{"id":11165,"date":"2025-12-06T09:43:43","date_gmt":"2025-12-06T01:43:43","guid":{"rendered":"https:\/\/aobosteel.com\/?page_id=11165"},"modified":"2026-10-14T14:08:32","modified_gmt":"2026-10-14T06:08:32","slug":"5crmnmo-tool-steel","status":"publish","type":"page","link":"https:\/\/aobosteel.com\/ko\/5crmnmo-tool-steel\/","title":{"rendered":"5CrMnMo \uc5f4\uac04 \uac00\uacf5 \uacf5\uad6c\uac15 \uacf5\uae09\uc5c5\uccb4"},"content":{"rendered":"<style id=\"aobo-steel-rebuild\" data-noptimize=\"1\">\n\/* Rebuilt tool-steel page: banner is full-bleed, the body keeps the site's normal\n   content width. All layout rules live in this page, so a missing external\n   stylesheet can no longer collapse the page. *\/\n.ads2 *, .ads2 *::before, .ads2 *::after { box-sizing: border-box; }\n.ads2 { font-size: 16px; line-height: 1.75; color: #2b2b2b; }\n.ads2-hero { position: relative; width: 100vw !important; max-width: 100vw !important;\n  margin-left: calc(50% - 50vw) !important; margin-right: 0 !important;\n  min-height: 430px; display: flex; align-items: center; overflow: hidden; background: #1d1d1d; }\n.ads2-hero-img { position: absolute; inset: 0; width: 100%; height: 100%; object-fit: cover; }\n.ads2-hero-ov { position: absolute; inset: 0; background: #4e4b40; opacity: .5; }\n.ads2-hero-scrim { position: absolute; inset: 0;\n  background: linear-gradient(90deg, rgba(0,0,0,.42) 0%, rgba(0,0,0,.32) 45%, rgba(0,0,0,.16) 78%, rgba(0,0,0,.04) 100%); }\n.ads2-hero-in { position: relative; width: 100%; max-width: 1200px; margin: 0 auto; padding: 56px 24px; color: #fff; }\n.ads2-crumb, .ads2-crumb a, .ads2-crumb h6, .ads2-crumb mark { color: #dfe6ef !important; font-size: 13px;\n  text-decoration: none; letter-spacing: .2px; }\n.ads2-crumb h6 { display: inline; font-weight: 400; margin: 0; }\n.ads2-crumb a:hover { color: #fff !important; text-decoration: underline; }\n.ads2-tag { margin: 10px 0 6px; color: #eef1f5 !important; font-size: 14px; text-shadow: 0 1px 6px rgba(0,0,0,.8); }\n.ads2-h1 { margin: 0 0 12px; font-size: 40px; line-height: 1.2; font-weight: 800; color: #fff !important;\n  letter-spacing: -.2px; max-width: 900px; text-shadow: 0 2px 14px rgba(0,0,0,.85), 0 0 4px rgba(0,0,0,.55); }\n.ads2-sub { margin: 0 0 20px; font-size: 17px; color: #fff !important; text-shadow: 0 1px 8px rgba(0,0,0,.9), 0 0 3px rgba(0,0,0,.6); }\n.ads2-checks { list-style: none; margin: 0 0 26px; padding: 0; display: flex; flex-wrap: wrap; gap: 8px 22px; }\n.ads2-checks li { position: relative; margin: 0; padding-left: 20px; font-size: 15px; color: #fff !important;\n  text-shadow: 0 1px 6px rgba(0,0,0,.85); }\n.ads2-checks li::before { content: \"\\2713\"; position: absolute; left: 0; top: 0; color: #4ade80; font-weight: 700; }\n.ads2-cta { margin: 24px 0 6px; text-align: center; }\n.ads2-hero .ads2-cta { text-align: left; margin-top: 26px; }\n.ads2-btn { display: inline-block; background: #074fd0; color: #fff !important; font-weight: 400;\n  font-size: 16px; line-height: 16px; padding: 14px 30px; border-radius: 100px;\n  text-decoration: none !important; cursor: pointer; }\n.ads2-btn:hover { background: #063c9e; color: #fff !important; }\n.ads2-body { max-width: 1200px; margin: 0 auto; padding: 48px 24px 64px; }\n.ads2-sec { margin: 0 0 54px; }\n.ads2-sec:last-child { margin-bottom: 0; }\n.ads2 h2 { font-size: 27px; line-height: 1.3; color: #062a5a; font-weight: 700; margin: 0 0 20px;\n  padding-bottom: 12px; border-bottom: 1px solid #e6eaef; }\n.ads2 h3 { font-size: 21px; color: #062a5a; margin: 28px 0 12px; }\n.ads2 h4 { font-size: 18px; color: #062a5a; margin: 22px 0 10px; }\n.ads2 p { margin: 0 0 16px; }\n.ads2 a { color: #005fcf; text-decoration: none; }\n.ads2 a:hover { text-decoration: underline; }\n.ads2 ul, .ads2 ol { margin: 0 0 18px; padding-left: 22px; }\n.ads2 li { margin: 0 0 8px; }\n.ads2-cols2 { display: grid; grid-template-columns: 1fr 1fr; gap: 8px 40px; }\n.ads2-cols2 ul { margin-bottom: 0; }\n.ads2-row { display: grid; grid-template-columns: 1.05fr .95fr; gap: 36px; align-items: center; }\n.ads2-row-flip .ads2-col-i { order: -1; }\n.ads2-row .ads2-col-t > *:last-child { margin-bottom: 0; }\n.ads2-row .ads2-cta { margin-top: 16px; }\n.ads2-fig { margin: 0 0 22px; }\n.ads2-fig img { width: 100%; height: auto; display: block; }\n.ads2-gal { display: grid; grid-template-columns: repeat(3, 1fr); gap: 16px; margin: 0 0 22px; }\n.ads2-gal .ads2-fig { margin: 