{"id":18375,"date":"2026-09-15T12:39:58","date_gmt":"2026-09-15T04:39:58","guid":{"rendered":"https:\/\/aobosteel.com\/?page_id=18375"},"modified":"2026-10-21T11:44:23","modified_gmt":"2026-10-21T03:44:23","slug":"surface-roughness-chart","status":"publish","type":"page","link":"https:\/\/aobosteel.com\/ko\/surface-roughness-chart\/","title":{"rendered":"\ud45c\uba74 \uac70\uce60\uae30 \ucc28\ud2b8"},"content":{"rendered":"<h1 class=\"wp-block-heading has-text-align-center\" id=\"h-surface-roughness-chart\">\ud45c\uba74 \uac70\uce60\uae30 \ucc28\ud2b8<\/h1>\n\n\n\n<p class=\"wp-block-paragraph\">\ud654\uc5fc \uc808\ub2e8 \ubc0f \ud1b1\uc9c8\ubd80\ud130 \ub798\ud551 \ubc0f \uc288\ud37c\ud53c\ub2c8\uc2f1\uae4c\uc9c0 \uac01 \uc0dd\uc0b0 \ubc29\ubc95\uc774 \uac15\uc7ac\uc5d0 \ub0a8\uae30\ub294 Ra \ud45c\uba74 \uc870\ub3c4\uc785\ub2c8\ub2e4. \uac01 \ud589\uc740 \ud1b5\uc0c1\uc801\uc73c\ub85c \uc0dd\uc0b0\ub418\ub294 \ubc94\uc704\uc640 \uc5ec\uc804\ud788 \ubc1c\uc0dd\ud560 \uc218 \uc788\ub294 \ub354 \ub113\uc740 \ubc94\uc704\ub97c \ub9c8\uc774\ud06c\ub85c\ubbf8\ud130 \ubc0f \ub9c8\uc774\ud06c\ub85c\uc778\uce58\ub85c \ud45c\uc2dc\ud558\uba70, \uc870\ub3c4 \ub4f1\uae09 \ubc88\ud638\uc640 \ud574\ub2f9 \ucef7\uc624\ud504 \uac12\uc744 \ud568\uaed8 \ubcf4\uc5ec\uc90d\ub2c8\ub2e4.<\/p>\n\n\n\n<h2 id=\"h-roughness-produced-by-common-production-methods\" class=\"wp-block-heading\">\uc77c\ubc18\uc801\uc778 \uc0dd\uc0b0 \ubc29\ubc95\uc73c\ub85c \uc0dd\uc131\ub418\ub294 \uac70\uce60\uae30<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">\uc5b4\ub450\uc6b4 \ub9c9\ub300\ub294 \ud574\ub2f9 \uacf5\uc815\uc73c\ub85c \uac00\uacf5\uc5c5\uccb4\uac00 \ud1b5\uc0c1\uc801\uc73c\ub85c \uc720\uc9c0\ud558\ub294 \ubc94\uc704\uc785\ub2c8\ub2e4. \ud68c\uc0c9 \ub9c9\ub300\ub294 \uc720\ub9ac\ud55c \uc870\uac74\uc5d0\uc11c \uac00\ub2a5\ud55c \ub354 \ub113\uc740 \ubc94\uc704\ub97c \ub098\ud0c0\ub0c5\ub2c8\ub2e4. \uac12\uc740 Machinery&#8217;s Handbook 28\ud310, \ud45c 1\uc5d0 \uae30\uc7ac\ub41c \ub0b4\uc6a9\uc785\ub2c8\ub2e4.<\/p>\n\n\n\n<div style=\"overflow-x:auto;-webkit-overflow-scrolling:touch\">\n<div style=\"min-width:820px\">\n<svg viewbox=\"0 0 980 781\" width=\"100%\" preserveaspectratio=\"xMidYMid meet\" role=\"img\" aria-label=\"Surface roughness chart: Ra ranges produced by common production methods\" font-family=\"system-ui, -apple-system, Segoe UI, Roboto, Arial, sans-serif\">\n<rect x=\"0\" y=\"0\" width=\"980\" height=\"781\" fill=\"#ffffff\"\/>\n<line x1=\"216.0\" y1=\"58\" x2=\"216.0\" y2=\"717\" stroke=\"#e5e7eb\" stroke-width=\"1\"\/>\n<text x=\"216.0\" y=\"40\" font-size=\"11\" fill=\"#212121\" text-anchor=\"middle\">50<\/text>\n<text x=\"216.0\" y=\"54\" font-size=\"9\" fill=\"#888888\" text-anchor=\"middle\">(2000)<\/text>\n<text x=\"216.0\" y=\"731\" font-size=\"9\" fill=\"#888888\" text-anchor=\"middle\">2000<\/text>\n<line x1=\"278.2\" y1=\"58\" x2=\"278.2\" y2=\"717\" stroke=\"#e5e7eb\" stroke-width=\"1\"\/>\n<text x=\"278.2\" y=\"40\" font-size=\"11\" fill=\"#212121\" text-anchor=\"middle\">25<\/text>\n<text x=\"278.2\" y=\"54\" font-size=\"9\" fill=\"#888888\" text-anchor=\"middle\">(1000)<\/text>\n<text x=\"278.2\" y=\"731\" font-size=\"9\" fill=\"#888888\" text-anchor=\"middle\">1000<\/text>\n<line x1=\"340.4\" y1=\"58\" x2=\"340.4\" y2=\"717\" stroke=\"#e5e7eb\" stroke-width=\"1\"\/>\n<text x=\"340.4\" y=\"40\" font-size=\"11\" fill=\"#212121\" text-anchor=\"middle\">12.5<\/text>\n<text x=\"340.4\" y=\"54\" font-size=\"9\" fill=\"#888888\" text-anchor=\"middle\">(500)<\/text>\n<text x=\"340.4\" y=\"731\" font-size=\"9\" fill=\"#888888\" text-anchor=\"middle\">500<\/text>\n<line x1=\"401.9\" y1=\"58\" x2=\"401.9\" y2=\"717\" stroke=\"#e5e7eb\" stroke-width=\"1\"\/>\n<text x=\"401.9\" y=\"40\" font-size=\"11\" fill=\"#212121\" text-anchor=\"middle\">6.3<\/text>\n<text x=\"401.9\" y=\"54\" font-size=\"9\" fill=\"#888888\" text-anchor=\"middle\">(250)<\/text>\n<text x=\"401.9\" y=\"731\" font-size=\"9\" fill=\"#888888\" text-anchor=\"middle\">250<\/text>\n<line x1=\"462.7\" y1=\"58\" x2=\"462.7\" y2=\"717\" stroke=\"#e5e7eb\" stroke-width=\"1\"\/>\n<text x=\"462.7\" y=\"40\" font-size=\"11\" fill=\"#212121\" text-anchor=\"middle\">3.2<\/text>\n<text x=\"462.7\" y=\"54\" font-size=\"9\" fill=\"#888888\" text-anchor=\"middle\">(125)<\/text>\n<text x=\"462.7\" y=\"731\" font-size=\"9\" fill=\"#888888\" text-anchor=\"middle\">125<\/text>\n<line x1=\"524.9\" y1=\"58\" x2=\"524.9\" y2=\"717\" stroke=\"#e5e7eb\" stroke-width=\"1\"\/>\n<text x=\"524.9\" y=\"40\" font-size=\"11\" fill=\"#212121\" text-anchor=\"middle\">1.6<\/text>\n<text x=\"524.9\" y=\"54\" font-size=\"9\" fill=\"#888888\" text-anchor=\"middle\">(63)<\/text>\n<text x=\"524.9\" y=\"731\" font-size=\"9\" fill=\"#888888\" text-anchor=\"middle\">63<\/text>\n<line x1=\"587.1\" y1=\"58\" x2=\"587.1\" y2=\"717\" stroke=\"#e5e7eb\" stroke-width=\"1\"\/>\n<text x=\"587.1\" y=\"40\" font-size=\"11\" fill=\"#212121\" text-anchor=\"middle\">0.80<\/text>\n<text x=\"587.1\" y=\"54\" font-size=\"9\" fill=\"#888888\" text-anchor=\"middle\">(32)<\/text>\n<text x=\"587.1\" y=\"731\" font-size=\"9\" fill=\"#888888\" text-anchor=\"middle\">32<\/text>\n<line x1=\"649.3\" y1=\"58\" x2=\"649.3\" y2=\"717\" stroke=\"#e5e7eb\" stroke-width=\"1\"\/>\n<text x=\"649.3\" y=\"40\" font-size=\"11\" fill=\"#212121\" text-anchor=\"middle\">0.40<\/text>\n<text x=\"649.3\" y=\"54\" font-size=\"9\" fill=\"#888888\" text-anchor=\"middle\">(16)<\/text>\n<text x=\"649.3\" y=\"731\" font-size=\"9\" fill=\"#888888\" text-anchor=\"middle\">16<\/text>\n<line x1=\"711.5\" y1=\"58\" x2=\"711.5\" y2=\"717\" stroke=\"#e5e7eb\" stroke-width=\"1\"\/>\n<text x=\"711.5\" y=\"40\" font-size=\"11\" fill=\"#212121\" text-anchor=\"middle\">0.20<\/text>\n<text x=\"711.5\" y=\"54\" font-size=\"9\" fill=\"#888888\" text-anchor=\"middle\">(8)<\/text>\n<text x=\"711.5\" y=\"731\" font-size=\"9\" fill=\"#888888\" text-anchor=\"middle\">8<\/text>\n<line x1=\"773.7\" y1=\"58\" x2=\"773.7\" y2=\"717\" stroke=\"#e5e7eb\" stroke-width=\"1\"\/>\n<text x=\"773.7\" y=\"40\" font-size=\"11\" fill=\"#212121\" text-anchor=\"middle\">0.10<\/text>\n<text x=\"773.7\" y=\"54\" font-size=\"9\" fill=\"#888888\" text-anchor=\"middle\">(4)<\/text>\n<text x=\"773.7\" y=\"731\" font-size=\"9\" fill=\"#888888\" text-anchor=\"middle\">4<\/text>\n<line x1=\"835.9\" y1=\"58\" x2=\"835.9\" y2=\"717\" stroke=\"#e5e7eb\" stroke-width=\"1\"\/>\n<text x=\"835.9\" y=\"40\" font-size=\"11\" fill=\"#212121\" text-anchor=\"middle\">0.05<\/text>\n<text x=\"835.9\" y=\"54\" font-size=\"9\" fill=\"#888888\" text-anchor=\"middle\">(2)<\/text>\n<text x=\"835.9\" y=\"731\" font-size=\"9\" fill=\"#888888\" text-anchor=\"middle\">2<\/text>\n<line