{"id":25012,"date":"2026-11-04T23:10:26","date_gmt":"2026-11-04T15:10:26","guid":{"rendered":"https:\/\/aobosteel.com\/?page_id=25012"},"modified":"2026-11-04T23:10:26","modified_gmt":"2026-11-04T15:10:26","slug":"aluminum-extrusion-press-selection","status":"publish","type":"page","link":"https:\/\/aobosteel.com\/ko\/aluminum-extrusion-press-selection\/","title":{"rendered":"\ud504\ub808\uc2a4 \uc120\ud0dd: \ube44\uc555\ub825, \uc9c1\uc811\uc2dd \ub610\ub294 \uac04\uc811\uc2dd, \uadf8\ub9ac\uace0 \ub2e4\uc774 \ub4a4\uc758 \ub77c\uc778"},"content":{"rendered":"<h1 class=\"wp-block-heading\">\ud504\ub808\uc2a4 \uc120\ud0dd: \ube44\uc555\ub825, \uc9c1\uc811\uc2dd \ub610\ub294 \uac04\uc811\uc2dd, \uadf8\ub9ac\uace0 \ub2e4\uc774 \ub4a4\uc758 \ub77c\uc778<\/h1>\n\n\n\n<p class=\"wp-block-paragraph\">\ud504\ub808\uc2a4\ub294 \ud1a4\uc218\ub85c \uad6c\ub9e4\ud558\uace0 \uc555\ub825\uc73c\ub85c \uc0ac\uc6a9\ub429\ub2c8\ub2e4. \ud1a4\uc218\ub294 \uc720\uc555 \uc7a5\uce58\uc5d0 \uc758\ud574 \uace0\uc815\ub418\uba70, \ube4c\ub9bf\uc774 \uc2e4\uc81c\ub85c \ubc1b\ub294 \uc555\ub825\uc740 \uadf8 \ud1a4\uc218\ub97c \ucee8\ud14c\uc774\ub108 \ubcf4\uc5b4 \uba74\uc801\uc73c\ub85c \ub098\ub208 \uac12\uc774\ubbc0\ub85c, \ucee8\ud14c\uc774\ub108\ub97c \uad50\uccb4\ud558\uba74 \uac19\uc740 \ud504\ub808\uc2a4\ub3c4 \ub2e4\ub978 \uae30\uacc4\uac00 \ub429\ub2c8\ub2e4. 254 mm \ubcf4\uc5b4\uc758 2,500\ud1a4 \ud504\ub808\uc2a4\ub294 439 MPa\uc758 \ube44\uc555\ub825\uc744 \ubc1c\uc0dd\uc2dc\ud0a4\uace0, 203 mm \ubcf4\uc5b4\uc758 \uac19\uc740 \ud504\ub808\uc2a4\ub294 685 MPa\ub97c \ubc1c\uc0dd\uc2dc\ud0b5\ub2c8\ub2e4. \ud558\ub098\ub294 \uc800\uc628\uc5d0\uc11c \uacbd\uc9c8 \ud569\uae08\uc744 \uc555\ucd9c\ud560 \uc218 \uc788\uace0 \ub2e4\ub978 \ud558\ub098\ub294 \uadf8\ub807\uc9c0 \uc54a\uc73c\uba70, \uc5b4\ub290 \uc218\uce58\ub3c4 \uba85\ud310\uc5d0 \ud45c\uc2dc\ub418\uc9c0 \uc54a\uc2b5\ub2c8\ub2e4. \uc774 \ud398\uc774\uc9c0\ub294 \uadf8 \uacc4\uc0b0, \uc9c1\uc811\uc2dd\uacfc \uac04\uc811\uc2dd \uc555\ucd9c\uc758 \uc120\ud0dd, \uadf8\ub9ac\uace0 \ube4c\ub9bf\uacfc \uc2dc\ud6a8\ub85c \uc0ac\uc774\uc5d0\uc11c \ud504\ub808\uc2a4\uac00 \ubcd1\ubaa9\uc774 \ub418\ub294\uc9c0 \uc5ec\ubd80\ub97c \uacb0\uc815\ud558\ub294 \uc124\ube44\uc5d0 \uad00\ud55c \uac83\uc785\ub2c8\ub2e4.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">\ud1a4\uc218\ub294 \ub2a5\ub825\uc774 \uc544\ub2c8\uba70, \ube44\uc555\ub825\uc774 \ub2a5\ub825\uc785\ub2c8\ub2e4<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">\uacf5\uac1c\ub41c \uc120\ud0dd \uaddc\uce59\uc740 \uc555\ucd9c\uc5d0 \ud544\uc694\ud55c \ub2e8\uc704 \uc555\ub825\uc774 \uc8fc\uc694 \uace0\ub824 \uc0ac\ud56d\uc774\uba70, \ud504\ub808\uc2a4\uc758 \ube44\uc555\ub825\uc774 \uc774\ub97c \ucd08\uacfc\ud574\uc57c \ud55c\ub2e4\ub294 \uac83\uc785\ub2c8\ub2e4. \uc774\ub294 &#8220;\ucda9\ubd84\ud55c \ud1a4\uc218\ub97c \uad6c\ub9e4\ud558\ub77c&#8221;\ub294 \uac83\uacfc \ub2e4\ub978 \uc9c4\uc220\uc778\ub370, \ucee8\ud14c\uc774\ub108 \ubcf4\uc5b4\ub97c \ud0a4\uc6b0\uba74 \uac19\uc740 \ud1a4\uc218\uc5d0\uc11c \ube44\uc555\ub825\uc774 \ub0ae\uc544\uc9c0\uace0 \uc555\ucd9c \ub2a5\ub825\ub3c4 \uadf8\uc5d0 \ub530\ub77c \ub5a8\uc5b4\uc9c0\uae30 \ub54c\ubb38\uc785\ub2c8\ub2e4.<\/p>\n\n\n\n<figure class=\"wp-block-table is-style-stripes\"><table class=\"has-fixed-layout\"><thead><tr><th class=\"has-text-align-left\" data-align=\"left\">\ud504\ub808\uc2a4 \ub2a5\ub825<\/th><th class=\"has-text-align-left\" data-align=\"left\">\ubcf4\uc5b4 1<\/th><th class=\"has-text-align-left\" data-align=\"left\">\ubcf4\uc5b4 2<\/th><th class=\"has-text-align-left\" data-align=\"left\">\ubcf4\uc5b4 3<\/th><\/tr><\/thead><tbody><tr><td class=\"has-text-align-left\" data-align=\"left\">500 t (5.0 MN)<\/td><td class=\"has-text-align-left\" data-align=\"left\">76.2 mm &mdash; 971 MPa<\/td><td class=\"has-text-align-left\" data-align=\"left\">101.6 mm &mdash; 547 MPa<\/td><td class=\"has-text-align-left\" data-align=\"left\">127.0 mm &mdash; 352 MPa<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">1,000 t (10.0 MN)<\/td><td class=\"has-text-align-left\" data-align=\"left\">101.6 mm &mdash; 1,089 MPa<\/td><td class=\"has-text-align-left\" data-align=\"left\">127.0 mm &mdash; 703 MPa<\/td><td class=\"has-text-align-left\" data-align=\"left\">152.4 mm &mdash; 487 MPa<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">1,500 t (15.0 MN)<\/td><td class=\"has-text-align-left\" data-align=\"left\">152.4 mm &mdash; 731 MPa<\/td><td class=\"has-text-align-left\" data-align=\"left\">177.8 mm &mdash; 537 MPa<\/td><td class=\"has-text-align-left\" data-align=\"left\">203.2 mm &mdash; 407 MPa<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">2,000 t (20.0 MN)<\/td><td class=\"has-text-align-left\" data-align=\"left\">177.8 mm &mdash; 716 MPa<\/td><td class=\"has-text-align-left\" data-align=\"left\">203.2 mm &mdash; 548 MPa<\/td><td class=\"has-text-align-left\" data-align=\"left\">228.6 mm &mdash; 434 MPa<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">2,500 t (25.0 MN)<\/td><td class=\"has-text-align-left\" data-align=\"left\">203.2 mm &mdash; 685 MPa<\/td><td class=\"has-text-align-left\" data-align=\"left\">228.6 mm &mdash; 542 MPa<\/td><td class=\"has-text-align-left\" data-align=\"left\">254.0 mm &mdash; 439 MPa<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">3,500 t (35.0 MN)<\/td><td