{"id":20772,"date":"2026-10-03T15:04:40","date_gmt":"2026-10-03T07:04:40","guid":{"rendered":"https:\/\/aobosteel.com\/?page_id=20772"},"modified":"2026-10-16T08:17:10","modified_gmt":"2026-10-16T00:17:10","slug":"tool-steel-hardenability-and-section-size","status":"publish","type":"page","link":"https:\/\/aobosteel.com\/es\/tool-steel-hardenability-and-section-size\/","title":{"rendered":"Templabilidad del acero para herramientas y tama\u00f1o de secci\u00f3n"},"content":{"rendered":"<h1 class=\"wp-block-heading\">Templabilidad del acero para herramientas y tama\u00f1o de secci\u00f3n<\/h1>\n\n\n\n<p class=\"wp-block-paragraph\">La templabilidad determina qu\u00e9 tan gruesa es la secci\u00f3n de un acero para herramientas dado que realmente se templa, y es el primer dato que un taller necesita antes de pedir barras. Un grado que se templa a 65 HRC en la superficie de un bloque de 100 mm puede seguir blando en su interior, y solo los datos de templabilidad indican cu\u00e1l. Esta p\u00e1gina re\u00fane las cuatro gr\u00e1ficas de ASM para aceros para herramientas: las bandas de temple por extremo para los grados de temple en aceite, la dureza tal como se templa de <a href=\"https:\/\/aobosteel.com\/es\/o1-tool-steel\/\">O1<\/a>, <a href=\"https:\/\/aobosteel.com\/es\/o2-tool-steel\/\">O2<\/a>, barras O6 y O7 medidas en la superficie, a tres cuartos de radio y en el centro, la dureza de superficie a centro de <a href=\"https:\/\/aobosteel.com\/es\/m2-tool-steel\/\">M2<\/a>, barras de acero r\u00e1pido M3, T1 y T2, y la profundidad hasta 60 HRC en un W1 con 1% de carbono.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">La templabilidad no es lo mismo que la dureza<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">La templabilidad es la profundidad a la que se templa un acero, no qu\u00e9 tan duro queda. La distinci\u00f3n recorre toda la familia de aceros para herramientas. Los grados de temple al aire para trabajo en fr\u00edo (grupo A) alcanzan la dureza completa en secciones de hasta unos 102 mm, y uno de ellos, el A6, se templa en toda la secci\u00f3n en tama\u00f1os de hasta 178 mm. Los grados de alto cromo (grupo D) tambi\u00e9n son de temple al aire, con la excepci\u00f3n del D3, que se templa en aceite y por lo tanto es el grado de ese grupo que se distorsiona y agrieta. Los grados de temple en aceite (grupo O) templan secciones peque\u00f1as a moderadas en aceite, lo que es m\u00e1s seguro y recto que el temple en agua. Los grados de temple en agua (grupo W) necesitan el enfriamiento m\u00e1s r\u00e1pido de todos y son los m\u00e1s propensos a agrietarse en el tanque.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">El contenido de carbono juega en contra de la profundidad. Los aceros del grupo O y del grupo D contienen tanto carbono que una gran parte queda como carburo sin disolver a las temperaturas normales de temple, y ese carburo no contribuye a la templabilidad. El resultado es un acero que alcanza una dureza superficial muy alta y se templa en toda la secci\u00f3n de un tama\u00f1o menor que el que lograr\u00eda un acero de menor carbono con contenido de aleaci\u00f3n similar. Elevar la temperatura de austenizaci\u00f3n disuelve m\u00e1s de ese carburo y aumenta la profundidad de temple, pero tambi\u00e9n engrosa el grano, reduce la tenacidad y aumenta el riesgo de agrietamiento en el temple. Ese compromiso es la raz\u00f3n por la que las gr\u00e1ficas siguientes est\u00e1n todas vinculadas a una temperatura de austenizaci\u00f3n declarada.