THE FOLLOWING STORIES OF OUR CLIENTS ARE ALL REAL. TO PROTECT THE PRIVACY OF OUR CLIENTS, WE HAVE REFRAINED FROM MENTIONING THEIR NAMES. Stories from an Indian client In 2017, we had the privilege of forming a partnership with one of India’s largest importers of tool steel, thanks to an introduction from one of our […]

Clients’ Stores Read More »

D2 vs D3 tool steel

When choosing the right tool steel for your project, you may come across D2 and D3 tool steels. Both tool steels are high-carbon, high-chromium tool steels that are widely used in the tool and die industry for cold work tools such as cutting tools, dies and punches. They are classified as D series in the

D2 vs D3 tool steel Read More »

ESR equipments

what is ESR

In the tool steel industry, ESR means Electroslag Remelting. To improve quality, some steel grades undergo remelting processes, such as vacuum arc remelting (VAR) and electro-slag remelting (ESR). As molds become bigger and require more specialized features, the use of remelted steel has been growing. Compared to VAR, ESR offers several advantages. It is cheaper because it doesn’t

what is ESR Read More »

comparsion of h11 and h13 tool steel

H11 and H13 tool steel

H11 tool steel and H13 tool steel are both hot work tool steels. They belong to the H series of the American Society for Testing and Materials (ASTM) system. H11 and H13 are representative of hot work tool steels. They offer a good balance of cost and performance, making them a reference point for various applications in hot-forming

H11 and H13 tool steel Read More »

D2 TOOL STEEL

D2 vs. A2 tool steel

D2 tool steel and A2 tool steel are often used in industrial production. This article compares the data of the two steels so that the user can choose in practice. So, let’s look at the following article about D2 vs. A2 tool steel! D2 and A2 tool steel equivalent grades USA/ASTM USA/UNS Germany/DIN Germany/W-Nr. Japan/JIS ISO China/GB D2

D2 vs. A2 tool steel Read More »

deep drawing die

Selection of drawing die steel

Drawing dies stretch and deform metal sheets between a punch and a die to produce a cup-shaped workpiece. Their effectiveness depends on excellent wear resistance and anti-seizure properties. In many applications, choosing the right tool steel is critical. For example, steels like D2, D3, H13, H11, 1.2379, 1.2080, 1.2343, or 1.2344 can achieve optimal performance.

Selection of drawing die steel Read More »

Hot Work Tool Steel Introduction

Hot Work Die Steel: Types and Developments Hot work die steel is crucial for manufacturing die materials used in the hot forming of metals. The three primary categories of hot work die steels are low alloy, medium alloy, and high alloy steels. Below, we explore the most commonly used grades and recent advancements in hot

Hot Work Tool Steel Introduction Read More »