class=\"has-text-align-left\" data-align=\"left\">228.6 mm &mdash; 759 MPa<\/td><td class=\"has-text-align-left\" data-align=\"left\">254.0 mm &mdash; 615 MPa<\/td><td class=\"has-text-align-left\" data-align=\"left\">279.4 mm &mdash; 508 MPa<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">4,000 t (40.0 MN)<\/td><td class=\"has-text-align-left\" data-align=\"left\">254.0 mm &mdash; 703 MPa<\/td><td class=\"has-text-align-left\" data-align=\"left\">279.4 mm &mdash; 581 MPa<\/td><td class=\"has-text-align-left\" data-align=\"left\">304.8 mm &mdash; 487 MPa<\/td><\/tr><\/tbody><\/table><\/figure>\n\n\n\n<p class=\"wp-block-paragraph\"><em>\ud45c\uc900 \ud504\ub808\uc2a4 \ub2a5\ub825, \uc77c\ubc18\uc801\uc73c\ub85c \ud568\uaed8 \uc81c\uacf5\ub418\ub294 \ucee8\ud14c\uc774\ub108 \ubcf4\uc5b4, \uadf8\ub9ac\uace0 \uac01 \uc870\ud569\uc774 \ubc1c\uc0dd\uc2dc\ud0a4\ub294 \ube44\uc555\ub825. \uacf5\uac1c\ub41c \uac12\uc73c\ub85c, \uc704 \ub2a5\ub825\uc5d0 \ub300\ud574 \uc7ac\ud604\ud55c \uac83\uc785\ub2c8\ub2e4. \ucd9c\ucc98\uc5d0\ub294 500\ud1a4\uc5d0\uc11c 4,000\ud1a4\uae4c\uc9c0 \ubaa8\ub4e0 \ub2a5\ub825\uc774 \ub098\uc5f4\ub418\uc5b4 \uc788\uc2b5\ub2c8\ub2e4.<\/em><\/p>\n\n\n\n<p class=\"wp-block-paragraph\">\ud45c\uc5d0\uc11c \ub450 \uac00\uc9c0 \uc2e4\uc6a9\uc801 \ud574\uc11d\uc774 \ub098\uc635\ub2c8\ub2e4. \uccab\uc9f8, \uace0\uac1d\uc774 \ud615\uc0c1\uc758 \uac00\ub2a5 \uc5ec\ubd80\ub97c \ubb3c\uc744 \ub54c \uc778\uc6a9\ud574\uc57c \ud560 \uc218\uce58\ub294 \ud1a4\uc218\uac00 \uc544\ub2c8\ub77c \ucee8\ud14c\uc774\ub108 \ubcf4\uc5b4\uc785\ub2c8\ub2e4. 279 mm\uc758 3,500\ud1a4 \ud504\ub808\uc2a4\ub294 178 mm\uc758 2,000\ud1a4 \ud504\ub808\uc2a4\ubcf4\ub2e4 \uc81c\uacf1\ubc00\ub9ac\ubbf8\ud130\ub2f9 \ub354 \uc57d\ud55c \uae30\uacc4\uc785\ub2c8\ub2e4. \ub458\uc9f8, \ud544\uc694\ud55c \uc555\ub825 \uc790\uccb4\ub294 \uc0c1\uc218\uac00 \uc544\ub2d9\ub2c8\ub2e4. \uc774\ub294 \ud569\uae08\uacfc \uadf8 \uc0c1\ud0dc, \uc555\ucd9c\ube44, \ube4c\ub9bf \uae38\uc774\uc640 \uc628\ub3c4, \uc555\ucd9c \uc18d\ub3c4, \ud615\uc0c1\uc758 \uc678\uc811\uc6d0\uc5d0 \ub530\ub77c \ubcc0\ud569\ub2c8\ub2e4. \ud070 \uc6d0\uc758 \uc911\ud615 \ub2e8\uba74\uc740 \uace0\ub2a5\ub825 \uc9c1\uc811\uc2dd \ud504\ub808\uc2a4\uc5d0 \uc801\ud569\ud558\uba70, \uc791\uace0 \uc587\uc73c\uba70 \uc5c4\uaca9\ud55c \uacf5\ucc28\uc758 \uc791\uc5c5\uc740 \uac04\uc811\uc2dd \uacf5\uc815\uc774 \uadf8 \uc790\ub9ac\ub97c \ucc28\uc9c0\ud558\ub294 \ubd84\uc57c\uc785\ub2c8\ub2e4.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">\uc9c1\uc811\uc2dd, \uac04\uc811\uc2dd, \uadf8\ub9ac\uace0 \uadf8 \uc0ac\uc774\uc758 \ub9c8\ucc30 \ucc28\uc774<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">\uc9c1\uc811\uc2dd \uc555\ucd9c\uc5d0\uc11c\ub294 \ube4c\ub9bf\uc774 \ucee8\ud14c\uc774\ub108 \uc548\uc5d0\uc11c \ubbf8\ub044\ub7ec\uc9c0\uba70, \uadf8 \ub9c8\ucc30\uc774 \ub450 \uacf5\uc815\uc744 \uad6c\ubd84\ud569\ub2c8\ub2e4. \uac04\uc811\uc2dd \uc555\ucd9c\uc5d0\uc11c\ub294 \ub2e4\uc774\uac00 \ucee8\ud14c\uc774\ub108\ub97c \uad00\ud1b5\ud558\ub294 \uc911\uacf5 \uc2a4\ud15c\uc758 \uc804\uba74\uc5d0 \uc704\uce58\ud558\uba70, \ube4c\ub9bf\uacfc \ucee8\ud14c\uc774\ub108 \uc0ac\uc774\uc5d0 \uc0c1\ub300\uc801 \ubcc0\uc704\uac00 \uc804\ud600 \uc5c6\uc2b5\ub2c8\ub2e4. \uacf5\uac1c\ub41c \uacb0\uacfc\ub294 \ud504\ub808\uc2a4 \uc0ac\uc591\uc744 \ubc14\uafc0 \ub9cc\ud07c \ud07d\ub2c8\ub2e4. \uac04\uc811\uc2dd \uc555\ucd9c\uc740 \ube4c\ub9bf \uc911\ub7c9\uacfc \uc555\ucd9c \uc18d\ub3c4\ub97c \ub450 \ubc30\ub85c \ub298\ub9b4 \uc218 \uc788\uc73c\uba70, \uc555\ucd9c\ub825\uc740 30~45% \uac10\uc18c\ud569\ub2c8\ub2e4.<\/p>\n\n\n\n<figure class=\"wp-block-table is-style-stripes\"><table class=\"has-fixed-layout\"><thead><tr><th class=\"has-text-align-left\" data-align=\"left\">\uac04\uc811 \uc555\ucd9c\uc758 \uc7a5\uc810<\/th><th class=\"has-text-align-left\" data-align=\"left\">\uac04\uc811 \uc555\ucd9c\uc758 \ub2e8\uc810<\/th><\/tr><\/thead><tbody><tr><td class=\"has-text-align-left\" data-align=\"left\">\ub354 \uae34 \ucd08\uae30 \ube4c\ub9bf<\/td><td class=\"has-text-align-left\" data-align=\"left\">\ud45c\uba74 \uacb0\ud568 \ubc29\uc9c0\ub97c \uc704\ud574 \ube4c\ub9bf \uc2a4\ud0a8\uc744 \uae30\uacc4 \uac00\uacf5\ud574\uc57c \ud568<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\ub9ce\uc740 \uc18c\uc7ac\uc5d0\uc11c \ub354 \ub192\uc740 \uc555\ucd9c \uc18d\ub3c4<\/td><td class=\"has-text-align-left\" data-align=\"left\">\uc911\uacf5 \uc2a4\ud15c\uc758 \ub0b4\uacbd\uc5d0 \uc758\ud574 \uc555\ucd9c \ud06c\uae30\uac00 \uc81c\ud55c\ub428<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\ub354 \uc587\uc740 \ubc84\ud2b8 \ub2e8\ubd80<\/td><td class=\"has-text-align-left\" data-align=\"left\">\ub2e4\uc774 \ucde8\uae09\uc774 \uc5b4\ub824\uc6c0<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\uae38\uc774 \ubc29\ud5a5\uc73c\ub85c \ub354 \uade0\uc77c\ud55c \uc870\uc9c1<\/td><td class=\"has-text-align-left\" data-align=\"left\">\ub3d9\uc77c \uc6a9\ub7c9\uc758 \uc9c1\uc811 \ud504\ub808\uc2a4\ubcf4\ub2e4 \uc791\uc740 \uc678\uc811\uc6d0<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\uc804\uccb4 \uae38\uc774\uc5d0 \uac78\uccd0 \ub354 \uc587\uc740 \ub2e8\uba74\uacfc \ub354 \uc881\uc740 \uacf5\ucc28<\/td><td class=\"has-text-align-left\" data-align=\"left\">\uc2a4\ud15c\uc5d0 \ub354 \ub192\uc740 \uc751\ub825<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\ub354 \uade0\uc77c\ud55c \ucee8\ud14c\uc774\ub108 \ubc0f \ube4c\ub9bf \uc628\ub3c4; \ub354 \uae34 \ucee8\ud14c\uc774\ub108 \ubc0f \ub77c\uc774\ub108 \uc218\uba85<\/td><td class=\"has-text-align-left\" data-align=\"left\">\ubcf5\ud569 \ud504\ub808\uc2a4\ub294 \uac04\uc811 \uc555\ucd9c\uc758 \uc7a5\uc810\uc744 \ubcf4\uc0c1\ud558\uc9c0 \ubabb\ud568<\/td><\/tr><\/tbody><\/table><\/figure>\n\n\n\n<p class=\"wp-block-paragraph\"><em>\uc9c1\uc811 \uc555\ucd9c\uacfc \uac04\uc811 \uc555\ucd9c\uc758 \uacf5\uac1c\ub41c \ube44\uad50. \uc2a4\uce98\ud551 \uc694\uad6c \uc0ac\ud56d\uc740 \ud504\ub808\uc2a4 \uc81c\uc791\uc0ac\uac00 \uc544\ub2c8\ub77c \ube4c\ub9bf \uacf5\uae09\uc5c5\uccb4\uc5d0 \ubd80\uacfc\ub418\ub294 \ud56d\ubaa9\uc774\ub2e4.