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">Bandas de templabilidad por temple de extremo para los grados de temple en aceite<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">El ensayo de temple por extremo (Jominy) templa un extremo de una barra redonda de 25 mm y mide la dureza a intervalos de un dieciseisavo de pulgada a lo largo de ella, de modo que el eje de distancia representa la velocidad de enfriamiento. Una banda de templabilidad es la envolvente de varias coladas del mismo grado, y es contra ella que se le debe cotizar a un comprador de acero. El panel (c) coloca O1 y O2 en una misma cuadr\u00edcula: la l\u00ednea superior es O1 y la inferior es O2, y ambas est\u00e1n separadas por aproximadamente 3 a 5 HRC en la parte media de la banda. Ambos grados comienzan cerca de 65 HRC en el extremo templado. Hacia el extremo final de la banda bajan a unos 40 HRC. El O6, graficado a partir de una estructura esferoidizada, se ubica cerca del O1 en la primera parte de la banda.<\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img decoding=\"async\" src=\"https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/10\/Aobo-Steel-Tool-Steel-Hardenability-fig-3-end-quench-bands-O-crop.jpg\" alt=\"End quench hardenability bands for O1, O2 and O6 oil hardening tool steel\"\/><figcaption class=\"wp-element-caption\">Fig. 3. Bandas de templabilidad por temple en el extremo para aceros para herramientas del grupo O: (a) O1, fuente A, (b) O2, fuente A, (c) O1 y O2, fuente B (cinco coladas cada uno), (d) O6 de una estructura esferoidizada. O1 y O6 se austenizaron a 815 \u00b0C, O2 a 790 \u00b0C. Reproducido de la figura de la fuente.<\/figcaption><\/figure>\n\n\n\n<h2 class=\"wp-block-heading\">Dureza tal como se templa frente al di\u00e1metro de barra, O1 a O7<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">El ensayo de temple por extremo clasifica los grados; esta gr\u00e1fica indica al taller lo que realmente medir\u00e1 en una barra de un di\u00e1metro dado. Cada panel es un grado medido en la superficie, a tres cuartos de radio y en el centro, con la fuente indicada en el pie de figura. L\u00e9ala as\u00ed, en los di\u00e1metros que normalmente compra un taller de matrices. El O1 tomado desde 815 &#176;C da unos 65 HRC en la superficie hasta aproximadamente 60 mm, 46 HRC en la superficie de una barra de 100 mm, y solo unos 35 HRC en el centro de esa misma barra de 100 mm. El O2 mantiene su dureza superficial m\u00e1s lejos: unos 65 HRC hasta casi 85 mm y a\u00fan alrededor de 53 HRC a 100 mm, lo que es lo inverso de la clasificaci\u00f3n por temple de extremo y se explica por las diferentes temperaturas de austenizaci\u00f3n usadas en las dos series de ensayos. El O7 es el menos templable de los cuatro: su curva central cae de unos 66 HRC a 20-30 mm a unos 38 HRC a 100 mm. Eso es consistente con la nota del manual de que el O7 tiene menor templabilidad pero mejor resistencia al desgaste que los dem\u00e1s grados del grupo O. El O6 se lee cerca del O1 en las tres posiciones.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">El dato de trabajo es la brecha entre la curva de superficie y la de centro en su tama\u00f1o de barra. Una matriz que debe estar dura en toda la secci\u00f3n de un bloque de 60 mm es un problema de otro orden que la misma matriz en material de 25 mm, y ninguna l\u00ednea de una ficha t\u00e9cnica muestra eso tan directamente como las tres curvas de un panel.<\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img decoding=\"async\" src=\"https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/10\/Aobo-Steel-Tool-Steel-Hardenability-fig-4-o-group-bar-diameter-crop.jpg\" alt=\"As quenched hardness against bar diameter for O1, O2, O6 and O7 tool steel at surface, three quarter radius and center\"\/><figcaption class=\"wp-element-caption\">Fig. 4. Dureza despu\u00e9s del temple frente al di\u00e1metro de la barra para los aceros para herramientas de temple en aceite O1, O2, O6 y O7, medida en la superficie, a tres cuartos del radio y en el centro. O1 se austeniz\u00f3 a 815 \u00b0C (fuente A) y 775 \u00b0C (fuente B), O2 a 790 \u00b0C. Los datos del centro para O2 y los datos de la superficie para O7 no est\u00e1n disponibles en la fuente. Reproducido de la figura de la fuente.