{"id":21262,"date":"2026-10-08T04:06:04","date_gmt":"2026-10-07T20:06:04","guid":{"rendered":"https:\/\/aobosteel.com\/?page_id=21262"},"modified":"2026-10-16T01:53:18","modified_gmt":"2026-10-15T17:53:18","slug":"automated-heat-treating-tool-steel","status":"publish","type":"page","link":"https:\/\/aobosteel.com\/es\/automated-heat-treating-tool-steel\/","title":{"rendered":"Tratamiento t\u00e9rmico automatizado de aceros para herramientas"},"content":{"rendered":"<h1 class=\"wp-block-heading\">Tratamiento t\u00e9rmico automatizado de aceros para herramientas<\/h1>\n\n\n\n<p class=\"wp-block-paragraph\">El tratamiento t\u00e9rmico de producci\u00f3n de acero para herramientas se realiza en l\u00edneas automatizadas de ba\u00f1o de sales en lugar de una herramienta a la vez. La l\u00ednea transporta las piezas a trav\u00e9s del precalentamiento, el calentamiento alto y el temple en un ciclo fijo, y el tiempo de ciclo lo determina la pieza de trabajo y no el operador. Esta p\u00e1gina presenta la secuencia de etapas con sus temperaturas de operaci\u00f3n, y los tiempos de ciclo publicados para brocas helicoidales y otras herramientas.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">C\u00f3mo se dispone una l\u00ednea automatizada de acero para herramientas<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">La descripci\u00f3n publicada de una l\u00ednea de producci\u00f3n de acero para herramientas tiene las piezas suspendidas en dispositivos de sujeci\u00f3n tipo tenaza y transportadas a trav\u00e9s del proceso por un transportador de cadena sobre barras portadoras. Los brazos de transferencia rotativos se ubican entre las unidades de precalentamiento y calentamiento alto y entre las unidades de calentamiento alto y temple. La ubicaci\u00f3n del brazo de transferencia se rige principalmente por la tasa de producci\u00f3n, pero siempre se requiere un brazo entre el calentamiento alto y el temple, porque la parte metal\u00fargica del ciclo depende de que la transferencia sea r\u00e1pida.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">Las l\u00edneas tambi\u00e9n tienen \u00e1reas libres sobre los hornos para que las herramientas puedan enfriarse al aire en su lugar. Est\u00e1n equipadas para ciclos que van desde menos de un minuto hasta diez minutos. Donde el volumen lo justifica, se agrega una estaci\u00f3n para un temple isot\u00e9rmico en nitrato despu\u00e9s del temple en sal neutra. Esa etapa adicional baja r\u00e1pidamente la temperatura de las herramientas y reduce el tiempo de enfriamiento al aire de 24 veces el tiempo a la temperatura de calentamiento alto a 6 veces.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">Etapas del proceso y temperaturas de operaci\u00f3n<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">Las etapas se ejecutan en un orden fijo desde el primer precalentamiento hasta el enjuague. Cada una tiene su propio rango de temperatura de trabajo, y el rango se ampl\u00eda o se estrecha seg\u00fan el grado y la secci\u00f3n que se trate. La columna de tiempo se escribe como un m\u00faltiplo del tiempo a la temperatura de calentamiento alto en lugar de en minutos, porque ese tiempo base depende de la pieza de trabajo y lo establece la segunda tabla a continuaci\u00f3n.