>\n<script type=\"application\/ld+json\" class=\"yoast-schema-graph\">{\"@context\":\"https:\\\/\\\/schema.org\",\"@graph\":[{\"@type\":\"TechArticle\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/astm-grain-size-chart-tool-steel\\\/#article\",\"isPartOf\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/astm-grain-size-chart-tool-steel\\\/\"},\"author\":{\"name\":\"Evan\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#\\\/schema\\\/person\\\/96118415c30ca6bb52eaf1127b052ef7\"},\"headline\":\"ASTM Grain Size Chart for Tool Steel\",\"datePublished\":\"2026-09-29T23:08:32+00:00\",\"dateModified\":\"2026-10-19T14:56:45+00:00\",\"mainEntityOfPage\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/astm-grain-size-chart-tool-steel\\\/\"},\"wordCount\":957,\"publisher\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#organization\"},\"inLanguage\":\"pt-BR\"},{\"@type\":\"WebPage\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/astm-grain-size-chart-tool-steel\\\/\",\"url\":\"https:\\\/\\\/aobosteel.com\\\/astm-grain-size-chart-tool-steel\\\/\",\"name\":\"ASTM Grain Size Chart for Tool Steel | Aobo Steel\",\"isPartOf\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#website\"},\"datePublished\":\"2026-09-29T23:08:32+00:00\",\"dateModified\":\"2026-10-19T14:56:45+00:00\",\"description\":\"ASTM grain size number against average grain diameter in microns, the bands from very coarse to ultrafine, and how austenitizing sets the number in tool steel.\",\"breadcrumb\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/astm-grain-size-chart-tool-steel\\\/#breadcrumb\"},\"inLanguage\":\"pt-BR\",\"potentialAction\":[{\"@type\":\"ReadAction\",\"target\":[\"https:\\\/\\\/aobosteel.com\\\/astm-grain-size-chart-tool-steel\\\/\"]}]},{\"@type\":\"BreadcrumbList\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/astm-grain-size-chart-tool-steel\\\/#breadcrumb\",\"itemListElement\":[{\"@type\":\"ListItem\",\"position\":1,\"name\":\"\u9996\u9875\",\"item\":\"https:\\\/\\\/aobosteel.com\\\/\"},{\"@type\":\"ListItem\",\"position\":2,\"name\":\"ASTM Grain Size Chart for Tool Steel\"}]},{\"@type\":\"WebSite\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#website\",\"url\":\"https:\\\/\\\/aobosteel.com\\\/\",\"name\":\"AoboSteel\",\"description\":\"\",\"publisher\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#organization\"},\"potentialAction\":[{\"@type\":\"SearchAction\",\"target\":{\"@type\":\"EntryPoint\",\"urlTemplate\":\"https:\\\/\\\/aobosteel.com\\\/?s={search_term_string}\"},\"query-input\":{\"@type\":\"PropertyValueSpecification\",\"valueRequired\":true,\"valueName\":\"search_term_string\"}}],\"inLanguage\":\"pt-BR\"},{\"@type\":\"Organization\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#organization\",\"name\":\"AoboSteel\",\"url\":\"https:\\\/\\\/aobosteel.com\\\/\",\"logo\":{\"@type\":\"ImageObject\",\"inLanguage\":\"pt-BR\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#\\\/schema\\\/logo\\\/image\\\/\",\"url\":\"https:\\\/\\\/aobosteel.com\\\/wp-content\\\/uploads\\\/2025\\\/01\\\/cropped-aobo-steel-1.avif\",\"contentUrl\":\"https:\\\/\\\/aobosteel.com\\\/wp-content\\\/uploads\\\/2025\\\/01\\\/cropped-aobo-steel-1.avif\",\"width\":1052,\"height\":592,\"caption\":\"AoboSteel\"},\"image\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#\\\/schema\\\/logo\\\/image\\\/\"},\"sameAs\":[\"https:\\\/\\\/www.facebook.com\\\/profile.php?id=61565368220197\",\"https:\\\/\\\/www.linkedin.com\\\/in\\\/aobosteel-evan\\\/\"]},{\"@type\":\"Person\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#\\\/schema\\\/person\\\/96118415c30ca6bb52eaf1127b052ef7\",\"name\":\"Evan\",\"image\":{\"@type\":\"ImageObject\",\"inLanguage\":\"pt-BR\",\"@id\":\"https:\\\/\\\/secure.gravatar.com\\\/avatar\\\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