<\/figcaption><\/figure>\n\n\n\n<p class=\"wp-block-paragraph\">Aobo Steel suministra O1 en barra redonda recocida esferoidizada de 20 mm a 600 mm de di\u00e1metro y barra plana de 20 mm a 400 mm de espesor, cortada a la secci\u00f3n que requiere el trabajo. Cuando una secci\u00f3n es demasiado grande para los grados de temple al aceite, D2 y DC53 se suministran como barra y bloque cortado con MTC EN 10204 3.1 y UT.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\"><a href=\"javascript:void(0);\">Enviar consulta<\/a><\/p>\n\n\n\n<h2 class=\"wp-block-heading\">El acero r\u00e1pido mantiene su dureza en toda la secci\u00f3n<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">Los aceros r\u00e1pidos son el caso opuesto. Los cuatro paneles siguientes grafican la dureza de superficie y de centro para barras de 25, 50 y 75 mm de M2, M3, T1 y T2. A 25 mm el centro de la barra est\u00e1 a unos 65 a 66 HRC, e incluso en una barra de 75 mm el centro sigue midiendo aproximadamente 62 a 65 HRC con la superficie a 62 a 64 HRC. La dispersi\u00f3n de superficie a centro a lo largo de 75 mm es de uno a tres puntos. Frente a los grados de temple en aceite anteriores, donde la misma secci\u00f3n puede costar veinte puntos o m\u00e1s en el centro, esa es toda la raz\u00f3n por la que una herramienta de forma grande o un cortador grande se fabrica en acero r\u00e1pido mientras que una matriz de corte peque\u00f1a no.<\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img decoding=\"async\" src=\"https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/10\/Aobo-Steel-Tool-Steel-Hardenability-fig-2-hss-bar-diameter.jpg\" alt=\"Surface and center hardness against bar diameter for M2, M3, T1 and T2 high speed steel\"\/><figcaption class=\"wp-element-caption\">Fig. 2. Dureza en la superficie y en el centro en funci\u00f3n del di\u00e1metro de la barra para cuatro aceros r\u00e1pidos: (a) M2, (b) M3, (c) T1, (d) T2. Las barras son redondas de 25, 50 y 75 mm; M2 y M3 se templaron en aceite desde 1205 y 1230 \u00b0C, T1 y T2 desde 1290 \u00b0C. Reproducido de la figura original.<\/figcaption><\/figure>\n\n\n\n<h2 class=\"wp-block-heading\">Profundidad hasta 60 HRC en un W1 con 1% de carbono<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">Los grados de temple en agua muestran el otro extremo de la escala. Esta gr\u00e1fica representa la profundidad a la que todav\u00eda se mide 60 HRC frente al di\u00e1metro de barra, para las variantes de temple superficial, medio y profundo del W1 con 1% de carbono. En una barra de 20 mm el grado de temple profundo alcanza 60 HRC hasta una profundidad de aproximadamente 4\/16 in (6 mm), el grado medio hasta unos 2,8\/16 in (4 mm) y el grado superficial hasta unos 1,5\/16 in (2 mm). Lleve la barra a 65 mm y los tres caen a aproximadamente 3, 2,5 y 1,2 dieciseisavos. Incluso el W1 de temple profundo, por lo tanto, no se templa m\u00e1s all\u00e1 de unos 5 mm en una barra de 65 mm a 60 HRC, que es exactamente por qu\u00e9 los grados de temple en agua necesitan un enfriamiento violento, por qu\u00e9 son los que se agrietan, y por qu\u00e9 las familias de temple en aceite y temple al aire los reemplazaron para cualquier cosa que no sea la secci\u00f3n m\u00e1s simple.<\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img decoding=\"async\" src=\"https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/10\/Aobo-Steel-Tool-Steel-Hardenability-fig-5-w1-depth-60-hrc-crop.jpg\" alt=\"Depth to 60 HRC against bar diameter for shallow, medium and deep hardening W1 tool steel\"\/><figcaption class=\"wp-element-caption\">Fig. 5. Di\u00e1metro de la barra frente a la profundidad a la que todav\u00eda se alcanzan 60 HRC, para los grados de temple superficial, medio y profundo del acero para herramientas W1 con 1% C. La profundidad est\u00e1 en dieciseisavos de pulgada. Reproducido de la figura de la fuente.