<\/p>\n\n\n\n<figure class=\"wp-block-table is-style-stripes\"><table class=\"has-fixed-layout\"><thead><tr><th class=\"has-text-align-left\" data-align=\"left\">Etapa del proceso<\/th><th class=\"has-text-align-left\" data-align=\"left\">Temperatura de operaci\u00f3n, &deg;C<\/th><th class=\"has-text-align-left\" data-align=\"left\">Temperatura de operaci\u00f3n, &deg;F<\/th><th class=\"has-text-align-left\" data-align=\"left\">Tiempo total en el horno<\/th><\/tr><\/thead><tbody><tr><td class=\"has-text-align-left\" data-align=\"left\">Primer precalentamiento<\/td><td class=\"has-text-align-left\" data-align=\"left\">650-870<\/td><td class=\"has-text-align-left\" data-align=\"left\">1200-1600<\/td><td class=\"has-text-align-left\" data-align=\"left\">X<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">Segundo precalentamiento<\/td><td class=\"has-text-align-left\" data-align=\"left\">760-1040<\/td><td class=\"has-text-align-left\" data-align=\"left\">1400-1900<\/td><td class=\"has-text-align-left\" data-align=\"left\">X<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">Calentamiento alto<\/td><td class=\"has-text-align-left\" data-align=\"left\">1010-1290<\/td><td class=\"has-text-align-left\" data-align=\"left\">1850-2350<\/td><td class=\"has-text-align-left\" data-align=\"left\">X<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">Temple isot\u00e9rmico<\/td><td class=\"has-text-align-left\" data-align=\"left\">540-705<\/td><td class=\"has-text-align-left\" data-align=\"left\">1000-1300<\/td><td class=\"has-text-align-left\" data-align=\"left\">X<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">Enfriar al aire<\/td><td class=\"has-text-align-left\" data-align=\"left\">Temperatura ambiente<\/td><td class=\"has-text-align-left\" data-align=\"left\">Temperatura ambiente<\/td><td class=\"has-text-align-left\" data-align=\"left\">6X, 12X o 24X<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">Lavado, agua caliente<\/td><td class=\"has-text-align-left\" data-align=\"left\">80-95<\/td><td class=\"has-text-align-left\" data-align=\"left\">180-200<\/td><td class=\"has-text-align-left\" data-align=\"left\">6X<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">Enjuague, agua caliente<\/td><td class=\"has-text-align-left\" data-align=\"left\">80-95<\/td><td class=\"has-text-align-left\" data-align=\"left\">180-200<\/td><td class=\"has-text-align-left\" data-align=\"left\">X<\/td><\/tr><\/tbody><\/table><\/figure>\n\n\n\n<p class=\"wp-block-paragraph\"><em>Tiempos y temperaturas relativos del proceso para una l\u00ednea automatizada de tratamiento t\u00e9rmico de acero para herramientas. La columna de tiempo se expresa como un m\u00faltiplo del tiempo a la temperatura de calentamiento alto, que lo establece la pieza y se indica en la tabla a continuaci\u00f3n, por lo que una X es un m\u00faltiplo de ese tiempo. Fuente, Tabla 2 de Automatic Heat Treating of Tool Steels, en ASM Handbook, Volumen 4, Heat Treating.<\/em><\/p>\n\n\n\n<h2 class=\"wp-block-heading\">Tiempos de ciclo para brocas helicoidales y otras herramientas<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">Los tiempos publicados para brocas helicoidales se dan al segundo y se agrupan por di\u00e1metro, de modo que un taller puede leer el tiempo de calentamiento alto directamente del di\u00e1metro. Las copas y las fresas de extremo se tratan como piezas de trabajo individuales a tiempos fijos. Estos son los tiempos a la temperatura de calentamiento alto, y son la X en la tabla de etapas anterior.<\/p>\n\n\n\n<figure class=\"wp-block-table is-style-stripes\"><table class=\"has-fixed-layout\"><thead><tr><th class=\"has-text-align-left\" data-align=\"left\">Pieza de trabajo<\/th><th class=\"has-text-align-left\" data-align=\"left\">Tiempo en calentamiento alto<\/th><\/tr><\/thead><tbody><tr><td class=\"has-text-align-left\" data-align=\"left\">Brocas helicoidales de 2.54-4.78 mm (0.100-0.188 in.)