{"version":"1.0","provider_name":"\uc544\uc624\ubcf4\uc2a4\ud2f8","provider_url":"https:\/\/aobosteel.com\/ko","author_name":"Evan","author_url":"https:\/\/aobosteel.com\/ko\/blog\/author\/admin\/","title":"Press Quench and Aging: Why the Same 6061 Shape Tests Different Along Its Length","type":"rich","width":600,"height":338,"html":"<blockquote class=\"wp-embedded-content\" data-secret=\"G641sJQaVF\"><a href=\"https:\/\/aobosteel.com\/ko\/aluminum-extrusion-press-quench-and-aging\/\">\ud504\ub808\uc2a4 \uae09\ub0c9 \ubc0f \uc2dc\ud6a8 \ucc98\ub9ac: \ub3d9\uc77c\ud55c 6061 \ud615\uc0c1\uc774 \uae38\uc774 \ubc29\ud5a5\uc5d0 \ub530\ub77c \ub2e4\ub978 \uc2dc\ud5d8 \uacb0\uacfc\ub97c \ubcf4\uc774\ub294 \uc774\uc720<\/a><\/blockquote><iframe sandbox=\"allow-scripts\" security=\"restricted\" src=\"https:\/\/aobosteel.com\/ko\/aluminum-extrusion-press-quench-and-aging\/embed\/#?secret=G641sJQaVF\" width=\"600\" height=\"338\" title=\"&#8220;Press Quench and Aging: Why the Same 6061 Shape Tests Different Along Its Length&#8221; &#8212; AoboSteel\" data-secret=\"G641sJQaVF\" frameborder=\"0\" marginwidth=\"0\" marginheight=\"0\" scrolling=\"no\" class=\"wp-embedded-content\"><\/iframe><script>\n\/*! This file is auto-generated *\/\n!function(d,l){\"use strict\";l.querySelector&&d.addEventListener&&\"undefined\"!=typeof URL&&(d.wp=d.wp||{},d.wp.receiveEmbedMessage||(d.wp.receiveEmbedMessage=function(e){var t=e.data;if((t||t.secret||t.message||t.value)&&!\/[^a-zA-Z0-9]\/.test(t.secret)){for(var s,r,n,a=l.querySelectorAll('iframe[data-secret=\"'+t.secret+'\"]'),o=l.querySelectorAll('blockquote[data-secret=\"'+t.secret+'\"]'),c=new RegExp(\"^https?:$\",\"i\"),i=0;i<o.length;i++)o[i].style.display=\"none\";for(i=0;i<a.length;i++)s=a[i],e.source===s.contentWindow&&(s.removeAttribute(\"style\"),\"height\"===t.message?(1e3<(r=parseInt(t.value,10))?r=1e3:~~r<200&&(r=200),s.height=r):\"link\"===t.message&&(r=new URL(s.getAttribute(\"src\")),n=new URL(t.value),c.test(n.protocol))&&n.host===r.host&&l.activeElement===s&&(d.top.location.href=t.value))}},d.addEventListener(\"message\",d.wp.receiveEmbedMessage,!1),l.addEventListener(\"DOMContentLoaded\",function(){for(var e,t,s=l.querySelectorAll(\"iframe.wp-embedded-content\"),r=0;r<s.length;r++)(t=(e=s[r]).getAttribute(\"data-secret\"))||(t=Math.random().toString(36).substring(2,12),e.src+=\"#?secret=\"+t,e.setAttribute(\"data-secret\",t)),e.contentWindow.postMessage({message:\"ready\",secret:t},\"*\")},!1)))}(window,document);\n\/\/# sourceURL=https:\/\/aobosteel.com\/wp-includes\/js\/wp-embed.min.js\n<\/script>","description":"What the press quench must achieve, when heavy sections need a furnace instead, 6xxx aging practices and the annual oven survey."}