x1=\"898.1\" y1=\"58\" x2=\"898.1\" y2=\"717\" stroke=\"#e5e7eb\" stroke-width=\"1\"\/>\n<text x=\"898.1\" y=\"40\" font-size=\"11\" fill=\"#212121\" text-anchor=\"middle\">0.025<\/text>\n<text x=\"898.1\" y=\"54\" font-size=\"9\" fill=\"#888888\" text-anchor=\"middle\">(1)<\/text>\n<text x=\"898.1\" y=\"731\" font-size=\"9\" fill=\"#888888\" text-anchor=\"middle\">1<\/text>\n<line x1=\"964.0\" y1=\"58\" x2=\"964.0\" y2=\"717\" stroke=\"#e5e7eb\" stroke-width=\"1\"\/>\n<text x=\"964.0\" y=\"40\" font-size=\"11\" fill=\"#212121\" text-anchor=\"middle\">0.012<\/text>\n<text x=\"964.0\" y=\"54\" font-size=\"9\" fill=\"#888888\" text-anchor=\"middle\">(0.5)<\/text>\n<text x=\"964.0\" y=\"731\" font-size=\"9\" fill=\"#888888\" text-anchor=\"middle\">0.5<\/text>\n<text x=\"216\" y=\"16\" font-size=\"11\" fill=\"#212121\" font-weight=\"600\">Ra, \ub9c8\uc774\ud06c\ub85c\ubbf8\ud130 (\uad04\ud638 \uc548\uc740 \ub9c8\uc774\ud06c\ub85c\uc778\uce58)<\/text>\n<text x=\"964\" y=\"16\" font-size=\"11\" fill=\"#212121\" text-anchor=\"end\">Ra, \ub9c8\uc774\ud06c\ub85c\uc778\uce58 (\ud558\ub2e8 \ub208\uae08)<\/text>\n<text x=\"206\" y=\"80\" font-size=\"11\" fill=\"#212121\" text-anchor=\"end\">\ud654\uc5fc \uc808\ub2e8<\/text>\n<rect x=\"216.0\" y=\"69\" width=\"185.9\" height=\"11\" rx=\"1.5\" fill=\"#cfd6df\"\/>\n<rect x=\"278.2\" y=\"69\" width=\"62.2\" height=\"11\" rx=\"1.5\" fill=\"#1e1e2e\"\/>\n<text x=\"206\" y=\"101\" font-size=\"11\" fill=\"#212121\" text-anchor=\"end\">\uc2a4\ub0b4\uae45<\/text>\n<rect x=\"216.0\" y=\"90\" width=\"246.7\" height=\"11\" rx=\"1.5\" fill=\"#cfd6df\"\/>\n<rect x=\"278.2\" y=\"90\" width=\"123.7\" height=\"11\" rx=\"1.5\" fill=\"#1e1e2e\"\/>\n<text x=\"206\" y=\"122\" font-size=\"11\" fill=\"#212121\" text-anchor=\"end\">\ud1b1\uc9c8<\/text>\n<rect x=\"216.0\" y=\"111\" width=\"371.1\" height=\"11\" rx=\"1.5\" fill=\"#cfd6df\"\/>\n<rect x=\"278.2\" y=\"111\" width=\"246.7\" height=\"11\" rx=\"1.5\" fill=\"#1e1e2e\"\/>\n<text x=\"206\" y=\"143\" font-size=\"11\" fill=\"#212121\" text-anchor=\"end\">\ud3c9\uc0ad, \uc131\ud615<\/text>\n<rect x=\"278.2\" y=\"132\" width=\"371.1\" height=\"11\" rx=\"1.5\" fill=\"#cfd6df\"\/>\n<rect x=\"340.4\" y=\"132\" width=\"184.5\" height=\"11\" rx=\"1.5\" fill=\"#1e1e2e\"\/>\n<text x=\"206\" y=\"164\" font-size=\"11\" fill=\"#212121\" text-anchor=\"end\">\uad50\ub828<\/text>\n<rect x=\"340.4\" y=\"153\" width=\"246.7\" height=\"11\" rx=\"1.5\" fill=\"#cfd6df\"\/>\n<rect x=\"401.9\" y=\"153\" width=\"123.0\" height=\"11\" rx=\"1.5\" fill=\"#1e1e2e\"\/>\n<text x=\"206\" y=\"185\" font-size=\"11\" fill=\"#212121\" text-anchor=\"end\">\ud654\ud559 \ubc00\ub9c1<\/text>\n<rect x=\"340.4\" y=\"174\" width=\"246.7\" height=\"11\" rx=\"1.5\" fill=\"#cfd6df\"\/>\n<rect x=\"401.9\" y=\"174\" width=\"123.0\" height=\"11\" rx=\"1.5\" fill=\"#1e1e2e\"\/>\n<text x=\"206\" y=\"206\" font-size=\"11\" fill=\"#212121\" text-anchor=\"end\">\uc804\uae30 \ubc29\uc804 \uac00\uacf5<\/text>\n<rect x=\"340.4\" y=\"195\" width=\"246.7\" height=\"11\" rx=\"1.5\" fill=\"#cfd6df\"\/>\n<rect x=\"432.3\" y=\"195\" width=\"92.6\" height=\"11\" rx=\"1.5\" fill=\"#1e1e2e\"\/>\n<text x=\"206\" y=\"227\" font-size=\"11\" fill=\"#212121\" text-anchor=\"end\">\ubc00\ub9c1<\/text>\n<rect x=\"278.2\" y=\"216\" width=\"464.4\" height=\"11\" rx=\"1.5\" fill=\"#cfd6df\"\/>\n<rect x=\"401.9\" y=\"216\" width=\"185.2\" height=\"11\" rx=\"1.5\" fill=\"#1e1e2e\"\/>\n<text x=\"206\" y=\"248\" font-size=\"11\" fill=\"#212121\" text-anchor=\"end\">\ube0c\ub85c\uce6d<\/text>\n<rect x=\"401.9\" y=\"237\" width=\"247.4\" height=\"11\" rx=\"1.5\" fill=\"#cfd6df\"\/>\n<rect x=\"462.7\" y=\"237\" width=\"124.4\" height=\"11\" rx=\"1.5\" fill=\"#1e1e2e\"\/>\n<text x=\"206\" y=\"269\" font-size=\"11\" fill=\"#212121\" text-anchor=\"end\">\ub9ac\ubc0d<\/text>\n<rect x=\"401.9\" y=\"258\" width=\"247.4\" height=\"11\" rx=\"1.5\" fill=\"#cfd6df\"\/>\n<rect x=\"462.7\" y=\"258\" width=\"124.4\" height=\"11\" rx=\"1.5\" fill=\"#1e1e2e\"\/>\n<text x=\"206\" y=\"290\" font-size=\"11\" fill=\"#212121\" text-anchor=\"end\">\uc804\uc790 \ube54<\/text>\n<rect x=\"401.9\" y=\"279\" width=\"309.6\" height=\"11\" rx=\"1.5\" fill=\"#cfd6df\"\/>\n<rect x=\"401.9\" y=\"279\" width=\"185.2\" height=\"11\" rx=\"1.5\" fill=\"#1e1e2e\"\/>\n<text x=\"206\" y=\"311\" font-size=\"11\" fill=\"#212121\" text-anchor=\"end\">\ub808\uc774\uc800<\/text>\n<rect x=\"401.9\" y=\"300\" width=\"309.6\" height=\"11\" rx=\"1.5\" fill=\"#cfd6df\"\/>\n<rect x=\"401.9\" y=\"300\" width=\"185.2\" height=\"11\" rx=\"1.5\" fill=\"#1e1e2e\"\/>\n<text x=\"206\" y=\"332\" font-size=\"11\" fill=\"#212121\" text-anchor=\"end\">\uc804\uae30 \ud654\ud559<\/text>\n<rect x=\"340.4\" y=\"321\" width=\"495.5\" height=\"11\" rx=\"1.5\" fill=\"#cfd6df\"\/>\n<rect x=\"462.7\" y=\"321\" width=\"248.8\" height=\"11\" rx=\"1.5\" fill=\"#1e1e2e\"\/>\n<text x=\"206\" y=\"353\" font-size=\"11\" fill=\"#212121\" text-anchor=\"end\">\ubcf4\ub9c1, \uc120\uc0ad<\/text>\n<rect x=\"278.2\" y=\"342\" width=\"619.9\" height=\"11\" rx=\"1.5\" fill=\"#cfd6df\"\/>\n<rect x=\"401.9\" y=\"342\" width=\"247.4\" height=\"11\" rx=\"1.5\" fill=\"#1e1e2e\"\/>\n<text x=\"206\" y=\"374\" font-size=\"11\" fill=\"#212121\" text-anchor=\"end\">\ubc30\ub7f4 \ub9c8\uac10<\/text>\n<rect x=\"462.7\" y=\"363\" width=\"373.2\" height=\"11\" rx=\"1.5\" fill=\"#cfd6df\"\/>\n<rect x=\"587.1\" y=\"363\" width=\"124.4\" height=\"11\" rx=\"1.5\" fill=\"#1e1e2e\"\/>\n<text x=\"206\" y=\"395\" font-size=\"11\" fill=\"#212121\" text-anchor=\"end\">\uc804\ud574 \uc5f0\uc0ad<\/text>\n<rect x=\"587.1\" y=\"384\" width=\"186.6\" height=\"11\" rx=\"1.5\" fill=\"#cfd6df\"\/>\n<rect x=\"618.2\" y=\"384\" width=\"93.3\" height=\"11\" rx=\"1.5\" fill=\"#1e1e2e\"\/>\n<text x=\"206\" y=\"416\" font-size=\"11\" fill=\"#212121\" text-anchor=\"end\">\ub864\ub7ec \ubc84\ub2c8\uc2f1<\/text>\n<rect x=\"587.1\" y=\"405\" width=\"186.6\" height=\"11\" rx=\"1.5\" fill=\"#cfd6df\"\/>\n<rect x=\"649.3\" y=\"405\" width=\"62.2\" height=\"11\" rx=\"1.5\" fill=\"#1e1e2e\"\/>\n<text x=\"206\" y=\"437\" font-size=\"11\" fill=\"#212121\" text-anchor=\"end\">\uc5f0\ub9c8<\/text>\n<rect x=\"401.9\" y=\"426\" width=\"496.2\" height=\"11\" rx=\"1.5\" fill=\"#cfd6df\"\/>\n<rect x=\"524.9\" y=\"426\" width=\"248.8\" height=\"11\" rx=\"1.5\" fill=\"#1e1e2e\"\/>\n<text x=\"206\" y=\"458\" font-size=\"11\" fill=\"#212121\" text-anchor=\"end\">\ud638\ub2dd<\/text>\n<rect x=\"524.9\" y=\"447\" width=\"373.2\" height=\"11\" rx=\"1.5\" fill=\"#cfd6df\"\/>\n<rect x=\"587.1\" y=\"447\" width=\"186.6\" height=\"11\" rx=\"1.5\" fill=\"#1e1e2e\"\/>\n<text x=\"206\" y=\"479\" font-size=\"11\" fill=\"#212121\" text-anchor=\"end\">\uc804\ud574 \uc5f0\ub9c8<\/text>\n<rect