<\/td><td class=\"has-text-align-left\" data-align=\"left\">1 min 30 s<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">Brocas helicoidales de 4.80-8.08 mm (0.189-0.318 in.)<\/td><td class=\"has-text-align-left\" data-align=\"left\">1 min 40 s<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">Brocas helicoidales de 8.10-12.90 mm (0.319-0.508 in.)<\/td><td class=\"has-text-align-left\" data-align=\"left\">1 min 50 s<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">Brocas helicoidales de 12.93-18.24 mm (0.509-0.718 in.)<\/td><td class=\"has-text-align-left\" data-align=\"left\">2 min 0 s<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">Brocas helicoidales de 18.26-23.32 mm (0.719-0.918 in.)<\/td><td class=\"has-text-align-left\" data-align=\"left\">2 min 20 s<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">Brocas helicoidales de 23.34-38.10 mm (0.919-1.500 in.)<\/td><td class=\"has-text-align-left\" data-align=\"left\">2 min 40 s<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">Copas de 102 mm (4 in.) de di\u00e1metro<\/td><td class=\"has-text-align-left\" data-align=\"left\">6 min<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">Fresas de extremo de 64 mm (2&frac12; in.) de di\u00e1metro<\/td><td class=\"has-text-align-left\" data-align=\"left\">7 min<\/td><\/tr><tr><td class=\"has-text-align-left\" data-align=\"left\">Fresas de extremo de 76 mm (3 in.) de di\u00e1metro<\/td><td class=\"has-text-align-left\" data-align=\"left\">10 min<\/td><\/tr><\/tbody><\/table><\/figure>\n\n\n\n<p class=\"wp-block-paragraph\"><em>Tiempos de ciclo para brocas helicoidales y otras herramientas en la etapa de calentamiento alto. Los di\u00e1metros son las bandas utilizadas por la fuente, y los tiempos son los tiempos programados a temperatura. Fuente, Tabla 3 de Automatic Heat Treating of Tool Steels, en ASM Handbook, Volumen 4, Heat Treating.<\/em><\/p>\n\n\n\n<p class=\"wp-block-paragraph\">Para los di\u00e1metros m\u00e1s peque\u00f1os la misma fuente tambi\u00e9n registra la carga. Las brocas de 2.54 mm (0.100 in.) funcionan a 160 piezas por tenaza, 480 piezas en el ba\u00f1o, lo que es 1.2 kg (2.6 lb) de trabajo en una sola carga.<\/p>\n\n\n\n<div class=\"wp-block-group has-background is-layout-constrained wp-container-core-group-is-layout-3e4fb3d2 wp-block-group-is-layout-constrained\" style=\"border-radius:8px;background-color:#f4f8ff;margin-bottom:24px;padding-top:20px;padding-right:24px;padding-bottom:20px;padding-left:24px\">\n<p class=\"wp-block-paragraph\"><strong>Ciclo de tratamiento t\u00e9rmico automatizado, PDF imprimible<\/strong><\/p>\n\n<p class=\"wp-block-paragraph\">Las etapas de la l\u00ednea con sus temperaturas de operaci\u00f3n y los tiempos de ciclo para brocas helicoidales, copas y fresas de extremo, en un solo PDF con nuestros datos de contacto.<\/p>\n\n<div class=\"wp-block-buttons is-layout-flex wp-block-buttons-is-layout-flex\">\n<div class=\"wp-block-button\"><a class=\"wp-block-button__link wp-element-button\" href=\"https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/10\/Aobo-Steel-Automated-Heat-Treating.pdf\">Descargar PDF<\/a><\/div>\n\n<\/div>\n<\/div>\n\n\n\n<h2 class=\"wp-block-heading\">Por qu\u00e9 el temple en nitrato se mantiene alejado del horno de calentamiento alto<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">El temple en nitrato y el horno de calentamiento alto son unidades separadas por una raz\u00f3n que se indica claramente en la fuente. Si se permite que tan solo 600 ppm de sales de nitrato entren en el horno de calentamiento alto, se puede causar un da\u00f1o superficial extremo a la herramienta que se est\u00e1 tratando. La disposici\u00f3n de transferencia y las estaciones separadas existen para mantener los dos ba\u00f1os aparte.