DC53 Steel – High-Performance Tool Steel by Aobo Steel

DC53 steel is a high-chromium steel and a general-purpose high-toughness cold-work die steel. After quenching and tempering at 520-530°C, its hardness can reach 62-63 HRC, which is higher than that of SKD11 steel. Although its hardness is 2-3 HRC higher, its wear resistance is greatly improved, and its impact toughness is significantly enhanced, making it an excellent steel grade to replace D2.

Aobo Steel specializes in DC53 steel, which is available in round bar and plate forms. The composition and properties of the DC53 we supply fully comply with the standards.

DC53 STEEL

Application Scenarios

Plastic Injection Molds
Die Casting Dies
die holders
Shear Blades

Blanking dies, cold forming dies, cold drawing dies, forming roll punches, and cold extrusion dies are essential for shaping and cutting materials in cold-working processes.

Precision blanking and various types of stamping dies for wire cutting processing are ideal for intricate and accurate cutting tasks.

Plastic deformation dies for difficult-to-machine materials: This includes cold forging, deep drawing, and thread rolling dies, as well as high-speed blanking punches and stainless steel sheet punches, suited for challenging material processing.

Cold stamping dies requiring high wear resistance, hardness, and toughness are perfect for demanding stamping operations that require durability and strength.

Dies with higher performance requirements than D2 steel and molds needing exceptional toughness: DC53 offers superior performance and excellent cost-effectiveness in these scenarios.

Large molds and precision molds: Suitable for applications where size and precision are critical.

Why choose Aobo Steel as your DC53 supplier

Under the premise of ensuring quality, our prices are approximately 3% lower than the market price.

Before shipment, all goods undergo 100% strict chemical, UT, and hardness testing.

With over 20 years of experience in forged tool steel production, we have a deep understanding of our products.

DC53 material properties

Dc53 steel composition

ElementCarbon (C)Silicon (Si)Manganese (Mn)Chromium (Cr)Molybdenum (Mo)Vanadium (V)
Percentage (%)0.90 – 1.1010.4820.3

Dc53 heat treatment

Quenching and Tempering Specifications

Quenching Temperature: 940–960°C

Tempering Temperature: 180–220°C

Hardness: 60–62 HRC

The benefits of DC53

Higher Hardness: DC53 achieves a higher hardness (62-64 HRc) after heat treatment than D2 steel.  
Superior Toughness: It boasts twice the toughness of D2 steel, leading to improved durability and reduced chipping and cracking in dies.  
High Fatigue Strength: DC53 exhibits substantially higher fatigue strength than D2, making it suitable for repetitive stress applications.

DC53 steel VS D2

DC53 and D2 are both cold work die steels; we will compare their information.

PropertyDC53 SteelD2 Steel
CompositionC: 0.95%, Cr: 8.0%, Mo: 2.0%, V: 0.3%, Si: 1.0%, Mn: 0.4%, Fe: BalanceC: 1.40-1.60%, Cr: 10.00-13.00%, Mo: 0.70-1.20%, V: 0.90%, Si: 0.60%, Mn: 0.60%, Fe: Balance
Hardness (HRC)62-6455-62
ToughnessHigh, twice that of D2Good, less than DC53
Wear ResistanceBetter, due to smaller carbidesExcellent, standard for cold work
MachinabilityEasy, 20-40% faster than D2Difficult, abrasive, work hardens
Corrosion ResistancePoor, requires maintenancePoor, slightly better due to higher Cr
Heat TreatmentAir-hardening, less residual stressAir-hardening, standard process
CostPotentially higher, modern developmentLower, well-established standard
AvailabilityLess common outside AsiaWidely available globally
Typical UsesPrecision dies, molds, punchesCutting tools, shear blades, punches