x=\"524.9\" y=\"468\" width=\"439.1\" height=\"11\" rx=\"1.5\" fill=\"#cfd6df\"\/>\n<rect x=\"587.1\" y=\"468\" width=\"186.6\" height=\"11\" rx=\"1.5\" fill=\"#1e1e2e\"\/>\n<text x=\"206\" y=\"500\" font-size=\"11\" fill=\"#212121\" text-anchor=\"end\">\uc5f0\ub9c8<\/text>\n<rect x=\"587.1\" y=\"489\" width=\"376.9\" height=\"11\" rx=\"1.5\" fill=\"#cfd6df\"\/>\n<rect x=\"649.3\" y=\"489\" width=\"124.4\" height=\"11\" rx=\"1.5\" fill=\"#1e1e2e\"\/>\n<text x=\"206\" y=\"521\" font-size=\"11\" fill=\"#212121\" text-anchor=\"end\">\ub798\ud551<\/text>\n<rect x=\"587.1\" y=\"510\" width=\"376.9\" height=\"11\" rx=\"1.5\" fill=\"#cfd6df\"\/>\n<rect x=\"649.3\" y=\"510\" width=\"186.6\" height=\"11\" rx=\"1.5\" fill=\"#1e1e2e\"\/>\n<text x=\"206\" y=\"542\" font-size=\"11\" fill=\"#212121\" text-anchor=\"end\">\uc288\ud37c\ud53c\ub2c8\uc2f1<\/text>\n<rect x=\"587.1\" y=\"531\" width=\"376.9\" height=\"11\" rx=\"1.5\" fill=\"#cfd6df\"\/>\n<rect x=\"711.5\" y=\"531\" width=\"186.6\" height=\"11\" rx=\"1.5\" fill=\"#1e1e2e\"\/>\n<text x=\"206\" y=\"563\" font-size=\"11\" fill=\"#212121\" text-anchor=\"end\">\uc0ac\ud615 \uc8fc\uc870<\/text>\n<rect x=\"216.0\" y=\"552\" width=\"185.9\" height=\"11\" rx=\"1.5\" fill=\"#cfd6df\"\/>\n<rect x=\"278.2\" y=\"552\" width=\"62.2\" height=\"11\" rx=\"1.5\" fill=\"#1e1e2e\"\/>\n<text x=\"206\" y=\"584\" font-size=\"11\" fill=\"#212121\" text-anchor=\"end\">\uc5f4\uac04 \uc555\uc5f0<\/text>\n<rect x=\"216.0\" y=\"573\" width=\"185.9\" height=\"11\" rx=\"1.5\" fill=\"#cfd6df\"\/>\n<rect x=\"278.2\" y=\"573\" width=\"62.2\" height=\"11\" rx=\"1.5\" fill=\"#1e1e2e\"\/>\n<text x=\"206\" y=\"605\" font-size=\"11\" fill=\"#212121\" text-anchor=\"end\">\ub2e8\uc870<\/text>\n<rect x=\"278.2\" y=\"594\" width=\"246.7\" height=\"11\" rx=\"1.5\" fill=\"#cfd6df\"\/>\n<rect x=\"340.4\" y=\"594\" width=\"122.3\" height=\"11\" rx=\"1.5\" fill=\"#1e1e2e\"\/>\n<text x=\"206\" y=\"626\" font-size=\"11\" fill=\"#212121\" text-anchor=\"end\">\uc601\uad6c \uae08\ud615 \uc8fc\uc870<\/text>\n<rect x=\"401.9\" y=\"615\" width=\"185.2\" height=\"11\" rx=\"1.5\" fill=\"#cfd6df\"\/>\n<rect x=\"462.7\" y=\"615\" width=\"62.2\" height=\"11\" rx=\"1.5\" fill=\"#1e1e2e\"\/>\n<text x=\"206\" y=\"647\" font-size=\"11\" fill=\"#212121\" text-anchor=\"end\">\uc778\ubca0\uc2a4\ud2b8\uba3c\ud2b8 \uc8fc\uc870<\/text>\n<rect x=\"401.9\" y=\"636\" width=\"247.4\" height=\"11\" rx=\"1.5\" fill=\"#cfd6df\"\/>\n<rect x=\"462.7\" y=\"636\" width=\"62.2\" height=\"11\" rx=\"1.5\" fill=\"#1e1e2e\"\/>\n<text x=\"206\" y=\"668\" font-size=\"11\" fill=\"#212121\" text-anchor=\"end\">\uc555\ucd9c<\/text>\n<rect x=\"340.4\" y=\"657\" width=\"308.9\" height=\"11\" rx=\"1.5\" fill=\"#cfd6df\"\/>\n<rect x=\"462.7\" y=\"657\" width=\"124.4\" height=\"11\" rx=\"1.5\" fill=\"#1e1e2e\"\/>\n<text x=\"206\" y=\"689\" font-size=\"11\" fill=\"#212121\" text-anchor=\"end\">\ub0c9\uac04 \uc555\uc5f0, \uc778\ubc1c<\/text>\n<rect x=\"401.9\" y=\"678\" width=\"309.6\" height=\"11\" rx=\"1.5\" fill=\"#cfd6df\"\/>\n<rect x=\"462.7\" y=\"678\" width=\"124.4\" height=\"11\" rx=\"1.5\" fill=\"#1e1e2e\"\/>\n<text x=\"206\" y=\"710\" font-size=\"11\" fill=\"#212121\" text-anchor=\"end\">\ub2e4\uc774\uce90\uc2a4\ud305<\/text>\n<rect x=\"462.7\" y=\"699\" width=\"186.6\" height=\"11\" rx=\"1.5\" fill=\"#cfd6df\"\/>\n<rect x=\"524.9\" y=\"699\" width=\"62.2\" height=\"11\" rx=\"1.5\" fill=\"#1e1e2e\"\/>\n<rect x=\"216\" y=\"745\" width=\"26\" height=\"10\" rx=\"1.5\" fill=\"#1e1e2e\"\/>\n<text x=\"248\" y=\"754\" font-size=\"11\" fill=\"#212121\">\ud3c9\uade0 \uc801\uc6a9<\/text>\n<rect x=\"431\" y=\"745\" width=\"26\" height=\"10\" rx=\"1.5\" fill=\"#cfd6df\"\/>\n<text x=\"463\" y=\"754\" font-size=\"11\" fill=\"#212121\">\ub35c \ube48\ubc88\ud55c \uc801\uc6a9<\/text>\n<\/svg>\n<\/div>\n<\/div>\n\n\n\n<p class=\"wp-block-paragraph\">\uc0dd\uc0b0 \ubc29\ubc95\ubcc4 \uac70\uce60\uae30 \ubc94\uc704, \uc6d0\ubcf8 \ucc28\ud2b8\uc5d0\uc11c \uc7ac\uc791\uc131. \uc67c\ucabd\uc5d0\uc11c \uc624\ub978\ucabd\uc73c\ub85c \uac70\uce5c \uac83\uc5d0\uc11c \ub9e4\ub044\ub7ec\uc6b4 \uac83\uc73c\ub85c \uc9c4\ud589\ub429\ub2c8\ub2e4.<\/p>\n\n\n\n<figure class=\"wp-block-table is-style-stripes\"><table class=\"has-fixed-layout\"><thead><tr><th class=\"has-text-align-left\" data-align=\"left\">\ud504\ub85c\uc138\uc2a4<\/th><th class=\"has-text-align-left\" data-align=\"left\">\ud3c9\uade0 \uc801\uc6a9, Ra<\/th><th class=\"has-text-align-left\" data-align=\"left\">\ub35c \ube48\ubc88\ud55c \uc801\uc6a9, Ra<\/th><\/tr><\/thead><tbody><tr><td class=\"has-text-align-left\" data-align=\"left\">\ud654\uc5fc \uc808\ub2e8<\/td><td class=\"has-text-align-left\" data-align=\"left\">25 to 12.5 \u00b5m<br>1000 to 500 \u00b5in<\/td><td class=\"has-text-align-left\" data-align=\"left\">50 to 6.3 \u00b5m<br>2000 to 250 \u00b5in<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\uc2a4\ub0b4\uae45<\/td><td class=\"has-text-align-left\" data-align=\"left\">25 to 6.3 \u00b5m<br>1000 to 250 \u00b5in<\/td><td class=\"has-text-align-left\" data-align=\"left\">50 to 3.2 \u00b5m<br>2000 to 125 \u00b5in<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\ud1b1\uc9c8<\/td><td class=\"has-text-align-left\" data-align=\"left\">25 to 1.6 \u00b5m<br>1000 to 63 \u00b5in<\/td><td class=\"has-text-align-left\" data-align=\"left\">50 to 0.80 \u00b5m<br>2000 to 32 \u00b5in<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\ud3c9\uc0ad, \uc131\ud615<\/td><td class=\"has-text-align-left\" data-align=\"left\">12.5 to 1.6 \u00b5m<br>500 to 63 \u00b5in<\/td><td class=\"has-text-align-left\" data-align=\"left\">25 to 0.40 \u00b5m<br>1000 to 16 \u00b5in<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\uad50\ub828<\/td><td class=\"has-text-align-left\" data-align=\"left\">6.3 to 1.6 \u00b5m<br>250 to 63 \u00b5in<\/td><td class=\"has-text-align-left\" data-align=\"left\">12.5 to 0.80 \u00b5m<br>500 to 32 \u00b5in<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\ud654\ud559 \ubc00\ub9c1<\/td><td class=\"has-text-align-left\" data-align=\"left\">6.3 to 1.6 \u00b5m<br>250 to 63 \u00b5in<\/td><td class=\"has-text-align-left\" data-align=\"left\">12.5 to 0.80 \u00b5m<br>500 to 32 \u00b5in<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\uc804\uae30 \ubc29\uc804 \uac00\uacf5<\/td><td class=\"has-text-align-left\" data-align=\"left\">4.5 to 1.6 \u00b5m<br>180 to 63 \u00b5in<\/td><td class=\"has-text-align-left\" data-align=\"left\">12.5 to 0.80 \u00b5m<br>500 to 32 \u00b5in<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\ubc00\ub9c1<\/td><td class=\"has-text-align-left\" data-align=\"left\">6.3 to 0.80 \u00b5m<br>250 to 32 \u00b5in<\/td><td class=\"has-text-align-left\" data-align=\"left\">25 to 0.141 \u00b5m<br>1000 to 5.66 \u00b5in<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\ube0c\ub85c\uce6d<\/td><td class=\"has-text-align-left\" data-align=\"left\">3.2 to 0.80 \u00b5m<br>125 to 32 \u00b5in<\/td><td class=\"has-text-align-left\" data-align=\"left\">6.3 to 0.40 \u00b5m<br>250 to 16 \u00b5in<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\ub9ac\ubc0d<\/td><td class=\"has-text-align-left\" data-align=\"left\">3.2 to 0.80 \u00b5m<br>125 to 32 \u00b5in<\/td><td class=\"has-text-align-left\" data-align=\"left\">6.3 to 0.40 \u00b5m<br>250 to 16 \u00b5in<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\uc804\uc790 \ube54<\/td><td class=\"has-text-align-left\" data-align=\"left\">6.3 to 0.80 \u00b5m<br>250 to 32 \u00b5in<\/td><td class=\"has-text-align-left\" data-align=\"left\">6.3 to 0.20 \u00b5m<br>250 to 8 \u00b5in<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\ub808\uc774\uc800<\/td><td class=\"has-text-align-left\" data-align=\"left\">6.3 to 0.80 \u00b5m<br>250 to 32 \u00b5in<\/td><td class=\"has-text-align-left\" data-align=\"left\">6.3 to 0.20 \u00b5m<br>250 to 8 \u00b5in<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\uc804\uae30 \ud654\ud559<\/td><td class=\"has-text-align-left\" data-align=\"left\">3.2 to 0.20 \u00b5m<br>125 to 8 \u00b5in<\/td><td class=\"has-text-align-left\" data-align=\"left\">12.5 to 0.05 \u00b5m<br>500 to 2 \u00b5in<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\ubcf4\ub9c1, \uc120\uc0ad<\/td><td class=\"has-text-align-left\" data-align=\"left\">6.3 to 0.40 \u00b5m<br>250 to 16 \u00b5in<\/td><td class=\"has-text-align-left\" data-align=\"left\">25 to 0.025 \u00b5m<br>1000 to 1 \u00b5in<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\ubc30\ub7f4 \ub9c8\uac10<\/td><td class=\"has-text-align-left\" data-align=\"left\">0.80 ~ 0.20 \u00b5m<br>32 ~ 8 \u00b5in<\/td><td class=\"has-text-align-left\" data-align=\"left\">3.2 ~ 0.05 \u00b5m<br>125 ~ 2 \u00b5in<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\uc804\ud574 \uc5f0\uc0ad<\/td><td class=\"has-text-align-left\" data-align=\"left\">0.566 ~ 0.20 \u00b5m<br>22.6 ~ 8 \u00b5in<\/td><td class=\"has-text-align-left\" data-align=\"left\">0.80 ~ 0.10 \u00b5m<br>32 ~ 4 \u00b5in<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\ub864\ub7ec \ubc84\ub2c8\uc2f1<\/td><td class=\"has-text-align-left\" data-align=\"left\">0.40 ~ 0.20 \u00b5m<br>16 ~ 8 \u00b5in<\/td><td class=\"has-text-align-left\" data-align=\"left\">0.80 ~ 0.10 \u00b5m<br>32 ~ 4 \u00b5in<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\uc5f0\ub9c8<\/td><td class=\"has-text-align-left\" data-align=\"left\">1.6 ~ 0.10 \u00b5m<br>63 ~ 4 \u00b5in<\/td><td class=\"has-text-align-left\" data-align=\"left\">6.3 ~ 0.025 \u00b5m<br>250 ~ 1 \u00b5in<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\ud638\ub2dd<\/td><td class=\"has-text-align-left\" data-align=\"left\">0.80 ~ 0.10 \u00b5m<br>32 ~ 4 \u00b5in<\/td><td class=\"has-text-align-left\" data-align=\"left\">1.6 ~ 0.025 \u00b5m<br>63 ~ 1 \u00b5in<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\uc804\ud574 \uc5f0\ub9c8<\/td><td class=\"has-text-align-left\" data-align=\"left\">0.80 ~ 0.10 \u00b5m<br>32 ~ 4 \u00b5in<\/td><td class=\"has-text-align-left\" data-align=\"left\">1.6 ~ 0.012 \u00b5m<br>63 ~ 0.5 \u00b5in<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\uc5f0\ub9c8<\/td><td class=\"has-text-align-left\" data-align=\"left\">0.40 ~ 0.10 \u00b5m<br>16 ~ 4 \u00b5in<\/td><td class=\"has-text-align-left\" data-align=\"left\">0.80 ~ 0.012 \u00b5m<br>32 ~ 0.5 \u00b5in<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\ub798\ud551<\/td><td class=\"has-text-align-left\" data-align=\"left\">0.40 ~ 0.05 \u00b5m<br>16 ~ 2 \u00b5in<\/td><td class=\"has-text-align-left\" data-align=\"left\">0.80 ~ 0.012 \u00b5m<br>32 ~ 0.5 \u00b5in<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\uc288\ud37c\ud53c\ub2c8\uc2f1<\/td><td class=\"has-text-align-left\" data-align=\"left\">0.20 ~ 0.025 \u00b5m<br>8 ~ 1 \u00b5in<\/td><td class=\"has-text-align-left\" data-align=\"left\">0.80 ~ 0.012 \u00b5m<br>32 ~ 0.5 \u00b5in<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\uc0ac\ud615 \uc8fc\uc870<\/td><td class=\"has-text-align-left\" data-align=\"left\">25 to 12.5 \u00b5m<br>1000 to 500 \u00b5in<\/td><td class=\"has-text-align-left\" data-align=\"left\">50 to 6.3 \u00b5m<br>2000 to 250 \u00b5in<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\uc5f4\uac04 \uc555\uc5f0<\/td><td class=\"has-text-align-left\" data-align=\"left\">25 to 12.5 \u00b5m<br>1000 to 500 \u00b5in<\/td><td class=\"has-text-align-left\" data-align=\"left\">50 to 6.3 \u00b5m<br>2000 to 250 \u00b5in<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\ub2e8\uc870<\/td><td class=\"has-text-align-left\" data-align=\"left\">12.5 ~ 3.2 \u00b5m<br>500 ~ 125 \u00b5in<\/td><td class=\"has-text-align-left\" data-align=\"left\">25 to 1.6 \u00b5m<br>1000 to 63 \u00b5in<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\uc601\uad6c \uae08\ud615 \uc8fc\uc870<\/td><td class=\"has-text-align-left\" data-align=\"left\">3.2 ~ 1.6 \u00b5m<br>125 ~ 63 \u00b5in<\/td><td class=\"has-text-align-left\" data-align=\"left\">6.3 to 0.80 \u00b5m<br>250 to 32 \u00b5in<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\uc778\ubca0\uc2a4\ud2b8\uba3c\ud2b8 \uc8fc\uc870<\/td><td class=\"has-text-align-left\" data-align=\"left\">3.2 ~ 1.6 \u00b5m<br>125 ~ 63 \u00b5in<\/td><td class=\"has-text-align-left\" data-align=\"left\">6.3 to 0.40 \u00b5m<br>250 to 16 \u00b5in<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\uc555\ucd9c<\/td><td class=\"has-text-align-left\" data-align=\"left\">3.2 to 0.80 \u00b5m<br>125 to 32 \u00b5in<\/td><td class=\"has-text-align-left\" data-align=\"left\">12.5 ~ 0.40 \u00b5m<br>500 ~ 16 \u00b5in<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\ub0c9\uac04 \uc555\uc5f0, \uc778\ubc1c<\/td><td class=\"has-text-align-left\" data-align=\"left\">3.2 to 0.80 \u00b5m<br>125 to 32 \u00b5in<\/td><td class=\"has-text-align-left\" data-align=\"left\">6.3 to 0.20 \u00b5m<br>250 to 8 \u00b5in<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">\ub2e4\uc774\uce90\uc2a4\ud305<\/td><td class=\"has-text-align-left\" data-align=\"left\">1.6 ~ 0.80 \u00b5m<br>63 ~ 32 \u00b5in<\/td><td class=\"has-text-align-left\" data-align=\"left\">3.2 ~ 0.40 \u00b5m<br>125 ~ 16 \u00b5in<\/td><\/tr><\/tbody><\/table><\/figure>\n\n\n\n<h2 id=\"h-roughness-grades-n1-to-n12\" class=\"wp-block-heading\">\uac70\uce60\uae30 \ub4f1\uae09 N1~N12<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">\uc624\ub798\ub41c \ub3c4\uba74\uacfc \uc0ac\uc591\uc11c\ub294 Ra \uac12 \ub300\uc2e0 \ub4f1\uae09 \ubc88\ud638\ub97c \ud45c\uae30\ud569\ub2c8\ub2e4. \ub4f1\uae09 \ubc88\ud638\ub294 Ra\uc640 \ubc18\ub300 \ubc29\ud5a5\uc73c\ub85c \uc9c4\ud589\ub418\uba70, \uc22b\uc790\uac00 \ub192\uc744\uc218\ub85d \ud45c\uba74\uc774 \ub354 \uac70\uce69\ub2c8\ub2e4. \ucd9c\ucc98, \ud45c 4.