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">Los ba\u00f1os de sales tambi\u00e9n necesitan rectificaci\u00f3n peri\u00f3dica, porque las sales de austenizaci\u00f3n neutras captan \u00f3xidos solubles y metales disueltos durante su uso. Una vez que el ba\u00f1o se vuelve oxidante y decarburizante hacia el acero, debe rectificarse, y cuanto mayor sea la temperatura de operaci\u00f3n, con m\u00e1s frecuencia. Los ba\u00f1os que funcionan por encima de 1080 &deg;C (1975 &deg;F) requieren rectificaci\u00f3n al menos una vez al d\u00eda. Una prueba de lima sobre una probeta endurecida, o un an\u00e1lisis que muestre m\u00e1s de 0.5% de BaO, es la verificaci\u00f3n com\u00fan de que un ba\u00f1o de calentamiento alto se ha desviado.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">Qu\u00e9 grados se procesan en estas l\u00edneas<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">El rango de calentamiento alto en la tabla, 1010 a 1290 &deg;C (1850 a 2350 &deg;F), es el rango de acero r\u00e1pido, y las brocas helicoidales, fresas de extremo, machos, fresas madre y escariadores son las herramientas que llenan esas l\u00edneas. Las brocas y fresas de extremo en la segunda tabla t\u00edpicamente est\u00e1n hechas de <a href=\"https:\/\/aobosteel.com\/es\/m2-tool-steel\/\">Acero r\u00e1pido M2<\/a>, el grado de molibdeno de uso general utilizado para la mayor parte de las herramientas de corte.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">El ciclo completo para estos grados, desde el recocido hasta la austenizaci\u00f3n, el temple y el revenido m\u00faltiple, se expone <a href=\"https:\/\/aobosteel.com\/es\/high-speed-steel-heat-treatment-detail\/\">en la p\u00e1gina de detalle del tratamiento t\u00e9rmico del acero r\u00e1pido<\/a>, que contiene las temperaturas y la respuesta al revenido que acompa\u00f1an a los tiempos de calentamiento alto aqu\u00ed indicados.<\/p>\n\n\n\n<div class=\"wp-block-group has-background is-layout-constrained wp-container-core-group-is-layout-3e4fb3d2 wp-block-group-is-layout-constrained\" style=\"border-radius:8px;background-color:#f4f8ff;margin-bottom:24px;padding-top:20px;padding-right:24px;padding-bottom:20px;padding-left:24px\">\n<p class=\"wp-block-paragraph\"><strong>Ciclo de tratamiento t\u00e9rmico automatizado, PDF imprimible<\/strong><\/p>\n\n<p class=\"wp-block-paragraph\">Las etapas de la l\u00ednea con sus temperaturas de operaci\u00f3n y los tiempos de ciclo para brocas helicoidales, copas y fresas de extremo, en un solo PDF con nuestros datos de contacto.<\/p>\n\n<div class=\"wp-block-buttons is-layout-flex wp-block-buttons-is-layout-flex\">\n<div class=\"wp-block-button\"><a class=\"wp-block-button__link wp-element-button\" href=\"https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/10\/Aobo-Steel-Automated-Heat-Treating.pdf\">Descargar PDF<\/a><\/div>\n\n<\/div>\n<\/div>\n\n\n\n<h3 class=\"wp-block-heading\">Antes de usar estos valores<\/h3>\n\n\n\n<p class=\"wp-block-paragraph\">Esta p\u00e1gina es un resumen de referencia de la pr\u00e1ctica publicada y no es una especificaci\u00f3n de Aobo Steel. Las etapas y los tiempos son las cifras publicadas para las herramientas nombradas, y una l\u00ednea diferente, carga de sujeci\u00f3n o tama\u00f1o de secci\u00f3n los modificar\u00e1. Los par\u00e1metros finales del ciclo los establece el tratador t\u00e9rmico.