0; }\n.ads2-row .ads2-fig { margin: 0; }\n.ads2-tw { margin: 0 0 22px; overflow-x: auto; }\n.ads2-t { width: 100%; border-collapse: collapse; font-size: 15px; }\n.ads2-t td, .ads2-t th { border: 1px solid #e3e7ec; padding: 11px 14px; vertical-align: top; text-align: left; }\n.ads2-t.kv td:first-child { background: #f6f8fa; font-weight: 600; color: #062a5a; width: 34%; }\n.ads2-t.data { font-size: 14.5px; }\n.ads2-t.data td, .ads2-t.data th { padding: 9px 11px; }\n.ads2-t.data thead th, .ads2-t.data tr:first-child td { background: #eef3f9; font-weight: 700; color: #062a5a; }\n.ads2-t.data tbody tr:nth-child(odd) td { background: #fbfcfd; }\n@media (max-width: 1000px) {\n  .ads2-row { grid-template-columns: 1fr; gap: 22px; }\n  .ads2-row-flip .ads2-col-i { order: 0; }\n  .ads2-cols2 { grid-template-columns: 1fr; }\n  .ads2-h1 { font-size: 30px; }\n  .ads2-hero { min-height: 340px; }\n}\n@media (max-width: 700px) {\n  .ads2-gal { grid-template-columns: 1fr; }\n  .ads2-body { padding: 32px 18px 44px; }\n  .ads2-t { font-size: 14px; }\n  .ads2-t td, .ads2-t th { padding: 9px 10px; }\n  .ads2-t.kv td:first-child { width: 42%; }\n  .ads2-tw { -webkit-overflow-scrolling: touch; }\n}\n@media (max-width: 640px) {\n  .ads2-hero-in { padding: 34px 18px 38px; }\n  .ads2-h1 { font-size: 25px; }\n  .ads2 h2 { font-size: 22px; }\n  .ads2-tag { font-size: 13px; }\n  .ads2-sub { font-size: 15px; }\n  .ads2-checks { gap: 6px 16px; }\n  .ads2-checks li { font-size: 14px; }\n  .ads2-btn { padding: 12px 24px; font-size: 15px; }\n  .ads2-sec { margin-bottom: 40px; }\n}\n<\/style>\n<div class=\"ads2\">\n<section class=\"ads2-hero\">\n  <img class=\"ads2-hero-img\" src=\"https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/05\/banner3.webp\" sizes=\"100vw\" alt=\"Bulk tool steel bar stock in the Aobo Steel warehouse\" loading=\"eager\" decoding=\"async\">\n  <div class=\"ads2-hero-ov\"><\/div>\n  <div class=\"ads2-hero-scrim\"><\/div>\n  <div class=\"ads2-hero-in\">\n    <nav class=\"ads2-crumb\"><a href=\"https:\/\/aobosteel.com\/ko\/\">\uc9d1 <\/a>&gt; <a href=\"https:\/\/aobosteel.com\/ko\/tool-steel-heat-treatment-guide\/\"> \uacf5\uad6c\uac15 \uc5f4\ucc98\ub9ac \uae30\uc220\uc13c\ud130 <\/a> &gt; M2 Tool Steel Heat Treatment Guide<\/nav>\n    <p class=\"ads2-tag\"><em>\uc544\uc624\ubcf4 \uc2a4\ud2f8 | \uc911\uad6d\uc758 \uae00\ub85c\ubc8c \uacf5\uad6c\uac15 \uacf5\uae09\uc5c5\uccb4<\/em><\/p>\n    <h1 class=\"ads2-h1\">5CrMnMo \uc5f4\uac04 \uac00\uacf5 \uacf5\uad6c\uac15 \uacf5\uae09\uc5c5\uccb4<\/h1>\n    <div class=\"ads2-cta popmake-16052\"><a class=\"ads2-btn\" href=\"#\">\ube60\ub978 \ubb38\uc758\ub97c \uc694\uccad\ud558\uc138\uc694<\/a><\/div>\n  <\/div>\n<\/section>\n<div class=\"ads2-body\">\n<section class=\"ads2-sec\">\n<h2>1.\u00a0 5CrMnMo Steel\u00a0Overview and Chemical Composition<\/h2>\n<p>5CrMnMo \uc5f4\uac04 \uac00\uacf5 \uacf5\uad6c\uac15\uc740 \uc800\ud569\uae08 \uc5f4\uac04 \uac00\uacf5 \uae08\ud615\uac15\uc73c\ub85c \ubd84\ub958\ub429\ub2c8\ub2e4. \uc774 \uac15\uc885\uc758 \uc131\ub2a5 \ud2b9\uc131\uc740 \ud2b9\uc815\ud55c \ud654\ud559 \uc870\uc131\uc5d0\uc11c \ube44\ub86f\ub429\ub2c8\ub2e4.<\/p>\n<p>GB\/T1299-2000 \ud45c\uc900\uc5d0 \ub530\ub974\uba74 \uc77c\ubc18\uc801\uc778 \uc870\uc131(\uc911\ub7c9 \uae30\uc900 %)\uc740 \ub2e4\uc74c\uacfc \uac19\uc2b5\ub2c8\ub2e4.<\/p>\n<ul>\n<li><strong>\ud0c4\uc18c(C):<\/strong>\u00a00.50% \u2013 0.60%<\/li>\n\n\n\n<li><strong>\ub9dd\uac04(Mn):<\/strong>\u00a01.20% \u2013 1.60%<\/li>\n\n\n\n<li><strong>\ud06c\ub86c(Cr):<\/strong>\u00a00.60% \u2013 0.90%<\/li>\n\n\n\n<li><strong>\ub2c8\ucf08(Ni):<\/strong>\u00a01.40% \u2013 1.80%<\/li>\n\n\n\n<li><strong>\ubab0\ub9ac\ube0c\ub374(Mo):<\/strong>\u00a00.15% \u2013 0.30%<\/li>\n\n\n\n<li><strong>\uc2e4\ub9ac\ucf58(Si):<\/strong>\u00a0\u2264 0.40% (\uc77c\ubd80 \uc0ac\uc591\uc5d0\uc11c\ub294 0.25-0.60%\ub97c \ud5c8\uc6a9\ud569\ub2c8\ub2e4)<\/li>\n\n\n\n<li><strong>\uc778(P):<\/strong>\u00a0\u2264 0.030%<\/li>\n\n\n\n<li><strong>\ud669(S):<\/strong>\u00a0\u2264 0.030%<\/li>\n<\/ul>\n<p>\ud2b9\uc815 \ud45c\uc900\ud310\uc5d0 \ub530\ub77c \ubc94\uc704\uc5d0 \uc57d\uac04\uc758 \ucc28\uc774\uac00 \uc788\uc744 \uc218 \uc788\uc2b5\ub2c8\ub2e4.<\/p>\n<\/section>\n<section class=\"ads2-sec\">\n<h2>2. 