<\/p>\n\n\n\n<figure class=\"wp-block-table is-style-stripes\"><table class=\"has-fixed-layout\"><thead><tr><th class=\"has-text-align-left\" data-align=\"left\">\ub4f1\uae09<\/th><th class=\"has-text-align-left\" data-align=\"left\">Ra, \u00b5m<\/th><th class=\"has-text-align-left\" data-align=\"left\">Ra, \u00b5in<\/th><\/tr><\/thead><tbody><tr><td class=\"has-text-align-left\" data-align=\"left\">N12<\/td><td class=\"has-text-align-left\" data-align=\"left\">50<\/td><td class=\"has-text-align-left\" data-align=\"left\">2000<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">N11<\/td><td class=\"has-text-align-left\" data-align=\"left\">25<\/td><td class=\"has-text-align-left\" data-align=\"left\">1000<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">N10<\/td><td class=\"has-text-align-left\" data-align=\"left\">12.5<\/td><td class=\"has-text-align-left\" data-align=\"left\">500<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">N9<\/td><td class=\"has-text-align-left\" data-align=\"left\">6.3<\/td><td class=\"has-text-align-left\" data-align=\"left\">250<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">N8<\/td><td class=\"has-text-align-left\" data-align=\"left\">3.2<\/td><td class=\"has-text-align-left\" data-align=\"left\">125<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">N7<\/td><td class=\"has-text-align-left\" data-align=\"left\">1.6<\/td><td class=\"has-text-align-left\" data-align=\"left\">63<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">N6<\/td><td class=\"has-text-align-left\" data-align=\"left\">0.80<\/td><td class=\"has-text-align-left\" data-align=\"left\">32<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">N5<\/td><td class=\"has-text-align-left\" data-align=\"left\">0.40<\/td><td class=\"has-text-align-left\" data-align=\"left\">16<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">N4<\/td><td class=\"has-text-align-left\" data-align=\"left\">0.20<\/td><td class=\"has-text-align-left\" data-align=\"left\">8<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">N3<\/td><td class=\"has-text-align-left\" data-align=\"left\">0.10<\/td><td class=\"has-text-align-left\" data-align=\"left\">4<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">N2<\/td><td class=\"has-text-align-left\" data-align=\"left\">0.05<\/td><td class=\"has-text-align-left\" data-align=\"left\">2<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">N1<\/td><td class=\"has-text-align-left\" data-align=\"left\">0.025<\/td><td class=\"has-text-align-left\" data-align=\"left\">1<\/td><\/tr><\/tbody><\/table><\/figure>\n\n\n\n<h2 id=\"h-preferred-ra-values-to-specify\" class=\"wp-block-heading\">\uc9c0\uc815\ud560 \uad8c\uc7a5 Ra \uac12<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">\ud45c\uc900 Ra \uac12 \uc2dc\ub9ac\uc988 (ISO 1302 \ubc0f \ub3d9\ub4f1\ud55c \uad6d\uac00 \ud45c\uc900). (a)\ub85c \ud45c\uc2dc\ub41c \uac12\uc774 \uad8c\uc7a5 \uac12\uc774\uba70, \uc774 \uc2dc\ub9ac\uc988\uc5d0\uc11c \uac12\uc744 \uc9c0\uc815\ud558\uba74 \ud45c\uc900 \uac70\uce60\uae30 \uc2dc\ud3b8\uc73c\ub85c \ubd80\ud488\uc744 \uce21\uc815\ud560 \uc218 \uc788\uc2b5\ub2c8\ub2e4. \ucd9c\ucc98, \ud45c 3.<\/p>\n\n\n\n<figure class=\"wp-block-table is-style-stripes\"><table><thead><tr><th class=\"has-text-align-left\" data-align=\"left\">Ra \uac12\uc758 \uc6b0\uc120 \uacc4\uc5f4, \u00b5m(\uc0c1\ub2e8) \ubc0f \u00b5in(\ud558\ub2e8)<\/th><th class=\"has-text-align-left\" data-align=\"left\"><\/th><th class=\"has-text-align-left\" data-align=\"left\"><\/th><th class=\"has-text-align-left\" data-align=\"left\"><\/th><th class=\"has-text-align-left\" data-align=\"left\"><\/th><th class=\"has-text-align-left\" data-align=\"left\"><\/th><th class=\"has-text-align-left\" data-align=\"left\"><\/th><th class=\"has-text-align-left\" data-align=\"left\"><\/th><th class=\"has-text-align-left\" data-align=\"left\"><\/th><th class=\"has-text-align-left\" data-align=\"left\"><\/th><\/tr><\/thead><tbody><tr><td class=\"has-text-align-left\" data-align=\"left\">0.012<br>0.5<\/td><td class=\"has-text-align-left\" data-align=\"left\">0.025 <sup>(a)<\/sup><br>1<\/td><td class=\"has-text-align-left\" data-align=\"left\">0.050 <sup>(a)<\/sup><br>2<\/td><td class=\"has-text-align-left\" data-align=\"left\">0.075<br>3<\/td><td class=\"has-text-align-left\" data-align=\"left\">0.10 <sup>(a)<\/sup><br>4<\/td><td class=\"has-text-align-left\" data-align=\"left\">0.125<br>5<\/td><td class=\"has-text-align-left\" data-align=\"left\">0.15<br>6<\/td><td class=\"has-text-align-left\" data-align=\"left\">0.20 <sup>(a)<\/sup><br>8<\/td><td class=\"has-text-align-left\" data-align=\"left\">0.25<br>10<\/td><td class=\"has-text-align-left\" data-align=\"left\">0.32<br>13<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">0.40 <sup>(a)<\/sup><br>16<\/td><td class=\"has-text-align-left\" data-align=\"left\">0.50<br>20<\/td><td class=\"has-text-align-left\" data-align=\"left\">0.63<br>25<\/td><td class=\"has-text-align-left\" data-align=\"left\">0.80 <sup>(a)<\/sup><br>32<\/td><td class=\"has-text-align-left\" data-align=\"left\">1.00<br>40<\/td><td class=\"has-text-align-left\" data-align=\"left\">1.25<br>50<\/td><td class=\"has-text-align-left\" data-align=\"left\">1.60 <sup>(a)<\/sup><br>63<\/td><td class=\"has-text-align-left\" data-align=\"left\">2.0<br>80<\/td><td class=\"has-text-align-left\" data-align=\"left\">2.5<br>100<\/td><td class=\"has-text-align-left\" data-align=\"left\">3.2 <sup>(a)<\/sup><br>125<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">4.0<br>160<\/td><td class=\"has-text-align-left\" data-align=\"left\">5.0<br>200<\/td><td class=\"has-text-align-left\" data-align=\"left\">6.3 <sup>(a)<\/sup><br>250<\/td><td class=\"has-text-align-left\" data-align=\"left\">8.0<br>320<\/td><td class=\"has-text-align-left\" data-align=\"left\">10.0<br>400<\/td><td class=\"has-text-align-left\" data-align=\"left\">12.5 <sup>(a)<\/sup><br>500<\/td><td class=\"has-text-align-left\" data-align=\"left\">15<br>600<\/td><td class=\"has-text-align-left\" data-align=\"left\">20<br>800<\/td><td class=\"has-text-align-left\" data-align=\"left\">25 <sup>(a)<\/sup><br>1000<\/td><\/tr><\/tbody><\/table><\/figure>\n\n\n\n<p class=\"wp-block-paragraph\">(a) \uad8c\uc7a5 \uac12.<\/p>\n\n\n\n<h2 id=\"h-cutoff-the-roughness-sampling-length\" class=\"wp-block-heading\">\ucef7\uc624\ud504, \uac70\uce60\uae30 \uc0d8\ud50c\ub9c1 \uae38\uc774<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">\ucef7\uc624\ud504\ub294 \uae30\uae30\uac00 \ud504\ub85c\ud30c\uc77c\uc744 \uc0d8\ud50c\ub9c1\ud558\ub294 \uae38\uc774\uc785\ub2c8\ub2e4. \ub3c4\uba74\uc5d0 \uba85\uc2dc\ub418\uc9c0 \uc54a\uc740 \uacbd\uc6b0 0.80 mm (0.030 in.) \uac12\uc774 \uc801\uc6a9\ub429\ub2c8\ub2e4. \ucd9c\ucc98, \ud45c 2.