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">Fuente: ASM Handbook, Volume 4, Heat Treating, ASM International, 1991.<\/p>","protected":false},"excerpt":{"rendered":"<p>Automated Heat Treating of Tool Steels Production heat treating of tool steel is done on automated salt bath lines rather than one tool at a time. The line carries the parts through preheat, high heat and quench on a fixed cycle, and the cycle time is set by the workpiece rather than by the operator. [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":0,"parent":0,"menu_order":0,"comment_status":"closed","ping_status":"closed","template":"","meta":{"_uag_custom_page_level_css":"","site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"normal-width-container","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"disabled","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","ast-disable-related-posts":"","theme-transparent-header-meta":"","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"default","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"footnotes":""},"class_list":["post-21262","page","type-page","status-publish","hentry"],"yoast_head":"<!-- This site is optimized with the Yoast SEO Premium plugin v28.9 (Yoast SEO v28.9) - https:\/\/yoast.com\/product\/yoast-seo-premium-wordpress\/ -->\n<title>Automated Heat Treating of Tool Steels: Line Stages<\/title>\n<meta name=\"description\" content=\"Line stages, operating temperatures and published cycle times for automated heat treating of tool steels, with times for twist drills, cups and end mills.\" \/>\n<meta name=\"robots\" content=\"index, follow, max-snippet:-1, max-image-preview:large, max-video-preview:-1\" \/>\n<link rel=\"canonical\" href=\"https:\/\/aobosteel.com\/es\/automated-heat-treating-tool-steel\/\" \/>\n<meta property=\"og:locale\" content=\"es_ES\" \/>\n<meta property=\"og:type\" content=\"article\" \/>\n<meta property=\"og:title\" content=\"Automated Heat Treating of Tool Steels\" \/>\n<meta property=\"og:description\" content=\"Line stages, operating temperatures and published cycle times for automated heat treating of tool steels, with times for twist drills, cups and end mills.\" \/>\n<meta property=\"og:url\" content=\"https:\/\/aobosteel.com\/es\/automated-heat-treating-tool-steel\/\" \/>\n<meta property=\"og:site_name\" content=\"AoboSteel\" \/>\n<meta property=\"article:publisher\" content=\"https:\/\/www.facebook.com\/profile.php?id=61565368220197\" \/>\n<meta property=\"article:modified_time\" content=\"2026-10-15T17:53:18+00:00\" \/>\n<meta name=\"twitter:card\" content=\"summary_large_image\" \/>\n<meta name=\"twitter:label1\" content=\"Tiempo de lectura\" \/>\n\t<meta name=\"twitter:data1\" content=\"5 minutos\" \/>\n<script type=\"application\/ld+json\" class=\"yoast-schema-graph\">{\"@context\":\"https:\\\/\\\/schema.org\",\"@graph\":[{\"@type\":\"TechArticle\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/automated-heat-treating-tool-steel\\\/#article\",\"isPartOf\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/automated-heat-treating-tool-steel\\\/\"},\"author\":{\"name\":\"Evan\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#\\\/schema\\\/person\\\/96118415c30ca6bb52eaf1127b052ef7\"},\"headline\":\"Automated Heat Treating of Tool