5CrMnMo \uac15\ucca0\uc758 \uc751\uc6a9 \ubd84\uc57c<\/h2>\n<p>5CrMnMo \uc5f4\uac04 \uac00\uacf5 \uacf5\uad6c\uac15\uc740 \uc77c\ubc18\uc801\uc73c\ub85c \ubcc0\uc758 \uae38\uc774\uac00 \ucd5c\ub300 400mm\uc778 \uc911\uc18c\ud615 \uc5f4\uac04 \ub2e8\uc870 \uae08\ud615 \uc81c\uc791\uc5d0 \uc801\ud569\ud55c \uc2e4\uc6a9\uc801\uc778 \uc18c\uc7ac\uc785\ub2c8\ub2e4. \uc6b0\uc218\ud55c \uc778\uc131 \ub355\ubd84\uc5d0 \ub2e4\uc74c\uacfc \uac19\uc740 \uc6a9\ub3c4\uc5d0 \uc801\ud569\ud569\ub2c8\ub2e4.<\/p>\n<ul>\n<li>\ubcf5\uc7a1\ud55c \ubaa8\uc591\uc758 \uae08\ud615.<\/li>\n\n\n\n<li>\ud574\uba38 \ub2e8\uc870 \uae08\ud615\uc740 \uc0c1\ub2f9\ud55c \ucda9\uaca9\uc744 \ubc1b\uc2b5\ub2c8\ub2e4.<\/li>\n\n\n\n<li>\uace0\uc628 \uac00\uacf5 \uae08\ud615\uc758 \uc791\ub3d9 \ubd80\ud488\uc740 \ub192\uc740 \ucda9\uaca9 \ud558\uc911\uc744 \ubc1b\uc2b5\ub2c8\ub2e4.<\/li>\n\n\n\n<li>\uc544\uc5f0, \uc54c\ub8e8\ubbf8\ub284 \ubc0f \ud569\uae08 \ub2e4\uc774\uce90\uc2a4\ud305 \uae08\ud615.<\/li>\n\n\n\n<li>\uc5f4\uc555\ucc29 \uae08\ud615 \ubc0f \uc77c\ubd80 \ud50c\ub77c\uc2a4\ud2f1 \uae08\ud615.<\/li>\n\n\n\n<li>\ud2b9\uc815 \uc804\ub2e8\/\ud380\uce6d \uacf5\uad6c \ubc0f \ub0c9\uac04 \ub2e8\uc870 \ub2e4\uc774\uc758 \uae30\ubcf8 \uc7ac\ub8cc(\ub354 \ud070 \ub2e8\uba74\uc758 \uacbd\uc6b0 T10A, 9SiCr, Cr12MoV\ub97c \ub300\uccb4\ud560 \uc218 \uc788\uc74c).<\/li>\n<\/ul>\n<\/section>\n<section class=\"ads2-sec\">\n<h2>3. \uae30\uacc4\uc801 \ud2b9\uc131 \ubc0f 5CrNiMo\uc640\uc758 \ube44\uad50<\/h2>\n<ul>\n<li><strong>\ud798:<\/strong>\u00a0\uc57d\uac04 \ub354 \ub192\uc74c\u00a0<a href=\"https:\/\/aobosteel.com\/ko\/5crnimo-tool-steel\/\">5CrNiMo \uac15\ucca0<\/a>.<\/li>\n\n\n\n<li><strong>\uc778\uc131 \ubc0f \uac00\uc18c\uc131:<\/strong>\u00a0\ub9dd\uac04\uc774 \ub2c8\ucf08\uc758 \uc77c\ubd80\ub97c \ub300\uccb4\ud558\uae30 \ub54c\ubb38\uc5d0 \uc0c1\uc628 \ubc0f \uace0\uc628 \ubaa8\ub450\uc5d0\uc11c 5CrNiMo\ubcf4\ub2e4 \ub0ae\uc740 \uc628\ub3c4\ub97c \ub098\ud0c0\ub0c5\ub2c8\ub2e4.<\/li>\n\n\n\n<li><strong>\uac15\ud654\uc131:<\/strong>\u00a05CrNiMo\ubcf4\ub2e4 \ub0ae\uc74c.<\/li>\n\n\n\n<li><strong>\uc5f4\ud53c\ub85c \uc800\ud56d\uc131:<\/strong>\u00a0\uace0\uc628 \uc791\ub3d9 \ud658\uacbd\uc5d0\uc11c 5CrNiMo\ubcf4\ub2e4 \uc131\ub2a5\uc774 \ub5a8\uc5b4\uc9c0\uba70, \uacfc\uc5f4\uc5d0 \ub300\ud55c \ubbfc\uac10\ub3c4\uac00 \ub354 \ub192\uc2b5\ub2c8\ub2e4.<\/li>\n<\/ul>\n<p>5CrMnMo \uc5f4\uac04 \uac00\uacf5 \uacf5\uad6c\uac15\uc740 \ubaa9\ud45c \uc6a9\ub3c4\uc5d0 \uc801\ud569\ud55c \uc6b0\uc218\ud55c \uac00\uc131\ube44\uc640 \uc131\ub2a5\uc744 \uc81c\uacf5\ud558\uc9c0\ub9cc, \ub354 \ud06c\uac70\ub098 \uae4c\ub2e4\ub85c\uc6b4 \uc5f4\uac04 \ub2e8\uc870 \uc791\uc5c5\uc5d0\ub294 5CrNiMo\uac00 \ub354 \uc801\ud569\ud55c \uc120\ud0dd\uc77c \uc218 \uc788\uc2b5\ub2c8\ub2e4. \uadf8\ub7ec\ub098 \ub9e4\uc6b0 \ud070 \ub2e8\uba74\uc758 \uae08\ud615 \uc81c\uc791\uc5d0\ub294 \uacbd\ud654\uc131\uc774 \ub6f0\uc5b4\ub09c 5Cr2NiMoVSi\uc640 \uac19\uc740 \ub2e4\ub978 \ub4f1\uae09\uc774 \uc885\uc885 \uc120\ud0dd\ub429\ub2c8\ub2e4.<\/p>\n<\/section>\n<section class=\"ads2-sec\">\n<h2>4. 5CrMnMo\uac15\uc758 \uc5f4\ucc98\ub9ac<\/h2>\n<p>5CrMnMo\uac15\uc5d0\uc11c \uc6d0\ud558\ub294 \uc131\ub2a5\uc744 \uc5bb\uc73c\ub824\uba74 \uc801\uc808\ud55c \uc5f4\ucc98\ub9ac\uac00 \ub9e4\uc6b0 \uc911\uc694\ud569\ub2c8\ub2e4. \uc544\uc624\ubcf4 \uc2a4\ud2f8\uc740 \uc774\ub7ec\ud55c \uac00\uacf5 \uc694\uac74\uc744 \ucda9\uc871\ud558\ub294 \uac15\uc7ac\ub97c \uacf5\uae09\ud558\ub294 \ub370 \uc788\uc5b4 \ud48d\ubd80\ud55c \uacbd\ud5d8\uc744 \ubcf4\uc720\ud558\uace0 \uc788\uc2b5\ub2c8\ub2e4.<\/p>\n<h3>4.1 \ub2e8\uc870<\/h3>\n<p>5CrNiMo\uc640 \uc720\uc0ac\ud55c \uacf5\uc815 \ub9e4\uac1c\ubcc0\uc218\ub97c \ub530\ub974\uc2ed\uc2dc\uc624. \uade0\uc5f4\uc744 \ubc29\uc9c0\ud558\uae30 \uc704\ud574 \uac00\uc5f4 \ubc0f \ub0c9\uac01\uc744 \uc138\uc2ec\ud558\uac8c \uc81c\uc5b4\ud574\uc57c \ud569\ub2c8\ub2e4. \ub2e8\uc870 \ud6c4 \uc11c\uc11c\ud788 \ub0c9\uac01(\ub300\ud615 \ub2e8\uc870\ud488\uc758 \uacbd\uc6b0 150~200\u00b0C\uae4c\uc9c0 \ub178\ub0c9)\ud558\ub294 \uac83\uc774 \ubc31\ubc18 \ubc1c\uc0dd\uc744 \ubc29\uc9c0\ud558\ub294 \ub370 \ud544\uc218\uc801\uc785\ub2c8\ub2e4.<\/p>\n<h3>4.2 \uc5b4\ub2d0\ub9c1<\/h3>\n<p>\ub4f1\uc628 \uc5b4\ub2d0\ub9c1\uc744 \uad8c\uc7a5\ud569\ub2c8\ub2e4.<\/p>\n<ol>\n<li>850~870\u00b0C\ub85c \uac00\uc5f4\ud558\uace0 4~6\uc2dc\uac04 \ub3d9\uc548 \uc720\uc9c0\ud569\ub2c8\ub2e4.<\/li>\n\n\n\n<li>680\u00b0C\uc758 \ub4f1\uc628 \uc628\ub3c4\ub85c \ub0c9\uac01\ud55c \ud6c4 4~6\uc2dc\uac04 \ub3d9\uc548 \uc720\uc9c0\ud569\ub2c8\ub2e4.