{"id":14671,"date":"2026-04-10T16:19:50","date_gmt":"2026-04-10T08:19:50","guid":{"rendered":"https:\/\/aobosteel.com\/?page_id=14671"},"modified":"2026-10-16T12:53:11","modified_gmt":"2026-10-16T04:53:11","slug":"h11-tool-steel-properties","status":"publish","type":"page","link":"https:\/\/aobosteel.com\/ko\/h11-tool-steel-properties\/","title":{"rendered":"H11 \uacf5\uad6c\uac15\uc758 \uace0\uc628 \uac00\uacf5 \uc6a9\ub3c4\uc5d0 \ub300\ud55c \ud2b9\uc131 \ubc0f \uc131\ub2a5 \uac00\uc774\ub4dc"},"content":{"rendered":"<h1 class=\"wp-block-heading\">H11 \uacf5\uad6c\uac15\uc758 \ud2b9\uc131 \ubc0f \uc131\ub2a5 \uac00\uc774\ub4dc<\/h1>\n\n\n\n<p class=\"wp-block-paragraph\">H11 \uacf5\uad6c\uac15\uc744 \uc120\ud0dd\ud558\ub294 \uac83\uc740 \ub2e8\uc21c\ud788 \ud2b9\uc131 \ubaa9\ub85d\uc744 \ub098\uc5f4\ud558\ub294 \uac83\uc774 \uc544\ub2d9\ub2c8\ub2e4. \ud2b9\uc815 \uc6a9\ub3c4\uc5d0\uc11c \uace0\uc7a5 \ubc1c\uc0dd\uc744 \uc88c\uc6b0\ud558\ub294 \uc131\ub2a5 \uc694\uc18c\ub97c \ud30c\uc545\ud558\ub294 \uac83\uc774 \uc911\uc694\ud569\ub2c8\ub2e4.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">\uad6c\ub9e4 \ub2f4\ub2f9\uc790\uc640 \uc720\ud1b5\uc5c5\uccb4\uc5d0\uac8c \uc788\uc5b4 \ud575\uc2ec\uc801\uc778 \uacb0\uc815 \uc0ac\ud56d\uc740 \ud574\ub2f9 \uc790\uc7ac\uac00 \uc0dd\uc0b0 \uacfc\uc815\uc5d0\uc11c \ubc1c\uc0dd\ud558\ub294 \uc8fc\uc694 \uace0\uc7a5 \uba54\ucee4\ub2c8\uc998(\uc608: \uade0\uc5f4, \ubcc0\ud615 \ub610\ub294 \ud45c\uba74 \uc5f4\ud654)\uc744 \uacac\ub51c \uc218 \uc788\ub294\uc9c0 \uc5ec\ubd80\uc785\ub2c8\ub2e4.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">\uacf5\uae09 \uc635\uc158\uc744 \uac80\ud1a0 \uc911\uc778 \uad6c\ub9e4\uc790\ub294 \ub2f9\uc0ac \uc790\ub8cc\ub97c \ucc38\uc870\ud558\uc2ed\uc2dc\uc624. <a href=\"https:\/\/aobosteel.com\/ko\/h11-tool-steel\/\">H11 \uacf5\uad6c\uac15 \uc81c\ud488 \ud398\uc774\uc9c0<\/a> \uc0ac\uc6a9 \uac00\ub2a5\ud55c \ud06c\uae30, \ubc30\uc1a1 \uc870\uac74 \ubc0f \ub300\ub7c9 \uc8fc\ubb38 \uc0ac\uc591\uc5d0 \ub300\ud574\uc11c\ub294 \ubb38\uc758\ud558\uc2ed\uc2dc\uc624.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">\uc7ac\ub8cc \ud2b9\uc131\uc774 \uc120\ud0dd\uc744 \uc88c\uc6b0\ud558\ub294 \uc774\uc720\ub294 \ubb34\uc5c7\uc77c\uae4c\uc694?<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">\uacf5\uad6c \uace0\uc7a5\uc740 \uc77c\ubc18\uc801\uc73c\ub85c \ud558\ub098\uc758 \uc8fc\uc694 \uba54\ucee4\ub2c8\uc998\uc5d0 \uc758\ud574 \ubc1c\uc0dd\ud569\ub2c8\ub2e4.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">\uc5f4\uac04 \ub2e8\uc870\uc5d0\uc11c \ud30c\uc190\uc740 \uc885\uc885 \ucda9\uaca9\uc73c\ub85c \uc778\ud55c \uade0\uc5f4 \ub54c\ubb38\uc5d0 \ubc1c\uc0dd\ud569\ub2c8\ub2e4.<br>\ub2e4\uc774\uce90\uc2a4\ud305 \uacf5\uc815\uc5d0\uc11c \ubc18\ubcf5\uc801\uc778 \uac00\uc5f4 \ubc0f \ub0c9\uac01\uc740 \uc5f4 \ud53c\ub85c\uc640 \ud45c\uba74 \uade0\uc5f4\uc744 \uc720\ubc1c\ud569\ub2c8\ub2e4.<br>\uc555\ucd9c \uacf5\uc815\uc5d0\uc11c \uc9c0\uc18d\uc801\uc778 \uc5f4\uacfc \ub9c8\ucc30\uc740 \ud45c\uba74 \ub9c8\ubaa8\uc640 \ubcc0\ud615\uc744 \uac00\uc18d\ud654\ud569\ub2c8\ub2e4.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">\uc7ac\ub8cc \uc120\ud0dd\uc740 \uc774\ub7ec\ud55c \ud604\uc2e4\uc744 \ubc18\uc601\ud574\uc57c \ud569\ub2c8\ub2e4. \uc8fc\uc694 \ud30c\uc190 \uba54\ucee4\ub2c8\uc998\uc5d0 \ube44\ud574 \uc7ac\ub8cc\uc758 \uac15\ub3c4\uac00 \ubd80\uc871\ud558\uba74 \uc870\uae30 \uade0\uc5f4, \ud615\uc0c1 \uc190\uc2e4 \ub610\ub294 \uae09\uaca9\ud55c \ub9c8\ubaa8\uac00 \ubc1c\uc0dd\ud569\ub2c8\ub2e4.