<\/em><\/p>\n\n\n\n<p class=\"wp-block-paragraph\">\uacbd\uc9c8 \ud569\uae08\uc758 \uc9c1\uc811 \uc555\ucd9c \u2014 \uc6d0\ubb38\uc5d0\uc11c 2024 \ubc0f 7075\ub85c \uba85\uc2dc \u2014 \uc740 \uc790\uccb4\uc801\uc778 \ud55c\uacc4 \ubaa9\ub85d\uc744 \uac16\ub294\ub2e4: \ube4c\ub9bf \uc911\ub7c9, \uc555\ucd9c \uc18d\ub3c4, \ud68c\uc218\uc728, \uc0dd\uc0b0\uc131, \uce58\uc218 \uc815\ubc00\ub3c4, \uadf8\ub9ac\uace0 \uae38\uc774 \ubc29\ud5a5\uc758 \uc870\uc9c1 \uade0\uc77c\uc131. \uc774 \ubaa9\ub85d\uc774 \ud56d\uacf5\uc6b0\uc8fc \uc791\uc5c5\uc744 \uc218\ud589\ud558\ub294 \uacf5\uc7a5\uc774 \uac04\uc811 \ud504\ub808\uc2a4\ub97c \uace0\ub824\ud558\ub294 \uc774\uc720\uc774\ub2e4.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">\uc774\ub4e4 \uc0ac\uc774\uc5d0 \uc138 \ubc88\uc9f8 \uacf5\uc815\uc774 \uc788\uc73c\uba70, \ub4dc\ubb3c\uc9c0\ub9cc \uc774\ub984\uc73c\ub85c \uc54c\uc544\ub458 \uac00\uce58\uac00 \uc788\ub2e4: \ud65c\uc131 \ub9c8\ucc30\ub825\uc744 \uc774\uc6a9\ud55c \uc555\ucd9c, \uc989 \ud65c\uc131 \uac04\uc811 \uc555\ucd9c\ub85c, \ucee8\ud14c\uc774\ub108 \ub610\ub294 \ub2e4\uc774\uac00 \ub7a8\uc5d0 \ub300\ud574 \uc0c1\ub300\uc801\uc73c\ub85c \uc6c0\uc9c1\uc5ec \ucee8\ud14c\uc774\ub108 \ub9c8\ucc30\uc774 \uae08\uc18d \ud750\ub984\uc5d0 \ubc18\ud558\ub294 \ub300\uc2e0 \uae08\uc18d \ud750\ub984 \ubc29\ud5a5\uc73c\ub85c \uc791\uc6a9\ud558\uac8c \ud55c\ub2e4. \uacf5\uac1c\ub41c \uc218\uce58\uc5d0 \ub530\ub974\uba74 \uc9c1\uc811 \uacf5\uc815\uc758 3~4\ubc30, \uac04\uc811 \uacf5\uc815\uc758 2~3\ubc30 \uc18d\ub3c4\ub85c \uc555\ucd9c\ub418\uba70 \uacb0\ud568\uc774 \uc801\uace0 \uc870\uc9c1\uc774 \ub354 \uade0\uc77c\ud558\ub2e4. 1988\ub144\ubd80\ud130 \ub7ec\uc2dc\uc544\uc5d0\uc11c 1,600\ud1a4 \ubc0f 3,500\ud1a4 \ud504\ub808\uc2a4\ub85c \uc0b0\uc5c5\uc801\uc73c\ub85c \uc0ac\uc6a9\ub418\uc5b4 \uc654\ub2e4.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">\uc815\ub82c\uacfc \uac15\uc131: \uc544\ubb34\ub3c4 \ub450 \ubc88 \uc77d\uc9c0 \uc54a\ub294 \uc0ac\uc591 \ubd80\ubd84<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">\ub2e4\uc774\uac00 \uc124\uacc4\ub300\ub85c \uc791\ub3d9\ud558\ub824\uba74 \uc138 \uad6c\uc131 \uc694\uc18c\uac00 \ud558\ub098\uc758 \uc911\uc2ec\uc120\uc5d0 \ub193\uc5ec\uc57c \ud55c\ub2e4: \ub77c\uc774\ub108\uac00 \uc788\ub294 \ucee8\ud14c\uc774\ub108, \ub354\ubbf8 \ud328\ub4dc\uac00 \uc788\ub294 \uc2a4\ud15c, \ub2e4\uc774 \uc2a4\ud0dd\uc774 \uc788\ub294 \ub2e4\uc774 \uc2ac\ub77c\uc774\ub4dc. \ud604\ub300 \ud504\ub808\uc2a4\ub294 \uc2a4\ud2b8\ub85c\ud06c \ub3d9\uc548 \ucee8\ud14c\uc774\ub108\uc640 \uc774\ub3d9 \ud06c\ub85c\uc2a4\ud5e4\ub4dc \uc815\ub82c\uc744 \ubaa8\ub2c8\ud130\ub9c1\ud558\ub294 \uc0c1\ub300 \uc704\uce58 \ud45c\uc2dc\uae30\ub97c \uac16\ucd94\uace0 \uc788\uc73c\uba70, \uae30\uacc4 \uc790\uccb4\ub294 \uae34 \ub2e4\uc774 \uc2a4\ud0dd\uacfc \ud568\uaed8 \ud504\ub9ac\uc2a4\ud2b8\ub808\uc2a4\ud2b8 \ud0c0\uc774\ub85c\ub4dc \ud504\ub808\uc784\uc73c\ub85c \uc81c\uc791\ub418\uc5b4 \ud558\uc911 \ud558\uc758 \ubcc0\ud615\uc774 \uc791\ub2e4 \u2014 \uc774 \ubcc0\ud615\uc774 \ubc14\ub85c \uc587\uc740 \ubcbd\uc774 \uacf5\ucc28 \ub0b4\ub85c \ub098\uc624\ub294\uc9c0\ub97c \uacb0\uc815\ud558\ub294 \ubcc0\ud615\uc774\ub2e4.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">\ud1a4\uc218\uac00 \uc544\ub2cc \uac15\uc131\uc744 \uad6c\ub9e4\ud558\ub294 \uc774\uc720\ub294 \uc751\uc6a9 \ubd84\uc57c\uc5d0 \uc788\ub2e4. \ubcc0\ud615\ub418\ub294 \ud504\ub808\uc2a4\ub294 \ub2e8\uba74 \uc911\uc2ec\uc5d0\uc11c \ub2e4\uc774 \uac1c\uad6c\ubd80\ub97c \ub2eb\uc73c\uba70, \uc5b4\ub5a4 \ub2e4\uc774 \ubcf4\uc815\ub3c4 \ud558\uc911 \ud558\uc5d0\uc11c \ud615\uc0c1\uc774 \ubcc0\ud558\ub294 \ud504\ub808\uc2a4\ub97c \ubcf4\uc0c1\ud560 \uc218 \uc5c6\ub2e4.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">\ucee8\ud14c\uc774\ub108\uc640 \uadf8 \ub77c\uc774\ub108<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">\ucee8\ud14c\uc774\ub108\ub294 \ub77c\uc778\uc5d0\uc11c \uac00\uc7a5 \ube44\uc2fc \ub9c8\ubaa8 \ubd80\ud488\uc774\uba70 \uadf8 \uc218\uba85\uc740 \uc720\uc9c0\ubcf4\uc218 \ud56d\ubaa9\uc774 \uc544\ub2c8\ub77c \uc218\uc775\uc131 \ud56d\ubaa9\uc774\ub2e4. \uacf5\uac1c\ub41c \uc124\uacc4 \uae30\uc900\uc740 \ub77c\uc774\ub108 \ub0b4\ubd80\uc758 \ube44\uc555\ub825, \ucee8\ud14c\uc774\ub108\uc758 \ucd5c\ub300 \uc678\uacbd, \uadf8\ub9ac\uace0 \uc9c1\uc0ac\uac01\ud615 \ucee8\ud14c\uc774\ub108\uc758 \uacbd\uc6b0 \ud3ed \ub300 \ub192\uc774 \ube44\uc728\uc774\ub2e4. \ucee8\ud14c\uc774\ub108\ub294 \ucee8\ud14c\uc774\ub108 \ub610\ub294 \uadf8 \ud640\ub354\uc758 \uc800\ud56d \uac00\uc5f4 \uc720\ub2db\uc5d0 \uc758\ud574 \uc57d 427 &deg;C\ub85c \uac00\uc5f4\ub418\uba70, \ub300\ud615 \ud504\ub808\uc2a4\ub294 \ub2e4\uad6c\uc5ed \uc81c\uc5b4\ub97c \uc0ac\uc6a9\ud55c\ub2e4 \u2014 \uacf5\uac1c\ub41c \uc608\uc5d0\uc11c\ub294 6\uac1c\uc758 \ub3c5\ub9bd \uad6c\uc5ed \u2014 \uc65c\ub0d0\ud558\uba74 \uac10\uc2f8\ub294 \ud615\ud0dc\uc758 \ubc1c\uc5f4\uccb4\ub294 \ub9e4\uc6b0 \uae34 \ub77c\uc774\ub108\ub97c \ub530\ub77c \uade0\uc77c\ud55c \uc628\ub3c4\ub97c \uc720\uc9c0\ud560 \uc218 \uc5c6\uae30 \ub54c\ubb38\uc774\ub2e4. \ucee8\ud14c\uc774\ub108 \ub0b4 \uc720\ub3c4 \uac00\uc5f4\uae30\ub294 \uc57d 500 &deg;C\uc5d0 \ub3c4\ub2ec\ud560 \uc218 \uc788\ub2e4.