<\/figcaption><\/figure>\n\n\n\n<h2 class=\"wp-block-heading\">Qu\u00e9 hacer con las gr\u00e1ficas al hacer un pedido<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">Lea la curva de centro de su grado en el di\u00e1metro que est\u00e1 comprando. Si esa lectura est\u00e1 por debajo de la dureza que necesita la herramienta, las opciones son, en orden: comprar una secci\u00f3n m\u00e1s peque\u00f1a, pasar a un grado m\u00e1s templable del mismo grupo, o subir a la familia de temple al aire. Por encima de unos 100 mm, los grados de temple al aire son la respuesta pr\u00e1ctica para una matriz de trabajo en fr\u00edo, y los grados de trabajo en caliente y de acero r\u00e1pido son la respuesta donde la herramienta tambi\u00e9n debe trabajar en caliente y no solo templarse en toda la secci\u00f3n. Cada cifra de esta p\u00e1gina es dureza tal como se templa. La dureza a la que trabaja la herramienta proviene del ciclo de revenido, que es donde el <a href=\"https:\/\/aobosteel.com\/es\/tool-steel-tempering-chart\/\">Tabla de revenido del acero para herramientas<\/a> toma el relevo, y la dureza que la herramienta conserva una vez que est\u00e1 caliente est\u00e1 en el <a href=\"https:\/\/aobosteel.com\/es\/tool-steel-hot-hardness-chart\/\">tabla de dureza en caliente del acero para herramientas<\/a>. Los medios de temple que necesitan los grados anteriores, y las velocidades de enfriamiento que ofrecen, se comparan en el <a href=\"https:\/\/aobosteel.com\/es\/quenching-chart-water-oil-air-hardening\/\">Tabla de temple para aceros de temple en agua, aceite y aire<\/a>, y el l\u00edmite de tama\u00f1o de secci\u00f3n que aplica cuando una pieza se austemperiza en lugar de templarse est\u00e1 en la <a href=\"https:\/\/aobosteel.com\/es\/austempering-section-size-bainite-hardness-chart\/\">gr\u00e1fica de tama\u00f1o de secci\u00f3n para austempering<\/a>. Cuando el mismo acero se suministra en un bloque grande, el <a href=\"https:\/\/aobosteel.com\/es\/d2-tool-steel\/\">D2 de temple al aire<\/a> y sus similares son la especificaci\u00f3n habitual.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">Fuente: ASM Handbook, Vol 1, Properties and Selection: Irons, Steels and High-Performance Alloys.<\/p>\n\n\n\n<div class=\"wp-block-group has-background is-layout-constrained wp-container-core-group-is-layout-7da068b4 wp-block-group-is-layout-constrained\" style=\"border-radius:10px;background-color:#e6f0ff;margin-bottom:0;padding-top:20px;padding-right:24px;padding-bottom:20px;padding-left:24px\">\n<h2 class=\"wp-block-heading\">\u00bfNecesita acero para herramientas dimensionado a su secci\u00f3n?<\/h2>\n\n<p class=\"wp-block-paragraph\">Env\u00ede el grado, el tama\u00f1o de secci\u00f3n y la cantidad que necesita. Aobo Steel suministra O1, D2 y DC53 en barra redonda y barra plana recocidas, pedido m\u00ednimo 5 toneladas.<\/p>\n\n<div class=\"wp-block-buttons is-layout-flex wp-block-buttons-is-layout-flex\">\n<div class=\"wp-block-button popmake-16052\"><a class=\"wp-block-button__link wp-element-button\">Enviar consulta<\/a><\/div>\n\n<\/div>\n<\/div>","protected":false},"excerpt":{"rendered":"<p>Tool Steel Hardenability and Section Size Hardenability decides how thick a section of a given tool steel actually hardens, and it is the first number a shop needs before it orders bar stock. A grade that hardens to 65 HRC at the surface of a 100 mm block may still be soft in the middle [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":0,"parent":0,"menu_order":0,"comment_status":"closed","ping_status":"closed","template":"","meta":{"_uag_custom_page_level_css":"","site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"normal-width-container","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"disabled","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","ast-disable-related-posts":"","theme-transparent-header-meta":"","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"default","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"footnotes":""},"class_list":["post-20772","page","type-page","status-publish","hentry"],"yoast_head":"<!