<\/li>\n\n\n\n<li>500\u00b0C \uc774\ud558\ub85c \ub178\ub0c9\ud55c \ud6c4 \uacf5\ub7ad\ud569\ub2c8\ub2e4. \uc608\uc0c1 \uacbd\ub3c4: 197-241 HBW (\ud384\ub77c\uc774\ud2b8 + \ud398\ub77c\uc774\ud2b8 \uad6c\uc870).<\/li>\n<\/ol>\n<h3>4.3 \ub2f4\uae08\uc9c8<\/h3>\n<ol>\n<li>840~860\u00b0C\ub85c \uac00\uc5f4\ud558\uc2ed\uc2dc\uc624. \ub354 \ub192\uc740 \uc628\ub3c4(\uc57d 900\u00b0C)\uc5d0\uc11c\ub294 \ud310\uc0c1 \ub9c8\ub974\ud150\uc0ac\uc774\ud2b8\uac00 \uc99d\uac00\ud558\uc5ec \uc778\uc131\uc774 \ud5a5\uc0c1\ub420 \uc218 \uc788\uc2b5\ub2c8\ub2e4.<\/li>\n\n\n\n<li>\uc624\uc77c \ub2f4\uae08\uc9c8 \ud6c4 150~180\u00b0C\uae4c\uc9c0 \ub0c9\uac01\uc2dc\ud0a8 \ub2e4\uc74c \uc989\uc2dc \ud15c\ud37c\ub9c1\ud569\ub2c8\ub2e4.<\/li>\n\n\n\n<li>\ubcc0\ud615 \ubc0f \uade0\uc5f4\uc744 \ucd5c\uc18c\ud654\ud558\ub824\uba74 \uc624\uc77c \ud01c\uce6d \uc804\uc5d0 \uacf5\uae30 \uc911\uc5d0\uc11c 740~780\u00b0C(\uc9c4\ud55c \ubd89\uc740\uc0c9)\uae4c\uc9c0 \uc608\ub0c9\ud558\uac70\ub098, \ub300\ud615 \uae08\ud615\uc758 \uacbd\uc6b0 780~810\u00b0C\uae4c\uc9c0 \uc608\ub0c9\ud558\ub294 \uac83\uc744 \uace0\ub824\ud558\uc2ed\uc2dc\uc624. \ub4f1\uc628 \ud01c\uce6d \ub2e8\uacc4(\uc608: 150~200\u00b0C\uae4c\uc9c0 \uc624\uc77c \ud01c\uce6d \ud6c4 280\u00b0C\uc5d0\uc11c \ub4f1\uc628 \uc720\uc9c0) \ub610\ud55c \ub3c4\uc6c0\uc774 \ub420 \uc218 \uc788\uc2b5\ub2c8\ub2e4.<\/li>\n<\/ol>\n<h3>4.4 \ud15c\ud37c\ub9c1<\/h3>\n<p>\ud15c\ud37c\ub9c1\uc740 \ucd5c\uc885 \uacbd\ub3c4\uc640 \uc778\uc131\uc744 \uc870\uc808\ud569\ub2c8\ub2e4. \ub610\ud55c \uc751\ub825\uc744 \uc644\ud654\ud558\uace0 \uad6c\uc870\ub97c \uc548\uc815\ud654\ud569\ub2c8\ub2e4.<\/p>\n<ol>\n<li><strong>\uc77c\ubc18\uc801\uc778:<\/strong>\u00a0450~500\u00b0C\uc5d0\uc11c \ubcf4\ud1b5 \ub450 \ubc88 \uc218\ud589\ud569\ub2c8\ub2e4.<\/li>\n\n\n\n<li><strong>\ub2e8\uc870 \uae08\ud615 \ubcf8\uccb4:<\/strong>\n<ul>\n<li>\uc18c\ud615 \uae08\ud615: 490-510\u00b0C (\uacbd\ub3c4: 44-47 HRC)<\/li>\n\n\n\n<li>\ub300\ud615 \uae08\ud615: 560-580\u00b0C (\uacbd\ub3c4: 34-37 HRC)<\/li>\n<\/ul>\n<\/li>\n\n\n\n<li><strong>\ub2e4\uc774 \ud14c\ub10c(\uac15\ub3c4 \ud5a5\uc0c1\uc6a9):<\/strong>\n<ul>\n<li>\uc18c\ud615 \uae08\ud615: 620-640\u00b0C (\uacbd\ub3c4: 34-37 HRC)<\/li>\n\n\n\n<li>\uc911\ud615 \ub2e4\uc774: 640-660\u00b0C (\uacbd\ub3c4: 30-35 HRC)<\/li>\n<\/ul>\n<\/li>\n\n\n\n<li><strong>\uc2a4\ud2b8\ub808\uc2a4 \ud574\uc18c:<\/strong>\u00a0\uc5f4\ucc98\ub9ac \ud6c4 280\u00b0C\uc5d0\uc11c 2~3\uc2dc\uac04 \ub3d9\uc548 \ucd5c\uc885 \uc751\ub825 \uc644\ud654 \ucc98\ub9ac\ub97c \ud558\ub294 \uac83\uc774 \uc88b\uc2b5\ub2c8\ub2e4.<\/li>\n<\/ol>\n<\/section>\n<section class=\"ads2-sec\">\n<h2>5. \uc131\ub2a5 \ud5a5\uc0c1<\/h2>\n<p>5CrMnMo \ub2e4\uc774\uc758 \uc218\uba85\uc740 \ub2e4\uc74c\uacfc \uac19\uc740 \ubc29\ubc95\uc73c\ub85c \uc5f0\uc7a5\ud560 \uc218 \uc788\uc2b5\ub2c8\ub2e4.<\/p>\n<ul>\n<li><strong>\ucd5c\uc801\ud654\ub41c \uc5f4\ucc98\ub9ac:<\/strong>\u00a0\uace0\uc628 \ub2f4\uae08\uc9c8(\uc57d 900\u00b0C), \ub2f4\uae08\uc9c8 \uc804 \uc608\ub0c9, \ub4f1\uc628 \ub2f4\uae08\uc9c8 \ud6c4 \uc774\uc911 \ud15c\ud37c\ub9c1\uacfc \uac19\uc740 \uae30\uc220\uc740 \uc778\uc131\uc744 \ud5a5\uc0c1\uc2dc\ud0a4\uace0 \uade0\uc5f4 \uc804\ud30c\ub97c \uc904\uc77c \uc218 \uc788\uc2b5\ub2c8\ub2e4.<\/li>\n\n\n\n<li><strong>\ud45c\uba74 \ucc98\ub9ac:<\/strong>\u00a0\ud0c4\uc9c8\ud654 \ub610\ub294 \ud76c\ud1a0\ub958 \ub3d9\uc2dc \ud655\uc0b0\uacfc \uac19\uc740 \uacf5\uc815\uc740 \ud45c\uba74 \uacbd\ub3c4, \ub0b4\ub9c8\ubaa8\uc131 \ubc0f \uc5f4\ud53c\ub85c \uc800\ud56d\uc131\uc744 \ud06c\uac8c \ud5a5\uc0c1\uc2dc\ud0ac \uc218 \uc788\uc2b5\ub2c8\ub2e4.<\/li>\n\n\n\n<li><strong>\uc608\uc5f4:<\/strong>\u00a0\uc5f4 \ucda9\uaca9\uacfc \ud30c\uc190 \uc704\ud5d8\uc744 \ucd5c\uc18c\ud654\ud558\ub824\uba74 \uc0ac\uc6a9 \uc804\uc5d0 \ud56d\uc0c1 \uae08\ud615\uc744 200~250\u00b0C\ub85c \uc608\uc5f4\ud558\uc2ed\uc2dc\uc624.<\/li>\n<\/ul>\n<div class=\"ads2-cta popmake-16052\"><a class=\"ads2-btn\" href=\"#\">\uacac\uc801 \uc694\uccad\uc11c \uc591\uc2dd \uc5f4\uae30<\/a><\/div>\n<\/section>\n<\/div>\n<\/div>","protected":false},"excerpt":{"rendered":"<p>Home &gt; Tool Steel Heat Treatment Technical Center &gt; M2 Tool Steel Heat Treatment Guide Aobo Steel | Global Tool Steel Supplier in China 5CrMnMo Hot Work Tool Steel Supplier Request a Quick Inquiry 1.