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">H11 \uacf5\uad6c\uac15\uc758 \ud575\uc2ec \uc131\ub2a5 \ud504\ub85c\ud544<\/h2>\n\n\n\n<h3 class=\"wp-block-heading\">H11 \uc778\uc131<\/h3>\n\n\n\n<p class=\"wp-block-paragraph\">\uc778\uc131\uc740 \uacf5\uad6c\uac00 \uae30\uacc4\uc801 \ucda9\uaca9\uc5d0 \uc758\ud574 \uade0\uc5f4\uc5d0 \uc800\ud56d\ud558\ub294\uc9c0 \uc5ec\ubd80\ub97c \uacb0\uc815\ud569\ub2c8\ub2e4.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">\uc778\uc131\uc774 \ubd80\uc871\ud558\uba74 \ucda9\uaca9 \ud558\uc911 \ud558\uc5d0\uc11c \ucde8\uc131 \ud30c\uad34 \ub610\ub294 \ubaa8\uc11c\ub9ac \ud30c\uc190\uc73c\ub85c \ub098\ud0c0\ub0a9\ub2c8\ub2e4. H11\uc740 \uac11\uc791\uc2a4\ub7ec\uc6b4 \uade0\uc5f4\uc5d0 \ub300\ud55c \uc800\ud56d\uc131\uc774 \uc694\uad6c\ub418\ub294 \uace0\ud558\uc911 \uc801\uc6a9 \ubd84\uc57c\uc5d0 \uc0ac\uc6a9\ub429\ub2c8\ub2e4.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">\uc774 \uc18d\uc131\uc774 \uc5b4\ub5bb\uac8c \uc791\ub3d9\ud558\ub294\uc9c0 \uc790\uc138\ud788 \uc774\ud574\ud558\ub824\uba74 \ub2e4\uc74c\uc744 \ucc38\uc870\ud558\uc138\uc694. <a href=\"https:\/\/aobosteel.com\/ko\/tool-steels-for-cracking-resistance\/\">H11 \uacf5\uad6c\uac15\uc758 \uc778\uc131: \ucda9\uaca9 \uc2dc \uade0\uc5f4 \uc800\ud56d\uc131<\/a>.<\/p>\n\n\n\n<h3 class=\"wp-block-heading\">H11 \uace0\uc628 \uacbd\ub3c4<\/h3>\n\n\n\n<p class=\"wp-block-paragraph\">\uace0\uc628 \uacbd\ub3c4\ub294 \uacf5\uad6c\uac00 \uace0\uc628\uc5d0\uc11c\ub3c4 \ud558\uc911 \uc9c0\uc9c0\ub825\uc744 \uc720\uc9c0\ud558\ub294\uc9c0 \uc5ec\ubd80\ub97c \uacb0\uc815\ud569\ub2c8\ub2e4.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">\uc774\ub7ec\ud55c \ud2b9\uc131\uc774 \ubd88\ucda9\ubd84\ud558\uba74 \uc791\ub3d9 \uc911\uc5d0 \uc7ac\ub8cc\uac00 \uc5f0\ud654\ub418\uc5b4 \uc555\ub825 \ud558\uc5d0\uc11c \uc18c\uc131 \ubcc0\ud615 \ubc0f \ud615\uc0c1 \uc190\uc2e4\uc774 \ubc1c\uc0dd\ud569\ub2c8\ub2e4.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">\uc628\ub3c4\uc5d0 \ub530\ub978 \uc790\uc138\ud55c \ub3d9\uc791 \uc591\uc0c1\uc740 \ub2e4\uc74c\uc744 \ucc38\uc870\ud558\uc2ed\uc2dc\uc624. <a href=\"https:\/\/aobosteel.com\/ko\/tool-steel-hot-hardness-chart\/\">H11 \uacf5\uad6c\uac15\uc758 \uace0\uc628 \uacbd\ub3c4: \uace0\uc628\uc5d0\uc11c\uc758 \uac15\ub3c4 \uc720\uc9c0\uc728<\/a>.<\/p>\n\n\n\n<h3 class=\"wp-block-heading\">H11 \ub0b4\ub9c8\ubaa8\uc131<\/h3>\n\n\n\n<p class=\"wp-block-paragraph\">\ub0b4\ub9c8\ubaa8\uc131\uc740 \uacf5\uad6c \ud45c\uba74\uc774 \ub9c8\ucc30 \ubc0f \uae08\uc18d \ud750\ub984 \ud558\uc5d0\uc11c \uce58\uc218\ub97c \uc5bc\ub9c8\ub098 \uc624\ub7ab\ub3d9\uc548 \uc720\uc9c0\ud558\ub294\uc9c0\ub97c \uacb0\uc815\ud569\ub2c8\ub2e4.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">\ub0b4\ub9c8\ubaa8\uc131\uc774 \ubd80\uc871\ud558\uba74 \ud45c\uba74 \uc7ac\ub8cc\uac00 \uc810\ucc28 \uc81c\uac70\ub418\uc5b4 \uce58\uc218 \uc190\uc2e4\uacfc \uc720\uc9c0 \ubcf4\uc218 \ube48\ub3c4 \uc99d\uac00\ub85c \uc774\uc5b4\uc9d1\ub2c8\ub2e4.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">\uc751\uc6a9 \ud504\ub85c\uadf8\ub7a8 \uc218\uc900 \ubd84\uc11d\uc740 \ub2e4\uc74c\uc744 \ucc38\uc870\ud558\uc2ed\uc2dc\uc624. <a href=\"https:\/\/aobosteel.com\/ko\/abrasive-wear-resistant-tool-steels\/\">H11 \uacf5\uad6c\uac15\uc758 \ub0b4\ub9c8\ubaa8\uc131: \uace0\uc628 \uac00\uacf5 \uc2dc \ud45c\uba74 \uc5f4\ud654 \uc81c\uc5b4<\/a>.