-- This site is optimized with the Yoast SEO Premium plugin v28.9 (Yoast SEO v28.9) - https:\/\/yoast.com\/product\/yoast-seo-premium-wordpress\/ -->\n<title>Tool Steel Hardenability and Section Size Charts<\/title>\n<meta name=\"description\" content=\"Hardenability and section size for tool steel: end-quench bands for the O grades, as-quenched hardness against bar diameter for O1, O2, O6 and O7, and depth to 60 HRC in W1.\" \/>\n<meta name=\"robots\" content=\"index, follow, max-snippet:-1, max-image-preview:large, max-video-preview:-1\" \/>\n<link rel=\"canonical\" href=\"https:\/\/aobosteel.com\/es\/tool-steel-hardenability-and-section-size\/\" \/>\n<meta property=\"og:locale\" content=\"es_ES\" \/>\n<meta property=\"og:type\" content=\"article\" \/>\n<meta property=\"og:title\" content=\"Tool Steel Hardenability and Section Size\" \/>\n<meta property=\"og:description\" content=\"Hardenability and section size for tool steel: end-quench bands for the O grades, as-quenched hardness against bar diameter for O1, O2, O6 and O7, and depth to 60 HRC in W1.\" \/>\n<meta property=\"og:url\" content=\"https:\/\/aobosteel.com\/es\/tool-steel-hardenability-and-section-size\/\" \/>\n<meta property=\"og:site_name\" content=\"AoboSteel\" \/>\n<meta property=\"article:publisher\" content=\"https:\/\/www.facebook.com\/profile.php?id=61565368220197\" \/>\n<meta property=\"article:modified_time\" content=\"2026-10-16T00:17:10+00:00\" \/>\n<meta property=\"og:image\" content=\"https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/10\/Aobo-Steel-Tool-Steel-Hardenability-fig-3-end-quench-bands-O-crop.jpg\" \/>\n<meta name=\"twitter:card\" content=\"summary_large_image\" \/>\n<meta name=\"twitter:label1\" content=\"Tiempo de lectura\" \/>\n\t<meta name=\"twitter:data1\" content=\"8 minutos\" \/>\n<script type=\"application\/ld+json\" class=\"yoast-schema-graph\">{\"@context\":\"https:\\\/\\\/schema.org\",\"@graph\":[{\"@type\":\"TechArticle\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/tool-steel-hardenability-and-section-size\\\/#article\",\"isPartOf\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/tool-steel-hardenability-and-section-size\\\/\"},\"author\":{\"name\":\"Evan\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#\\\/schema\\\/person\\\/96118415c30ca6bb52eaf1127b052ef7\"},\"headline\":\"Tool Steel Hardenability and Section Size\",\"datePublished\":\"2026-10-03T07:04:40+00:00\",\"dateModified\":\"2026-10-16T00:17:10+00:00\",\"mainEntityOfPage\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/tool-steel-hardenability-and-section-size\\\/\"},\"wordCount\":1547,\"publisher\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#organization\"},\"image\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/tool-steel-hardenability-and-section-size\\\/#primaryimage\"},\"thumbnailUrl\":\"https:\\\/\\\/aobosteel.com\\\/wp-content\\\/uploads\\\/2026\\\/10\\\/Aobo-Steel-Tool-Steel-Hardenability-fig-3-end-quench-bands-O-crop.jpg\",\"inLanguage\":\"es\"},{\"@type\":\"WebPage\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/tool-steel-hardenability-and-section-size\\\/\",\"url\":\"https:\\\/\\\/aobosteel.com\\\/tool-steel-hardenability-and-section-size\\\/\",\"name\":\"Tool Steel Hardenability and Section Size Charts\",\"isPartOf\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#website\"},\"primaryImageOfPage\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/tool-steel-hardenability-and-section-size\\\/#primaryimage\"},\"image\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/tool-steel-hardenability-and-section-size\\\/#primaryimage\"},\"thumbnailUrl\":\"https:\\\/\\\/aobosteel.com\\\/wp-content\\\/uploads\\\/2026\\\/10\\\/Aobo-Steel-Tool-Steel-Hardenability-fig-3-end-quench-bands-O-crop.jpg\",\"datePublished\":\"2026-10-03T07:04:40+00:00\",\"dateModified\":\"2026-10-16T00:17:10+00:00\",\"description\":\"Hardenability and section size for tool steel: end-quench bands for the O grades, as-quenched hardness against bar diameter for O1, O2, O6 and O7, and depth to 60 HRC in W1.