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">\ub77c\uc774\ub108 \uc218\uba85 \uc218\uce58\ub294 \ub77c\uc774\ub108 \uac15\uc7ac\uac00 \uc65c \uc911\uc694\ud55c\uc9c0 \ubb3b\ub294 \uc0ac\ub78c\uc5d0\uac8c \uc81c\uc2dc\ud560 \uac00\uce58\uac00 \uc788\ub2e4: \uc5f0\ud654 \uc800\ud56d\uc131\uc774 \ub192\uc740 \uc801\ud569\ud55c \uac15\uc7ac\ub85c \uc81c\uc791\ub418\uc5b4 \uc62c\ubc14\ub974\uac8c \uc124\uacc4\ub41c \ucee8\ud14c\uc774\ub108\uc5d0 \uc7a5\ucc29\ub41c \ub77c\uc774\ub108\ub294 30,000~40,000 \uc0ac\uc774\ud074\uc744 \uacac\ub51c \uc218 \uc788\ub2e4. \uc9c1\uc0ac\uac01\ud615 \ucee8\ud14c\uc774\ub108\ub294 \ub113\uc740 \ub2e8\uba74\uc774 \uc8fc\ub825\uc778 \uacbd\uc6b0\uc5d0 \uc0ac\uc6a9\ub418\uba70 \u2014 \ud56d\uacf5\uae30 \ucc29\ub959 \ub9e4\ud2b8\uac00 \uacf5\uac1c\ub41c \uc608 \u2014 \uae08\uc18d \ud750\ub984\uc774 \ub354 \uade0\uc77c\ud574\uc838 \ud504\ub808\uc2a4 \ube44\ud558\uc911\uc744 \ub0ae\ucd98\ub2e4.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">\ub2e4\uc774 \ub4a4\uc758 \ub77c\uc778\uc774 \uc0dd\uc0b0\ub7c9\uc744 \uacb0\uc815\ud55c\ub2e4<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">\uacf5\uac1c\ub41c \uc785\uc7a5\uc740 \uc555\ucd9c \uacf5\uc7a5\uc758 \uc131\ub2a5\uc774 \uc8fc\ub85c \ubcf4\uc870 \uc124\ube44\uc5d0 \ub2ec\ub824 \uc788\ub2e4\ub294 \uac83\uc774\uba70, \uc0dd\uc0b0\uc131 \ube14\ub85d \ub2e4\uc774\uc5b4\uadf8\ub7a8\uc5d0\ub294 \uc774\ub97c \uc9c0\uc6d0\ud558\ub294 \uc138 \uc2dc\uc2a4\ud15c\uc774 \uc788\ub2e4: \ube4c\ub9bf \uac00\uc5f4 \ubc0f \uae38\uc774 \uc81c\uc5b4, \ud504\ub808\uc2a4 \uc790\uccb4, \uadf8\ub9ac\uace0 \ucde8\uae09 \uc2dc\uc2a4\ud15c. \uac01\uac01\uc774 \ub2e4\uc6b4\ud0c0\uc784\uacfc \uc2a4\ud06c\ub7a9\uc744 \ubaa8\ub450 \uc81c\uc5b4\ud55c\ub2e4.<\/p>\n\n\n\n<figure class=\"wp-block-table is-style-stripes\"><table class=\"has-fixed-layout\"><thead><tr><th class=\"has-text-align-left\" data-align=\"left\">\uc7a5\ube44<\/th><th class=\"has-text-align-left\" data-align=\"left\">\uacf5\uc815\uc5d0 \ubbf8\uce58\ub294 \uc601\ud5a5<\/th><\/tr><\/thead><tbody><tr><td class=\"has-text-align-left\" data-align=\"left\">\ud56b \ub85c\uadf8 \uc804\ub2e8\uae30\uac00 \uc788\ub294 \ub85c\uadf8 \ud788\ud130<\/td><td class=\"has-text-align-left\" data-align=\"left\">\uac01 \ub85c\uadf8\ub97c \ud2b9\uc815 \ub2e4\uc774\uc5d0 \ud544\uc694\ud55c \ube4c\ub9bf \uae38\uc774\ub85c \uc804\ub2e8; \uc9e7\uc740 \ube4c\ub9bf\uc740 \uccab \ube4c\ub9bf\uc758 \ub3cc\ud30c \uc555\ub825\uc744 \ub0ae\ucd94\uc5b4 \ub2e4\uc774\uac00 \uc544\uc9c1 \uc5f4 \ud3c9\ud615\uc5d0 \ub3c4\ub2ec\ud558\uc9c0 \uc54a\uc558\uc744 \ub54c \ub2e4\uc774 \ube0c\ub9ac\uc9c0\ub97c \ubcf4\ud638\ud568<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\ud14c\uc774\ud37c \ud01c\uce58 \ub610\ub294 \uc720\ub3c4 \ucda9\uaca9 \ud788\ud130<\/td><td class=\"has-text-align-left\" data-align=\"left\">\ub4f1\uc628 \uc555\ucd9c\uc744 \uac00\ub2a5\ud558\uac8c \ud558\ub294 \uc804\ud6c4 \uc628\ub3c4 \uad6c\ubc30\ub97c \uc0dd\uc131\ud568<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\ud56b \ube4c\ub9bf \uc2a4\uce98\ud37c<\/td><td class=\"has-text-align-left\" data-align=\"left\">\ube4c\ub9bf\uc774 \ubbf8\ub044\ub7ec\uc9c0\uc9c0 \uc54a\uace0 \uc2a4\ud0a8\uc774 \uc7ac\ubd84\ubc30\ub420 \uc218 \uc5c6\ub294 \ud56d\uacf5 \ud569\uae08\uc758 \uac04\uc811 \uc555\ucd9c\uc744 \uc704\ud574 \uc2a4\ud0a8\uc744 \uae30\uacc4 \uac00\uacf5\ud568<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\ub2e4\ucc54\ubc84 \ub2e4\uc774 \uc624\ube10<\/td><td class=\"has-text-align-left\" data-align=\"left\">\uac01 \ub2e4\uc774\ub97c \uac1c\ubcc4 \uc628\ub3c4\ub85c \uc720\uc9c0; \uc9c8\uc18c \ubd84\uc704\uae30 \ubc84\uc804\uc740 \uace0\uc628 \uc0b0\ud654\ub3c4 \ubc29\uc9c0\ud558\uace0 \uccb4\uc2a4\ud2b8\ud615 \uc624\ube10\uc758 \uc5f4 \ucda9\uaca9\uc744 \uc81c\uac70\ud568<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\ub2e4\uc774 \uce74\uc138\ud2b8 \ud788\ud130<\/td><td class=\"has-text-align-left\" data-align=\"left\">\ub2e4\uc774 \uad50\uccb4 \uc704\uce58\uc5d0\uc11c \ub2e4\uc774\ub97c \uc628\ub3c4\ub85c \uc720\uc9c0\ud558\uace0 \uc5f4\ud33d\ucc3d\uc5d0 \ub300\ud56d\ud558\uc5ec \uc804\ub2e8\uba74\uc744 \uc81c\uc790\ub9ac\uc5d0 \uc720\uc9c0\ud568<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\ub7f0\uc544\uc6c3\uc758 \uc6cc\ud130 \uc2a4\ud504\ub808\uc774 \ud01c\uce58<\/td><td class=\"has-text-align-left\" data-align=\"left\">\ud0f1\ud06c \ud01c\uce58\uc640 \ub0c9\uac01 \ud32c\uc744 \ub300\uccb4; \uacf5\uae30 \ubcf4\uc870 \ubd84\ubb34\ud654\ub97c \uac16\ucd98 \uace0\uc18d \ubd84\uc0ac\ub294 \uc5b4\ub824\uc6b4 \ud615\uc0c1\uc744 \uc784\uacc4 \uc628\ub3c4 \uc774\ud558\ub85c \ub0c9\uac01\ud568<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\ud56b \uc18c\uac00 \uc788\ub294 \ub2e8\uc77c \ub610\ub294 \uc774\uc911 \ud480\ub7ec<\/td><td