g\",\"url\":\"https:\\\/\\\/secure.gravatar.com\\\/avatar\\\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g\",\"contentUrl\":\"https:\\\/\\\/secure.gravatar.com\\\/avatar\\\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g\",\"caption\":\"Evan\"},\"sameAs\":[\"http:\\\/\\\/www.aobosteel.com\",\"https:\\\/\\\/www.facebook.com\\\/profile.php?id=61565368220197\",\"https:\\\/\\\/www.instagram.com\\\/aobosteel\\\/\",\"https:\\\/\\\/www.linkedin.com\\\/in\\\/aobosteel-evan\\\/\",\"https:\\\/\\\/x.com\\\/AobosteelEvan\",\"https:\\\/\\\/www.youtube.com\\\/@aobosteel\"],\"url\":\"https:\\\/\\\/aobosteel.com\\\/pt\\\/blog\\\/author\\\/admin\\\/\"}]}<\/script>\n<!-- \/ Yoast SEO Premium plugin. -->","yoast_head_json":{"title":"Tabela de tamanho de gr\u00e3o ASTM para a\u00e7o ferramenta | Aobo Steel","description":"N\u00famero de tamanho de gr\u00e3o ASTM versus di\u00e2metro m\u00e9dio de gr\u00e3o em microns, as faixas de muito grosso a ultrafino e como a austenitiza\u00e7\u00e3o define o n\u00famero no a\u00e7o ferramenta.","robots":{"index":"index","follow":"follow","max-snippet":"max-snippet:-1","max-image-preview":"max-image-preview:large","max-video-preview":"max-video-preview:-1"},"canonical":"https:\/\/aobosteel.com\/pt\/astm-grain-size-chart-tool-steel\/","og_locale":"pt_BR","og_type":"article","og_title":"ASTM Grain Size Chart for Tool Steel","og_description":"ASTM grain size number against average grain diameter in microns, the bands from very coarse to ultrafine, and how austenitizing sets the number in tool steel.","og_url":"https:\/\/aobosteel.com\/pt\/astm-grain-size-chart-tool-steel\/","og_site_name":"AoboSteel","article_publisher":"https:\/\/www.facebook.com\/profile.php?id=61565368220197","article_modified_time":"2026-10-19T14:56:45+00:00","twitter_card":"summary_large_image","twitter_misc":{"Est. tempo de leitura":"5 minutos"},"schema":{"@context":"https:\/\/schema.org","@graph":[{"@type":"TechArticle","@id":"https:\/\/aobosteel.com\/astm-grain-size-chart-tool-steel\/#article","isPartOf":{"@id":"https:\/\/aobosteel.com\/astm-grain-size-chart-tool-steel\/"},"author":{"name":"Evan","@id":"https:\/\/aobosteel.com\/#\/schema\/person\/96118415c30ca6bb52eaf1127b052ef7"},"headline":"ASTM Grain Size Chart for Tool Steel","datePublished":"2026-09-29T23:08:32+00:00","dateModified":"2026-10-19T14:56:45+00:00","mainEntityOfPage":{"@id":"https:\/\/aobosteel.com\/astm-grain-size-chart-tool-steel\/"},"wordCount":957,"publisher":{"@id":"https:\/\/aobosteel.com\/#organization"},"inLanguage":"pt-BR"},{"@type":"WebPage","@id":"https:\/\/aobosteel.com\/astm-grain-size-chart-tool-steel\/","url":"https:\/\/aobosteel.com\/astm-grain-size-chart-tool-steel\/","name":"Tabela de tamanho de gr\u00e3o ASTM para a\u00e7o ferramenta | Aobo Steel","isPartOf":{"@id":"https:\/\/aobosteel.com\/#website"},"datePublished":"2026-09-29T23:08:32+00:00","dateModified":"2026-10-19T14:56:45+00:00","description":"N\u00famero de tamanho de gr\u00e3o ASTM versus di\u00e2metro m\u00e9dio de gr\u00e3o em microns, as faixas de muito grosso a ultrafino e como a austenitiza\u00e7\u00e3o define o n\u00famero no a\u00e7o ferramenta.","breadcrumb":{"@id":"https:\/\/aobosteel.com\/astm-grain-size-chart-tool-steel\/#breadcrumb"},"inLanguage":"pt-BR","potentialAction":[{"@type":"ReadAction","target":["https:\/\/aobosteel.com\/astm-grain-size-chart-tool-steel\/"]}]},{"@type":"BreadcrumbList","@id":"https:\/\/aobosteel.com\/astm-grain-size-chart-tool-steel\/#breadcrumb","itemListElement":[{"@type":"ListItem","position":1,"name":"\u9996\u9875","item":"https:\/\/aobosteel.com\/"},{"@type":"ListItem","position":2,"name":"ASTM Grain Size Chart for Tool