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">H11 \uc5f4\ud53c\ub85c \uc800\ud56d<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">\uc5f4\ud53c\ub85c \uc800\ud56d\uc131\uc740 \uacf5\uad6c\uac00 \ubc18\ubcf5\uc801\uc778 \uac00\uc5f4 \ubc0f \ub0c9\uac01 \uc8fc\uae30\uc5d0 \uc5b4\ub5bb\uac8c \ubc18\uc751\ud558\ub294\uc9c0\ub97c \ub098\ud0c0\ub0c5\ub2c8\ub2e4.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">\uc774\ub7ec\ud55c \ud2b9\uc131\uc774 \ubd88\ucda9\ubd84\ud560 \uacbd\uc6b0, \ud45c\uba74 \uade0\uc5f4\uc774 \ubc1c\uc0dd\ud558\uc5ec \ub9e4 \uc8fc\uae30\ub9c8\ub2e4 \ucee4\uc9c0\uace0, \uacb0\uad6d \ub354 \uae4a\uc740 \uad6c\uc870\uc801 \ud30c\uc190\uc73c\ub85c \uc774\uc5b4\uc9d1\ub2c8\ub2e4.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">\ub354 \uc790\uc138\ud55c \ubd84\uc11d\uc740 \ub2e4\uc74c\uc744 \ucc38\uc870\ud558\uc138\uc694. <a href=\"https:\/\/aobosteel.com\/ko\/thermal-fatigue-resistant-tool-steels\/\">H11 \uacf5\uad6c\uac15\uc758 \uc5f4\ud53c\ub85c \uc800\ud56d\uc131: \uc5f4 \uade0\uc5f4 \ud30c\uc190 \ubc29\uc9c0<\/a>.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">H11 \uce58\uc218 \uc548\uc815\uc131<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">\uce58\uc218 \uc548\uc815\uc131\uc740 \uacf5\uad6c\uac00 \uc5f4\ucc98\ub9ac \uacfc\uc815\uc5d0\uc11c \uc6d0\ub798\uc758 \ud615\uc0c1\uc744 \uc720\uc9c0\ud558\ub294\uc9c0 \uc5ec\ubd80\uc5d0 \uc601\ud5a5\uc744 \ubbf8\uce69\ub2c8\ub2e4.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">\uc548\uc815\uc131\uc774 \ub5a8\uc5b4\uc9c0\uba74 \uacbd\ud654 \ud6c4 \ubcc0\ud615\uc774\ub098 \ud06c\uae30 \ubcc0\ud654\uac00 \ubc1c\uc0dd\ud558\uc5ec \uac00\uacf5 \uc5ec\uc720\uac00 \ub298\uc5b4\ub098\uace0 \uc7ac\uc791\uc5c5 \ud544\uc694\ub7c9\uc774 \uc99d\uac00\ud569\ub2c8\ub2e4.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">\ucc98\ub9ac \uad00\ub828 \uc0ac\ud56d\uc740 \ub2e4\uc74c\uc744 \ucc38\uc870\ud558\uc138\uc694. <a href=\"https:\/\/aobosteel.com\/ko\/tool-steel-size-change-in-heat-treatment\/\">H11 \uacf5\uad6c\uac15\uc758 \uce58\uc218 \uc548\uc815\uc131: \uc5f4\ucc98\ub9ac \ud6c4 \ubcc0\ud615 \uc81c\uc5b4<\/a>.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">\uc560\ud50c\ub9ac\ucf00\uc774\uc158\uc5d0 \uc801\ud569\ud55c \uc18d\uc131\uc758 \uc6b0\uc120\uc21c\uc704\ub97c \uc815\ud558\ub294 \ubc29\ubc95<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">\uc7ac\ub8cc \uc120\ud0dd\uc740 \uc0dd\uc0b0 \uacfc\uc815\uc5d0\uc11c \ud5c8\uc6a9\ub418\uc9c0 \uc54a\ub294 \uace0\uc7a5 \uba54\ucee4\ub2c8\uc998\uc744 \uae30\uc900\uc73c\ub85c \ud574\uc57c \ud569\ub2c8\ub2e4.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">\ud30c\uc190\uc774 \ucda9\uaca9\uc73c\ub85c \uc778\ud574 \ubc1c\uc0dd\ud55c\ub2e4\uba74, \ub0b4\uad6c\uc131\uc774 \uac00\uc7a5 \uc911\uc694\ud55c \uc694\uac74\uc774 \ub429\ub2c8\ub2e4.<br>\uace0\uc7a5\uc758 \uc6d0\uc778\uc774 \ubc18\ubcf5\uc801\uc778 \uac00\uc5f4\uc5d0 \uc788\ub2e4\uba74 \uc5f4\ud53c\ub85c \uc800\ud56d\uc131\uc744 \uc6b0\uc120\uc801\uc73c\ub85c \uace0\ub824\ud574\uc57c \ud569\ub2c8\ub2e4.<br>\uc628\ub3c4 \ubcc0\ud654\uc5d0 \ub530\ub978 \ubcc0\ud615\uc774 \uacf5\uad6c \uc218\uba85\uc744 \uc81c\ud55c\ud558\ub294 \uacbd\uc6b0, \uace0\uc628 \uacbd\ub3c4\uac00 \ub9e4\uc6b0 \uc911\uc694\ud574\uc9d1\ub2c8\ub2e4.