class=\"has-text-align-left\" data-align=\"left\">\ucd9c\uad6c \uc18d\ub3c4\uc640 \uc7a5\ub825\uc744 \uc720\uc9c0\ud558\uace0 \ud504\ub808\uc2a4\uac00 \uc815\uc9c0\ud558\uc9c0 \uc54a\uace0 \uae38\uc774 \uc808\ub2e8\uc744 \uac00\ub2a5\ud558\uac8c \ud568<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\uc790\ub3d9 \uc2a4\ud2b8\ub808\ucc98, \ud1b1 \ubc0f \uc801\uc7ac\uae30<\/td><td class=\"has-text-align-left\" data-align=\"left\">\ucde8\uae09 \uc190\uc0c1 \uc5c6\uc774 \uad50\uc815, \uc808\ub2e8 \ubc0f \uc801\uc7ac\ud558\uba70, \uacf5\uac1c\ub41c \ub808\uc774\uc544\uc6c3\uc740 \uc2a4\ud2b8\ub808\ucc98\uc5d0 \ud154\ub808\ube44\uc804 \uce74\uba54\ub77c\ub97c, \uc591\ub2e8\uc5d0 \ub77c\ubbf8\ub124\uc774\ud2b8 \ud074\ub7a8\ud551 \ud5e4\ub4dc\ub97c \ubc30\uce58\ud569\ub2c8\ub2e4<\/td><\/tr><\/tbody><\/table><\/figure>\n\n\n\n<p class=\"wp-block-paragraph\"><em>\ud604\ub300\uc2dd \ub77c\uc778\uc758 \ubcf4\uc870 \uc124\ube44\uc640 \uac01 \uc124\ube44\uac00 \ub2f4\ub2f9\ud558\ub294 \uacf5\uc815 \ubcc0\uc218. \ucd9c\ucc98\ub294 \ube4c\ub9bf \uac00\uc5f4\ubd80\ud130 \uc2dc\ud6a8\ub85c\uae4c\uc9c0 \ud1b5\ud569 \uc124\ube44\uc758 \uc124\ube44\uc640 \ub3d9\uc77c\ud55c \ud56d\ubaa9\uc744 \ub098\uc5f4\ud569\ub2c8\ub2e4.<\/em><\/p>\n\n\n\n<p class=\"wp-block-paragraph\">\uacf5\uac1c\ub41c \uc0dd\uc0b0\uc131 \ubaa9\ub85d\uc740 \uccb4\ud06c\ub9ac\uc2a4\ud2b8\ub85c \uc0ac\uc6a9\ud558\uae30\uc5d0 \ucda9\ubd84\ud788 \uac04\uacb0\ud569\ub2c8\ub2e4: \ucd5c\uc801 \uc628\ub3c4\uc5d0\uc11c\uc758 \uc62c\ubc14\ub978 \ube4c\ub9bf \ud06c\uae30, \ud56b \ub85c\uadf8 \uc804\ub2e8\uacfc \ud14c\uc774\ud37c \ud01c\uce58\ub97c \uac16\ucd98 \ube4c\ub9bf \uac00\uc5f4 \uc0ac\uc6a9; \uc608\ubc29 \uac00\ub2a5\ud55c \ub2e4\uc6b4\ud0c0\uc784\uc744 \uc904\uc774\uae30 \uc704\ud55c \uc62c\ubc14\ub978 \ub2e4\uc774 \ubc0f \uacf5\uad6c \uc628\ub3c4; \uc790\ub3d9 \ub354\ube14 \ud480\ub7ec\ub85c \uc81c\uc5b4\ub418\ub294 \ucd9c\uad6c \uc18d\ub3c4\uc640 \uc628\ub3c4; \uadf8\ub9ac\uace0 \ucde8\uae09 \uc190\uc0c1\uacfc \uc778\ub825\uc744 \uc904\uc774\uae30 \uc704\ud55c \ub7f0\uc544\uc6c3\ubd80\ud130 \uc801\uc7ac \ubc0f \uc2dc\ud6a8\uae4c\uc9c0\uc758 \uc790\ub3d9 \ucde8\uae09 \uc2dc\uc2a4\ud15c.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">\ub2e4\uc774 \uad50\uccb4 \uc704\uce58\uc5d0\uc11c \uc5bb\uc740 \ud55c \uac00\uc9c0 \uc138\ubd80 \uc0ac\ud56d\uc740 \ub2e4\uc774 \uacf5\uc7a5\uc73c\ub85c \uac00\uc838\uac08 \uac00\uce58\uac00 \uc788\uc2b5\ub2c8\ub2e4. \ub300\ud615 \ud504\ub808\uc2a4\uc5d0\uc11c\ub294 \ub2e4\uc774 \uc2a4\ud0dd\uc774 \uae38\uace0 \uc804\ub2e8\uba74\uc774 \uc5f4\ud33d\ucc3d\uacfc \uc218\ucd95\uc5d0 \ub530\ub77c \uc6c0\uc9c1\uc785\ub2c8\ub2e4. \uc804\ub2e8\uba74\uc774 \uc81c\ub300\ub85c \uc704\uce58\ud558\uc9c0 \uc54a\uc73c\uba74 \ub2e4\uc774 \uba74\uc5d0 \ubc88\uc9c4 \uc54c\ub8e8\ubbf8\ub284\uc774 \ub098\ud0c0\ub098\uace0 \ub2e4\uc74c \ube4c\ub9bf\uc774 \ud50c\ub808\uc5b4 \ub610\ub294 \ube14\ub9ac\uc2a4\ud130\uac00 \uc0dd\uae41\ub2c8\ub2e4. \uc774\ub294 \ub2e4\uc774 \uba74 \uc99d\uc0c1\uc744 \uac00\uc9c4 \ub2e4\uc774 \uce90\ub9ac\uc9c0 \ubc0f \ud788\ud130 \ubb38\uc81c\ub85c, \ub2e4\uc774 \uac15\uc7ac\uc758 \ud0d3\uc73c\ub85c \ub3cc\ub824\uc9c0\uc9c0\ub9cc \uc2e4\uc81c\ub85c\ub294 \uadf8\ub807\uc9c0 \uc54a\uc740 \uc885\ub958\uc758 \uacb0\ud568\uc785\ub2c8\ub2e4.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">\uc774\uac83\uc774 \ub2e4\uc774 \uac15\uc7ac \uc8fc\ubb38\uc5d0 \uc8fc\ub294 \uc2dc\uc0ac\uc810<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">\ud504\ub808\uc2a4 \uc120\ud0dd\uc740 \ub2e4\uc774\uac00 \uac10\ub2f9\ud574\uc57c \ud560 \uac83\uc744 \uacb0\uc815\ud569\ub2c8\ub2e4: \ucee8\ud14c\uc774\ub108 \ubcf4\uc5b4\uc5d0\uc11c\uc758 \ube44\uc555\ub825, \uc2a4\ud0dd\uc758 \ucc98\uc9d0, \uadf8\ub9ac\uace0 \ub77c\uc778\uc774 \ucd9c\uad6c \uc628\ub3c4\ub97c \uc5bc\ub9c8\ub098 \uac15\ud558\uac8c \ubc00\uc5b4\ubd99\uc774\ub294\uc9c0. \uc774\uac83\ub4e4\uc774 \uace0\uc815\ub418\uba74 \ub0a8\uc740 \ubcc0\uc218\ub294 \ub2e4\uc774 \uc7ac\ub8cc\uc785\ub2c8\ub2e4 \u2014 \ud06c\ub86c \uc5f4\uac04 \uae08\ud615\uac15, AISI H13 \ubc0f \uadf8 \uc720\ub7fd \ub4f1\uac00\uc7ac 1.2344, \uc791\uc5c5 \uacbd\ub3c4\uc640 \ud15c\ud37c\ub9c1\uc740 \ub2e4\uc74c\uc5d0 \uba85\uc2dc\ub41c \ub300\ub85c <a href=\"https:\/\/aobosteel.com\/ko\/h13-tool-steel\/\">H13 \uacf5\uad6c\uac15 \ud398\uc774\uc9c0<\/a>, \uc555\ucd9c \uacf5\uad6c\uc6a9 ESR \ud504\ub85c\uadf8\ub7a8\uc740 \ub2e4\uc74c\uc5d0 <a href=\"https:\/\/aobosteel.com\/ko\/1-2344-esr-h13-aluminum-extrusion-distributors\/\">1.2344 ESR H13 \uacf5\uae09 \ud398\uc774\uc9c0<\/a>.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">\uccb4\uc778\uc758 \ub098\uba38\uc9c0: \ud504\ub808\uc2a4\uc5d0 \ub9de\uc544\uc57c \ud558\ub294 \uc2a4\ud0dd\uc740 \ub2e4\uc74c\uc5d0 <a href=\"https:\/\/aobosteel.com\/ko\/aluminum-extrusion-die-types-and-tooling\/\">\ub2e4\uc774 \uc720\ud615 \ubc0f \ud234\ub9c1 \ud398\uc774\uc9c0<\/a>, \uc555\ub825\uc744 \uac00\uc7a5 \uba3c\uc800 \ubc1b\ub294 \ub79c\ub4dc\ub294 \ub2e4\uc74c\uc5d0 <a href=\"https:\/\/aobosteel.com\/ko\/aluminum-extrusion-die-bearing-length\/\">\ub2e4\uc774 \ubca0\uc5b4\ub9c1 \uae38\uc774 \ud398\uc774\uc9c0<\/a>, \ub4a4\ub530\ub974\ub294 \ub9c8\ubaa8\ub294 \ub2e4\uc74c\uc5d0 <a href=\"https:\/\/aobosteel.com\/ko\/aluminum-extrusion-die-wear\/\">\ub2e4\uc774 \ub9c8\ubaa8 \ud398\uc774\uc9c0<\/a>, \uc774\ub97c \ubcf4\ud638\ud558\ub294 \uc9c8\ud654\ub294 \ub2e4\uc74c\uc5d0 <a href=\"https:\/\/aobosteel.com\/ko\/tool-steel-nitriding-guide\/\">\uacf5\uad6c\uac15 \uc9c8\ud654 \ud398\uc774\uc9c0<\/a>, \uadf8\ub9ac\uace0 \ub2e8\uba74 \ubc0f \ud504\ub808\uc2a4 \ud55c\uacc4 \uc790\uccb4\ub294 \ub2e4\uc74c\uc5d0 <a href=\"https:\/\/aobosteel.com\/ko\/extrusion-die-circumscribing-circle-diameter\/\">\uc678\uc811\uc6d0 \uc9c1\uacbd \ud398\uc774\uc9c0<\/a>.