<\/p>\n\n\n\n<figure class=\"wp-block-table is-style-stripes\"><table class=\"has-fixed-layout\"><thead><tr><th class=\"has-text-align-left\" data-align=\"left\">\ucef7\uc624\ud504, mm<\/th><th class=\"has-text-align-left\" data-align=\"left\">\ucef7\uc624\ud504, in.<\/th><\/tr><\/thead><tbody><tr><td class=\"has-text-align-left\" data-align=\"left\">0.08<\/td><td class=\"has-text-align-left\" data-align=\"left\">0.003<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">0.25<\/td><td class=\"has-text-align-left\" data-align=\"left\">0.010<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">0.80<\/td><td class=\"has-text-align-left\" data-align=\"left\">0.030<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">2.5<\/td><td class=\"has-text-align-left\" data-align=\"left\">0.1<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">8.0<\/td><td class=\"has-text-align-left\" data-align=\"left\">0.3<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">25.0<\/td><td class=\"has-text-align-left\" data-align=\"left\">1.0<\/td><\/tr><\/tbody><\/table><\/figure>\n\n\n\n<ul class=\"wp-block-list\">\n<li>Ra\ub294 \uc804\uccb4\uc801\uc73c\ub85c \ub9c8\uc774\ud06c\ub85c\ubbf8\ud130\uc640 \ub9c8\uc774\ud06c\ub85c\uc778\uce58\ub85c \ud45c\uae30\ub418\uba70, \uc6d0\ubcf8 \ucc28\ud2b8\uc758 \ub450 \ud589\uc785\ub2c8\ub2e4.<\/li>\n\n\n\n<li>\ud55c \uacf5\uc815\uc73c\ub85c \uac00\uacf5\ub41c \ud45c\uba74\uc740 \uacf5\uc815 \uccb4\uc778 \ub0b4 \ud6c4\uc18d \uc815\uc0ad \uacf5\uc815(\uc120\uc0ad \ud6c4 \uc5f0\uc0ad, \uc5f0\uc0ad \ud6c4 \ud638\ub2dd)\uc744 \ud1b5\ud574 \ud754\ud788 \uac1c\uc120\ub429\ub2c8\ub2e4. \ud6c4\uc18d \uacf5\uc815\uc740 \ucc28\ud2b8\ub97c \uc67c\ucabd\uc5d0\uc11c \uc624\ub978\ucabd\uc73c\ub85c \uc77d\uc73c\uc2ed\uc2dc\uc624.<\/li>\n\n\n\n<li>\ubc94\uc704\ub294 \uc77c\ubc18\uc801\uc778 \uc791\uc5c5\uc7a5 \uac12\uc785\ub2c8\ub2e4. \uc808\uc0ad\uc774 \uc2e4\uc81c\ub85c \ub0a8\uae30\ub294 \ub9c8\uac10\uc740 \uc7ac\ub8cc, \uacf5\uad6c \ub610\ub294 \ud720, \uc14b\uc5c5\uc758 \uac15\uc131 \ubc0f \uc0ac\uc6a9\ub41c \uc774\uc1a1\uc5d0 \ub530\ub77c \ub2ec\ub77c\uc9d1\ub2c8\ub2e4.<\/li>\n<\/ul>\n\n\n\n<h3 id=\"h-reading-the-chart\" class=\"wp-block-heading\">\ucc28\ud2b8 \uc77d\uae30<\/h3>\n\n\n\n<p class=\"wp-block-paragraph\">\uacf5\uc815 \ud589\uc740 \uc0c1\ub2e8\uc758 \uac00\uc7a5 \uac70\uce5c \ub9c8\ubb34\ub9ac\ubd80\ud130 \ud558\ub2e8\uc758 \uac00\uc7a5 \ub9e4\ub044\ub7ec\uc6b4 \ub9c8\ubb34\ub9ac\uae4c\uc9c0 \ubc30\uc5f4\ub418\uba70, \ub208\uae08\uc740 \uc67c\ucabd\uc758 Ra 50 \u00b5m\ubd80\ud130 \uc624\ub978\ucabd\uc758 0.012 \u00b5m\uae4c\uc9c0\uc785\ub2c8\ub2e4. \uac12\uc744 \ub118\uc5b4 \uc5f0\uc7a5\ub418\ub294 \ud68c\uc0c9 \ub9c9\ub300\ub294 \ud574\ub2f9 \uacf5\uc815\uc774 \uc720\ub9ac\ud55c \uc870\uac74\uc5d0\uc11c \uadf8 \uac70\uce60\uae30\uc5d0 \ub3c4\ub2ec\ud560 \uc218 \uc788\uc74c\uc744 \uc758\ubbf8\ud558\uba70, \uc5b4\ub450\uc6b4 \ubd80\ubd84\uc740 \ud574\ub2f9 \uacf5\uc815\uc774 \uc77c\ubc18\uc801\uc73c\ub85c \uc704\uce58\ud558\ub294 \ubc94\uc704\uc785\ub2c8\ub2e4. \ub3c4\uba74\uc5d0\uc11c \ub9c8\ubb34\ub9ac\ub97c \uc694\uad6c\ud560 \ub54c\ub294 \ubd80\ud488\uc758 \ucd5c\uc885 \uc791\uc5c5\uc5d0 \uc9c0\uc815\ub41c \uacf5\uc815\uc774 \uadf8 \ub9c8\ubb34\ub9ac\ub97c \uc720\uc9c0\ud560 \uc218 \uc788\ub294\uc9c0 \ud655\uc778\ud558\uc2ed\uc2dc\uc624. \ubc00\ub9c1 \uac00\uacf5 \ud45c\uba74\uc740 \uc77c\ubc18\uc801\uc73c\ub85c Ra 3.2~0.80 \u00b5m\ub85c \ud45c\uae30\ub418\ubbc0\ub85c, \ub3c4\uba74\uc774 \ub354 \uc5c4\uaca9\ud560 \uacbd\uc6b0 \uc5f0\uc0ad \ub610\ub294 \ub798\ud551\uc774 \ub4a4\ub530\ub985\ub2c8\ub2e4.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">\uac15\ucca0\uc744 \uc5bc\ub9c8\ub098 \ube60\ub974\uac8c \uac00\uacf5\ud560 \uc218 \uc788\ub294\uc9c0, \uadf8\ub9ac\uace0 \uc5b4\ub5a4 \uacf5\uad6c\ub85c \uac00\uacf5\ud560 \uc218 \uc788\ub294\uc9c0\ub294 <a href=\"https:\/\/aobosteel.com\/ko\/tool-steel-machinability-rating-chart\/\">\ud53c\uc0ad\uc131 \ub4f1\uae09 \ucc28\ud2b8<\/a> \uadf8\ub9ac\uace0 \ub2e4\uc74c\uc5d0 <a href=\"https:\/\/aobosteel.com\/ko\/tool-steel-cutting-speeds-and-feeds\/\">\uacf5\uad6c\uac15\uc758 \uc808\uc0ad \uc18d\ub3c4 \ubc0f \uc774\uc1a1<\/a>\uc5d0\uc11c \ub2e4\ub8f9\ub2c8\ub2e4. \uc808\uc0ad\uc774 \uc544\ub2cc \uce35\uc744 \ucd94\uac00\ud558\ub294 \ud45c\uba74 \ucc98\ub9ac\ub294 \ub2e4\ub978 \uc8fc\uc81c\ub85c, <a href=\"https:\/\/aobosteel.com\/ko\/blog\/tool-steel-surface-treatment\/\">\ud45c\uba74 \ucc98\ub9ac \ud398\uc774\uc9c0<\/a>.<\/p>\n\n\n\n<h3 id=\"h-related-reference-pages\" class=\"wp-block-heading\">\uad00\ub828 \ucc38\uc870 \ud398\uc774\uc9c0<\/h3>\n\n\n\n<p class=\"wp-block-paragraph\"><a href=\"https:\/\/aobosteel.com\/ko\/tool-steel-machining-allowance-chart\/\">\uac00\uacf5 \uc5ec\uc720 \ucc28\ud2b8<\/a> \u00b7 <a href=\"https:\/\/aobosteel.com\/ko\/tool-steel-properties-chart\/\">\uacf5\uad6c\uac15 \ud2b9\uc131 \ucc28\ud2b8<\/a><\/p>\n\n\n\n<p class=\"wp-block-paragraph\">\ucd9c\ucc98: Machinery&#8217;s Handbook 28th Edition (Industrial Press), Surface Texture \uc139\uc158: Table 1 (\uc77c\ubc18 \uc0dd\uc0b0 \ubc29\ubc95\uc73c\ub85c \uc0dd\uc131\ub418\ub294 \uac70\uce60\uae30), Table 2 (\ud45c\uc900 \ucef7\uc624\ud504 \uac12), Table 3 (Ra \uac12\uc758 \uc6b0\uc120 \uacc4\uc5f4), Table 4 (\uac70\uce60\uae30 \ub4f1\uae09). \ucc28\ud2b8\ub294 \ucd9c\ucc98\uc5d0\uc11c \ub2e4\uc2dc \uadf8\ub9b0 \uac83\uc785\ub2c8\ub2e4. \uac12\uc740 1 \u00b5m = 39.37 \u00b5in (0.0254 \u00b5m = 1 \u00b5in) \uae30\uc900\uc73c\ub85c \ub9c8\uc774\ud06c\ub85c\ubbf8\ud130\uc640 \ub9c8\uc774\ud06c\ub85c\uc778\uce58 \uac04\uc5d0 \ubcc0\ud658\ub418\uc5c8\uc2b5\ub2c8\ub2e4.<\/p>","protected":false},"excerpt":{"rendered":"<p>Surface Roughness Chart The Ra finish each production method leaves on steel, from flame cutting and sawing down to lapping and superfinishing. Each row shows the range routinely produced and the wider range that can still occur, in micrometers and microinches, along with the roughness grade numbers and their cut-off values. Roughness produced by common [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":0,"parent":0,"menu_order":0,"comment_status":"closed","ping_status":"closed","template":"","meta":{"_uag_custom_page_level_css":"","site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"default","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"disabled","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","ast-disable-related-posts":"","theme-transparent-header-meta":"","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"set","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"footnotes":""},"class_list":["post-18375","page","type-page","status-publish","hentry"],"yoast_head":"<!