Understanding Air-Hardening Tool Steel (like H13)

Air-hardening steel is a critically important category of tool steel in materials engineering. Its widespread application stems from its minimal distortion during heat treatment, excellent deep hardenability, and superior mechanical properties. Air-hardening steels, such as the A and H series, rely on air-cooling—a relatively mild method—to achieve a hard martensitic structure. This stands in stark […]

Understanding Air-Hardening Tool Steel (like H13) Číst více »