<\/p>\n\n\n\n<h3 class=\"wp-block-heading\">\uc774 \ud398\uc774\uc9c0\uc5d0\uc11c \ud504\ub808\uc2a4\ub97c \uad6c\ub9e4\ud558\uac70\ub098 \uacac\uc801\uc744 \ub0b4\uae30 \uc804\uc5d0<\/h3>\n\n\n\n<p class=\"wp-block-paragraph\">\ube44\uc555\ub825\uc740 \uc120\ud0dd \uae30\uc900\uc774\uc9c0 \ubcf4\uc99d\uc774 \uc544\ub2d9\ub2c8\ub2e4. \uacf5\uac1c\ub41c \ud45c\ub294 \ub098\uc5f4\ub41c \ucee8\ud14c\uc774\ub108 \ubcf4\uc5b4\ub97c \uac00\uc815\ud558\uba70, \uc2e4\uc81c \ud615\uc0c1\uc5d0 \ud544\uc694\ud55c \uc555\ub825\uc740 \uc5ec\uc804\ud788 \ud569\uae08, \uc555\ucd9c\ube44, \ube4c\ub9bf \uae38\uc774\uc640 \uc628\ub3c4, \uc18d\ub3c4 \ubc0f \uc678\uc811\uc6d0\uc5d0 \ub300\ud574 \ud655\uc778\ud574\uc57c \ud569\ub2c8\ub2e4. \uc885\uc774 \uc704\uc758 \uc218\uce58\ub97c \ucda9\uc871\ud558\uc9c0\ub9cc \ud558\uc911 \ud558\uc5d0\uc11c \ucc98\uc9c0\ub294 \ud504\ub808\uc2a4\ub294 \uacf5\ucc28\ub97c \uc720\uc9c0\ud558\uc9c0 \ubabb\ud558\uba70, \ucc45\uc758 \uc5b4\ub5a4 \ud45c\ub3c4 \uadc0\ud558\uc758 \uc791\uc5c5\uc7a5\uc5d0 \uc788\ub294 \uae30\uacc4\ub97c \ud655\uc778\ud560 \uc218 \uc5c6\uc2b5\ub2c8\ub2e4.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">\ucd9c\ucc98: Aluminum Extrusion Technology, P. K. Saha, ASM International, 2000, 3\uc7a5, \uc555\ucd9c \ud504\ub808\uc2a4 \ubc0f \ubcf4\uc870 \uc124\ube44, 56~85\ud398\uc774\uc9c0.<\/p>","protected":false},"excerpt":{"rendered":"<p>Choosing the Press: Specific Pressure, Direct or Indirect, and the Line Behind the Die A press is bought as a tonnage and used as a pressure. The tonnage is fixed by the hydraulics; the pressure the billet actually sees is that tonnage divided by the area of the container bore, so the same press becomes [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":0,"parent":0,"menu_order":0,"comment_status":"closed","ping_status":"closed","template":"","meta":{"_uag_custom_page_level_css":"","site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"default","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"disabled","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","ast-disable-related-posts":"","theme-transparent-header-meta":"","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"default","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"footnotes":""},"class_list":["post-25012","page","type-page","status-publish","hentry"],"yoast_head":"<!-- This site is optimized with the Yoast SEO Premium plugin v28.9 (Yoast SEO v28.9) - https:\/\/yoast.com\/product\/yoast-seo-premium-wordpress\/ -->\n<title>Aluminum Extrusion Press Selection by Specific Pressure<\/title>\n<meta name=\"description\" content=\"Specific pressure by press capacity and container bore, direct versus indirect extrusion, container liner life and the auxiliary line behind the die.\" \/>\n<meta name=\"robots\" content=\"index, follow, max-snippet:-1, max-image-preview:large, max-video-preview:-1\" \/>\n<link rel=\"canonical\" href=\"https:\/\/aobosteel.com\/ko\/aluminum-extrusion-press-selection\/\" \/>\n<meta property=\"og:locale\" content=\"ko_KR\" \/>\n<meta property=\"og:type\" content=\"article\" \/>\n<meta property=\"og:title\" content=\"Choosing the Press: Specific Pressure, Direct or Indirect, and the Line Behind the Die\" \/>\n<meta property=\"og:description\" content=\"Specific pressure by press capacity and container bore, direct versus indirect extrusion, container liner life and the auxiliary line behind the die.\" \/>\n<meta property=\"og:url\" content=\"https:\/\/aobosteel.com\/ko\/aluminum-extrusion-press-selection\/\" \/>\n<meta property=\"og:site_name\" content=\"AoboSteel\" \/>\n<meta property=\"article:publisher\" content=\"https:\/\/www.facebook.com\/profile.php?id=61565368220197\" \/>\n<meta name=\"twitter:card\" content=\"summary_large_image\" \/>\n<meta name=\"twitter:label1\" content=\"\uc608\uc0c1 \ub418\ub294 \ud310\ub3c5 \uc2dc\uac04\" \/>\n\t<meta name=\"twitter:data1\" content=\"9\ubd84\" \/>\n<script type=\"application\/ld+json\" class=\"yoast-schema-graph\">{\"@context\":\"https:\\\/\\\/schema.org\",\"@graph\":[{\"@type\":\"TechArticle\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/aluminum-extrusion-press-selection\\\/#article\",\"isPartOf\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/aluminum-extrusion-press-selection\\\/\"},\"author\":{\"name\":\"Evan\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#\\\/schema\\\/person\\\/96118415c30ca6bb52eaf1127b052ef7\"},\"headline\":\"Choosing the Press: Specific Pressure, Direct or Indirect, and the Line Behind the Die\",\"datePublished\":\"2026-11-04T15:10:26+00:00\",\"mainEntityOfPage\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/aluminum-extrusion-press-selection\\\/\"},\"wordCount\":1799,\"publisher\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#organization\"},\"inLanguage\":\"ko-KR\"},{\"@type\":\"WebPage\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/aluminum-extrusion-press-selection\\\/\",\"url\":\"https:\\\/\\\/aobosteel.com\\\/aluminum-extrusion-press-selection\\\/\",\"name\":\"Aluminum Extrusion Press Selection by Specific Pressure\",\"isPartOf\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#website\"},\"datePublished\":\"2026-11-04T15:10:26+00:00\",\"description\":\"Specific pressure by press capacity and container bore, direct versus indirect extrusion, container liner life and the auxiliary line behind the die.