<br>\ud45c\uba74 \uc5f4\ud654\uac00 \uc131\ub2a5\uc744 \uc88c\uc6b0\ud558\ub294 \uc694\uc778\uc774\ub77c\uba74 \ub0b4\ub9c8\ubaa8\uc131\uc744 \ucd5c\uc6b0\uc120\uc73c\ub85c \uace0\ub824\ud574\uc57c \ud569\ub2c8\ub2e4.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">\uc9c0\uc18d\uc801\uc73c\ub85c \uace0\uc628\uc774 \uc720\uc9c0\ub418\ub294 \ud658\uacbd\uc5d0\uc11c\ub294 \uc778\uc131\uc740 \ub2e4\uc18c \ub5a8\uc5b4\uc9c0\ub354\ub77c\ub3c4 \uace0\uc628 \uc548\uc815\uc131\uc774 \ub6f0\uc5b4\ub09c \ub2e4\ub978 \uc5f4\uac04 \uac00\uacf5\uc6a9 \uac15\uc7ac\uac00 \ub354 \uc801\ud569\ud560 \uc218 \uc788\uc2b5\ub2c8\ub2e4.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">\uc62c\ubc14\ub978 \uacb0\uc815\uc740 \uc18d\uc131\uc744 \ube44\uad50\ud558\ub294 \ub370 \uae30\ubc18\ud558\ub294 \uac83\uc774 \uc544\ub2c8\ub77c, \uc5b4\ub5a4 \uc2e4\ud328 \uc704\ud5d8\uc744 \ud1b5\uc81c\ud574\uc57c \ud558\ub294\uc9c0\ub97c \ud30c\uc545\ud558\ub294 \ub370 \uae30\ubc18\ud569\ub2c8\ub2e4.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">\uacb0\ub860<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">H11\uc740 \uadf8 \ud2b9\uc131\uc774 \uc801\uc6a9 \ubd84\uc57c\uc758 \uc8fc\ub41c \ud30c\uc190 \uba54\ucee4\ub2c8\uc998\uacfc \uc77c\uce58\ud560 \ub54c \ud6a8\uacfc\uc801\uc785\ub2c8\ub2e4.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">\uacf5\uad6c\uac00 \uace0\uc7a5\ub098\ub294 \ubc29\uc2dd\uacfc \uc774\uc720\uc5d0 \uc9d1\uc911\ud568\uc73c\ub85c\uc368 \uad6c\ub9e4\uc790\ub294 \uc77c\ubc18\uc801\uc778 \ub4f1\uae09 \uc124\uba85\uc5d0 \uc758\uc874\ud558\ub294 \ub300\uc2e0 \uade0\uc5f4, \ubcc0\ud615 \ubc0f \ub9c8\ubaa8\ub97c \uc904\uc774\ub294 \uc7ac\ub8cc\ub97c \uc120\ud0dd\ud560 \uc218 \uc788\uc2b5\ub2c8\ub2e4.<\/p>","protected":false},"excerpt":{"rendered":"<p>H11 Tool Steel Properties &amp; Performance Guide Selecting H11 tool steel is not about listing properties. It is about identifying which performance factor controls failure in a specific application. For procurement professionals and distributors, the key decision is whether the material can withstand the dominant failure mechanism in production\u2014such as cracking, deformation, or surface degradation. [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":0,"parent":0,"menu_order":0,"comment_status":"closed","ping_status":"closed","template":"","meta":{"_uag_custom_page_level_css":"","site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"normal-width-container","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"disabled","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","ast-disable-related-posts":"","theme-transparent-header-meta":"","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"set","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"footnotes":""},"class_list":["post-14671","page","type-page","status-publish","hentry"],"yoast_head":"<!-- This site is optimized with the Yoast SEO Premium plugin v28.8 (Yoast SEO v28.8) - https:\/\/yoast.com\/product\/yoast-seo-premium-wordpress\/ -->\n<title>H11 Tool Steel Properties &amp; Performance Guide for Hot Work Applications<\/title>\n<meta name=\"description\" content=\"Understand H11 tool steel properties including toughness, hot hardness, wear resistance, thermal fatigue, and dimensional stability. Learn how to match performance to failure risks in hot work applications.