Steel"}]},{"@type":"WebSite","@id":"https:\/\/aobosteel.com\/#website","url":"https:\/\/aobosteel.com\/","name":"AoboSteel","description":"","publisher":{"@id":"https:\/\/aobosteel.com\/#organization"},"potentialAction":[{"@type":"SearchAction","target":{"@type":"EntryPoint","urlTemplate":"https:\/\/aobosteel.com\/?s={search_term_string}"},"query-input":{"@type":"PropertyValueSpecification","valueRequired":true,"valueName":"search_term_string"}}],"inLanguage":"pt-BR"},{"@type":"Organization","@id":"https:\/\/aobosteel.com\/#organization","name":"AoboSteel","url":"https:\/\/aobosteel.com\/","logo":{"@type":"ImageObject","inLanguage":"pt-BR","@id":"https:\/\/aobosteel.com\/#\/schema\/logo\/image\/","url":"https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/01\/cropped-aobo-steel-1.avif","contentUrl":"https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/01\/cropped-aobo-steel-1.avif","width":1052,"height":592,"caption":"AoboSteel"},"image":{"@id":"https:\/\/aobosteel.com\/#\/schema\/logo\/image\/"},"sameAs":["https:\/\/www.facebook.com\/profile.php?id=61565368220197","https:\/\/www.linkedin.com\/in\/aobosteel-evan\/"]},{"@type":"Person","@id":"https:\/\/aobosteel.com\/#\/schema\/person\/96118415c30ca6bb52eaf1127b052ef7","name":"Evan","image":{"@type":"ImageObject","inLanguage":"pt-BR","@id":"https:\/\/secure.gravatar.com\/avatar\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g","url":"https:\/\/secure.gravatar.com\/avatar\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g","contentUrl":"https:\/\/secure.gravatar.com\/avatar\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g","caption":"Evan"},"sameAs":["http:\/\/www.aobosteel.com","https:\/\/www.facebook.com\/profile.php?id=61565368220197","https:\/\/www.instagram.com\/aobosteel\/","https:\/\/www.linkedin.com\/in\/aobosteel-evan\/","https:\/\/x.com\/AobosteelEvan","https:\/\/www.youtube.com\/@aobosteel"],"url":"https:\/\/aobosteel.com\/pt\/blog\/author\/admin\/"}]}},"uagb_featured_image_src":{"full":false,"thumbnail":false,"medium":false,"medium_large":false,"large":false,"1536x1536":false,"2048x2048":false,"trp-custom-language-flag":false},"uagb_author_info":{"display_name":"Evan","author_link":"https:\/\/aobosteel.com\/pt\/blog\/author\/admin\/"},"uagb_comment_info":0,"uagb_excerpt":"ASTM Grain Size Chart for Tool Steel ASTM grain size number versus average grain diameter in microns, the bands the scale is grouped into, and how the number is set during austenitizing. A reference summary of published practice and not an Aobo Steel specification. What the ASTM grain size number measures The ASTM grain size&hellip;","rttpg_featured_image_url":null,"rttpg_author":{"display_name":"Evan","author_link":"https:\/\/aobosteel.com\/pt\/blog\/author\/admin\/"},"rttpg_comment":0,"rttpg_category":null,"rttpg_excerpt":"ASTM Grain Size Chart for Tool Steel ASTM grain size number versus average grain diameter in microns, the bands the scale is grouped into, and how the number is set during austenitizing. A reference summary of published practice and not an Aobo Steel specification. What the ASTM grain size number measures The ASTM grain size&hellip;","_links":{"self":[{"href":"https:\/\/aobosteel.com\/pt\/wp-json\/wp\/v2\/pages\/20327","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/aobosteel.com\/pt\/wp-json\/wp\/v2\/pages"}],"about":[{"href":"https:\/\/aobosteel.com\/pt\/wp-json\/wp\/v2\/types\/page"}],"author":[{"embeddable":true,"href":"https:\/\/aobosteel.com\/pt\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/aobosteel.com\/pt\/wp-json\/wp\/v2\/comments?post=20327"}],"version-history":[{"count":8,"href":"https:\/\/aobosteel.com\/pt\/wp-json\/wp\/v2\/pages\/20327\/revisions"}],"predecessor-version":[{"id":23710,"href":"https:\/\/aobosteel.com\/pt\/wp-json\/wp\/v2\/pages\/20327\/revisions\/23710"}],"wp:attachment":[{"href":"https:\/\/aobosteel.com\/pt\/wp-json\/wp\/v2\/media?parent=20327"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}