\",\"breadcrumb\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/aluminum-extrusion-press-selection\\\/#breadcrumb\"},\"inLanguage\":\"ko-KR\",\"potentialAction\":[{\"@type\":\"ReadAction\",\"target\":[\"https:\\\/\\\/aobosteel.com\\\/aluminum-extrusion-press-selection\\\/\"]}]},{\"@type\":\"BreadcrumbList\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/aluminum-extrusion-press-selection\\\/#breadcrumb\",\"itemListElement\":[{\"@type\":\"ListItem\",\"position\":1,\"name\":\"\u9996\u9875\",\"item\":\"https:\\\/\\\/aobosteel.com\\\/\"},{\"@type\":\"ListItem\",\"position\":2,\"name\":\"Choosing the Press: Specific Pressure, Direct or Indirect, and the Line Behind the Die\"}]},{\"@type\":\"WebSite\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#website\",\"url\":\"https:\\\/\\\/aobosteel.com\\\/\",\"name\":\"AoboSteel\",\"description\":\"\",\"publisher\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#organization\"},\"potentialAction\":[{\"@type\":\"SearchAction\",\"target\":{\"@type\":\"EntryPoint\",\"urlTemplate\":\"https:\\\/\\\/aobosteel.com\\\/?s={search_term_string}\"},\"query-input\":{\"@type\":\"PropertyValueSpecification\",\"valueRequired\":true,\"valueName\":\"search_term_string\"}}],\"inLanguage\":\"ko-KR\"},{\"@type\":\"Organization\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#organization\",\"name\":\"AoboSteel\",\"url\":\"https:\\\/\\\/aobosteel.com\\\/\",\"logo\":{\"@type\":\"ImageObject\",\"inLanguage\":\"ko-KR\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#\\\/schema\\\/logo\\\/image\\\/\",\"url\":\"https:\\\/\\\/aobosteel.com\\\/wp-content\\\/uploads\\\/2025\\\/01\\\/cropped-aobo-steel-1.avif\",\"contentUrl\":\"https:\\\/\\\/aobosteel.com\\\/wp-content\\\/uploads\\\/2025\\\/01\\\/cropped-aobo-steel-1.avif\",\"width\":1052,\"height\":592,\"caption\":\"AoboSteel\"},\"image\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#\\\/schema\\\/logo\\\/image\\\/\"},\"sameAs\":[\"https:\\\/\\\/www.facebook.com\\\/profile.php?id=61565368220197\",\"https:\\\/\\\/www.linkedin.com\\\/in\\\/aobosteel-evan\\\/\"]},{\"@type\":\"Person\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#\\\/schema\\\/person\\\/96118415c30ca6bb52eaf1127b052ef7\",\"name\":\"Evan\",\"image\":{\"@type\":\"ImageObject\",\"inLanguage\":\"ko-KR\",\"@id\":\"https:\\\/\\\/secure.gravatar.com\\\/avatar\\\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g\",\"url\":\"https:\\\/\\\/secure.gravatar.com\\\/avatar\\\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g\",\"contentUrl\":\"https:\\\/\\\/secure.gravatar.com\\\/avatar\\\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g\",\"caption\":\"Evan\"},\"sameAs\":[\"http:\\\/\\\/www.aobosteel.com\",\"https:\\\/\\\/www.facebook.com\\\/profile.php?id=61565368220197\",\"https:\\\/\\\/www.instagram.com\\\/aobosteel\\\/\",\"https:\\\/\\\/www.linkedin.com\\\/in\\\/aobosteel-evan\\\/\",\"https:\\\/\\\/x.com\\\/AobosteelEvan\",\"https:\\\/\\\/www.youtube.com\\\/@aobosteel\"],\"url\":\"https:\\\/\\\/aobosteel.com\\\/ko\\\/blog\\\/author\\\/admin\\\/\"}]}<\/script>\n<!-- \/ Yoast SEO Premium plugin. -->","yoast_head_json":{"title":"\ube44\uc555\ub825 \uae30\uc900 \uc54c\ub8e8\ubbf8\ub284 \uc555\ucd9c \ud504\ub808\uc2a4 \uc120\uc815","description":"\ud504\ub808\uc2a4 \uc6a9\ub7c9 \ubc0f \ucee8\ud14c\uc774\ub108 \ubcf4\uc5b4\ubcc4 \ube44\uc555\ub825, \uc9c1\uc811 \uc555\ucd9c\uacfc \uac04\uc811 \uc555\ucd9c\uc758 \ube44\uad50, \ucee8\ud14c\uc774\ub108 \ub77c\uc774\ub108 \uc218\uba85, \ub2e4\uc774 \ub4a4 \ubcf4\uc870 \ub77c\uc778\uc744 \uc124\uba85\ud569\ub2c8\ub2e4.","robots":{"index":"index","follow":"follow","max-snippet":"max-snippet:-1","max-image-preview":"max-image-preview:large","max-video-preview":"max-video-preview:-1"},"canonical":"https:\/\/aobosteel.com\/ko\/aluminum-extrusion-press-selection\/","og_locale":"ko_KR","og_type":"article","og_title":"Choosing the Press: Specific Pressure, Direct or Indirect, and the Line Behind the Die","og_description":"Specific pressure by press capacity and container bore, direct versus indirect extrusion, container liner life and the auxiliary line behind the die.","og_url":"https:\/\/aobosteel.com\/ko\/aluminum-extrusion-press-selection\/","og_site_name":"AoboSteel","article_publisher":"https:\/\/www.facebook.com\/profile.php?id=61565368220197","twitter_card":"summary_large_image","twitter_misc":{"\uc608\uc0c1 \ub418\ub294 \ud310\ub3c5 \uc2dc\uac04":"9\ubd84"},"schema":{"@context":"https:\/\/schema.org","@graph":[{"@type":"TechArticle","@id":"https:\/\/aobosteel.com\/aluminum-extrusion-press-selection\/#article","isPartOf":{"@id":"https:\/\/aobosteel.com\/aluminum-extrusion-press-selection\/"},"author":{"name":"Evan","@id":"https:\/\/aobosteel.com\/#\/schema\/person\/96118415c30ca6bb52eaf1127b052ef7"},"headline":"Choosing the Press: Specific Pressure, Direct or Indirect, and the Line Behind the