\",\"breadcrumb\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/tool-steel-hardenability-and-section-size\\\/#breadcrumb\"},\"inLanguage\":\"es\",\"potentialAction\":[{\"@type\":\"ReadAction\",\"target\":[\"https:\\\/\\\/aobosteel.com\\\/tool-steel-hardenability-and-section-size\\\/\"]}]},{\"@type\":\"ImageObject\",\"inLanguage\":\"es\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/tool-steel-hardenability-and-section-size\\\/#primaryimage\",\"url\":\"https:\\\/\\\/aobosteel.com\\\/wp-content\\\/uploads\\\/2026\\\/10\\\/Aobo-Steel-Tool-Steel-Hardenability-fig-3-end-quench-bands-O-crop.jpg\",\"contentUrl\":\"https:\\\/\\\/aobosteel.com\\\/wp-content\\\/uploads\\\/2026\\\/10\\\/Aobo-Steel-Tool-Steel-Hardenability-fig-3-end-quench-bands-O-crop.jpg\"},{\"@type\":\"BreadcrumbList\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/tool-steel-hardenability-and-section-size\\\/#breadcrumb\",\"itemListElement\":[{\"@type\":\"ListItem\",\"position\":1,\"name\":\"\u9996\u9875\",\"item\":\"https:\\\/\\\/aobosteel.com\\\/\"},{\"@type\":\"ListItem\",\"position\":2,\"name\":\"Tool Steel Hardenability and Section Size\"}]},{\"@type\":\"WebSite\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#website\",\"url\":\"https:\\\/\\\/aobosteel.com\\\/\",\"name\":\"AoboSteel\",\"description\":\"\",\"publisher\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#organization\"},\"potentialAction\":[{\"@type\":\"SearchAction\",\"target\":{\"@type\":\"EntryPoint\",\"urlTemplate\":\"https:\\\/\\\/aobosteel.com\\\/?s={search_term_string}\"},\"query-input\":{\"@type\":\"PropertyValueSpecification\",\"valueRequired\":true,\"valueName\":\"search_term_string\"}}],\"inLanguage\":\"es\"},{\"@type\":\"Organization\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#organization\",\"name\":\"AoboSteel\",\"url\":\"https:\\\/\\\/aobosteel.com\\\/\",\"logo\":{\"@type\":\"ImageObject\",\"inLanguage\":\"es\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#\\\/schema\\\/logo\\\/image\\\/\",\"url\":\"https:\\\/\\\/aobosteel.com\\\/wp-content\\\/uploads\\\/2025\\\/01\\\/cropped-aobo-steel-1.avif\",\"contentUrl\":\"https:\\\/\\\/aobosteel.com\\\/wp-content\\\/uploads\\\/2025\\\/01\\\/cropped-aobo-steel-1.avif\",\"width\":1052,\"height\":592,\"caption\":\"AoboSteel\"},\"image\":{\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#\\\/schema\\\/logo\\\/image\\\/\"},\"sameAs\":[\"https:\\\/\\\/www.facebook.com\\\/profile.php?id=61565368220197\",\"https:\\\/\\\/www.linkedin.com\\\/in\\\/aobosteel-evan\\\/\"]},{\"@type\":\"Person\",\"@id\":\"https:\\\/\\\/aobosteel.com\\\/#\\\/schema\\\/person\\\/96118415c30ca6bb52eaf1127b052ef7\",\"name\":\"Evan\",\"image\":{\"@type\":\"ImageObject\",\"inLanguage\":\"es\",\"@id\":\"https:\\\/\\\/secure.gravatar.com\\\/avatar\\\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g\",\"url\":\"https:\\\/\\\/secure.gravatar.com\\\/avatar\\\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g\",\"contentUrl\":\"https:\\\/\\\/secure.gravatar.com\\\/avatar\\\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g\",\"caption\":\"Evan\"},\"sameAs\":[\"http:\\\/\\\/www.aobosteel.com\",\"https:\\\/\\\/www.facebook.com\\\/profile.php?id=61565368220197\",\"https:\\\/\\\/www.instagram.com\\\/aobosteel\\\/\",\"https:\\\/\\\/www.linkedin.com\\\/in\\\/aobosteel-evan\\\/\",\"https:\\\/\\\/x.com\\\/AobosteelEvan\",\"https:\\\/\\\/www.youtube.com\\\/@aobosteel\"],\"url\":\"https:\\\/\\\/aobosteel.com\\\/es\\\/blog\\\/author\\\/admin\\\/\"}]}<\/script>\n<!