Steels\",\"datePublished\":\"2026-10-07T20:06:04+00:00\",\"dateModified\":\"2026-10-15T17:53:18+00:00\",\"mainEntityOfPage\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/automated-heat-treating-tool-steel\\\/\"},\"wordCount\":1060,\"publisher\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#organization\"},\"inLanguage\":\"es\"},{\"@type\":\"WebPage\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/automated-heat-treating-tool-steel\\\/\",\"url\":\"https:\\\/\\\/aobosteel.com\\\/automated-heat-treating-tool-steel\\\/\",\"name\":\"Automated Heat Treating of Tool Steels: Line Stages\",\"isPartOf\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#website\"},\"datePublished\":\"2026-10-07T20:06:04+00:00\",\"dateModified\":\"2026-10-15T17:53:18+00:00\",\"description\":\"Line stages, operating temperatures and published cycle times for automated heat treating of tool steels, with times for twist drills, cups and end mills.\",\"breadcrumb\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/automated-heat-treating-tool-steel\\\/#breadcrumb\"},\"inLanguage\":\"es\",\"potentialAction\":[{\"@type\":\"ReadAction\",\"target\":[\"https:\\\/\\\/aobosteel.com\\\/automated-heat-treating-tool-steel\\\/\"]}]},{\"@type\":\"BreadcrumbList\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/automated-heat-treating-tool-steel\\\/#breadcrumb\",\"itemListElement\":[{\"@type\":\"ListItem\",\"position\":1,\"name\":\"\u9996\u9875\",\"item\":\"https:\\\/\\\/aobosteel.com\\\/\"},{\"@type\":\"ListItem\",\"position\":2,\"name\":\"Automated Heat Treating of Tool Steels\"}]},{\"@type\":\"WebSite\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#website\",\"url\":\"https:\\\/\\\/aobosteel.com\\\/\",\"name\":\"AoboSteel\",\"description\":\"\",\"publisher\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#organization\"},\"potentialAction\":[{\"@type\":\"SearchAction\",\"target\":{\"@type\":\"EntryPoint\",\"urlTemplate\":\"https:\\\/\\\/aobosteel.com\\\/?s={search_term_string}\"},\"query-input\":{\"@type\":\"PropertyValueSpecification\",\"valueRequired\":true,\"valueName\":\"search_term_string\"}}],\"inLanguage\":\"es\"},{\"@type\":\"Organization\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#organization\",\"name\":\"AoboSteel\",\"url\":\"https:\\\/\\\/aobosteel.com\\\/\",\"logo\":{\"@type\":\"ImageObject\",\"inLanguage\":\"es\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#\\\/schema\\\/logo\\\/image\\\/\",\"url\":\"https:\\\/\\\/aobosteel.com\\\/wp-content\\\/uploads\\\/2025\\\/01\\\/cropped-aobo-steel-1.avif\",\"contentUrl\":\"https:\\\/\\\/aobosteel.com\\\/wp-content\\\/uploads\\\/2025\\\/01\\\/cropped-aobo-steel-1.avif\",\"width\":1052,\"height\":592,\"caption\":\"AoboSteel\"},\"image\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#\\\/schema\\\/logo\\\/image\\\/\"},\"sameAs\":[\"https:\\\/\\\/www.facebook.com\\\/profile.php?id=61565368220197\",\"https:\\\/\\\/www.linkedin.com\\\/in\\\/aobosteel-evan\\\/\"]},{\"@type\":\"Person\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#\\\/schema\\\/person\\\/96118415c30ca6bb52eaf1127b052ef7\",\"name\":\"Evan\",\"image\":{\"@type\":\"ImageObject\",\"inLanguage\":\"es\",\"@id\":\"https:\\\/\\\/secure.gravatar.com\\\/avatar\\\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g\",\"url\":\"https:\\\/\\\/secure.gravatar.com\\\/avatar\\\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g\",\"contentUrl\":\"https:\\\/\\\/secure.gravatar.com\\\/avatar\\\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g\",\"caption\":\"Evan\"},\"sameAs\":[\"http:\\\/\\\/www.aobosteel.com\",\"https:\\\/\\\/www.facebook.com\\\/profile.php?id=61565368220197\",\"https:\\\/\\\/www.instagram.com\\\/aobosteel\\\/\",\"https:\\\/\\\/www.linkedin.com\\\/in\\\/aobosteel-evan\\\/\",\"https:\\\/\\\/x.com\\\/AobosteelEvan\",\"https:\\\/\\\/www.youtube.com\\\/@aobosteel\"],\"url\":\"https:\\\/\\\/aobosteel.com\\\/es\\\/blog\\\/author\\\/admin\\\/\"}]}<\/script>\n<!