\u00a0 5CrMnMo Steel\u00a0Overview and Chemical Composition 5CrMnMo Hot Work Tool Steel is classified as a low-alloy hot work die steel. Its [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":6262,"parent":0,"menu_order":0,"comment_status":"closed","ping_status":"closed","template":"","meta":{"_uag_custom_page_level_css":"","site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"default","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"disabled","ast-breadcrumbs-content":"","ast-featured-img":"disabled","footer-sml-layout":"","ast-disable-related-posts":"","theme-transparent-header-meta":"","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"default","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"footnotes":""},"class_list":["post-11165","page","type-page","status-publish","has-post-thumbnail","hentry"],"yoast_head":"<!-- This site is optimized with the Yoast SEO Premium plugin v28.7 (Yoast SEO v28.7) - https:\/\/yoast.com\/product\/yoast-seo-premium-wordpress\/ -->\n<title>5CrMnMo Hot Work Tool Steel Supplier - AoboSteel<\/title>\n<meta name=\"robots\" content=\"index, follow, max-snippet:-1, max-image-preview:large, max-video-preview:-1\" \/>\n<link rel=\"canonical\" href=\"https:\/\/aobosteel.com\/ko\/5crmnmo-tool-steel\/\" \/>\n<meta property=\"og:locale\" content=\"ko_KR\" \/>\n<meta property=\"og:type\" content=\"article\" \/>\n<meta property=\"og:title\" content=\"5CrMnMo Hot Work Tool Steel Supplier\" \/>\n<meta property=\"og:description\" content=\"Home &gt; Tool Steel Heat Treatment Technical Center &gt; M2 Tool Steel Heat Treatment Guide Aobo Steel | Global Tool Steel Supplier in China 5CrMnMo Hot Work Tool Steel Supplier Request a Quick Inquiry 1.\u00a0 5CrMnMo Steel\u00a0Overview and Chemical Composition 5CrMnMo Hot Work Tool Steel is classified as a low-alloy hot work die steel. Its [&hellip;]\" \/>\n<meta property=\"og:url\" content=\"https:\/\/aobosteel.com\/ko\/5crmnmo-tool-steel\/\" \/>\n<meta property=\"og:site_name\" content=\"AoboSteel\" \/>\n<meta property=\"article:publisher\" content=\"https:\/\/www.facebook.com\/profile.php?id=61565368220197\" \/>\n<meta property=\"article:modified_time\" content=\"2026-10-14T06:08:32+00:00\" \/>\n<meta property=\"og:image\" content=\"https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/04\/5CrMnMo-Hot-Work-Tool-Steel.avif\" \/>\n\t<meta property=\"og:image:width\" content=\"500\" \/>\n\t<meta property=\"og:image:height\" content=\"500\" \/>\n\t<meta property=\"og:image:type\" content=\"image\/jpeg\" \/>\n<meta name=\"twitter:card\" content=\"summary_large_image\" \/>\n<meta name=\"twitter:label1\" content=\"\uc608\uc0c1 \ub418\ub294 \ud310\ub3c5 \uc2dc\uac04\" \/>\n\t<meta name=\"twitter:data1\" content=\"4\ubd84\" \/>\n<script type=\"application\/ld+json\" class=\"yoast-schema-graph\">{\"@context\":\"https:\\\/\\\/schema.org\",\"@graph\":[{\"@type\":\"TechArticle\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/5crmnmo-tool-steel\\\/#article\",\"isPartOf\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/5crmnmo-tool-steel\\\/\"},\"author\":{\"name\":\"Evan\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#\\\/schema\\\/person\\\/96118415c30ca6bb52eaf1127b052ef7\"},\"headline\":\"5CrMnMo Hot Work Tool Steel Supplier\",\"datePublished\":\"2025-12-06T01:43:43+00:00\",\"dateModified\":\"2026-10-14T06:08:32+00:00\",\"mainEntityOfPage\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/5crmnmo-tool-steel\\\/\"},\"wordCount\":634,\"publisher\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#organization\"},\"image\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/5crmnmo-tool-steel\\\/#primaryimage\"},\"thumbnailUrl\":\"https:\\\/\\\/aobosteel.com\\\/wp-content\\\/uploads\\\/2025\\\/04\\\/5CrMnMo-Hot-Work-Tool-Steel.avif\",\"inLanguage\":\"ko-KR\"},{\"@type\":\"WebPage\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/5crmnmo-tool-steel\\\/\",\"url\":\"https:\\\/\\\/aobosteel.com\\\/5crmnmo-tool-steel\\\/\",\"name\":\"5CrMnMo Hot Work Tool Steel Supplier - AoboSteel\",\"isPartOf\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#website\"},\"primaryImageOfPage\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/5crmnmo-tool-steel\\\/#primaryimage\"},\"image\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/5crmnmo-tool-steel\\\/#primaryimage\"},\"thumbnailUrl\":\"https:\\\/\\\/aobosteel.com\\\/wp-content\\\/uploads\\\/2025\\\/04\\\/5CrMnMo-Hot-Work-Tool-Steel.avif\",\"datePublished\":\"2025-12-06T01:43:43+00:00\",\"dateModified\":\"2026-10-14T06:08:32+00:00\",\"breadcrumb\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/5crmnmo-tool-steel\\\/#breadcrumb\"},\"inLanguage\":\"ko-KR\",\"potentialAction\":[{\"@type\":\"ReadAction\",\"target\":[\"https:\\\/\\\/aobosteel.com\\\/5crmnmo-tool-steel\\\/\"]}]},{\"@type\":\"ImageObject\",\"inLanguage\":\"ko-KR\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/5crmnmo-tool-steel\\\/#primaryimage\",\"url\":\"https:\\\/\\\/aobosteel.com\\\/wp-content\\\/uploads\\\/2025\\\/04\\\/5CrMnMo-Hot-Work-Tool-Steel.avif\",\"contentUrl\":\"https:\\\/\\\/aobosteel.com\\\/wp-content\\\/uploads\\\/2025\\\/04\\\/5CrMnMo-Hot-Work-Tool-Steel.avif\",\"width\":500,\"height\":500,\"caption\":\"5CrMnMo Tool Steel\"},{\"@type\":\"BreadcrumbList\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/5crmnmo-tool-steel\\\/#breadcrumb\",\"itemListElement\":[{\"@type\":\"ListItem\",\"position\":1,\"name\":\"\u9996\u9875\",\"item\":\"https:\\\/\\\/aobosteel.com\\\/\"},{\"@type\":\"ListItem\",\"position\":2,\"name\":\"5CrMnMo Hot Work Tool Steel Supplier\"}]},{\"@type\":\"WebSite\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#website\",\"url\":\"https:\\\/\\\/aobosteel.com\\\/\",\"name\":\"AoboSteel\",\"description\":\"\",\"publisher\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#organization\"},\"potentialAction\":[{\"@type\":\"SearchAction\",\"target\":{\"@type\":\"EntryPoint\",\"urlTemplate\":\"https:\\\/\\\/aobosteel.com\\\/?s={search_term_string}\"},\"query-input\":{\"@type\":\"PropertyValueSpecification\",\"valueRequired\":true,\"valueName\":\"search_term_string\"}}],\"inLanguage\":\"ko-KR\"},{\"@type\":\"Organization\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#organization\",\"name\":\"AoboSteel\",\"url\":\"https:\\\/\\\/aobosteel.com\\\/\",\"logo\":{\"@type\":\"ImageObject\",\"inLanguage\":\"ko-KR\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#\\\/schema\\\/logo\\\/image\\\/\",\"url\":\"https:\\\/\\\/aobosteel.com\\\/wp-content\\\/uploads\\\/2025\\\/01\\\/cropped-aobo-steel-1.avif\",\"contentUrl\":\"https:\\\/\\\/aobosteel.com\\\/wp-content\\\/uploads\\\/2025\\\/01\\\/cropped-aobo-steel-1.avif\",\"width\":1052,\"height\":592,\"caption\":\"AoboSteel\"},\"image\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#\\\/schema\\\/logo\\\/image\\\/\"},\"sameAs\":[\"https:\\\/\\\/www.facebook.com\\\/profile.php?id=61565368220197\",\"https:\\\/\\\/www.linkedin.com\\\/in\\\/aobosteel-evan\\\/\"]},{\"@type\":\"Person\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#\\\/schema\\\/person\\\/96118415c30ca6bb52eaf1127b052ef7\",\"name\":\"Evan\",\"image\":{\"@type\":\"ImageObject\",\"inLanguage\":\"ko-KR\",\"@id\":\"https:\\\/\\\/secure.gravatar.com\\\/avatar\\\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g\",\"url\":\"https:\\\/\\\/secure.gravatar.com\\\/avatar\\\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g\",\"contentUrl\":\"https:\\\/\\\/secure.gravatar.com\\\/avatar\\\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g\",\"caption\":\"Evan\"},\"sameAs\":[\"http:\\\/\\\/www.aobosteel.com\",\"https:\\\/\\\/www.facebook.com\\\/profile.php?id=61565368220197\",\"https:\\\/\\\/www.instagram.com\\\/aobosteel\\\/\",\"https:\\\/\\\/www.linkedin.com\\\/in\\\/aobosteel-evan\\\/\",\"https:\\\/\\\/x.com\\\/AobosteelEvan\",\"https:\\\/\\\/www.youtube.com\\\/@aobosteel\"],\"url\":\"https:\\\/\\\/aobosteel.com\\\/ko\\\/blog\\\/author\\\/admin\\\/\"}]}<\/script>\n<!-- \/ Yoast SEO Premium plugin. -->","yoast_head_json":{"title":"5CrMnMo \uc5f4\uac04 \uac00\uacf5 \uacf5\uad6c\uac15 \uacf5\uae09\uc5c5\uccb4 - AoboSteel","robots":{"index":"index","follow":"follow","max-snippet":"max-snippet:-1","max-image-preview":"max-image-preview:large","max-video-preview":"max-video-preview:-1"},"canonical":"https:\/\/aobosteel.com\/ko\/5crmnmo-tool-steel\/","og_locale":"ko_KR","og_type":"article","og_title":"5CrMnMo Hot Work Tool Steel Supplier","og_description":"Home &gt; Tool Steel Heat Treatment Technical Center &gt; M2 Tool Steel Heat Treatment Guide Aobo Steel | Global Tool Steel Supplier in China 5CrMnMo Hot Work Tool Steel Supplier Request a Quick Inquiry 1.