Die","datePublished":"2026-11-04T15:10:26+00:00","mainEntityOfPage":{"@id":"https:\/\/aobosteel.com\/aluminum-extrusion-press-selection\/"},"wordCount":1799,"publisher":{"@id":"https:\/\/aobosteel.com\/#organization"},"inLanguage":"ko-KR"},{"@type":"WebPage","@id":"https:\/\/aobosteel.com\/aluminum-extrusion-press-selection\/","url":"https:\/\/aobosteel.com\/aluminum-extrusion-press-selection\/","name":"\ube44\uc555\ub825 \uae30\uc900 \uc54c\ub8e8\ubbf8\ub284 \uc555\ucd9c \ud504\ub808\uc2a4 \uc120\uc815","isPartOf":{"@id":"https:\/\/aobosteel.com\/#website"},"datePublished":"2026-11-04T15:10:26+00:00","description":"\ud504\ub808\uc2a4 \uc6a9\ub7c9 \ubc0f \ucee8\ud14c\uc774\ub108 \ubcf4\uc5b4\ubcc4 \ube44\uc555\ub825, \uc9c1\uc811 \uc555\ucd9c\uacfc \uac04\uc811 \uc555\ucd9c\uc758 \ube44\uad50, \ucee8\ud14c\uc774\ub108 \ub77c\uc774\ub108 \uc218\uba85, \ub2e4\uc774 \ub4a4 \ubcf4\uc870 \ub77c\uc778\uc744 \uc124\uba85\ud569\ub2c8\ub2e4.","breadcrumb":{"@id":"https:\/\/aobosteel.com\/aluminum-extrusion-press-selection\/#breadcrumb"},"inLanguage":"ko-KR","potentialAction":[{"@type":"ReadAction","target":["https:\/\/aobosteel.com\/aluminum-extrusion-press-selection\/"]}]},{"@type":"BreadcrumbList","@id":"https:\/\/aobosteel.com\/aluminum-extrusion-press-selection\/#breadcrumb","itemListElement":[{"@type":"ListItem","position":1,"name":"\u9996\u9875","item":"https:\/\/aobosteel.com\/"},{"@type":"ListItem","position":2,"name":"Choosing the Press: Specific Pressure, Direct or Indirect, and the Line Behind the Die"}]},{"@type":"WebSite","@id":"https:\/\/aobosteel.com\/#website","url":"https:\/\/aobosteel.com\/","name":"\uc544\uc624\ubcf4\uc2a4\ud2f8","description":"","publisher":{"@id":"https:\/\/aobosteel.com\/#organization"},"potentialAction":[{"@type":"SearchAction","target":{"@type":"EntryPoint","urlTemplate":"https:\/\/aobosteel.com\/?s={search_term_string}"},"query-input":{"@type":"PropertyValueSpecification","valueRequired":true,"valueName":"search_term_string"}}],"inLanguage":"ko-KR"},{"@type":"Organization","@id":"https:\/\/aobosteel.com\/#organization","name":"\uc544\uc624\ubcf4\uc2a4\ud2f8","url":"https:\/\/aobosteel.com\/","logo":{"@type":"ImageObject","inLanguage":"ko-KR","@id":"https:\/\/aobosteel.com\/#\/schema\/logo\/image\/","url":"https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/01\/cropped-aobo-steel-1.avif","contentUrl":"https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/01\/cropped-aobo-steel-1.avif","width":1052,"height":592,"caption":"AoboSteel"},"image":{"@id":"https:\/\/aobosteel.com\/#\/schema\/logo\/image\/"},"sameAs":["https:\/\/www.facebook.com\/profile.php?id=61565368220197","https:\/\/www.linkedin.com\/in\/aobosteel-evan\/"]},{"@type":"Person","@id":"https:\/\/aobosteel.com\/#\/schema\/person\/96118415c30ca6bb52eaf1127b052ef7","name":"\uc5d0\ubc18","image":{"@type":"ImageObject","inLanguage":"ko-KR","@id":"https:\/\/secure.gravatar.com\/avatar\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g","url":"https:\/\/secure.gravatar.com\/avatar\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g","contentUrl":"https:\/\/secure.gravatar.com\/avatar\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g","caption":"Evan"},"sameAs":["http:\/\/www.aobosteel.com","https:\/\/www.facebook.com\/profile.php?id=61565368220197","https:\/\/www.instagram.com\/aobosteel\/","https:\/\/www.linkedin.com\/in\/aobosteel-evan\/","https:\/\/x.com\/AobosteelEvan","https:\/\/www.youtube.com\/@aobosteel"],"url":"https:\/\/aobosteel.com\/ko\/blog\/author\/admin\/"}]}},"uagb_featured_image_src":{"full":false,"thumbnail":false,"medium":false,"medium_large":false,"large":false,"1536x1536":false,"2048x2048":false,"trp-custom-language-flag":false},"uagb_author_info":{"display_name":"Evan","author_link":"https:\/\/aobosteel.com\/ko\/blog\/author\/admin\/"},"uagb_comment_info":0,"uagb_excerpt":"Choosing the Press: Specific Pressure, Direct or Indirect, and the Line Behind the Die A press is bought as a tonnage and used as a pressure. The tonnage is fixed by the hydraulics; the pressure the billet actually sees is that tonnage divided by the area of the container bore, so the same press becomes&hellip;","rttpg_featured_image_url":null,"rttpg_author":{"display_name":"Evan","author_link":"https:\/\/aobosteel.com\/ko\/blog\/author\/admin\/"},"rttpg_comment":0,"rttpg_category":null,"rttpg_excerpt":"Choosing the Press: Specific Pressure, Direct or Indirect, and the Line Behind the Die A press is bought as a tonnage and used as a pressure. The tonnage is fixed by the hydraulics; the pressure the billet actually sees is that tonnage divided by the area of the container bore, so the same press becomes&hellip;","_links":{"self":[{"href":"https:\/\/aobosteel.com\/ko\/wp-json\/wp\/v2\/pages\/25012","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/aobosteel.com\/ko\/wp-json\/wp\/v2\/pages"}],"about":[{"href":"https:\/\/aobosteel.com\/ko\/wp-json\/wp\/v2\/types\/page"}],"author":[{"embeddable":true,"href":"https:\/\/aobosteel.com\/ko\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/aobosteel.com\/ko\/wp-json\/wp\/v2\/comments?post=25012"}],"version-history":[{"count":1,"href":"https:\/\/aobosteel.com\/ko\/wp-json\/wp\/v2\/pages\/25012\/revisions"}],"predecessor-version":[{"id":25013,"href":"https:\/\/aobosteel.com\/ko\/wp-json\/wp\/v2\/pages\/25012\/revisions\/25013"}],"wp:attachment":[{"href":"https:\/\/aobosteel.com\/ko\/wp-json\/wp\/v2\/media?parent=25012"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}