-- This site is optimized with the Yoast SEO Premium plugin v28.8 (Yoast SEO v28.8) - https:\/\/yoast.com\/product\/yoast-seo-premium-wordpress\/ -->\n<title>Surface Roughness Chart: Ra Values by Process | Aobo Steel<\/title>\n<meta name=\"description\" content=\"Ra surface roughness values for common production methods, from flame cutting to polishing, with roughness grades and preferred values in micrometres and microinches.\" \/>\n<meta name=\"robots\" content=\"index, follow, max-snippet:-1, max-image-preview:large, max-video-preview:-1\" \/>\n<link rel=\"canonical\" href=\"https:\/\/aobosteel.com\/ko\/surface-roughness-chart\/\" \/>\n<meta property=\"og:locale\" content=\"ko_KR\" \/>\n<meta property=\"og:type\" content=\"article\" \/>\n<meta property=\"og:title\" content=\"Surface Roughness Chart\" \/>\n<meta property=\"og:description\" content=\"Ra surface roughness values for common production methods, from flame cutting to polishing, with roughness grades and preferred values in micrometres and microinches.\" \/>\n<meta property=\"og:url\" content=\"https:\/\/aobosteel.com\/ko\/surface-roughness-chart\/\" \/>\n<meta property=\"og:site_name\" content=\"AoboSteel\" \/>\n<meta property=\"article:publisher\" content=\"https:\/\/www.facebook.com\/profile.php?id=61565368220197\" \/>\n<meta property=\"article:modified_time\" content=\"2026-10-21T03:44:23+00:00\" \/>\n<meta name=\"twitter:card\" content=\"summary_large_image\" \/>\n<meta name=\"twitter:label1\" content=\"\uc608\uc0c1 \ub418\ub294 \ud310\ub3c5 \uc2dc\uac04\" \/>\n\t<meta name=\"twitter:data1\" content=\"6\ubd84\" \/>\n<script type=\"application\/ld+json\" class=\"yoast-schema-graph\">{\"@context\":\"https:\\\/\\\/schema.org\",\"@graph\":[{\"@type\":\"TechArticle\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/surface-roughness-chart\\\/#article\",\"isPartOf\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/surface-roughness-chart\\\/\"},\"author\":{\"name\":\"Evan\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#\\\/schema\\\/person\\\/96118415c30ca6bb52eaf1127b052ef7\"},\"headline\":\"Surface Roughness Chart\",\"datePublished\":\"2026-09-15T04:39:58+00:00\",\"dateModified\":\"2026-10-21T03:44:23+00:00\",\"mainEntityOfPage\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/surface-roughness-chart\\\/\"},\"wordCount\":925,\"publisher\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#organization\"},\"inLanguage\":\"ko-KR\"},{\"@type\":\"WebPage\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/surface-roughness-chart\\\/\",\"url\":\"https:\\\/\\\/aobosteel.com\\\/surface-roughness-chart\\\/\",\"name\":\"Surface Roughness Chart: Ra Values by Process | Aobo Steel\",\"isPartOf\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#website\"},\"datePublished\":\"2026-09-15T04:39:58+00:00\",\"dateModified\":\"2026-10-21T03:44:23+00:00\",\"description\":\"Ra surface roughness values for common production methods, from flame cutting to polishing, with roughness grades and preferred values in micrometres and microinches.\",\"breadcrumb\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/surface-roughness-chart\\\/#breadcrumb\"},\"inLanguage\":\"ko-KR\",\"potentialAction\":[{\"@type\":\"ReadAction\",\"target\":[\"https:\\\/\\\/aobosteel.com\\\/surface-roughness-chart\\\/\"]}]},{\"@type\":\"BreadcrumbList\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/surface-roughness-chart\\\/#breadcrumb\",\"itemListElement\":[{\"@type\":\"ListItem\",\"position\":1,\"name\":\"\u9996\u9875\",\"item\":\"https:\\\/\\\/aobosteel.com\\\/\"},{\"@type\":\"ListItem\",\"position\":2,\"name\":\"Surface Roughness Chart\"}]},{\"@type\":\"WebSite\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#website\",\"url\":\"https:\\\/\\\/aobosteel.com\\\/\",\"name\":\"AoboSteel\",\"description\":\"\",\"publisher\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#organization\"},\"potentialAction\":[{\"@type\":\"SearchAction\",\"target\":{\"@type\":\"EntryPoint\",\"urlTemplate\":\"https:\\\/\\\/aobosteel.com\\\/?s={search_term_string}\"},\"query-input\":{\"@type\":\"PropertyValueSpecification\",\"valueRequired\":true,\"valueName\":\"search_term_string\"}}],\"inLanguage\":\"ko-KR\"},{\"@type\":\"Organization\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#organization\",\"name\":\"AoboSteel\",\"url\":\"https:\\\/\\\/aobosteel.com\\\/\",\"logo\":{\"@type\":\"ImageObject\",\"inLanguage\":\"ko-KR\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#\\\/schema\\\/logo\\\/image\\\/\",\"url\":\"https:\\\/\\\/aobosteel.com\\\/wp-content\\\/uploads\\\/2025\\\/01\\\/cropped-aobo-steel-1.avif\",\"contentUrl\":\"https:\\\/\\\/aobosteel.com\\\/wp-content\\\/uploads\\\/2025\\\/01\\\/cropped-aobo-steel-1.avif\",\"width\":1052,\"height\":592,\"caption\":\"AoboSteel\"},\"image\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#\\\/schema\\\/logo\\\/image\\\/\"},\"sameAs\":[\"https:\\\/\\\/www.facebook.com\\\/profile.php?id=61565368220197\",\"https:\\\/\\\/www.linkedin.com\\\/in\\\/aobosteel-evan\\\/\"]},{\"@type\":\"Person\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#\\\/schema\\\/person\\\/96118415c30ca6bb52eaf1127b052ef7\",\"name\":\"Evan\",\"image\":{\"@type\":\"ImageObject\",\"inLanguage\":\"ko-KR\",\"@id\":\"https:\\\/\\\/secure.gravatar.com\\\/avatar\\\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g\",\"url\":\"https:\\\/\\\/secure.gravatar.com\\\/avatar\\\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g\",\"contentUrl\":\"https:\\\/\\\/secure.gravatar.com\\\/avatar\\\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g\",\"caption\":\"Evan\"},\"sameAs\":[\"http:\\\/\\\/www.aobosteel.com\",\"https:\\\/\\\/www.facebook.com\\\/profile.php?id=61565368220197\",\"https:\\\/\\\/www.instagram.com\\\/aobosteel\\\/\",\"https:\\\/\\\/www.linkedin.com\\\/in\\\/aobosteel-evan\\\/\",\"https:\\\/\\\/x.com\\\/AobosteelEvan\",\"https:\\\/\\\/www.youtube.com\\\/@aobosteel\"],\"url\":\"https:\\\/\\\/aobosteel.com\\\/ko\\\/blog\\\/author\\\/admin\\\/\"}]}<\/script>\n<!