-- \/ Yoast SEO Premium plugin. -->","yoast_head_json":{"title":"Templabilidad del acero para herramientas y tablas de tama\u00f1o de secci\u00f3n","description":"Templabilidad y tama\u00f1o de secci\u00f3n del acero para herramientas: bandas de temple por extremo para los grados O, dureza tras temple frente al di\u00e1metro de barra para O1, O2, O6 y O7, y profundidad hasta 60 HRC en W1.","robots":{"index":"index","follow":"follow","max-snippet":"max-snippet:-1","max-image-preview":"max-image-preview:large","max-video-preview":"max-video-preview:-1"},"canonical":"https:\/\/aobosteel.com\/es\/tool-steel-hardenability-and-section-size\/","og_locale":"es_ES","og_type":"article","og_title":"Tool Steel Hardenability and Section Size","og_description":"Hardenability and section size for tool steel: end-quench bands for the O grades, as-quenched hardness against bar diameter for O1, O2, O6 and O7, and depth to 60 HRC in W1.","og_url":"https:\/\/aobosteel.com\/es\/tool-steel-hardenability-and-section-size\/","og_site_name":"AoboSteel","article_publisher":"https:\/\/www.facebook.com\/profile.php?id=61565368220197","article_modified_time":"2026-10-16T00:17:10+00:00","og_image":[{"url":"https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/10\/Aobo-Steel-Tool-Steel-Hardenability-fig-3-end-quench-bands-O-crop.jpg","type":"","width":"","height":""}],"twitter_card":"summary_large_image","twitter_misc":{"Tiempo de lectura":"8 minutos"},"schema":{"@context":"https:\/\/schema.org","@graph":[{"@type":"TechArticle","@id":"https:\/\/aobosteel.com\/tool-steel-hardenability-and-section-size\/#article","isPartOf":{"@id":"https:\/\/aobosteel.com\/tool-steel-hardenability-and-section-size\/"},"author":{"name":"Evan","@id":"https:\/\/aobosteel.com\/#\/schema\/person\/96118415c30ca6bb52eaf1127b052ef7"},"headline":"Tool Steel Hardenability and Section Size","datePublished":"2026-10-03T07:04:40+00:00","dateModified":"2026-10-16T00:17:10+00:00","mainEntityOfPage":{"@id":"https:\/\/aobosteel.com\/tool-steel-hardenability-and-section-size\/"},"wordCount":1547,"publisher":{"@id":"https:\/\/aobosteel.com\/#organization"},"image":{"@id":"https:\/\/aobosteel.com\/tool-steel-hardenability-and-section-size\/#primaryimage"},"thumbnailUrl":"https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/10\/Aobo-Steel-Tool-Steel-Hardenability-fig-3-end-quench-bands-O-crop.jpg","inLanguage":"es"},{"@type":"WebPage","@id":"https:\/\/aobosteel.com\/tool-steel-hardenability-and-section-size\/","url":"https:\/\/aobosteel.com\/tool-steel-hardenability-and-section-size\/","name":"Templabilidad del acero para herramientas y tablas de tama\u00f1o de secci\u00f3n","isPartOf":{"@id":"https:\/\/aobosteel.com\/#website"},"primaryImageOfPage":{"@id":"https:\/\/aobosteel.com\/tool-steel-hardenability-and-section-size\/#primaryimage"},"image":{"@id":"https:\/\/aobosteel.com\/tool-steel-hardenability-and-section-size\/#primaryimage"},"thumbnailUrl":"https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/10\/Aobo-Steel-Tool-Steel-Hardenability-fig-3-end-quench-bands-O-crop.jpg","datePublished":"2026-10-03T07:04:40+00:00","dateModified":"2026-10-16T00:17:10+00:00","description":"Templabilidad y tama\u00f1o de secci\u00f3n del acero para herramientas: bandas de temple por extremo para los grados O, dureza tras temple frente al di\u00e1metro de barra para O1, O2, O6 y O7, y profundidad hasta 60 HRC en W1.","breadcrumb":{"@id":"https:\/\/aobosteel.com\/tool-steel-hardenability-and-section-size\/#breadcrumb"},"inLanguage":"es","potentialAction":[{"@type":"ReadAction","target":["https:\/\/aobosteel.com\/tool-steel-hardenability-and-section-size\/"]}]},{"@type":"ImageObject","inLanguage":"es","@id":"https:\/\/aobosteel.com\/tool-steel-hardenability-and-section-size\/#primaryimage","url":"https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/10\/Aobo-Steel-Tool-Steel-Hardenability-fig-3-end-quench-bands-O-crop.jpg","contentUrl":"https:\/\/aobosteel.com\/wp-content\/uploads\/2026\/10\/Aobo-Steel-Tool-Steel-Hardenability-fig-3-end-quench-bands-O-crop.jpg"},{"@type":"BreadcrumbList","@id":"https:\/\/aobosteel.com\/tool-steel-hardenability-and-section-size\/#breadcrumb","itemListElement":[{"@type":"ListItem","position":1,"name":"\u9996\u9875","item":"https:\/\/aobosteel.com\/"},{"@type":"ListItem","position":2,"name":"Tool