\u00a0 5CrMnMo Steel\u00a0Overview and Chemical Composition 5CrMnMo Hot Work Tool Steel is classified as a low-alloy hot work die steel. Its [&hellip;]","og_url":"https:\/\/aobosteel.com\/ko\/5crmnmo-tool-steel\/","og_site_name":"AoboSteel","article_publisher":"https:\/\/www.facebook.com\/profile.php?id=61565368220197","article_modified_time":"2026-10-14T06:08:32+00:00","og_image":[{"width":500,"height":500,"url":"https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/04\/5CrMnMo-Hot-Work-Tool-Steel.avif","type":"image\/jpeg"}],"twitter_card":"summary_large_image","twitter_misc":{"\uc608\uc0c1 \ub418\ub294 \ud310\ub3c5 \uc2dc\uac04":"4\ubd84"},"schema":{"@context":"https:\/\/schema.org","@graph":[{"@type":"TechArticle","@id":"https:\/\/aobosteel.com\/5crmnmo-tool-steel\/#article","isPartOf":{"@id":"https:\/\/aobosteel.com\/5crmnmo-tool-steel\/"},"author":{"name":"Evan","@id":"https:\/\/aobosteel.com\/#\/schema\/person\/96118415c30ca6bb52eaf1127b052ef7"},"headline":"5CrMnMo Hot Work Tool Steel Supplier","datePublished":"2025-12-06T01:43:43+00:00","dateModified":"2026-10-14T06:08:32+00:00","mainEntityOfPage":{"@id":"https:\/\/aobosteel.com\/5crmnmo-tool-steel\/"},"wordCount":634,"publisher":{"@id":"https:\/\/aobosteel.com\/#organization"},"image":{"@id":"https:\/\/aobosteel.com\/5crmnmo-tool-steel\/#primaryimage"},"thumbnailUrl":"https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/04\/5CrMnMo-Hot-Work-Tool-Steel.avif","inLanguage":"ko-KR"},{"@type":"WebPage","@id":"https:\/\/aobosteel.com\/5crmnmo-tool-steel\/","url":"https:\/\/aobosteel.com\/5crmnmo-tool-steel\/","name":"5CrMnMo \uc5f4\uac04 \uac00\uacf5 \uacf5\uad6c\uac15 \uacf5\uae09\uc5c5\uccb4 - AoboSteel","isPartOf":{"@id":"https:\/\/aobosteel.com\/#website"},"primaryImageOfPage":{"@id":"https:\/\/aobosteel.com\/5crmnmo-tool-steel\/#primaryimage"},"image":{"@id":"https:\/\/aobosteel.com\/5crmnmo-tool-steel\/#primaryimage"},"thumbnailUrl":"https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/04\/5CrMnMo-Hot-Work-Tool-Steel.avif","datePublished":"2025-12-06T01:43:43+00:00","dateModified":"2026-10-14T06:08:32+00:00","breadcrumb":{"@id":"https:\/\/aobosteel.com\/5crmnmo-tool-steel\/#breadcrumb"},"inLanguage":"ko-KR","potentialAction":[{"@type":"ReadAction","target":["https:\/\/aobosteel.com\/5crmnmo-tool-steel\/"]}]},{"@type":"ImageObject","inLanguage":"ko-KR","@id":"https:\/\/aobosteel.com\/5crmnmo-tool-steel\/#primaryimage","url":"https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/04\/5CrMnMo-Hot-Work-Tool-Steel.avif","contentUrl":"https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/04\/5CrMnMo-Hot-Work-Tool-Steel.avif","width":500,"height":500,"caption":"5CrMnMo Tool Steel"},{"@type":"BreadcrumbList","@id":"https:\/\/aobosteel.com\/5crmnmo-tool-steel\/#breadcrumb","itemListElement":[{"@type":"ListItem","position":1,"name":"\u9996\u9875","item":"https:\/\/aobosteel.com\/"},{"@type":"ListItem","position":2,"name":"5CrMnMo Hot Work Tool Steel Supplier"}]},{"@type":"WebSite","@id":"https:\/\/aobosteel.com\/#website","url":"https:\/\/aobosteel.com\/","name":"\uc544\uc624\ubcf4\uc2a4\ud2f8","description":"","publisher":{"@id":"https:\/\/aobosteel.com\/#organization"},"potentialAction":[{"@type":"SearchAction","target":{"@type":"EntryPoint","urlTemplate":"https:\/\/aobosteel.com\/?s={search_term_string}"},"query-input":{"@type":"PropertyValueSpecification","valueRequired":true,"valueName":"search_term_string"}}],"inLanguage":"ko-KR"},{"@type":"Organization","@id":"https:\/\/aobosteel.com\/#organization","name":"\uc544\uc624\ubcf4\uc2a4\ud2f8","url":"https:\/\/aobosteel.com\/","logo":{"@type":"ImageObject","inLanguage":"ko-KR","@id":"https:\/\/aobosteel.com\/#\/schema\/logo\/image\/","url":"https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/01\/cropped-aobo-steel-1.avif","contentUrl":"https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/01\/cropped-aobo-steel-1.avif","width":1052,"height":592,"caption":"AoboSteel"},"image":{"@id":"https:\/\/aobosteel.com\/#\/schema\/logo\/image\/"},"sameAs":["https:\/\/www.facebook.com\/profile.php?id=61565368220197","https:\/\/www.linkedin.com\/in\/aobosteel-evan\/"]},{"@type":"Person","@id":"https:\/\/aobosteel.com\/#\/schema\/person\/96118415c30ca6bb52eaf1127b052ef7","name":"\uc5d0\ubc18","image":{"@type":"ImageObject","inLanguage":"ko-KR","@id":"https:\/\/secure.gravatar.com\/avatar\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g","url":"https:\/\/secure.gravatar.com\/avatar\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g","contentUrl":"https:\/\/secure.gravatar.com\/avatar\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g","caption":"Evan"},"sameAs":["http:\/\/www.aobosteel.com","https:\/\/www.facebook.com\/profile.php?id=61565368