-- \/ Yoast SEO Premium plugin. -->","yoast_head_json":{"title":"\ud45c\uba74 \uac70\uce60\uae30 \ucc28\ud2b8: \uacf5\uc815\ubcc4 Ra \uac12 | Aobo Steel","description":"\ud654\uc5fc \uc808\ub2e8\uc5d0\uc11c \ud3f4\ub9ac\uc2f1\uae4c\uc9c0 \uc8fc\uc694 \uc0dd\uc0b0 \uacf5\ubc95\ubcc4 Ra \ud45c\uba74 \uac70\uce60\uae30 \uac12\uacfc \uac70\uce60\uae30 \ub4f1\uae09, \ub9c8\uc774\ud06c\ub85c\ubbf8\ud130 \ubc0f \ub9c8\uc774\ud06c\ub85c\uc778\uce58 \uae30\uc900 \uad8c\uc7a5\uac12\uc744 \uc81c\uc2dc\ud569\ub2c8\ub2e4.","robots":{"index":"index","follow":"follow","max-snippet":"max-snippet:-1","max-image-preview":"max-image-preview:large","max-video-preview":"max-video-preview:-1"},"canonical":"https:\/\/aobosteel.com\/ko\/surface-roughness-chart\/","og_locale":"ko_KR","og_type":"article","og_title":"Surface Roughness Chart","og_description":"Ra surface roughness values for common production methods, from flame cutting to polishing, with roughness grades and preferred values in micrometres and microinches.","og_url":"https:\/\/aobosteel.com\/ko\/surface-roughness-chart\/","og_site_name":"AoboSteel","article_publisher":"https:\/\/www.facebook.com\/profile.php?id=61565368220197","article_modified_time":"2026-10-21T03:44:23+00:00","twitter_card":"summary_large_image","twitter_misc":{"\uc608\uc0c1 \ub418\ub294 \ud310\ub3c5 \uc2dc\uac04":"6\ubd84"},"schema":{"@context":"https:\/\/schema.org","@graph":[{"@type":"TechArticle","@id":"https:\/\/aobosteel.com\/surface-roughness-chart\/#article","isPartOf":{"@id":"https:\/\/aobosteel.com\/surface-roughness-chart\/"},"author":{"name":"Evan","@id":"https:\/\/aobosteel.com\/#\/schema\/person\/96118415c30ca6bb52eaf1127b052ef7"},"headline":"Surface Roughness Chart","datePublished":"2026-09-15T04:39:58+00:00","dateModified":"2026-10-21T03:44:23+00:00","mainEntityOfPage":{"@id":"https:\/\/aobosteel.com\/surface-roughness-chart\/"},"wordCount":925,"publisher":{"@id":"https:\/\/aobosteel.com\/#organization"},"inLanguage":"ko-KR"},{"@type":"WebPage","@id":"https:\/\/aobosteel.com\/surface-roughness-chart\/","url":"https:\/\/aobosteel.com\/surface-roughness-chart\/","name":"\ud45c\uba74 \uac70\uce60\uae30 \ucc28\ud2b8: \uacf5\uc815\ubcc4 Ra \uac12 | Aobo Steel","isPartOf":{"@id":"https:\/\/aobosteel.com\/#website"},"datePublished":"2026-09-15T04:39:58+00:00","dateModified":"2026-10-21T03:44:23+00:00","description":"\ud654\uc5fc \uc808\ub2e8\uc5d0\uc11c \ud3f4\ub9ac\uc2f1\uae4c\uc9c0 \uc8fc\uc694 \uc0dd\uc0b0 \uacf5\ubc95\ubcc4 Ra \ud45c\uba74 \uac70\uce60\uae30 \uac12\uacfc \uac70\uce60\uae30 \ub4f1\uae09, \ub9c8\uc774\ud06c\ub85c\ubbf8\ud130 \ubc0f \ub9c8\uc774\ud06c\ub85c\uc778\uce58 \uae30\uc900 \uad8c\uc7a5\uac12\uc744 \uc81c\uc2dc\ud569\ub2c8\ub2e4.","breadcrumb":{"@id":"https:\/\/aobosteel.com\/surface-roughness-chart\/#breadcrumb"},"inLanguage":"ko-KR","potentialAction":[{"@type":"ReadAction","target":["https:\/\/aobosteel.com\/surface-roughness-chart\/"]}]},{"@type":"BreadcrumbList","@id":"https:\/\/aobosteel.com\/surface-roughness-chart\/#breadcrumb","itemListElement":[{"@type":"ListItem","position":1,"name":"\u9996\u9875","item":"https:\/\/aobosteel.com\/"},{"@type":"ListItem","position":2,"name":"Surface Roughness Chart"}]},{"@type":"WebSite","@id":"https:\/\/aobosteel.com\/#website","url":"https:\/\/aobosteel.com\/","name":"\uc544\uc624\ubcf4\uc2a4\ud2f8","description":"","publisher":{"@id":"https:\/\/aobosteel.com\/#organization"},"potentialAction":[{"@type":"SearchAction","target":{"@type":"EntryPoint","urlTemplate":"https:\/\/aobosteel.com\/?s={search_term_string}"},"query-input":{"@type":"PropertyValueSpecification","valueRequired":true,"valueName":"search_term_string"}}],"inLanguage":"ko-KR"},{"@type":"Organization","@id":"https:\/\/aobosteel.com\/#organization","name":"\uc544\uc624\ubcf4\uc2a4\ud2f8","url":"https:\/\/aobosteel.com\/","logo":{"@type":"ImageObject","inLanguage":"ko-KR","@id":"https:\/\/aobosteel.com\/#\/schema\/logo\/image\/","url":"https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/01\/cropped-aobo-steel-1.avif","contentUrl":"https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/01\/cropped-aobo-steel-1.avif","width":1052,"height":592,"caption":"AoboSteel"},"image":{"@id":"https:\/\/aobosteel.com\/#\/schema\/logo\/image\/"},"sameAs":["https:\/\/www.facebook.com\/profile.php?id=61565368220197","https:\/\/www.linkedin.com\/in\/aobosteel-evan\/"]},{"@type":"Person","@id":"https:\/\/aobosteel.com\/#\/schema\/person\/96118415c30ca6bb52eaf1127b052ef7","name":"\uc5d0\ubc18","image":{"@type":"ImageObject","inLanguage":"ko-KR","@id":"https:\/\/secure.gravatar.com\/avatar\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g","url":"https:\/\/secure.gravatar.com\/avatar\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g","contentUrl":"https:\/\/secure.gravatar.com\/avatar\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g","caption":"Evan"},"sameAs":["http:\/\/www.aobosteel.com","https:\/\/www.facebook.com\/profile.php?id=61565368220197","https:\/\/www.instagram.com\/aobosteel\/","https:\/\/www.linkedin.com\/in\/aobosteel-evan\/","https:\/\/x.com\/AobosteelEvan","https:\/\/www.youtube.com\/@aobosteel"],"url":"https:\/\/aobosteel.com\/ko\/blog\/author\/admin\/"}]}},"uagb_featured_image_src":{"full":false,"thumbnail":false,"medium":false,"medium_large":false,"large":false,"1536x1536":false,"2048x2048":false,"trp-custom-language-flag":false},"uagb_author_info":{"display_name":"Evan","author_link":"https:\/\/aobosteel.com\/ko\/blog\/author\/admin\/"},"uagb_comment_info":0,"uagb_excerpt":"Surface Roughness Chart The Ra finish each production method leaves on steel, from flame cutting and sawing down to lapping and superfinishing. Each row shows the range routinely produced and the wider range that can still occur, in micrometers and microinches, along with the roughness grade numbers and their cut-off values. Roughness produced by common&hellip;","rttpg_featured_image_url":null,"rttpg_author":{"display_name":"Evan","author_link":"https:\/\/aobosteel.com\/ko\/blog\/author\/admin\/"},"rttpg_comment":0,"rttpg_category":null,"rttpg_excerpt":"Surface Roughness Chart The Ra finish each production method leaves on steel, from flame cutting and sawing down to lapping and superfinishing. Each row shows the range routinely produced and the wider range that can still occur, in micrometers and microinches, along with the roughness grade numbers and their cut-off values. Roughness produced by common&hellip;","_links":{"self":[{"href":"https:\/\/aobosteel.com\/ko\/wp-json\/wp\/v2\/pages\/18375","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/aobosteel.com\/ko\/wp-json\/wp\/v2\/pages"}],"about":[{"href":"https:\/\/aobosteel.com\/ko\/wp-json\/wp\/v2\/types\/page"}],"author":[{"embeddable":true,"href":"https:\/\/aobosteel.com\/ko\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/aobosteel.com\/ko\/wp-json\/wp\/v2\/comments?post=18375"}],"version-history":[{"count":8,"href":"https:\/\/aobosteel.com\/ko\/wp-json\/wp\/v2\/pages\/18375\/revisions"}],"predecessor-version":[{"id":23933,"href":"https:\/\/aobosteel.com\/ko\/wp-json\/wp\/v2\/pages\/18375\/revisions\/23933"}],"wp:attachment":[{"href":"https:\/\/aobosteel.com\/ko\/wp-json\/wp\/v2\/media?parent=18375"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}