42CrMo4 steel is a widely used medium-carbon low-alloy steel, often considered a standard against which other ultrahigh-strength steels are compared. It is known for its deep hardenability, high strength, and good toughness.
1. Ocel 42CrMo4 Složení1
| C | Si | Mn | P | S | Cr | Mo | Ni | PROTI |
| 0.38-0.45 | 0.17-0.37 | 0.50-0.80 | ≤0,035 | ≤0,035 | 0.90-1.20 | 0.15-0.25 | ≤0.30 | ≤0.06 |
2. 42CrMo4 Steel Equivalent Grades
- EN: 42CrMo4 (č. materiálu: 1.7225)
- ISO: 42CrMo4
- ASTM/AISI (USA): 4140 (G41400) a 4142 (G41420)
- JIS (Japonsko): SCM440 / SCM445
- GOST (Rusko): 38XM
- DIN (Německo): 42CrMo4
- BS (UK): 42CrMo4 / 708M40
- NF (Francie): 42CrMo4
- GB/T (Čína): 42CrMo (A30422) / 42CrMoH (A30425)
3. Tepelné zpracování z oceli 42CrMo4
42CrMo4 steel is a heat-treatable material, and its properties are highly dependent on the specific heat treatment process. It can be supplied in a pre-hardened state.
- 42CrMo4 QT (Quenching & Tempering). The standard quenching and tempering process includes heating to 850-870°C, oil quenching, and then tempering at 500-600°C for 2 hours to obtain a hardness of 28-35 HRC.
- Annealing. Hold at 830-850°C for 3-4 hours, then cool in the furnace to 500°C, followed by air cooling, resulting in a final hardness of ≤217 HBW. For softening annealing, heating to 740-800°C, cooling in the furnace at 15°C/h to 550°C, then air cooling.
- Normalizing. Hold at 870-880°C for 1-2 hours, then cool naturally, resulting in a final hardness of ≤255 HBW.
- High-temperature tempering. Temper at 680-700°C for 2-3 hours, then cool in the furnace to 500°C, followed by air cooling, resulting in a final hardness of ≤217 HBW.
- Stress Relief Treatment. After rough machining, it is recommended to heat to 530°C, hold for 2 hours, and then cool in air.

Please fill out the following contact form to get the best quotation for 42CrMo4 Steel!
4. Mechanické vlastnosti
V kaleném a temperovaném stavu (Q+T) poskytuje 42CrMo4 vynikající mechanický výkon. Typické hodnoty po kalení oleje (850 °C) a popouštění (580 °C) mohou zahrnovat:
- Pevnost v tahu (Rm): ≥ 1100 MPa
- Mez kluzu (ReL): ≥ 950 MPa
- Prodloužení (A): ≥ 12%
- Rázová houževnatost (KV/KU nebo aK): Hodnoty závisí na zkušební metodě, ale charakteristická je dobrá houževnatost (např. ≥ 80 J/cm²).
Pamatujte, že konečné vlastnosti přímo závisí na konkrétních použitých parametrech tepelného zpracování.
5. Applications
- Stavba strojů: Vysoce namáhané díly jako ozubená kola, hřídele, nápravy, ojnice, klikové hřídele a vysokopevnostní šrouby.
- Nástroje: Large and medium-sized plastic molds, mold frames, forging dies (depending on application demands), and cold heading dies.
- Ostatní: Velkoobjemové plynové lahve a součásti vyžadující vysokou únavovou pevnost.
- Mezinárodní ASM. (1991). ASM Handbook, Volume 4: Heat Treating (p. 700)ASM International. ↩︎
FAQ
AISI/SAE 4140 (USA).
UNS G41400 (USA).
JIS SCM440 or SCM440H (Japan).
BS 708M40 or 709M40 (UK). It also has a BS 970 equivalent of 708A42 (En19C).
AFNOR 42CD4 (France).
ISO 42CrMo4.
42CrMo4 is a medium-carbon alloy steel, specifically a chromium-molybdenum (Cr-Mo) steel. It is known as a heat-treatable steel, meaning its mechanical properties can be enhanced through processes like quenching and tempering. It typically has good overall mechanical properties, including strength and toughness.
Yes, 42CrMo4 has been listed with a British Standard (BS) equivalent of 970 708A42 (En19C), suggesting it is equivalent or a very close match to EN19.
Yes, 42CrMo4 (DIN designation) is widely considered equivalent to AISI/SAE 4140 steel (USA). Their chemical compositions are very similar, particularly in carbon, chromium, and molybdenum content.
No, 42CrMo4 is not classified as mild steel. Mild steels are typically low-carbon steels (1xxx series). 42CrMo4 is a medium-carbon alloy steel, with a carbon content typically ranging from 0.38% to 0.45%. Medium-carbon steels are distinct from low-carbon (mild) steels due to their higher carbon content and ability to be heat-treated for strength.
DIN 42CrMo4 (Germany).
JIS SCM440 or SCM440H (Japan).
ISO 42CrMo4.
BS 708M40 or 709M40 (UK), and 708A42 (En19C).
Yes, 42CrMo4 can rust. It is an alloy steel, not a stainless steel. While it contains chromium (0.90-1.20%), this amount is generally not sufficient to make it “stainless” (which typically requires a minimum of 11.5-13% chromium to be classified as stainless). Therefore, it will corrode, or rust, in certain environments.
4140 steel is generally considered the higher-strength option compared to 4130 steel. This is due to its slightly higher carbon content (4140: 0.38-0.43% C vs. 4130: 0.28-0.33% C) and often higher manganese content.
4140 is a type of steel, which is an alloy primarily composed of iron with carbon and other alloying elements like chromium and molybdenum. Aluminum, on the other hand, is a non-ferrous metal that is significantly lighter than steel. They are fundamentally different materials with distinct properties and applications.
Get a Competitive Quote for 42CrMo4 Steel
With over 20 years of forging expertise, Aobo Steel is your trusted partner for high-performance 42CrMo4 steel. We provide not just materials, but solutions. Leverage our deep industry knowledge and reliable supply chain for your project’s success.
✉ Kontaktujte nás vyplněním níže uvedeného formuláře.
Prozkoumejte naše další produkty
D2/1.2379/SKD11
D3/1.2080/SKD1
D6/1,2436/SKD2
A2/1.23663/SKD12
O1/1.2510/SKS3
O2/1,2842
S1/1,2550
S7/1,2355
DC53
H13/1.2344/SKD61
H11/1.2343/SKD6
H21/1,2581/SKD7
L6/1.2714/SKT4
M2/1.3343/SKH51
M35/1.3243/SKH55
M42/1.3247/SKH59
P20/1,2311
P20+Ni/1,2738
420/1.2083/2Cr13
422 z nerezové oceli
Ložisková ocel 52100
Nerezová ocel 440C
4140/42CrMo4/SCM440
4340/34CrNiMo6/1,6582
4130
5140/42Cr4/SCR440
SCM415