-- \/ Yoast SEO Premium plugin. -->","yoast_head_json":{"title":"Tratamiento t\u00e9rmico automatizado de aceros para herramientas: etapas de la l\u00ednea","description":"Etapas de la l\u00ednea, temperaturas de operaci\u00f3n y tiempos de ciclo publicados para el tratamiento t\u00e9rmico automatizado de aceros para herramientas, con tiempos para brocas helicoidales, copas y fresas.","robots":{"index":"index","follow":"follow","max-snippet":"max-snippet:-1","max-image-preview":"max-image-preview:large","max-video-preview":"max-video-preview:-1"},"canonical":"https:\/\/aobosteel.com\/es\/automated-heat-treating-tool-steel\/","og_locale":"es_ES","og_type":"article","og_title":"Automated Heat Treating of Tool Steels","og_description":"Line stages, operating temperatures and published cycle times for automated heat treating of tool steels, with times for twist drills, cups and end mills.","og_url":"https:\/\/aobosteel.com\/es\/automated-heat-treating-tool-steel\/","og_site_name":"AoboSteel","article_publisher":"https:\/\/www.facebook.com\/profile.php?id=61565368220197","article_modified_time":"2026-10-15T17:53:18+00:00","twitter_card":"summary_large_image","twitter_misc":{"Tiempo de lectura":"5 minutos"},"schema":{"@context":"https:\/\/schema.org","@graph":[{"@type":"TechArticle","@id":"https:\/\/aobosteel.com\/automated-heat-treating-tool-steel\/#article","isPartOf":{"@id":"https:\/\/aobosteel.com\/automated-heat-treating-tool-steel\/"},"author":{"name":"Evan","@id":"https:\/\/aobosteel.com\/#\/schema\/person\/96118415c30ca6bb52eaf1127b052ef7"},"headline":"Automated Heat Treating of Tool Steels","datePublished":"2026-10-07T20:06:04+00:00","dateModified":"2026-10-15T17:53:18+00:00","mainEntityOfPage":{"@id":"https:\/\/aobosteel.com\/automated-heat-treating-tool-steel\/"},"wordCount":1060,"publisher":{"@id":"https:\/\/aobosteel.com\/#organization"},"inLanguage":"es"},{"@type":"WebPage","@id":"https:\/\/aobosteel.com\/automated-heat-treating-tool-steel\/","url":"https:\/\/aobosteel.com\/automated-heat-treating-tool-steel\/","name":"Tratamiento t\u00e9rmico automatizado de aceros para herramientas: etapas de la l\u00ednea","isPartOf":{"@id":"https:\/\/aobosteel.com\/#website"},"datePublished":"2026-10-07T20:06:04+00:00","dateModified":"2026-10-15T17:53:18+00:00","description":"Etapas de la l\u00ednea, temperaturas de operaci\u00f3n y tiempos de ciclo publicados para el tratamiento t\u00e9rmico automatizado de aceros para herramientas, con tiempos para brocas helicoidales, copas y fresas.","breadcrumb":{"@id":"https:\/\/aobosteel.com\/automated-heat-treating-tool-steel\/#breadcrumb"},"inLanguage":"es","potentialAction":[{"@type":"ReadAction","target":["https:\/\/aobosteel.com\/automated-heat-treating-tool-steel\/"]}]},{"@type":"BreadcrumbList","@id":"https:\/\/aobosteel.com\/automated-heat-treating-tool-steel\/#breadcrumb","itemListElement":[{"@type":"ListItem","position":1,"name":"\u9996\u9875","item":"https:\/\/aobosteel.com\/"},{"@type":"ListItem","position":2,"name":"Automated Heat Treating of Tool