\" \/>\n<meta name=\"robots\" content=\"index, follow, max-snippet:-1, max-image-preview:large, max-video-preview:-1\" \/>\n<link rel=\"canonical\" href=\"https:\/\/aobosteel.com\/ko\/h11-tool-steel-properties\/\" \/>\n<meta property=\"og:locale\" content=\"ko_KR\" \/>\n<meta property=\"og:type\" content=\"article\" \/>\n<meta property=\"og:title\" content=\"H11 Tool Steel Properties &amp; Performance Guide for Hot Work Applications\" \/>\n<meta property=\"og:description\" content=\"Understand H11 tool steel properties including toughness, hot hardness, wear resistance, thermal fatigue, and dimensional stability. Learn how to match performance to failure risks in hot work applications.\" \/>\n<meta property=\"og:url\" content=\"https:\/\/aobosteel.com\/ko\/h11-tool-steel-properties\/\" \/>\n<meta property=\"og:site_name\" content=\"AoboSteel\" \/>\n<meta property=\"article:publisher\" content=\"https:\/\/www.facebook.com\/profile.php?id=61565368220197\" \/>\n<meta property=\"article:modified_time\" content=\"2026-10-16T04:53:11+00:00\" \/>\n<meta name=\"twitter:card\" content=\"summary_large_image\" \/>\n<meta name=\"twitter:label1\" content=\"\uc608\uc0c1 \ub418\ub294 \ud310\ub3c5 \uc2dc\uac04\" \/>\n\t<meta name=\"twitter:data1\" content=\"3\ubd84\" \/>\n<script type=\"application\/ld+json\" class=\"yoast-schema-graph\">{\"@context\":\"https:\\\/\\\/schema.org\",\"@graph\":[{\"@type\":\"TechArticle\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/h11-tool-steel-properties\\\/#article\",\"isPartOf\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/h11-tool-steel-properties\\\/\"},\"author\":{\"name\":\"Evan\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#\\\/schema\\\/person\\\/96118415c30ca6bb52eaf1127b052ef7\"},\"headline\":\"H11 Tool Steel Properties &amp; Performance Guide for Hot Work Applications\",\"datePublished\":\"2026-04-10T08:19:50+00:00\",\"dateModified\":\"2026-10-16T04:53:11+00:00\",\"mainEntityOfPage\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/h11-tool-steel-properties\\\/\"},\"wordCount\":584,\"publisher\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#organization\"},\"inLanguage\":\"ko-KR\"},{\"@type\":\"WebPage\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/h11-tool-steel-properties\\\/\",\"url\":\"https:\\\/\\\/aobosteel.com\\\/h11-tool-steel-properties\\\/\",\"name\":\"H11 Tool Steel Properties &amp; Performance Guide for Hot Work Applications\",\"isPartOf\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#website\"},\"datePublished\":\"2026-04-10T08:19:50+00:00\",\"dateModified\":\"2026-10-16T04:53:11+00:00\",\"description\":\"Understand H11 tool steel properties including toughness, hot hardness, wear resistance, thermal fatigue, and dimensional stability. Learn how to match performance to failure risks in hot work applications.\",\"breadcrumb\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/h11-tool-steel-properties\\\/#breadcrumb\"},\"inLanguage\":\"ko-KR\",\"potentialAction\":[{\"@type\":\"ReadAction\",\"target\":[\"https:\\\/\\\/aobosteel.com\\\/h11-tool-steel-properties\\\/\"]}]},{\"@type\":\"BreadcrumbList\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/h11-tool-steel-properties\\\/#breadcrumb\",\"itemListElement\":[{\"@type\":\"ListItem\",\"position\":1,\"name\":\"\u9996\u9875\",\"item\":\"https:\\\/\\\/aobosteel.com\\\/\"},{\"@type\":\"ListItem\",\"position\":2,\"name\":\"H11 Tool Steel Properties &amp; Performance Guide for Hot Work