220197","https:\/\/www.instagram.com\/aobosteel\/","https:\/\/www.linkedin.com\/in\/aobosteel-evan\/","https:\/\/x.com\/AobosteelEvan","https:\/\/www.youtube.com\/@aobosteel"],"url":"https:\/\/aobosteel.com\/ko\/blog\/author\/admin\/"}]}},"uagb_featured_image_src":{"full":["https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/04\/5CrMnMo-Hot-Work-Tool-Steel.avif",500,500,false],"thumbnail":["https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/04\/5CrMnMo-Hot-Work-Tool-Steel-150x150.avif",150,150,true],"medium":["https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/04\/5CrMnMo-Hot-Work-Tool-Steel-300x300.avif",300,300,true],"medium_large":["https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/04\/5CrMnMo-Hot-Work-Tool-Steel.avif",500,500,false],"large":["https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/04\/5CrMnMo-Hot-Work-Tool-Steel.avif",500,500,false],"1536x1536":["https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/04\/5CrMnMo-Hot-Work-Tool-Steel.avif",500,500,false],"2048x2048":["https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/04\/5CrMnMo-Hot-Work-Tool-Steel.avif",500,500,false],"trp-custom-language-flag":["https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/04\/5CrMnMo-Hot-Work-Tool-Steel-12x12.avif",12,12,true]},"uagb_author_info":{"display_name":"Evan","author_link":"https:\/\/aobosteel.com\/ko\/blog\/author\/admin\/"},"uagb_comment_info":0,"uagb_excerpt":"Home &gt; Tool Steel Heat Treatment Technical Center &gt; M2 Tool Steel Heat Treatment Guide Aobo Steel | Global Tool Steel Supplier in China 5CrMnMo Hot Work Tool Steel Supplier Request a Quick Inquiry 1.\u00a0 5CrMnMo Steel\u00a0Overview and Chemical Composition 5CrMnMo Hot Work Tool Steel is classified as a low-alloy hot work die steel. Its&hellip;","rttpg_featured_image_url":{"full":["https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/04\/5CrMnMo-Hot-Work-Tool-Steel.avif",500,500,false],"landscape":["https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/04\/5CrMnMo-Hot-Work-Tool-Steel.avif",500,500,false],"portraits":["https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/04\/5CrMnMo-Hot-Work-Tool-Steel.avif",500,500,false],"thumbnail":["https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/04\/5CrMnMo-Hot-Work-Tool-Steel-150x150.avif",150,150,true],"medium":["https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/04\/5CrMnMo-Hot-Work-Tool-Steel-300x300.avif",300,300,true],"large":["https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/04\/5CrMnMo-Hot-Work-Tool-Steel.avif",500,500,false],"1536x1536":["https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/04\/5CrMnMo-Hot-Work-Tool-Steel.avif",500,500,false],"2048x2048":["https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/04\/5CrMnMo-Hot-Work-Tool-Steel.avif",500,500,false],"trp-custom-language-flag":["https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/04\/5CrMnMo-Hot-Work-Tool-Steel-12x12.avif",12,12,true]},"rttpg_author":{"display_name":"Evan","author_link":"https:\/\/aobosteel.com\/ko\/blog\/author\/admin\/"},"rttpg_comment":0,"rttpg_category":null,"rttpg_excerpt":"Home &gt; Tool Steel Heat Treatment Technical Center &gt; M2 Tool Steel Heat Treatment Guide Aobo Steel | Global Tool Steel Supplier in China 5CrMnMo Hot Work Tool Steel Supplier Request a Quick Inquiry 1.\u00a0 5CrMnMo Steel\u00a0Overview and Chemical Composition 5CrMnMo Hot Work Tool Steel is classified as a low-alloy hot work die steel. Its&hellip;","_links":{"self":[{"href":"https:\/\/aobosteel.com\/ko\/wp-json\/wp\/v2\/pages\/11165","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/aobosteel.com\/ko\/wp-json\/wp\/v2\/pages"}],"about":[{"href":"https:\/\/aobosteel.com\/ko\/wp-json\/wp\/v2\/types\/page"}],"author":[{"embeddable":true,"href":"https:\/\/aobosteel.com\/ko\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/aobosteel.com\/ko\/wp-json\/wp\/v2\/comments?post=11165"}],"version-history":[{"count":4,"href":"https:\/\/aobosteel.com\/ko\/wp-json\/wp\/v2\/pages\/11165\/revisions"}],"predecessor-version":[{"id":22249,"href":"https:\/\/aobosteel.com\/ko\/wp-json\/wp\/v2\/pages\/11165\/revisions\/22249"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/aobosteel.com\/ko\/wp-json\/wp\/v2\/media\/6262"}],"wp:attachment":[{"href":"https:\/\/aobosteel.com\/ko\/wp-json\/wp\/v2\/media?parent=11165"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}