Steels"}]},{"@type":"WebSite","@id":"https:\/\/aobosteel.com\/#website","url":"https:\/\/aobosteel.com\/","name":"AoboSteel","description":"","publisher":{"@id":"https:\/\/aobosteel.com\/#organization"},"potentialAction":[{"@type":"SearchAction","target":{"@type":"EntryPoint","urlTemplate":"https:\/\/aobosteel.com\/?s={search_term_string}"},"query-input":{"@type":"PropertyValueSpecification","valueRequired":true,"valueName":"search_term_string"}}],"inLanguage":"es"},{"@type":"Organization","@id":"https:\/\/aobosteel.com\/#organization","name":"AoboSteel","url":"https:\/\/aobosteel.com\/","logo":{"@type":"ImageObject","inLanguage":"es","@id":"https:\/\/aobosteel.com\/#\/schema\/logo\/image\/","url":"https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/01\/cropped-aobo-steel-1.avif","contentUrl":"https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/01\/cropped-aobo-steel-1.avif","width":1052,"height":592,"caption":"AoboSteel"},"image":{"@id":"https:\/\/aobosteel.com\/#\/schema\/logo\/image\/"},"sameAs":["https:\/\/www.facebook.com\/profile.php?id=61565368220197","https:\/\/www.linkedin.com\/in\/aobosteel-evan\/"]},{"@type":"Person","@id":"https:\/\/aobosteel.com\/#\/schema\/person\/96118415c30ca6bb52eaf1127b052ef7","name":"Evan","image":{"@type":"ImageObject","inLanguage":"es","@id":"https:\/\/secure.gravatar.com\/avatar\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g","url":"https:\/\/secure.gravatar.com\/avatar\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g","contentUrl":"https:\/\/secure.gravatar.com\/avatar\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g","caption":"Evan"},"sameAs":["http:\/\/www.aobosteel.com","https:\/\/www.facebook.com\/profile.php?id=61565368220197","https:\/\/www.instagram.com\/aobosteel\/","https:\/\/www.linkedin.com\/in\/aobosteel-evan\/","https:\/\/x.com\/AobosteelEvan","https:\/\/www.youtube.com\/@aobosteel"],"url":"https:\/\/aobosteel.com\/es\/blog\/author\/admin\/"}]}},"uagb_featured_image_src":{"full":false,"thumbnail":false,"medium":false,"medium_large":false,"large":false,"1536x1536":false,"2048x2048":false,"trp-custom-language-flag":false},"uagb_author_info":{"display_name":"Evan","author_link":"https:\/\/aobosteel.com\/es\/blog\/author\/admin\/"},"uagb_comment_info":0,"uagb_excerpt":"Automated Heat Treating of Tool Steels Production heat treating of tool steel is done on automated salt bath lines rather than one tool at a time. The line carries the parts through preheat, high heat and quench on a fixed cycle, and the cycle time is set by the workpiece rather than by the operator.&hellip;","rttpg_featured_image_url":null,"rttpg_author":{"display_name":"Evan","author_link":"https:\/\/aobosteel.com\/es\/blog\/author\/admin\/"},"rttpg_comment":0,"rttpg_category":null,"rttpg_excerpt":"Automated Heat Treating of Tool Steels Production heat treating of tool steel is done on automated salt bath lines rather than one tool at a time. The line carries the parts through preheat, high heat and quench on a fixed cycle, and the cycle time is set by the workpiece rather than by the operator.&hellip;","_links":{"self":[{"href":"https:\/\/aobosteel.com\/es\/wp-json\/wp\/v2\/pages\/21262","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/aobosteel.com\/es\/wp-json\/wp\/v2\/pages"}],"about":[{"href":"https:\/\/aobosteel.com\/es\/wp-json\/wp\/v2\/types\/page"}],"author":[{"embeddable":true,"href":"https:\/\/aobosteel.com\/es\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/aobosteel.com\/es\/wp-json\/wp\/v2\/comments?post=21262"}],"version-history":[{"count":3,"href":"https:\/\/aobosteel.com\/es\/wp-json\/wp\/v2\/pages\/21262\/revisions"}],"predecessor-version":[{"id":22704,"href":"https:\/\/aobosteel.com\/es\/wp-json\/wp\/v2\/pages\/21262\/revisions\/22704"}],"wp:attachment":[{"href":"https:\/\/aobosteel.com\/es\/wp-json\/wp\/v2\/media?parent=21262"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}