Applications\"}]},{\"@type\":\"WebSite\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#website\",\"url\":\"https:\\\/\\\/aobosteel.com\\\/\",\"name\":\"AoboSteel\",\"description\":\"\",\"publisher\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#organization\"},\"potentialAction\":[{\"@type\":\"SearchAction\",\"target\":{\"@type\":\"EntryPoint\",\"urlTemplate\":\"https:\\\/\\\/aobosteel.com\\\/?s={search_term_string}\"},\"query-input\":{\"@type\":\"PropertyValueSpecification\",\"valueRequired\":true,\"valueName\":\"search_term_string\"}}],\"inLanguage\":\"ko-KR\"},{\"@type\":\"Organization\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#organization\",\"name\":\"AoboSteel\",\"url\":\"https:\\\/\\\/aobosteel.com\\\/\",\"logo\":{\"@type\":\"ImageObject\",\"inLanguage\":\"ko-KR\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#\\\/schema\\\/logo\\\/image\\\/\",\"url\":\"https:\\\/\\\/aobosteel.com\\\/wp-content\\\/uploads\\\/2025\\\/01\\\/cropped-aobo-steel-1.avif\",\"contentUrl\":\"https:\\\/\\\/aobosteel.com\\\/wp-content\\\/uploads\\\/2025\\\/01\\\/cropped-aobo-steel-1.avif\",\"width\":1052,\"height\":592,\"caption\":\"AoboSteel\"},\"image\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#\\\/schema\\\/logo\\\/image\\\/\"},\"sameAs\":[\"https:\\\/\\\/www.facebook.com\\\/profile.php?id=61565368220197\",\"https:\\\/\\\/www.linkedin.com\\\/in\\\/aobosteel-evan\\\/\"]},{\"@type\":\"Person\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#\\\/schema\\\/person\\\/96118415c30ca6bb52eaf1127b052ef7\",\"name\":\"Evan\",\"image\":{\"@type\":\"ImageObject\",\"inLanguage\":\"ko-KR\",\"@id\":\"https:\\\/\\\/secure.gravatar.com\\\/avatar\\\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g\",\"url\":\"https:\\\/\\\/secure.gravatar.com\\\/avatar\\\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g\",\"contentUrl\":\"https:\\\/\\\/secure.gravatar.com\\\/avatar\\\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g\",\"caption\":\"Evan\"},\"sameAs\":[\"http:\\\/\\\/www.aobosteel.com\",\"https:\\\/\\\/www.facebook.com\\\/profile.php?id=61565368220197\",\"https:\\\/\\\/www.instagram.com\\\/aobosteel\\\/\",\"https:\\\/\\\/www.linkedin.com\\\/in\\\/aobosteel-evan\\\/\",\"https:\\\/\\\/x.com\\\/AobosteelEvan\",\"https:\\\/\\\/www.youtube.com\\\/@aobosteel\"],\"url\":\"https:\\\/\\\/aobosteel.com\\\/ko\\\/blog\\\/author\\\/admin\\\/\"}]}<\/script>\n<!-- \/ Yoast SEO Premium plugin. -->","yoast_head_json":{"title":"H11 \uacf5\uad6c\uac15\uc758 \uace0\uc628 \uac00\uacf5 \uc6a9\ub3c4\uc5d0 \ub300\ud55c \ud2b9\uc131 \ubc0f \uc131\ub2a5 \uac00\uc774\ub4dc","description":"H11 \uacf5\uad6c\uac15\uc758 \uc778\uc131, \uace0\uc628 \uacbd\ub3c4, \ub0b4\ub9c8\ubaa8\uc131, \uc5f4\ud53c\ub85c \ubc0f \uce58\uc218 \uc548\uc815\uc131\uc744 \ud3ec\ud568\ud55c \ud2b9\uc131\uc744 \uc774\ud574\ud558\uc2ed\uc2dc\uc624. \uace0\uc628 \uc791\uc5c5 \ud658\uacbd\uc5d0\uc11c \uc131\ub2a5\uacfc \uace0\uc7a5 \uc704\ud5d8\uc744 \uc77c\uce58\uc2dc\ud0a4\ub294 \ubc29\ubc95\uc744 \ubc30\uc6b0\uc2ed\uc2dc\uc624.","robots":{"index":"index","follow":"follow","max-snippet":"max-snippet:-1","max-image-preview":"max-image-preview:large","max-video-preview":"max-video-preview:-1"},"canonical":"https:\/\/aobosteel.com\/ko\/h11-tool-steel-properties\/","og_locale":"ko_KR","og_type":"article","og_title":"H11 Tool Steel Properties &amp; Performance Guide for Hot Work Applications","og_description":"Understand