Steel Hardenability and Section Size"}]},{"@type":"WebSite","@id":"https:\/\/aobosteel.com\/#website","url":"https:\/\/aobosteel.com\/","name":"AoboSteel","description":"","publisher":{"@id":"https:\/\/aobosteel.com\/#organization"},"potentialAction":[{"@type":"SearchAction","target":{"@type":"EntryPoint","urlTemplate":"https:\/\/aobosteel.com\/?s={search_term_string}"},"query-input":{"@type":"PropertyValueSpecification","valueRequired":true,"valueName":"search_term_string"}}],"inLanguage":"es"},{"@type":"Organization","@id":"https:\/\/aobosteel.com\/#organization","name":"AoboSteel","url":"https:\/\/aobosteel.com\/","logo":{"@type":"ImageObject","inLanguage":"es","@id":"https:\/\/aobosteel.com\/#\/schema\/logo\/image\/","url":"https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/01\/cropped-aobo-steel-1.avif","contentUrl":"https:\/\/aobosteel.com\/wp-content\/uploads\/2025\/01\/cropped-aobo-steel-1.avif","width":1052,"height":592,"caption":"AoboSteel"},"image":{"@id":"https:\/\/aobosteel.com\/#\/schema\/logo\/image\/"},"sameAs":["https:\/\/www.facebook.com\/profile.php?id=61565368220197","https:\/\/www.linkedin.com\/in\/aobosteel-evan\/"]},{"@type":"Person","@id":"https:\/\/aobosteel.com\/#\/schema\/person\/96118415c30ca6bb52eaf1127b052ef7","name":"Evan","image":{"@type":"ImageObject","inLanguage":"es","@id":"https:\/\/secure.gravatar.com\/avatar\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g","url":"https:\/\/secure.gravatar.com\/avatar\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g","contentUrl":"https:\/\/secure.gravatar.com\/avatar\/8e402f2e6f36093f0bf1855dbf79269cde23cd659c44eefdd7ecf7ff9c05786f?s=96&d=mm&r=g","caption":"Evan"},"sameAs":["http:\/\/www.aobosteel.com","https:\/\/www.facebook.com\/profile.php?id=61565368220197","https:\/\/www.instagram.com\/aobosteel\/","https:\/\/www.linkedin.com\/in\/aobosteel-evan\/","https:\/\/x.com\/AobosteelEvan","https:\/\/www.youtube.com\/@aobosteel"],"url":"https:\/\/aobosteel.com\/es\/blog\/author\/admin\/"}]}},"uagb_featured_image_src":{"full":false,"thumbnail":false,"medium":false,"medium_large":false,"large":false,"1536x1536":false,"2048x2048":false,"trp-custom-language-flag":false},"uagb_author_info":{"display_name":"Evan","author_link":"https:\/\/aobosteel.com\/es\/blog\/author\/admin\/"},"uagb_comment_info":0,"uagb_excerpt":"Tool Steel Hardenability and Section Size Hardenability decides how thick a section of a given tool steel actually hardens, and it is the first number a shop needs before it orders bar stock. A grade that hardens to 65 HRC at the surface of a 100 mm block may still be soft in the middle&hellip;","rttpg_featured_image_url":null,"rttpg_author":{"display_name":"Evan","author_link":"https:\/\/aobosteel.com\/es\/blog\/author\/admin\/"},"rttpg_comment":0,"rttpg_category":null,"rttpg_excerpt":"Tool Steel Hardenability and Section Size Hardenability decides how thick a section of a given tool steel actually hardens, and it is the first number a shop needs before it orders bar stock. A grade that hardens to 65 HRC at the surface of a 100 mm block may still be soft in the middle&hellip;","_links":{"self":[{"href":"https:\/\/aobosteel.com\/es\/wp-json\/wp\/v2\/pages\/20772","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/aobosteel.com\/es\/wp-json\/wp\/v2\/pages"}],"about":[{"href":"https:\/\/aobosteel.com\/es\/wp-json\/wp\/v2\/types\/page"}],"author":[{"embeddable":true,"href":"https:\/\/aobosteel.com\/es\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/aobosteel.com\/es\/wp-json\/wp\/v2\/comments?post=20772"}],"version-history":[{"count":17,"href":"https:\/\/aobosteel.com\/es\/wp-json\/wp\/v2\/pages\/20772\/revisions"}],"predecessor-version":[{"id":22986,"href":"https:\/\/aobosteel.com\/es\/wp-json\/wp\/v2\/pages\/20772\/revisions\/22986"}],"wp:attachment":[{"href":"https:\/\/aobosteel.com\/es\/wp-json\/wp\/v2\/media?parent=20772"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}