H11 tool steel properties including toughness, hot hardness, wear resistance, thermal fatigue, and dimensional stability. Learn how to match performance to failure risks in hot work applications.","og_url":"https:\/\/aobosteel.com\/ko\/h11-tool-steel-properties\/","og_site_name":"AoboSteel","article_publisher":"https:\/\/www.facebook.com\/profile.php?id=61565368220197","article_modified_time":"2026-10-16T04:53:11+00:00","twitter_card":"summary_large_image","twitter_misc":{"\uc608\uc0c1 \ub418\ub294 \ud310\ub3c5 \uc2dc\uac04":"3\ubd84"},"schema":{"@context":"https:\/\/schema.org","@graph":[{"@type":"TechArticle","@id":"https:\/\/aobosteel.com\/h11-tool-steel-properties\/#article","isPartOf":{"@id":"https:\/\/aobosteel.com\/h11-tool-steel-properties\/"},"author":{"name":"Evan","@id":"https:\/\/aobosteel.com\/#\/schema\/person\/96118415c30ca6bb52eaf1127b052ef7"},"headline":"H11 Tool Steel Properties &amp; Performance Guide for Hot Work Applications","datePublished":"2026-04-10T08:19:50+00:00","dateModified":"2026-10-16T04:53:11+00:00","mainEntityOfPage":{"@id":"https:\/\/aobosteel.com\/h11-tool-steel-properties\/"},"wordCount":584,"publisher":{"@id":"https:\/\/aobosteel.com\/#organization"},"inLanguage":"ko-KR"},{"@type":"WebPage","@id":"https:\/\/aobosteel.com\/h11-tool-steel-properties\/","url":"https:\/\/aobosteel.com\/h11-tool-steel-properties\/","name":"H11 \uacf5\uad6c\uac15\uc758 \uace0\uc628 \uac00\uacf5 \uc6a9\ub3c4\uc5d0 \ub300\ud55c \ud2b9\uc131 \ubc0f \uc131\ub2a5 \uac00\uc774\ub4dc","isPartOf":{"@id":"https:\/\/aobosteel.com\/#website"},"datePublished":"2026-04-10T08:19:50+00:00","dateModified":"2026-10-16T04:53:11+00:00","description":"H11 \uacf5\uad6c\uac15\uc758 \uc778\uc131, \uace0\uc628 \uacbd\ub3c4, \ub0b4\ub9c8\ubaa8\uc131, \uc5f4\ud53c\ub85c \ubc0f \uce58\uc218 \uc548\uc815\uc131\uc744 \ud3ec\ud568\ud55c \ud2b9\uc131\uc744 \uc774\ud574\ud558\uc2ed\uc2dc\uc624. \uace0\uc628 \uc791\uc5c5 \ud658\uacbd\uc5d0\uc11c \uc131\ub2a5\uacfc \uace0\uc7a5 \uc704\ud5d8\uc744 \uc77c\uce58\uc2dc\ud0a4\ub294 \ubc29\ubc95\uc744 \ubc30\uc6b0\uc2ed\uc2dc\uc624.","breadcrumb":{"@id":"https:\/\/aobosteel.com\/h11-tool-steel-properties\/#breadcrumb"},"inLanguage":"ko-KR","potentialAction":[{"@type":"ReadAction","target":["https:\/\/aobosteel.com\/h11-tool-steel-properties\/"]}]},{"@type":"BreadcrumbList","@id":"https:\/\/aobosteel.com\/h11-tool-steel-properties\/#breadcrumb","itemListElement":[{"@type":"ListItem","position":1,"name":"\u9996\u9875","item":"https:\/\/aobosteel.com\/"},{"@type":"ListItem","position":2,"name":"H11 Tool Steel Properties &amp; Performance Guide for Hot Work Applications"}]},{"@type":"WebSite","@id":"https:\/\/aobosteel.com\/#website","url":"https:\/\/aobosteel.com\/","name":"\uc544\uc624\ubcf4\uc2a4\ud2f8","description":"","publisher":{"@id":"https:\/\/aobosteel.com\/#organization"},"potentialAction":[{"@type":"SearchAction","target":{"@type":"EntryPoint","urlTemplate":"https:\/\/aobosteel.com\/?s={search_term_string}"},"query-input":{"@type":"PropertyValueSpecification","valueRequired":true,"valueName":"search_term_string"}}],"inLanguage":"ko-KR"},{"@type":"Organization","@id":"https:\/\/aobosteel.com\/#organization","name":"\uc544\uc624\ubcf4\uc2a4\ud2f8","url":"https:\/\/aobosteel.com\/","logo":{"@type":"ImageObject","inLanguage":"ko-KR","@id":"https:\/\/aobosteel.com\/#\/schema\/logo\/image\/","url":"https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/01\/cropped-aobo-steel-1.avif","contentUrl":"https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/01\/cropped-aobo-steel-1.avif","width":1052,"height":592,"caption":"AoboSteel"},"image":{"@id":"https:\/\/aobosteel.com\/#\/schema\/logo\/image\/"},"sameAs":["https:\/\/www.facebook.com\/profile.php?id=61565368220197","https:\/\/www.linkedin.com\/in\/aobosteel-evan\/"]},{"@type":"Person","@id":"https:\/\/aobosteel.com\/#\/schema\/person\/96118415c30ca6bb52eaf1127b052ef7","name":"\uc5d0\ubc18","image":{"@type":"ImageObject","inLanguage":"ko-KR","@id":"https:\/\/secure.gravatar.com\/avatar\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g","url":"https:\/\/secure.gravatar.com\/avatar\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g","contentUrl":"https:\/\/secure.gravatar.com\/avatar\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g","caption":"Evan"},"sameAs":["http:\/\/www.aobosteel.com","https:\/\/www.facebook.com\/profile.php?id=61565368220197","https:\/\/www.instagram.com\/aobosteel\/","https:\/\/www.linkedin.com\/in\/aobosteel-evan\/","https:\/\/x.com\/AobosteelEvan","https:\/\/www.youtube.com\/@aobosteel"],"url":"https:\/\/aobosteel.com\/ko\/blog\/author\/admin\/"}]}},"uagb_featured_image_src":{"full":false,"thumbnail":false,"medium":false,"medium_large":false,"large":false,"1536x1536":false,"2048x2048":false,"trp-custom-language-flag":false},"uagb_author_info":{"display_name":"Evan","author_link":"https:\/\/aobosteel.com\/ko\/blog\/author\/admin\/"},"uagb_comment_info":0,"uagb_excerpt":"H11 Tool Steel Properties &amp; Performance Guide Selecting H11 tool steel is not about listing properties. It is about identifying which performance factor controls failure in a specific application. For procurement professionals and distributors, the key decision is whether the material can withstand the dominant failure mechanism in production\u2014such as cracking, deformation, or surface degradation.&hellip;","rttpg_featured_image_url":null,"rttpg_author":{"display_name":"Evan","author_link":"https:\/\/aobosteel.com\/ko\/blog\/author\/admin\/"},"rttpg_comment":0,"rttpg_category":null,"rttpg_excerpt":"H11 Tool Steel Properties &amp; Performance Guide Selecting H11 tool steel is not about listing properties. It is about identifying which performance factor controls failure in a specific application. For procurement professionals and distributors, the key decision is whether the material can withstand the dominant failure mechanism in production\u2014such as cracking, deformation, or surface degradation.&hellip;","_links":{"self":[{"href":"https:\/\/aobosteel.com\/ko\/wp-json\/wp\/v2\/pages\/14671","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/aobosteel.com\/ko\/wp-json\/wp\/v2\/pages"}],"about":[{"href":"https:\/\/aobosteel.com\/ko\/wp-json\/wp\/v2\/types\/page"}],"author":[{"embeddable":true,"href":"https:\/\/aobosteel.com\/ko\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/aobosteel.com\/ko\/wp-json\/wp\/v2\/comments?post=14671"}],"version-history":[{"count":4,"href":"https:\/\/aobosteel.com\/ko\/wp-json\/wp\/v2\/pages\/14671\/revisions"}],"predecessor-version":[{"id":23102,"href":"https:\/\/aobosteel.com\/ko\/wp-json\/wp\/v2\/pages\/14671\/revisions\/23102"}],"wp:attachment":[{"href":"https:\/\/aobosteel.com\/ko\/wp-json\/wp\/v2\/media?parent=14671"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}